MAGNET DESIGNS FOR THE MULTI-BEND ACHROMAT LATTICE AT THE ADVANCED PHOTON SOURCE

The Advanced Photon Source (APS) is currently investigating replacing the existing two-bend 7 GeV lattice with a 6 GeV seven-bend achromat magnet lattice in order to achieve a low electron beam emittance [1]. This new lattice requires 1320 magnets, of which there are nine types. These include high strength quadrupoles (gradient up to ~97 T/m), sextupoles with second derivative of field up to ~7000 T/m2, longitudinal gradient dipoles with field ratio of up to 5, and transverse gradient dipoles with gradients of ~50 T/m and central field of ~0.6 T. These field requirements and the limited space available pose several design challenges. This paper presents a summary of magnet designs for the various magnet types developed through a collaboration of APS with FNAL and BNL.

Jaski, M.↗

Bend inducible self-folding Origami flexures and microsystems

The present disclosure relates to a spatio-temporal stimulus responsive foldable structure. The structure may have a substrate having at least a region formed to provide engineered weakness to help facilitate bending or folding of the substrate about the region of engineered weakness. The substrate is formed to have a first shape. A stimulus responsive polymer (SRP) flexure is disposed at the region of engineered weakness. The SRP flexure is responsive to a predetermined stimulus actuation signal to bend or fold in response to exposure to the stimulus actuation signal, to cause the substrate to assume a second shape different from the first shape.

Kampasi, Komal↗

Bending with large deflection of a clamped rectangular plate with length-width ratio of 1.5 under normal pressure

The Von Karman equations for a thin flat plate with large deflections are solved for the special case of a plate with clamped edges having a ratio of length to width of 1.5 and loaded by uniform normal pressure. Center deflections, membrane stresses, and extreme-fiber bending stresses are given as a function of pressure for center deflections up to twice the thickness of the plate. For small deflections the results coincide with those obtained by Hencky from the linear theory. The maximum stresses and center deflection at high pressures differ less than 3 percent from those derived by Bostnov for an infinitely long plate with clamped edges. This agreement suggests that clamped plates with a length-to-width ratio greater than 1.5 may be reared as infinitely long plates for purposes of design.

PLATES-BENDING CIRCULAR↗

Theoretical and Experimental Studies of Bending of Inorganic Electronic Materials on Plastic Substrates

This paper describes materials and mechanics aspects of bending in systems consisting of ribbons and bars of single crystalline silicon supported by sheets of plastic. The combined experimental and theoretical results provide an understanding for the essential behaviors and for mechanisms associated with layouts that achieve maximum bendability. Examples of highly bendable silicon devices on plastic illustrate some of these concepts. Although the studies presented here focus on ribbons and bars of silicon, the same basic considerations apply to other implementations of inorganic materials on plastic substrates, ranging from amorphous or polycrystalline thin films, to collections of nanowires and nanoparticles. Here, the contents are, as a result, relevant to the growing community of researchers interested in the use of inorganic materials in flexible electronics.

36 MATERIALS SCIENCE↗

Microstructure and Three-Point Bending Fatigue Behavior of Al-Cu-Mg-Ag Alloys with Various Mg Contents

This paper presents an investigation on the influence of Mg content on the microstructures, tensile properties and three-point bending fatigue behavior of Al-Cu-Mg-Ag alloys. The results indicate that the alloy containing 0.70 wt.% Mg possesses lower tensile properties and higher fatigue performance compared to the one with 1.15 wt.% Mg. Increasing Mg content in Al-Cu-Mg-Ag alloys can enhance the nucleation and precipitation of Ω phase, as well as increase the volume fraction and number density of constituent particles. The investigation of the fatigue crack initiation and growth behavior of Al-Cu-Mg-Ag alloy using interrupted fatigue tests suggests that micro-cracks mainly nucleate on Al{sub 2}Cu constituent particles and the fatigue life is mainly associated with the density of constituent particles.

36 MATERIALS SCIENCE↗

Characterisation of bending cracks in R/FRC using image analysis

In this study, experiments were conducted to induce bending cracks of specific surface crack width to reinforced concrete beams made of plain concrete (RC) and reinforced concrete beams made of fibre reinforced concrete (R/FRC). After injecting and impregnating the cracks with dyed epoxy resin, image processing and analysis were employed to investigate the internal crack morphology. Several crack features including crack width (accumulated, effective and maximum), branching and tortuosity were defined and quantified. The results showed that in addition to arrested crack development, the presence of fibres yielded a distinctive change in the internal crack pattern, including increased branching and tortuosity, both of which have positive implications regarding concrete permeation. Likewise, specimens with fibres exhibited reduced maximum individual crack widths near the rebar, potentially increasing the ability of autogenous crack healing and reducing the risk of corrosion initiation.

