CHARACTERIZATION OF DEFECTS IN ALLOY 152, 52 AND 52M WELDS

Defect distributions have been documented by optical metallography, scanning electron microscopy and electron backscatter diffraction in alloy 152 and 52 mockups welds, alloy 52 and 52M overlay mockups and an alloy 52M inlay. Primary defects were small cracks at grain boundaries except for more extensive cracking in the dilution zone of an alloy 52 overlay on 304SS. Detailed characterizations of the dilution zone cracks were performed by analytical transmission electron microscopy identifying grain boundary titanium-nitride precipitation associated with the intergranular separations. I. INTRODUCTION Weldments continue to be a primary location of stress-corrosion cracking (SCC) in light-water reactor systems. While problems related to heat-affected-zone (HAZ) sensitization and intergranular (IG) SCC of austenitic stainless alloys in boiling-water reactors (BWRs) have been significantly reduced, SCC has now been observed in HAZs of non-sensitized materials and in dissimilar metal welds where Ni-base alloy weld metals are used. IGSCC in weld metals has been observed in both BWRs and pressurized water reactors (PWRs) with recent examples for PWR pressure vessel penetrations producing the most concern. This has led to the replacement of alloy 600/182/82 welds with higher Cr, more corrosion-resistant replacement materials (alloy 690/152/52/52M). Complicating this issue has been a known susceptibility to cracking during welding [1-7] of these weld metals. There is a critical need for an improved understanding of the weld metal metallurgy and defect formation in Ni-base alloy welds to effectively assess long-term performance. A series of macroscopic to microscopic examinations were performed on available mockup welds made with alloy 52 or alloy 152 plus selected overlay and inlay mockups. The intent was to expand our understanding of weld metal structures in simulated LWR service components with a focus on as-welded defects. Microstructural features, defect distributions, defect characteristics and weld residual strains were examined by optical metallography, scanning electron microscopy, electron backscatter diffraction and transmission electron microscopy. Industry-supplied mock-up welds were characterized including alloy 52 and 152 weldments, alloy 52M overlay and inlay welds, and an alloy 52 overlay. II. WELDMENTS II.A. Alloy 52 and 152 Weld Mockups The alloy 52 and 152 weld mockups were fabricated by MHI for the Kewaunee reactor and were obtained from the EPRI NDE Center. The mockups were U-groove welds joining two plates of 304SS as shown in Figure 1. Alloy 152 butter (heat 307380) was placed on the U-groove surface for both mockups by shielded metal arc welding (SMAW). For the alloy 152 weld mockup, the alloy 152 fill (heat 307380) was also applied using SMAW while for the alloy 52 weld mockup, the alloy 52 fill (heat NX2686JK) was applied using gas tungsten arc welding (GTAW). Welding parameters for the fill materials were substantially different with the alloy 152 SMAW having a deposition speed of 4-25 cm/min with a current of 95-145 A and the alloy 52 GTAW having a deposition speed of 4-10 cm/min with a current of 150-300 A. One prominent feature in these mockup welds is the presence of a crack starting at the 304SS butt joint at the bottom of the U-groove and extending up into the weld. It appears that the 304SS plate on either side of the butt joint acted as an anchor for the weld resulting in a stress rise across the slit that drove crack formation and extension up into the fill weld. As will be shown in the next section, the extent of the cracking around this stress riser was much greater in the MHI 52 weld mockup.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Evaluation of salt particle collection device for preventing SCC on canister - Effect on particle collection rate by electric field

