Search NASA⌕ Search

SEARCH · Search NASA

Results for “Capacity degradation”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 469 records · Page 26

High-performance all-solid-state Li–S batteries enabled by an all-electrochem-active prelithiated Si anode

The development of all-solid-state Li–S batteries has been greatly impeded by dendrite growth and dendrite penetration, which are both related to the Li metal anode. As a compromised alternative, we report lithium silicide (Li x Si) as a dendrite-free and high-capacity anode with Li source. Here, the as-synthesized Li x Si is relatively soft, highly electronically conductive, and with a high Li diffusivity. These distinctive properties make Li x Si anode viable as an “all-electrochem-active” electrode (consisted of 100 wt.% Li x Si). Compared with the typical composite electrode, the all-electrochem-active electrode not merely maximizes the electrode-level energy density but also minimizes the electrolyte-related interfacial degradation. Li x Si symmetric cell demonstrates a reversible cycling at 4 mA cm –2 for over 320 h. Stress change and morphological evolution of the Li x Si electrode are investigated upon dealloying/alloying. When paired with a S cathode (active mass loading of 3 mg cm –2 ), Li x Si–S full cell shows a good cycling behavior over 500 cycles and rate performance (69% capacity retained at 1.2C) even at 25 °C.

25 ENERGY STORAGE↗

Understanding Discharge‐Driven Growth of Cathode Impedance in Ni‐Rich NMC Cathodes

Degradation of LiNi x Mn y Co 1-x-y O 2 (NMC)-based lithium-ion batteries depends strongly on cut-off voltage ranges. In addition to the high upper cut-off voltage, a high depth of discharge (i.e., lower cut-off voltage) significantly worsens cathode impedance growth and capacity fade during long-term cycling. However, there is currently no consensus on the mechanism behind the negative role of a deep discharge. Here, this phenomenon was investigated in graphite||NMC cells with single-crystal cathodes (LiNi 0.6 Co 0.2 Mn 0.2 O 2 (NMC622) or LiNi 0.76 Co 0.14 Mn 0.10 O 2 (NMC76)) using targeted aging protocols (constant high-voltage holds vs. charge–discharge cycling), while monitoring transition-metal (TM) dissolution, cathode-electrolyte interface (CEI) impedance, and NMC surface composition. We demonstrate a correlation between discharge-driven CEI impedance growth and increased TM dissolution. Furthermore, this degradation pathway is more pronounced in lower-Ni NMC622 than in higher-Ni (NMC76) under comparable delithiation states at charge, with both compositions undergoing the H2→H3 phase transition. X-ray photoelectron spectroscopy (XPS) reveals NMC composition-dependent evolution of surface lattice oxygen and restructured surface layer composition between charged and discharged states. These findings add mechanistic depth to the role of discharge as an active driver of interfacial degradation and provide new insights into its composition dependence.

25 ENERGY STORAGE↗

The Quest for Stable Potassium‐Ion Battery Chemistry

Abstract Potassium‐ion batteries (KIBs) have attracted wide interest for energy storage because of the abundance of the electrode materials involved; however, their electrochemical performances are far behind what can be achieved from lithium‐ion batteries (LIBs) or sodium‐ion batteries (SIBs). Herein, key promising electrode and electrolyte materials for potassium‐ion batteries are identified, the coupled electrochemical reactions in the cell are investigated, and the compatibility between different materials is demonstrated to play the most important role. K 2 Mn[Fe(CN) 6 ] cathode can deliver a high capacity of ≈125 mAh g −1 and exceptional cycling stability over 61 000 cycles (≈9 months) if the side reactions from the anode can be prevented. Graphite is a good anode material but is subjected to degradation in traditional carbonate electrolytes. New concentrated electrolytes are developed and evaluated. A stable KIB system is demonstrated by coupling a stable K 2 Mn[Fe(CN) 6 ] cathode, a prepotassiated graphite anode with a concentrated electrolyte to achieve a high energy density of ≈260 Wh kg −1 (based on the active mass of cathode and anode) and good cycling of over 1000 cycles.