36 MATERIALS SCIENCE↗

On the failure mechanisms of Cr-coated 316 stainless steel in bending fatigue tests

Here, fully-reversed cyclic bending tests were conducted on uncoated and Cr-coated 316 stainless steel specimens. At high stresses, the uncoated specimens outperformed the Cr-coated ones, while the trend reversed at low stresses. For Cr-coated specimens subjected to high stress amplitude loading, experimental observations showed crack initiation at the Cr/substrate interface due to shear steps formed from dislocation activities in the substrate—a conclusion supported by accompanying finite element analysis. Interfacial crack initiation was not observed under low stress amplitudes. This difference in fatigue crack initiation mechanisms induced an opposite trend in fatigue life between high and low stress amplitudes.

36 MATERIALS SCIENCE↗

Microstructural effects on the rotating bending fatigue behavior of Ti–6Al–4V produced via laser powder bed fusion with novel heat treatments

The rotating bending fatigue (RBF) behavior (fully reversed, R = -1) of additively manufactured (AM) Ti–6Al–4V alloy produced via laser powder bed fusion (PBF-L) was investigated with respect to different microstructures achieved through novel heat treatments. The investigation herein seeks to elucidate the effect of microstructure by controlling variables that can affect fatigue behavior in Ti–6Al–4V, such as chemistry, porosity, and surface roughness. In order to control these variables, different hot isostatic pressing (HIP) treatments at 800 °C, 920 °C, and 1050 °C with a 920 °C temper were applied to three sets of Ti–6Al–4V cylinders that originated from the same PBF-L build, such that there were 30 tests per condition. After HIP treatment, the specimens were machined and tested. The highest runout stress was achieved after sub-β transus HIP at 800 °C for 2 h at 200 MPa of pressure. A significant drop in fatigue strength was attributed to large prior-β grains and grain boundary α resulting from super-β transus HIP treated specimens. In conclusion, for the sub-β transus HIP specimens, differences in fatigue strength were attributed to α lath thickness, relative dislocation density, and dislocation boundary strengthening.

36 MATERIALS SCIENCE↗

Damage evolution and ductile fracture of commercially-pure titanium sheets subjected to simple tension and cyclic bending under tension

This paper describes a study into the evolution of damage in commercial-purity titanium (CP–Ti) sheets subjected to cyclic bending under tension (CBT) and uniaxial tension (simple tension, ST). Sections were taken from sheets that were strained to various levels under both methods and were imaged using X-ray computed tomography (XCT) to reveal insights into the size, density, and distribution of microvoids in the sheets. Digital image correlation (DIC) was also used to observe the surface strain of CBT and ST sheets during testing. These results showed that elongation to failure (ETF) for CBT deformation is about 2.5× higher than for ST, local longitudinal strains in the bulk of the CBT sample are around 1.3× higher than the peak strain in the ST necked region, and 1.7× higher in the localized region of CBT failure. It was found that the volume-density of voids in both sheets followed a similar exponential increase with strain, reaching nearly 45× higher in the CBT than the ST sheets before the onset of failure, mainly due to the higher strain levels achieved. A higher volume density of voids developed in the center of sheets at high levels of strain, for both processes, with the density in the sheet center becoming approximately double that found near the edges. Scanning electron microscopy (SEM) was used to examine the fracture surface of CBT and ST sheets after failure. The observations are presented and discussed highlighting the CBT process as effective to delay ductile fracture of the CP-Ti sheets.

Commercially pure titanium↗

The roles of interfaces and other microstructural features in Cu/Nb nanolayers as revealed by in situ beam bending experiments inside an scanning electron microscope (SEM)

Interfaces and their interactions with other microstructural features, such as grain boundaries or twin structures, have been widely viewed as parameters for designing metallic nanolayers. These interfaces could play a role in hindering cracks from propagating across the nanolayers while in operation. To date, many studies have focused on the roles of interfaces in affecting the plasticity mechanisms and thus the deformability of nanolayers. However, no studies have investigated on the subsequent mechanisms of fracture leading to the final failure. In this study, in situ microfracture bending tests inside a scanning electron microscope (SEM) were performed on the notched clamped beams of Cu/Nb nanolayers with a similar layer thickness using two different fabrication processes: physical vapor deposition (PVD) and accumulative roll bonding (ARB). Due to the columnar grains of the Cu/Nb PVD beams, a sudden catastrophic linear elastic, brittle fracture phenomenon was observed; in the Cu/Nb ARB beams, fracture events of notch widening phase and crack initiation and fracture along the shear instability were observed. Detailed examinations showed the presence of competing mechanisms between the multilayered interface, columnar grain boundary, and experimental factors of beam geometry and the position of the tip. With this newfound knowledge, new types of metallic nanolayers can be designed with enhanced strength and fracture resistant properties.