Now, in Japan, while metal casks are used for spent nuclear fuel storage, a practical use of concrete casks is under review because of its cost effectiveness and procurement easiness. In reviewing the practical use, stress corrosion cracking (SCC) of a canister container in the concrete cask becomes an issue and is needed to be resolved soon. A natural ventilation system is generally adopted for the storage facilities, especially in Japan where facilities are built near coasts so that the cooling air includes sea salt particles. Therefore, the occurrence of SCC is concerned when the sea salt particles adhere to welded parts of the canisters. In this study, we proposed a salt particle collection device with low pressure loss which does not interfere with the air flow into the building or the concrete casks. The device is composed of a stack of 10 parallel stainless steel plates, the air is free to circulate in the space between them. Pressure loss tests in a laboratory and salt particle collection tests in the field have been performed. It has been clarified that the pressure loss of the device is one-thirtieth to one-twentieth of that of a commercial filter and 40% of the particles in the air could be collected and the device would not influence the heat removal performance. Moreover, we evaluated the effect of electric field on the particle collection under supposing the particle charge. In the case of electric field over 10{sup 3} kV/m the particle collection rate could be improved dramatically.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Assessment of the mechanical performance of the Westinghouse BWR control rod CR 99 at high depletion levels

A long-term program assessing the mechanical performance of the Westinghouse BWR control rod CR 99 at high depletion levels has been performed. The scope of the program has mainly been based on the operation of four CR 99 Generation 2 control rods in demanding positions during 6 and 7 cycles in the Leibstadt Nuclear Power Plant (KKL) and on the detailed visual inspections and blade wing thickness measurements that were performed after the rods were discharged. By correlating statistically the blade wing thickness measurements to the appearance of irradiation-assisted stress corrosion cracking (IASCC), the probability of IASCC appearance as function of the blade wing swelling was estimated. In order to correlate the IASCC probability of a CR 99 to its depletion, the {sup 10}B depletion of the studied rods was calculated in detail on a local level with the stochastic Monte Carlo code MCNP in combination with the Westinghouse nodal code system PHOENIX4/POLCA7. Using this information coupled to the blade wing measurement data, a finite element model describing the blade wing swelling of an arbitrary CR 99 design as function of {sup 10}B depletion could then be generated. In the final step, these relationships were used to quantify the probability of IASCC appearance as function of the {sup 10}B depletion of the CR 99 Generations 2 and 3. Applying this detailed mapping of the CR 99 behavior at high depletion levels and using an on-line core monitoring system with explicit {sup 10}B depletion tracking capabilities will enable a reliable prediction of the probability for IASCC appearance, thus enhancing the optimized design and the sound operation of the CR 99 control rod. Another important outcome of the program was that it was clearly shown that no significant amount of boron leakage did occur through any of the detected IASCC cracks, despite the very high depletion levels achieved. (authors)

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Advanced Instrumentation, Information, and Control System Technologies: Nondestructive Examination Technologies - FY11 Report

Licensees of commercial nuclear power plants in the US are expected to submit license renewal applications for the period of operation of 60 to 80 years which has also been referred to as long term operation (LTO). The greatest challenges to LTO are associated with degradation of passive components as active components are routinely maintained and repaired or placed through maintenance programs. Some passive component degradation concerns include stress corrosion cracking (SCC) of metal components, radiation induced embrittlement of the reactor pressure vessel (RPV), degradation of buried piping, degradation of concrete containment structures, and degradation of cables. Proactive management of passive component aging employs three important elements including online monitoring of degradation, early detection of degradation at precursor stages, and application of prognostics for the prediction of remaining useful life (RUL). This document assesses several nondestructive examination (NDE) measurement technologies for integration into proactive aging management programs. The assessment is performed by discussing the three elements of proactive aging management identified above, considering the current state of the industry with respect to adopting these key elements, and analyzing measurement technologies for monitoring large cracks in metal components, monitoring early degradation at precursor stages, monitoring the degradation of concrete containment structures, and monitoring the degradation of cables. Specific and general needs have been identified through this assessment. General needs identified include the need for environmentally rugged sensors are needed that can operate reliably in an operating reactor environment, the need to identify parameters from precursor monitoring technologies that are unambiguously correlated with the level of pre-macro defect damage, and a methodology for identifying regions where precursor damage is most likely to initiate.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Ultrasonic Phased Array Assessment of the Interference Fit and Leak Path of the North Anna Unit 2 Control Rod Drive Mechanism Nozzle 63 with Destructive Validation