Wu, Xianyong↗

The Role of Catholyte Modulation in Suppressing the Initial Capacity Fade of Zinc Electrolytic Manganese Dioxide Coin Cells

Despite its potential for zinc–manganese oxide batteries, electrolytic manganese dioxide (EMD) can experience capacity fade due to a deficiency in the Mn 2+ supply at the cathode electrolyte interphase (CEI) from side reactions, even in the presence of an electrolyte additive. In this work, electrolyte loading modulation at the cathode electrolyte interface (CEI) was correlated with Zn∥EMD cell capacity retention and cycling performance, as a proposed measure to curb the initial capacity fade observed in EMD. Initial galvanostatic charge/discharge cycling, with varied electrolyte loading, revealed severe capacity fade (from ~188 to 10 mAh g –1 for the highest loading of 200 μL) within the first 15 cycles. Such a decrease in cell capacity is correlated with the formation of a Mn 4+ deposit on the current collector and consequently, the Mn 2+ depletion at CEI, as was supported by elemental and Raman analyses. Interestingly, confinement of the electrolyte to the CEI at a lower (≤15 μL) electrolyte loading mitigated Mn 4+ side-deposition, maintaining the cell capacity at >80% over the first 15 cycles. Interfacial Mn supply/depletion could be monitored via voltammetric analysis based on changes of the Zn 2+ insertionreduction peak. Additional galvanostatic experiments corroborated the voltammetric interpretation and the proposed degradation pathway in the studied cell conditions. The outcomes of this work provide practical insight into coin-cell design and configuration strategies for developing Zn∥EMD batteries.

25 ENERGY STORAGE↗

Modest functional diversity decline and pronounced composition shifts of microbial communities in a mixed waste-contaminated aquifer

Background: Microbial taxonomic diversity declines with increased environmental stress. Yet, few studies have explored whether phylogenetic and functional diversities track taxonomic diversity along the stress gradient. Here, we investigated microbial communities within an aquifer in Oak Ridge, Tennessee, USA, which is characterized by a broad spectrum of stressors, including extremely high levels of nitrate, heavy metals like cadmium and chromium, radionuclides such as uranium, and extremely low pH (< 3). Results: Both taxonomic and phylogenetic α-diversities were reduced in the most impacted wells, while the decline in functional α-diversity was modest and statistically insignificant, indicating a more robust buffering capacity to environmental stress. Differences in functional gene composition (i.e., functional β-diversity) were pronounced in highly contaminated wells, while convergent functional gene composition was observed in uncontaminated wells. The relative abundances of most carbon degradation genes were decreased in contaminated wells, but genes associated with denitrification, adenylylsulfate reduction, and sulfite reduction were increased. Compared to taxonomic and phylogenetic compositions, environmental variables played a more significant role in shaping functional gene composition, suggesting that niche selection could be more closely related to microbial functionality than taxonomy. Conclusions: Overall, we demonstrated that despite a reduced taxonomic α-diversity, microbial communities under stress maintained functionality underpinned by environmental selection.

59 BASIC BIOLOGICAL SCIENCES↗

West Africa Battery Energy Storage Systems (BESS) Capacity Building - Discussion of BESS Tariffs: Payment Structures and Case Studies [Slides]

Battery Energy Storage Systems (BESS) are emerging as critical assets for enhancing grid reliability, integrating renewable energy, and enabling system flexibility. Yet, the regulatory and financial frameworks that determine how BESS projects are compensated vary widely across jurisdictions. This presentation explores international case studies - from Honduras, Costa Rica, Chile, South Africa, Mexico, and Brazil - to illustrate how tariff design and payment structures are evolving to support large-scale BESS deployment. The cases highlight a range of ownership and revenue models, including cost-of-service mechanisms, energy and capacity payments, and market-based arbitrage, as well as hybrid approaches under development. The discussion will examine key challenges such as defining remuneration for ancillary services, addressing double charging, and accounting for efficiency losses and degradation over time. By comparing experiences across markets, the presentation identifies emerging best practices for valuing BESS and designing tariffs that align technical performance with economic incentives, providing insights for regulators, utilities, and policymakers pursuing storage integration.

