Search NASA⌕ Search

SEARCH · Search NASA

Results for “Microstructural Refinement”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 469 records · Page 26

The strong influence of Ti, Zr, Hf solutes and their oxidation on microstructure and performance of Nb 3 Sn superconductors

The strong influence of Ti, Zr, Hf solutes and their oxidation on microstructure and performance of Nb 3 Sn superconductors Over the last few years a new type of Nb 3 Sn superconducting composite based on the internal oxidation approach has emerged and has demonstrated performance significantly superior to conventional Nb 3 Sn. It requires a supply of O and the use of a Nb alloy – Nb-X, where X is a solute element that can be selectively oxidized to form oxide particles within the Nb 3 Sn. Such oxide particles not only refine Nb 3 Sn grain size, but also have the proper size to act as artificial pinning centers (APC) directly restraining fluxon motion, and thus dramatically improve superconducting properties. In this article we show that the size and volume fraction of the oxide particles determine both the levels of grain refinement and the shift in the peak field of the flux pinning force (F p -B) curve. Additionally, we explore the factors influencing these microstructure and properties, which we find include: selection of the solute element X, solute content, O content, and heat treatment. For the selection of X, we searched the periodic table for all promising candidates but focused down on the group-IVB elements (Ti, Zr, Hf) here as the drawability of Nb 3 Sn wires made from Nb-Ti, Nb-Zr, and Nb-Hf alloys has been demonstrated in the past few decades. We found that while internally oxidizing Nb-1.5at.%Ti led to negligible grain refinement and F p -B peak shift, Nb-Zr alloys led to much more dramatic results, and internally oxidizing Nb-Hf alloys led to the strongest grain refinement and F p -B peak shift. For Hf alloying in particular, we compared our internal oxidation method with another method for grain refinement, which uses Hf alloying itself without oxidation, and found that internal oxidation led to much stronger grain refinement and F p -B peak shift. We also found that higher solute content and lower reaction temperature led to stronger grain refinement and F p -B peak shift. We conclude with a discussion of the possible mechanisms for the influence of these factors.

43 PARTICLE ACCELERATORS↗

Mechanical characterization of fine-grain dispersion-strengthened tungsten as a plasma facing material

Field-Assisted Sintering Technology (FAST) was used to produce fine-grained, dispersion-strengthened tungsten (W) materials. Investigated materials 4138, 4353, and 4355 composed of 3 wt% ZrC sintered at 1800 °C, 5 wt% ZrC sintered at 1800 °C, and 3 wt% ZrC sintered at 2000 °C, respectively. They were compared against ITER-grade W. A series of mechanical and thermal property testing and microstructure studies were conducted to study them as a potential plasma facing material (PFM) for fusion reactors. Hardness testing showed that manufacturing conditions substantially altered hardness. Material 4355 had an average HV10 value of 497.2 ± 16.8, slightly higher than ITER-grade at 378.5 ± 40.3. However, material 4353 was substantially higher with an HV10 value of 738.9 ± 31.7 over the investigated temperature range. Electron Backscatter Diffraction (EBSD) analysis showed that FAST produced substantially smaller grains than the hot-rolled ITER-grade W material, offering notable control over grain size. Materials 4353 and 4355 had grain sizes of 0.44 ± 0.20 µm and 3.67 ± 0.89 µm, respectively, whereas ITER-grade 27.14 ± 19.76 µm at room temperature. The fine grain structures showed no net coarsening after 1 hr. anneals up to 1800 °C, several hundred degrees above the 1100 – 1500 °C recrystallization range reported for conventional W. Inverse application of the Zener pinning relationship to the measured grain sizes indicates that these two FAST sintering conditions produce markedly different effective dispersoid populations, with effective particle diameters of approximately 90 nm at a peak sintering temperature of 1800 °C and approximately 460 nm at 2000 °C, respectively. This result demonstrates that the FAST thermal condition itself, and not the nominal ZrC content alone, governs the pinning effectiveness of the dispersion. Thermal diffusivity measurements support this finding independently. Materials of identical composition sintered at different temperatures differ by approximately 19% in measured thermal diffusivity with statistically indistinguishable density, while materials of different composition and sintering temperature converge to within approximately 2%. At a representative divertor heat flux of 10 MW/m², the lower thermal conductivity of the fine-grained materials corresponds to approximately 28 to 33 °C per millimeter of armor thickness relative to ITER-grade W, traded against a substantially larger margin to recrystallization-driven degradation. While high temperature tensile testing revealed likely contamination that motivates refinement of the manufacturing process, FAST-produced, fine-grained, dispersion-strengthened W offers process-controlled microstructural stability well above the operating temperatures of conventional W and supports its continued development as a PFM for economically viable commercial fusion power.