The objective of this investigation was to evaluate the efficacy of ultrasonic testing (UT) for primary water leak path assessments of reactor pressure vessel (RPV) upper head penetrations. Operating reactors have experienced leakage when stress corrosion cracking of nickel-based alloy penetrations allowed primary water into the annulus of the interference fit between the penetration and the low-alloy steel RPV head. In this investigation, UT leak path data were acquired for an Alloy 600 control rod drive mechanism nozzle penetration, referred to as Nozzle 63, which was removed from the North Anna Unit 2 reactor when the RPV head was replaced in 2002. In-service inspection prior to the head replacement indicated that Nozzle 63 had a probable leakage path through the interference fit region. Nozzle 63 was examined using a phased-array UT probe with a 5.0-MHz, eight-element annular array. Immersion data were acquired from the nozzle inner diameter surface. The UT data were interpreted by comparing to responses measured on a mockup penetration with known features. Following acquisition of the UT data, Nozzle 63 was destructively examined to determine if the features identified in the UT examination, including leakage paths and crystalline boric acid deposits, could be visually confirmed. Additional measurements of boric acid deposit thickness and low-alloy steel wastage were made to assess how these factors affect the UT response. The implications of these findings for interpreting UT leak path data are described.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

NDE to Manage Atmospheric SCC in Canisters for Dry Storage of Spent Fuel: An Assessment

This report documents efforts to assess representative horizontal (Transuclear NUHOMS®) and vertical (Holtec HI-STORM) storage systems for the implementation of non-destructive examination (NDE) methods or techniques to manage atmospheric stress corrosion cracking (SCC) in canisters for dry storage of used nuclear fuel. The assessment is conducted by assessing accessibility and deployment, environmental compatibility, and applicability of NDE methods. A recommendation of this assessment is to focus on bulk ultrasonic and eddy current techniques for direct canister monitoring of atmospheric SCC. This assessment also highlights canister regions that may be most vulnerable to atmospheric SCC to guide the use of bulk ultrasonic and eddy current examinations. An assessment of accessibility also identifies canister regions that are easiest and more difficult to access through the ventilation paths of the concrete shielding modules. A conceivable sampling strategy for canister inspections is to sample only the easiest to access portions of vulnerable regions. There are aspects to performing an NDE inspection of dry canister storage system (DCSS) canisters for atmospheric SCC that have not been addressed in previous performance studies. These aspects provide the basis for recommendations of future efforts to determine the capability and performance of eddy current and bulk ultrasonic examinations for atmospheric SCC in DCSS canisters. Finally, other important areas of investigation are identified including the development of instrumented surveillance specimens to identify when conditions are conducive for atmospheric SCC, characterization of atmospheric SCC morphology, and an assessment of air flow patterns over canister surfaces and their influence on chloride deposition.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Crack-Free 30% Chromium-Nickel Alloy Welding Products for Nuclear Service

We report prior research in the development of 30% chromium-nickel alloy nuclear welding wires has resulted in the resolution of primary water stress corrosion cracking (PWSCC) and ductility dip cracking (DDC) as well as improvement in solidification cracking (SC) resistance. The resolution of DDC exhibits some Laves phase, which has a negative effect on SC resistance. In this study, the use of an alternate carbide former, tantalum (Ta), in combination with niobium (Nb) was researched. Three heats of recently designed Filler Metal 52MSS-Ta (i.e., HV1648, HV1673A, and VX131WXW) were melted, fabricated, and systematically studied. DDC and SC were evaluated with thermodynamic modeling using the Scheil solidification simulation model, two types of varestraint tests, and strain-to-fracture (STF) testing. The varestraint and STF test results showed an improved SC resistance with reduced Laves phase and concurrent excellent DDC resistance. Optimized compositions with low Laves phase also exhibited high threshold strain values (TSVs) in the STF test. VX131WXW — which contains 2.81 wt-% Ta, 0.6 wt-% Nb, and 6 wt-% iron (Fe) - exhibited a TSV of 24%. Thermo-Calc computed the Laves phase to be 0.24% for VX131WXW compared to 0.06% in HV1673A. This difference in Laves phase resulted in the lower SC resistance of VX131WXW compared to HV1673A when measured with longitudinal varestraint testing. The maximum crack distance for HV1673A was about 0.6 mm while that of heat VX131WXW was about 1.0 mm. The typical diluted weld deposit made with VX131WXW was also resistant to PWSCC due to the chromium content exceeding 24%. These simultaneous results mark progress toward crack-free welds and provide direction for further optimization of Ta-containing filler metals.