25 ENERGY STORAGE↗

Oxidation Behavior and Property Degradation of Nuclear Graphites

During its multidecade operation in the core of nuclear reactors, graphite components are subjected to aggressive and continuous exposure to a high field of ionizing and neutron irradiation, high temperature, and various types of present and postulated chemical attacks. High density, high crystallinity polygranular synthetic graphite is unique among other materials for its extraordinary capacity of resisting and adapting to the aggression inflicted by high temperature, high energy neutron bombardment and ionizing gamma radiation. But, as a carbonaceous material, even though of very high purity, graphite is reactive towards common oxidizing agents: oxygen, carbon dioxide, water. Safe operation of HTGRs relies, among other aspects, on engineered safeguard systems for efficient and continuous protection of graphite components against oxidation. Graphite oxidation behavior was, and continues to be, an important direction of theoretical and experimental research, engineering analyses, models and simulations, and design and safety regulations. The avalanche of publications, reports, experimental data, computer codes, and regulatory documents related to oxidation behavior of nuclear graphite is now accelerating to new levels, prompted by the increased interest for nuclear energy as a clean, carbon-free energy source. Even though public’s perception of nuclear energy advantages may still be influenced by the memories of past accidents of nuclear reactors from generations II and III, the community of informed scientists and engineers, regulators and statemen knows that generation IV of nuclear reactors is designed at very high safety standards, doubled by great advances of scientific knowledge and technological progress. One of routes of these recent advances is directed at better understanding of graphite oxidation behavior, its relationship with graphite manufacturing and microstructural properties, along with the effects of various environmental factors and process variables. Together, the recent progress in manufacturing, properties characterization, and modeling of intricated physical and chemical processes that concur to the oxidation behavior led to development of powerful simulation codes able to analyze various scenarios of normal operation and hypothetical off-normal events, and thus to clearly specify the allowable parameters envelopes for the designers, constructors, and operators of current and future modular HTGRs. This review begins with an introduction on manufacturing methods, structure, and properties of nuclear graphite, including basic requirements that this specialty graphite type must satisfy for nuclear use. It continues with a chapter on environmental effects on nuclear graphite, where emphasis is placed less on irradiation and much more on oxidation phenomena, their safety implications, and the basic traits of chronic and acute oxidation by air (oxygen) and water (humidity, steam). Particular attention is placed on the three graphite grades of interest for this document (IG-110, NBG-18, PCEA). A chapter on properties degradation induced by oxidation follows, with focus on density, dimensional, and mechanical properties changes. The next chapter is intended as a brief review of various approaches used for modeling of graphite oxidation behavior. It summarizes the progress of oxidation models, from the early attempts to complex computational approaches interfaced with specialized computer codes designed for nuclear reactor simulations. Last, a list is presented of knowledge gaps where more research is needed. A short summary concludes the review.

36 MATERIALS SCIENCE↗

Voltage-Based Strategies for Preventing Battery Degradation under Diverse Fast-Charging Conditions

Maintaining safe operating conditions is a key challenge for high-performance lithium-ion battery applications. The lithium-plating reaction remains a risk during charging, but limited studies consider the highly variable charging conditions possible in commercial cells. Here we combine pseudo-2D electrochemical modeling with data visualization methods to reveal important relationships between the measurable cell voltage and difficult-to-predict Li-plating onset criteria. An extensively validated model is used to compute Li plating for thousands of multistep charging conditions spanning diverse rates, temperatures, states-of-charge, and cell aging. Here we observe an empirical cell operating voltage limit below which plating does not occur across all conditions, and this limit varies with the battery state-of-charge and aging. A model sensitivity analysis also indicates that, when comparing two charging voltage profiles, the capacity difference at 4.0 V correlates well with the difference in the plating onset capacity. These results encourage simple strategies for Li-plating prevention that are complementary to existing battery controls.

25 ENERGY STORAGE↗

Electrochemical-driven green recovery of lithium, graphite and cathode from lithium-ion batteries using water

The expected exponential increase in consumption of lithium-ion batteries (LIBs) would pose a unique challenge to the availability of near-critical resources like lithium and graphite in the upcoming decade. In this work, we present a lithium recovery process that utilizes a degradation mechanism, i.e., lithium plating, as a tool to concentrate metallic lithium at the anode/separator interface for convenient extraction at room temperature – using only water. Electrochemical characterization of fast charged (1–6 C) LIBs yielded a maximum capacity fade of 50% over ten cycles. The lithium plating was confirmed via voltage plateau analysis, coulombic efficiency, and DC resistance measurements. A maximum lithium plating condition was observed to exist between 4C and 5C, thereby limiting the energy consumption in the extraction process. Post-mortem film thickness measurement showed an incrementing film deposition with a maximum of 35 µm thickness. SEM and XPS analysis confirmed increasing concentration of a dense dendritic metallic lithium deposition on the anode/separator interface with C-rate. A green recovery process was adopted to extract the concentrated metallic lithium using distilled water. The lithium from the plated film, solid/electrolyte interface (SEI), electrolyte, anode, and cathode, was extracted as salts. A 37% improvement in lithium recoverability was achieved with fast charging under ambient conditions. XPS analysis showed ~92% of lithium yield with no residual lithium in the graphite. In addition, the battery-grade graphite was recovered with 97% purity after heat treatment of the washed anode film, and concentrated transition metals oxides in the cathode to 93% purity for convenient extraction.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Stationary Oxygen Vacancy Construction toward a Superior-Performance Ultrahigh Nickel Single-Crystal Cathode