36 MATERIALS SCIENCE↗

A 90 ° bend curved light-guide for TOF scintillating detectors

We report here a bench study of TOF resolution using a 90° bend curved solid light-guide (LG) used to transport the light from a plastic scintillator counter to a photomultiplier (PMT). The 90° LG allows the rotation of the PMT axis to be vertical to the detector axis, in an environment featured by a strong magnetic field along the detector surface, or other geometrical constrains. We show that with a TOF counter of 2000 x 100 x 60 mm 3 and light read-out by PMTs at its two 100 × 60 mm 2 sides, when 90° LG benders are used between the scintillating bar and the PMTs on both sides, the TOF resolution is worsen, by 5–10%.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Effect of layer bending on montmorillonite hydration and structure from molecular simulation

Conceptual models of smectite hydration include planar (flat) clay layers that undergo stepwise expansion as successive monolayers of water molecules fill the interlayer regions. However, X-ray diffraction (XRD) studies indicate the presence of interstratified hydration states, suggesting non-uniform interlayer hydration in smectites. Additionally, recent theoretical studies have shown that clay layers can adopt bent configurations over nanometer-scale lateral dimensions with minimal effect on mechanical properties. Therefore, in this study we used molecular simulations to evaluate structural properties and water adsorption isotherms for montmorillonite models composed of bent clay layers in mixed hydration states. Results are compared with models consisting of planar clay layers with interstratified hydration states (e.g. 1W–2W). The small degree of bending in these models (up to 1.5 Å of vertical displacement over a 1.3 nm lateral dimension) had little or no effect on bond lengths and angle distributions within the clay layers. Except for models that included dry states, porosities and simulated water adsorption isotherms were nearly identical for bent or flat clay layers with the same averaged layer spacing. Similar agreement was seen with Na- and Ca-exchanged clays. In conclusion, while the small bent models did not retain their configurations during unconstrained molecular dynamics simulation with flexible clay layers, we show that bent structures are stable at much larger length scales by simulating a 41.6×7.1 nm 2 system that included dehydrated and hydrated regions in the same interlayer.

58 GEOSCIENCES↗

Note: Rigid holder to host and bend a crystal for multiple volume reflection of a particle beam

A holder to lodge and bend a silicon crystal to excite multivolume reflection of a high-energy particle beam has been designed and fabricated. A mechanically robust and stable structure fastens a crystal at best condition for experiments. The holder has allowed the observation of 12-time repeated volume reflection with very high efficiency. We detail the most important features behind the construction of the holder together with the characterization of the crystal being bent by the holder.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Finite Element Analysis on Spread for In-plane Roll-bending Process

The in-plane roll-bending process is a special wedge rolling with a configuration of two conical rolls which can form strips into open ring products. The spread of a ring is usually not considered in previous radius predicting models by Yang et al. and Xian et al. However, the spread increases to 10% for a ring with average reduction of 56%, and there is a discrepancy between the predicted radius and the experiment. Spread analysis/calculation has become an urgent problem in radius prediction and precision control of unequal deformation in this process. A finite element (FE) model considering spread effect is established and evaluated by experiments. A comparison between the predicted results with/without considering spread by FE analysis and experiments is carried out. The result shows that the predicted results considering spread are much closer to the experiments than those without considering spread effect. Based on the FE simulation, the spread characteristics of the ring with two types of cross section (including partly and entirely compressed cross section) are investigated. It is found that, there exist three spread regions, including outer positive region, middle negative region and inner positive region for the partly compressed ring; and there are outer positive region and inner negative region for the entirely compressed ring. The spread mostly happens at the outer positive region for both types of ring. The effects of process parameters, such as wedge angle, bite location, friction coefficient and rotational speed of roll, on spread for three aluminum alloys, 3A21O, 5A02O and 2A12T4, are investigated. The results indicate that the spread decreases with an increase in wedge angle, whereas increases with the growth of bite location; the spread remains stable with increasing friction coefficient and fluctuates within 3%-8% with a rise in rotational speed of roll. The spread of the partly compressed ring is less than 6%; large spread (larger than 6%) occurs when the ring is entirely compressed; the spread may reach a maximum value of 18.8% for material 5A02O.

36 MATERIALS SCIENCE↗

Interfacial energy level bending in a crystalline p/p-type organic heterostructure

A conduction channel was observed at the heterointerface of the crystalline p-type organic films copper phthalocyanine (CuPc) and 2,5-bis(4-biphenylyl) bithiophene (BP2T). Energy level bending at the interface is confirmed by photoemission spectroscopy, which verifies a charge transfer between CuPc and BP2T. This provides a further route to utilize interfacial electronic properties in functional devices and also documents the importance of reconsidering the interfacial electronic structure of organic heterostructures.

36 MATERIALS SCIENCE↗