30% chromium-nickel alloy↗

Thermal Aging Degradation of Cast Stainless Steels in LWR Systems

Cast austenitic stainless steels (CASSs) have been extensively used for the large components of light water reactor (LWR) power plants such as primary coolant piping and pump casing. Since a large number of massive CASS components are installed in every modern nuclear power plant, any significant degradation of CASS components will raise serious concerns on the integrity of the entire power plant. Upon the presumption that the replacement cost of such massive components is prohibitive, therefore, thorough scientific understanding and systematic monitoring the thermal aging degradation of CASS components should be essential requirements for assessing the plant safety. In the past few decades many researches have concluded that the formation of Cr-rich α-phase by Spinoidal decomposition of δ-ferrite phase, which is formed in high temperature region during cooling, is the primary mechanism for the thermal embrittlement. Cracking mechanism in the thermally-embrittled duplex stainless steels consists of cleavage initiation at ferrite and crack propagation via separation of ferrite-austenite interphase. It has been known, however, that such thermal aging embrittlement is observed only in accelerated aging conditions and the cast stainless steel grades used in nuclear plants have performed well without experiencing real embrittlement. It has been speculated that long-term thermal aging for ≥ 60 years could lead to further decomposition of designed phases and increase of precipitation. This will result in significantly increased susceptibility to embrittlement or other degradation due to thermal aging-radiation synergistic effect, irradiation-induced degradation, stress-corrosion cracking, and general corrosion. Currently, therefore, the thermal embrittlement of CASS components is one of the most serious concerns for extended operation of nuclear power plants. A scientific research is underway to address the issues related to the thermal aging degradation of CASS components. The research aims to provide knowledge-based conclusive prediction for the integrity of the CASS components of LWR power plants during extended operation up to and beyond 60 years. This presentation intends to provide an introductory overview on the thermal aging phenomena in LWR relevant conditions and discussion on the measurements of mechanical property degradation after accelerated and LWR relevant thermal aging treatments. First, the thermal aging effect on toughness is discussed in terms of the causes of embrittlement and influential parameters. Second, the talk will include a comprehensive discussion on the thermal aging effects in different CASS grades (i.e., CF3, CF3M, CF8, and CF8M), which will focus on the influence of alloying elements such as molybdenum and carbon. Third, approximate analysis on thermal reaction in CASS was carried out using Arrhenius equation to decide the effective temperature range for accelerated aging experiments to simulate 60 and 80 years of services in limited time frame. The results will provide valuable insights in the degree of thermal aging. Fourth, calculation on equilibrium precipitation was performed for model CASS alloys using the CALPHAD program, and the results will be used to describe the precipitation behaviors in association with the degradation in mechanical properties. (authors)

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Cracking behavior and microstructure of austenitic stainless steels and alloy 690 irradiated in BOR-60 reactor, phase I.

Cracking behavior of stainless steels specimens irradiated in the BOR-60 at about 320 C is studied. The primary objective of this research is to improve the mechanistic understanding of irradiation-assisted stress corrosion cracking (IASCC) of core internal components under conditions relevant to pressurized water reactors. The current report covers several baseline tests in air, a comparison study in high-dissolved-oxygen environment, and TEM characterization of irradiation defect structure. Slow strain rate tensile (SSRT) tests were conducted in air and in high-dissolved-oxygen (DO) water with selected 5- and 10-dpa specimens. The results in high-DO water were compared with those from earlier tests with identical materials irradiated in the Halden reactor to a similar dose. The SSRT tests produced similar results among different materials irradiated in the Halden and BOR-60 reactors. However, the post-irradiation strength for the BOR-60 specimens was consistently lower than that of the corresponding Halden specimens. The elongation of the BOR-60 specimens was also greater than that of their Halden specimens. Intergranular cracking in high-DO water was consistent for most of the tested materials in the Halden and BOR-60 irradiations. Nonetheless, the BOR-60 irradiation was somewhat less effective in stimulating IG fracture among the tested materials. Microstructural characterization was also carried out using transmission electron microscopy on selected BOR-60 specimens irradiated to {approx}25 dpa. No voids were observed in irradiated austenitic stainless steels and cast stainless steels, while a few voids were found in base and grain-boundary-engineered Alloy 690. All the irradiated microstructures were dominated by a high density of Frank loops, which varied in mean size and density for different alloys.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Aging Management Considerations for Dry Cask Storage Canisters - 18472