Oxygen vacancies exert a complex and profound influence on the layered cathodes, especially those with ultrahigh nickel content. They can facilitate lithium-ion transport and enhance electronic conductivity, while aggressive oxygen vacancy formation causes structural degradation and electrolyte decomposition. Herein, taking ultrahigh nickel single-crystal LiNi 0.92 Co 0.06 Mn 0.02 O 2 (SC-Ni92) as a model material, we propose a pinning strategy to harness the benefits of oxygen vacancies while mitigating their detrimental effects. Through a carefully controlled thermal process, both oxygen vacancies and pinning atoms are successfully introduced into the surface region. The resulting anchored oxygen vacancies, capitalizing on their inherent advantages, improve conductivity and lithium-ion diffusion. Simultaneously, the neighboring pinning atoms effectively increase the migration barrier and suppress the adverse effects of these vacancies, including electrolyte decomposition and structural degradation during long-term electrochemical cycling. Consequently, oxygen vacancy-anchored single-crystal LiNi 0.92 Co 0.06 Mn 0.02 O 2 (SC-Ni92-OV) demonstrates significantly improved high-voltage electrochemical performance, with 86.16% capacity retention after 200 cycles at 4.6 V and 1 C in a half-cell and 90.71% after 300 cycles at 4.5 V and 1 C in a full cell. Furthermore, this study not only provides valuable insights into the chemistry of oxygen vacancy but also introduces a viable strategy for leveraging oxygen vacancies to achieve stable high-voltage performance in ultrahigh nickel single-crystal cathodes.

defects in solids↗

A genomic analysis reveals the diversity of cellulosome displaying bacteria

Introduction Several species of cellulolytic bacteria display cellulosomes, massive multi-cellulase containing complexes that degrade lignocellulosic plant biomass (LCB). A greater understanding of cellulosome structure and enzyme content could facilitate the development of new microbial-based methods to produce renewable chemicals and materials. Methods To identify novel cellulosome-displaying microbes we searched 305,693 sequenced bacterial genomes for genes encoding cellulosome proteins; dockerin-fused glycohydrolases (DocGHs) and cohesin domain containing scaffoldins. Results and discussion This analysis identified 33 bacterial species with the genomic capacity to produce cellulosomes, including 10 species not previously reported to produce these complexes, such asAcetivibrio mesophilus. Cellulosome-producing bacteria primarily originate from theAcetivibrio, Ruminococcus, Ruminiclostridium, andClostridiumgenera. A rigorous analysis of their enzyme, scaffoldin, dockerin, and cohesin content reveals phylogenetically conserved features. Based on the presence of a high number of genes encoding both scaffoldins and dockerin-fused GHs, the cellulosomes inAcetivibrioandRuminococcusbacteria possess complex architectures that are populated with a large number of distinct LCB degrading GH enzymes. Their complex cellulosomes are distinguishable by their mechanism of attachment to the cell wall, the structures of their primary scaffoldins, and by how they are transcriptionally regulated. In contrast, bacteria in theRuminiclostridiumandClostridiumgenera produce ‘simple’ cellulosomes that are constructed from only a few types of scaffoldins that based on their distinct complement of GH enzymes are predicted to exhibit high and low cellulolytic activity, respectively. Collectively, the results of this study reveal conserved and divergent architectural features in bacterial cellulosomes that could be useful in guiding ongoing efforts to harness their cellulolytic activities for bio-based chemical and materials production.