Dry cask storage systems (DCSSs) are used to store used nuclear fuel (UNF) at independent spent fuel storage installations (ISFSIs) prior to final geologic storage or reprocessing. As storage durations increase beyond the twenty-year period commonly implemented for licensing the storage sites, it is important to consider aging related degradation issues for DCSS components. A large portion of the DCSS designs used throughout the world employ a ventilated concrete overpack with a welded stainless steel canister that confines the UNF. This paper explores key issues related to aging management for these canister components, including: (1) canister environment, (2) inspection limitations, and (3) aging management program guidance and requirements. While the austenitic stainless steel used for the canisters are generally resistant to most forms of environmental attack, it is possible for conditions to arise that lead to pitting and even stress corrosion cracking of the canister systems. A large number of studies related to canister degradation have been performed by industry groups and government researchers, both in the US and worldwide. These advances in the collective knowledge provide insight into risk factors for DCSS. Such information is beneficial to improve ISFSI siting decisions and ensure successful relicensing of existing ISFSIs. This paper highlights relevant research and also discusses applicability to degradation of other equipment and containers used to process and isolate UNF and other nuclear waste streams from the public and the environment. Inspection of the canister surface is an important tool to investigate and evaluate the potential for degradation. Existing DCSS designs typically do not offer ready access to the canister surface in order to perform the inspection. Further complicating inspection efforts are the surface conditions present on the sheltered canisters after extended storage times, including atmospheric debris such as dust and pollen. Given ongoing development efforts, inspection capabilities and associated limitations should be assessed at multiple points in time over the course of an aging management program to incorporate new advances in the field. This paper explores the limitations of currently available capabilities in inspection and delivery, and provides insight into the gaps remaining to be filled to permit an effective inspection program. Recommendations and requirements related to programs for aging management of canisters have been published or are in progress from a variety of groups, including industry groups, regulatory authorities, and Codes and Standards. An effective aging management program should consider the technical bases of these various inputs and maintain compliance with requirements. Given multiple sources, decisions will be required when considering conflicting guidance, and this paper will include discussion of the relative merits of the various approaches. (author)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Nitrate Conversion of HB-Line Reillex™ HPQ Resin

Reillex™ HPQ ion exchange resin is used by HB Line to remove plutonium from aqueous streams. Reillex™ HPQ resin currently available from Vertellus Specialties LLC is a chloride ionic form, which can cause stress corrosion cracking in stainless steels. Therefore, HB Line Engineering requested that Savannah River National Laboratory (SRNL) convert resin from chloride form to nitrate form in the Engineering Development Laboratory (EDL). To perform this task, SRNL treated two batches of resin in 2012. The first batch of resin from Reilly Industries Batch 80302MA was initially treated at SRNL in 2001 to remove chloride. This batch of resin, nominally 30 liters, has been stored wet in carboys since that time until being retreated in 2012. The second batch of resin from Batch 23408 consisted of 50 kg of new resin purchased from Vertellus Specialties in 2012. Both batches were treated in a column designed to convert resin using downflow of 1.0 M sodium nitrate solution through the resin bed followed by rinsing with deionized water. Both batches were analyzed for chloride concentration, before and after treatment, using Neutron Activation Analysis (NAA). The resin specification [Werling, 2003] states the total chlorine and chloride concentration shall be less than 250 ppm. The resin condition for measuring this concentration is not specified; however, in service the resin would always be fully wet. Measurements in SRNL showed that changing from oven dry resin to fully wet resin, with liquid in the particle interstices but no supernatant, increases the total weight by a factor of at least three. Therefore, concentration of chlorine or chloride expressed as parts per million (ppm) decreases by a factor of three. Therefore, SRNL recommends measuring chlorine concentration on an oven dry basis, then dividing by three to estimate chloride concentration in the fully wet condition. Chloride concentration in the first batch (No.80302MA) was nearly the same before the current treatment (759 ppm dry) and after treatment (745 ppm dry or ~248 ppm wet). Treatment of the second batch of resin (No.23408) was very successful. Chloride concentration decreased from 120,000 ppm dry to an average of 44 ppm dry or ~15ppm wet, which easily passes the 250 ppm wet criterion. Per guidance from HB Line Engineering, SRNL blended Batch 80302 resin with Batch P9059 resin which had been treated previously by ResinTech to remove chloride. The chloride concentrations for the two drums of Batch P9059 were 248 ppm dry (~83 ppm wet) ±22.8% and 583 ppm dry (~194 ppm wet) ± 11.8%. The blended resin was packaged in five gallon buckets.