Microbiology↗

Facile Dual-Protection Layer and Advanced Electrolyte Enhancing Performances of Cobalt-free/Nickel-rich Cathodes in Lithium-Ion Batteries

Despite cobalt (Co)-free/nickel (Ni)-rich layered oxides being considered as one of the promising cathode materials due to their high specific capacity, their highly reactive surface is one of the shortcomings that still hinder their practical usages in high-energy-density batteries. Herein, a polyimide/polyvinylpyrrolidone (PI/PVP, denoted as PP) coating layer is demonstrated as dual-protection for LiNi 0.96 Mg 0.02 Ti 0.02 O 2 (NMT) cathode material to suppress surface contamination against moisty air and to prevent unwanted side reactions between cathode and electrolyte during electrochemical cycling. The optimal PP-coated NMT (PP@NMT) preserves a clean surface without generation of lithium (Li) residues, structural degradation, and gas evolution after exposure to air with ~30% humidity for 2 weeks. Contrarily, the exposed bare NMT shows severe contamination, structural shrinkage due to Li loss, and increased gas release during charging. In addition, the exposed PP@NMT significantly enhances the electrochemical performance of graphite (Gr)||NMT cells by decreasing byproducts and maintaining structural stability. Moreover, the exposed PP@NMT achieves a high capacity retention of 86.7% after 500 cycles in Gr||NMT cells using an advanced localized high-concentration electrolyte. Furthermore, this work demonstrates a promising facile approach to the protection of Co-free/Ni-rich layered cathodes for their practical applications even after exposure to moisty air.

25 ENERGY STORAGE↗

Electrochemo-mechanics unlocks hidden dynamics of lithium plating under stacking pressure

Understanding and mitigating lithium plating remains one of the most pressing challenges in advancing the safety and longevity of lithium-ion batteries (LIBs). Here, we present a novel integrative framework that combines in-operando swelling force measurements with a physics-based electro-chemo-mechanical model to uncover previously inaccessible insights into lithium plating dynamics under mechanical constraints. Unlike existing approaches that focus primarily on electrochemical signatures, our approach captures the coupled mechanical responses of commercial pouch cells during cycling, revealing how mechanical constraints fundamentally alter degradation pathways. We demonstrate that the use of a moderate stacking pressure suppresses lithium plating and enhances lithium stripping. This mechanically driven structural effect, coupled with the electrochemical process, significantly extends the linear aging regime in LIBs. Intriguingly, intermittent capacity recovery events that were observed during the battery cycling suggest dynamic lithium reactivation, a phenomenon rarely captured in real-time. This study pioneers a stress-aware methodology for diagnosing and managing lithium plating, establishing a new paradigm for real-time battery health monitoring. The findings offer transformative implications for the design of durable, high-performance LIB systems, opening new avenues for intelligent control strategies in battery management systems.

Bhowmick, Amit↗

Iodine Removal from Carbonate-Containing Alkaline Liquids Using Strong Base Resins, Hybrid Resins, and Silver Precipitation

The ability of several material types to remove aqueous iodine from a mildly alkaline, carbonate-rich nuclear waste stream was evaluated: strong base anion exchange resins (SBAR), hybrid resins, Ag-containing materials and Bi-containing hybrid resins. A combination of batch testing and flow through column testing were used in the evaluation. In batch testing, hybrid resins CHM-20, SIR-110-CE and RTBI were shown to have high efficiency for the removal of both iodide and iodate simultaneously, while Ag-containing materials and SBAR demonstrated high capacity for iodide removal. One example of each material type (CHM-20, A532E and Ionex 400) were further evaluated for their sorption isotherms and column performance. The Langmuir isotherm, or a Langmuir-Freundlich hybrid isotherm, best described the sorption of iodide to the CHM-20 hybrid resin and Purolite A532E. The Freundlich isotherm best described the uptake of iodate to CHM-20 and A532E and for both iodide and iodate to the Ag-containing Ionex-400. In column testing the Purolite A532E had exceptional performance for overall iodide removal. With the capacity demonstrated the A532E resin would exceed Class C waste classification before breakthrough initiated, and column change outs in processing would be dictated by eventual waste classification, not breakthrough. The Ionex 400, a Ag-zeolite, was observed to degrade over time in the column in the mild alkaline conditions whereas the hybrid CHM-20 was limited in the single pass through design and would be best suited for applications where iodide and iodate are present and recirculation of the column effluent is feasible. Here this work highlights the feasibility of commercially available materials to separate radioiodine from liquid environments.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Probing the Reactivity of the Active Material of a Li-Ion Silicon Anode with Common Battery Solvents