38 RADIATION CHEMISTRY, RADIOCHEMISTRY, AND NUCLEA↗

Numerical Analysis of JNES Seismic Tests on Degraded Combined Piping System

Nuclear power plant safety under seismic conditions is an important consideration. The piping systems may have some defects caused by fatigue, stress corrosion cracking, etc., in aged plants. These cracks may not only affect the seismic response but also grow and break through causing loss of coolant. Therefore, an evaluation method needs to be developed to predict crack growth behavior under seismic excitation. This paper describes efforts conducted to analyze and better understand a series of degraded pipe tests under seismic loading that was conducted by Japan Nuclear Energy Safety Organization (JNES). A special 'cracked-pipe element' (CPE) concept, where the element represented the global moment-rotation response due to the crack, was developed. This approach was developed to significantly simplify the dynamic finite element analysis in fracture mechanics fields. In this paper, model validation was conducted by comparisons with a series of pipe tests with circumferential through-wall and surface cracks under different excitation conditions. These analyses showed that reasonably accurate predictions could be made using the abaqus connector element to model the complete transition of a circumferential surface crack to a through-wall crack under cyclic dynamic loading. The JNES primary loop recirculation piping test was analyzed in detail. This combined-component test had three crack locations and multiple applied simulated seismic block loadings. Comparisons were also made between the ABAQUS finite element (FE) analyses results to the measured displacements in the experiment. Good agreement was obtained, and it was confirmed that the simplified modeling is applicable to a seismic analysis for a cracked pipe on the basis of fracture mechanics. Pipe system leakage did occur in the JNES tests. The analytical predictions using the CPE approach did not predict leakage, suggesting that cyclic ductile tearing with large-scale plasticity was not the crack growth mode for the acceleration excitations considered here. Hence, the leakage was caused by low-cycle fatigue with small-scale yielding. The procedure used to make predictions of low-cycle fatigue crack growth with small-scale yielding was based on the Dowling {Delta}J procedure, which is an extension of linear-elastic fatigue crack growth methodology into the nonlinear plasticity region. The predicted moments from the CPE approach were used using a cycle-by-cycle crack growth procedure. The predictions compare quite well with the experimental measurements.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Effects of Laser Etching on the Corrosion Susceptibility of SAVY 4000 and Hagan Containers

Since the late 1990’s, the Hagan container was used as the primary container for packaging of plutonium-bearing materials. The Hagan design consisted of a threaded closure, a Viton® ORing, a carbon-carbon filter, and a 304L stainless steel (SS) body. Over the years, Hagans have shown vulnerability in their design [1]. In 2008, The Department of Energy (DOE) issued DOE M 441.1-1, Nuclear Material Packaging Manual, which detailed an approach to obtain highconfidence in containers by including specific design requirements, material contents and an approach to determine life span from said contents, and surveillance techniques [2]. In response to both the vulnerability issues with the Hagan and DOE M 441.1-1, the SAVY 4000 container with its twist style closure, Viton® O-Ring, Fiberfrax-Gortex filter, and annealed 316L SS body, was designed as the replacement for Hagan containers, but only for a short term lifespan of 5 years [1]. However, both the Hagan and SAVY 4000 are being pushed to maintain a lifespan of 40 years. Therefore, proper confidence must be placed on each component of each container to last a minimum of 40 years. So far, the biggest concern found during surveillance of these containers is corrosion and the potential for failure by corrosion. One concern is that the containers fail due to stress corrosion cracking (SCC), especially around the weld between the collar and the body as welds leave residual stresses. One advantage the SAVY 4000 has is that the body is annealed, but its weld is still susceptible as it was welded after annealing [3, 4]. Moreover, 316L SS is known to have a higher pitting resistance (pits are a precursor to SCC and can also lead to extensive failure of the material), than 304L SS [4]. During recent surveillance activities, two SAVY 4000’s containing Solution Assay Instrument (SAI) solutions were opened. The SAI SAVY 4000’s contained plutonium (Pu) in 3M HCl solution in plastic volumetric flasks placed inside of polyethylene bags. Historically, a SAVY 4000 containing an SAI solution is packaged for 3 weeks, however, these particular containers were not reopened until 14 months later. When opened, brown-red corrosion product was found all over the inside of the container as shown in Figure 1.

36 MATERIALS SCIENCE↗

Electrochemical techniques and mechanisms for the corrosion of metals and alloys in sub- and supercritical aqueous systems

Corrosion has become a decisive factor hindering supercritical water technologies' long-cycle, safe implementation. Electrochemical experiments performed in supercritical aqueous systems can capture essential, real-time information about the micro/nanoscale processes of corrosion and their kinetics. As a starting point, this paper first summarizes the critical chemical properties of supercritical aqueous systems and analyzes their role in determining the duality of corrosion mechanisms (whether electrochemical or chemical micro-processes predominate). Next, it reviews the available electrochemical techniques such as pH sensors, electrochemical noise measurements, and related applications for quantitatively elaborating the corrosion issues in supercritical aqueous systems. With thick and heavy colors, a series of mechanistic models, such as the mixed potential model and the coupled environment models were introduced from the fundamental theories to the related applications, which have been applied widely in ambient and subcritical aqueous systems and exhibit great values and potential to be employed in high-density supercritical water environments. The passivity, depassivation, and passivity breakdown of metals and alloys in terms of the Point Defect Model (PDM) were also successfully implemented and discussed. Further, the newly built SCW_PDM describes the film growth kinetics at the atomic level of metals and alloys in supercritical water and is being developed to quantitatively analyze and resolve a series of corrosion issues such as the passivity breakdown and the stress corrosion cracking that occur in supercritical aqueous systems. This review is helpful by promoting the development of the electrochemical corrosion theory in supercritical aqueous systems and by identifying corrosion prevention and control methods for the safe implementation of relevant supercritical water technologies.

36 MATERIALS SCIENCE↗

Crack Growth Rate and Fracture Toughness of Stainless Steel Welds in Light Water Reactor Environment

Austenitic stainless steel welds play a crucial role in maintaining the structural integrity of light water reactors. Within the reactor core, stainless steel welds endure a harsh service environment including elevated temperature, corrosive coolant, and intense neutron irradiation. Long-term exposure to such a severe service environment could lead to performance degradation. To ensure the safe and economic operation of light water reactors, this study performed crack growth rate and fracture toughness tests on irradiated and thermally aged weld samples harvested from decommissioned reactor components. In a low-corrosion-potential environment, stainless steel welds showed resistance to stress corrosion cracking, and the measured crack propagation rates were comparable to those of wrought stainless steels under similar test conditions. However, a marked decline in fracture toughness was observed in weld samples, particularly in irradiated samples. Fracture instability was observed at ~0.8 dpa, significantly lower than those observed in wrought stainless steels. Further research at higher doses is needed to evaluate the dose dependence of irradiation-induced embrittlement, and to understand the interplay between thermal aging and neutron irradiation in stainless steel welds.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Lifetime estimation of a BWR core shroud in terms of IGSCC