Calculations and modeling have shown that replacing the traditional graphite anode with silicon can greatly improve the energy density of lithium-ion batteries. However, the large volume change of silicon particles and high reactivity of lithiated silicon when in contact with the electrolyte lead to rapid capacity fading during charging/discharging processes. In this report, we use specific lithium silicides (LS) as model compounds to systematically study the reaction between lithiated Si and different electrolyte solvents, which provides a powerful platform to deconvolute and evaluate the degradation of various organic solvents in contact with the active lithiated Si-electrode surface after lithiation. Nuclear Magnetic Resonance (NMR) characterization results show that a cyclic carbonate such as ethylene carbonate is chemically less stable than a linear carbonate such as ethylmethyl carbonate, fluoroethylene carbonate, and triglyme as they are found to be more stable when mixed with LS model compounds. Furthermore, guided by the experimental results, two ethylene carbonate (EC)-free electrolytes are studied, and the electrochemical results show improvements with graphite-free Si electrodes relative to the traditional ethylene-carbonate-based electrolytes. More importantly, the study contributes to our understanding of the significant fundamental chemical and electrochemical stability differences between silicon and traditional graphite lithium-ion battery (LIB) anodes and suggests a focused development of electrolytes with specific chemical stability vs lithiated silicon which can passivate the surface more effectively.

25 ENERGY STORAGE↗

Evaluation of Lithium Metal Anode Volumetric Expansion through Laser Plasma Focused Ion Beam Cross-Sectional Imaging

Lithium metal is an ideal anode for high energy density batteries, however the implementation of lithium metal anodes remains challenging. Beyond the development of highly efficient electrolytes, degradation processes restrict cycle life and reduce practical energy density. Herein lithium volumetric expansion and degradation pathways are studied in half cells through coupling electrochemical analysis with cross-sectional imaging of the intact electrode stack using a cryogenic laser plasma focused ion beam and scanning electron microscope. Here, we find that the volumetric capacity is compromised as early as the first cycle, at best reaching values only half the theoretical capacity (1033 vs 2045 mAh cm -3 ). By the 101st electrodeposition, the practical volumetric capacity decreases to values ranging from 143 to 343 mAh cm -3 .

25 ENERGY STORAGE↗

The TRANSCEND University Consortium: Theme 2 - Site Decommissioning, Deconstruction and Remediation - 20329

This paper will discuss the aims, objectives and progress to-date under Theme 2 of the TRANSCEND consortium project: Site decommissioning, deconstruction and remediation. Decommissioning nuclear sites involves waste retrieval, decontamination, deconstruction and, where necessary, containment and/or remediation of the remaining structure and surrounding land. Critical to management of these processes is limiting radiation exposure for the workforce, restricting the spread of radionuclides in groundwater, surface water and airborne particulates, and minimising the volume of contaminated waste for disposal. The aim of Theme 2 research is to develop new technologies for monitoring, remediation and containment that serve to minimise the volume of radioactively contaminated waste for disposal, for application prior to, during and after retrieval, deconstruction and decontamination operations. Prior research, conducted under the previous DISTINCTIVE project, demonstrated that colloidal silica grout can penetrate low permeability materials (including cement) for hydraulic barrier formation, and improved sorption capacity. The silica grout can be injected at surface using extremely small (potentially gravity-driven) fluid pressures, without the need for borehole drilling. Current work is investigating the erodibility of silica-grouted soils for inhibition of airborne and water-borne particulates as well as enhancing the grout's sorption capacity by addition of other materials to provide a chemical, as well as hydraulic, barrier to subsurface migration. EK remediation uses low voltage DC current to control migration of contaminants in porous media as well as to remove or degrade them. Researchers in the consortium have already demonstrated that low-energy ex-situ EK techniques can be used to provide remediation and volume minimisation for AWE legacy wastes in the UK. Under the current project researchers are building EK test cells containing simulated site materials at laboratory and intermediate(m)-scales to: remove, focus or degrade contaminants (remediation or waste minimisation); and direct subsurface water, chemical and colloid flow (fencing/containment or forced migration). This lab-based research is being informed by numerical models of EK processes that can subsequently be used to design full-scale on-site applications by nuclear site holders. Research under theme 2 of TRANSCEND will ultimately combine novel non-invasive detection technologies with EK techniques and colloidal silica grout barriers, to optimise the containment of radionuclide contamination in soils. Thus, allowing us to detect in-situ contamination, mobilise it to a selected location and grout it in-situ, prior to the initiation of decommissioning and deconstruction operations. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