The continued operation of aging Boiling Water Reactors (BWRs) worldwide requires gradually increasing cost of inspection, maintenance, and repair. Intergranular Stress Corrosion Cracking (IGSCC) in sensitized austenitic stainless steel piping first became a major issue for BWRs in the 1980s, resulting in recognition of the susceptibility of reactor internals to IGSCC. Shroud cracking identified in 1993–1994 confirmed that IGSCC of internals is a significant issue for BWRs. IGSCC is a time-dependent, material degradation process, which is caused and accelerated by the presence of residual stresses, material sensitization, irradiation, cold work, elevated temperature, and corrosive environments. This paper emphasizes the importance of accounting for corrosive environments, or more exactly, electrochemical phenomena in modelling IGSCC and predicting the service life of BWR in-vessel components, and stresses the necessity of performing such modeling not just for a single state point under full power conditions, but for the whole operating history of the reactor, including startups and shutdowns. Overall, this paper demonstrates that ignoring electrochemical considerations may result in underestimating component lifetime and lead to unnecessary expenses for inspection and repair.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Crack Growth Rate and Fracture Toughness Tests on Irradiated Ex-Plant Materials

The performance of structural materials is critical for the safe and economic operation of light water reactors. Exposed to neutron irradiation during service, the reactor core internal materials can undergo significant microstructural and microchemical changes, leading to irradiation hardening and embrittlement. To ensure the structural integrity and functionality of nuclear reactor components during long-term operation, material degradation and damage mechanisms must be understood and managed adequately. In this work, irradiated materials harvested from the decommissioned Zorita reactor were studied for their cracking susceptibility and fracture resistance as a function of irradiation dose up to 47 displacement per atom (dpa). The material is a Type 304 stainless steel sectioned from the baffle plates of this pressurized water reactor with 38 years of service. Crack growth rate and fracture toughness J-resistance (J-R) curve tests were performed in low-corrosion-potential environments at ~315°C. All samples behaved similarly under cyclic loading, and no deteriorated corrosion-fatigue behavior was observed in the test environments. Under constant stress intensity factors, most samples did not show elevated crack growth rates, suggesting an adequate stress corrosion cracking resistance in the test environments. However, an unstable cracking behavior was observed in a 47-dpa sample, resulting in significantly higher crack growth rates than expected at high stress intensity factors. Crack instability was also observed in a 0.06-dpa sample but did not lead to a sustained high crack growth rate. The impact of neutron irradiation was more evident in the fracture toughness J-R curve tests. As the dose increased, the J-R curve declined considerably and became very shallow at high doses. A fully intergranular fracture morphology was also observed among the high-dose samples ruptured in an air atmosphere at room temperature. This brittle fracture mode in the absence of high temperature water environment confirmed a high degree of embrittlement of this material resulting from its service exposure to neutron irradiation.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Atomistic Mechanisms of Stress-Dependent Molten Salt Corrosion in NiCr Alloys

Ni-based structural alloys in molten salt environments often experience simultaneous mechanical loading and corrosive attack, yet the mechanisms governing stress-corrosion interactions remain unclear. Prior studies largely emphasize tensile stress, while the role of compressive stress has received limited attention. Here, reactive molecular dynamics simulations are used to investigate the coupled effects of applied strain and corrosion in Ni 0.75 Cr 0.25 exposed to molten FLiNaK at 800 °C. A Σ5(210) grain boundary model is subjected to tensile (+4%) to compressive (−4%) uniaxial strains, and corrosion behavior is evaluated through fluorine adsorption, charge redistribution, and grain boundary evolution. Tensile strain accelerates intergranular corrosion susceptibility by reducing local atomic packing through elastic dilation and increasing excess free volume at the grain boundary, which enhances atomic mobility and salt infiltration. In contrast, compressive strain can suppress corrosion by promoting the formation of a ridge-like surface layer along the grain boundary, limiting salt access to the underlying alloy. These results provide atomistic insight into how stress states influence grain boundary corrosion in molten salts.