Parker, Gabe [ORNL] (ORCID:0000000190394100)↗

Improvement of high-frequency characteristics of Z-type hexaferrite by dysprosium doping

Z-type hexaferrite has great potential applications as anti-EMI material for magnetic devices in the GHz region. In this work, Dy-doped Z-type hexaferrites with nominal stoichiometry of Ba{sub 3}Co{sub 2}Dy{sub x}Fe{sub 24-x}O{sub 41} (x 0.0, 0.05, 0.5, 1.0) were prepared by an improved solid-state reaction method. The effects of rare earth oxide (Dy{sub 2}O{sub 3}) addition on the phase composition, microstructure and electromagnetic properties of the ceramics were investigated. Structure and micromorphology characterizations indicate that certain content of Dy doping will cause the emergence of the second phase Dy{sub 3}Fe{sub 5}O{sub 12} at the grain boundaries of the majority phase Z-type hexaferrite, due to which the straightforward result is the grain refinement during the successive sintering process. Permeability spectra measurements show that the initial permeability reaches its maximum of 17 at 300 MHz with x = 0.5, while the cutoff frequency keeps above 800 MHz. The apparent specific anisotropy field H{sub K} of Dy-doped Z-type hexaferrites decreases with x increasing. The relationships among phase composition, grain size, permeability spectra, and anisotropy are theoretically investigated, and according to the analysis, Dy doping effects on its magnetic properties can be well explained and understood.

36 MATERIALS SCIENCE↗

Effect of Nb micro-alloying on microstructure and properties of thermo-mechanically processed high carbon pearlitic steel

Highlights: • Effect of Nb micro-alloying on high carbon steels has been established. • Fine and degenerated pearlite with fine PAGS is achieved due to Nb micro-alloying. • AFM study indicates true interlamellar spacing which conforms well to TEM study. • Hardness and yield strength have been obviously improved with the addition of Nb. - Abstract: Two C-Mn-Si steels with and without Nb micro-alloying are selected in the present study. Both these high carbon steels have been thermo-mechanically processed using Gleeble 3800 simulator. Optical microscope (OM), scanning electron microscope (SEM), transmission electron microscope (TEM), atomic force microscope (AFM) were utilised for microstructural characterisation. The austenitising temperature was varied from 1150 °C to 1200 °C followed by hot compression and subjected to free cooling to evaluate the influence of austenite grain size on transformed microstructure and mechanical properties. It is evident that higher austenite grain size is obtained for both types of steels subjected to higher austenitising temperature. The refinement of pearlite interlamellar spacing (<0.20 μm) with degenerated morphology as well as finer prior austenite grain size (<40 μm) is found to be more prominent for Nb micro-alloyed sample. The average hardness values of both the steels are higher for the specimens, treated at a higher austenitising temperature which is attributed to finer interlamellar spacing. Finally, the correlation between the evolving microstructure and resulting mechanical properties (hardness and yield strength) has been made.

36 MATERIALS SCIENCE↗

Tailoring mechanical properties of a multi-principal element alloy through a multi-length-scale approach

In this study, a multi-length-scale strengthening approach was used to tailor the microstructure and the mechanical properties of a NiCoCr-based multi-principal element alloy (MPEA). Grain size refinement, severe lattice distortion, and stacking fault energy (SFE) reduction with Mo addition (up to 10 at.%) enhance yield strength by 85% with only 10% reduction in ductility in as-annealed MPEAs. A pronounced increase in the strain hardening rate was observed with the addition of Mo, which is ascribed to the promotion of complex stacking fault (SF) interaction and intersection, accompanied by Lomer-Cottrell (L-C) and Hirth locks inhibiting dislocation motion and substantial increase in the accumulation of back stress. To push the limit of the yield strength further, the Suzuki segregation phenomenon was manipulated by a careful control of SF density by pre-straining and a subsequent 500 °C heat treatment. The stress-strain responses of the pre-strained and heat treated MPEAs showed an obvious SF density and Mo concentration dependence. Furthermore, the yield strength of the pre-strained Mo-added MPEAs with subsequent heat treatment was increased up to true stress of 2.3 GPa with a corresponding fracture elongation of 12% true strain. SFs formed during pre-straining served as Cr segregation sites during subsequent heat treatment, which substantially varies the local SFE within the SF, presenting a roughened landscape and frustrating the dislocation dynamics.

mechanical properties↗

An innovative and alternative approach toward gear fabrication

In this paper, we present the first demonstration of single-step gear manufacturing via an innovative in-situ friction stir forging approach. This novel process is a natural extension to the friction stir processing technique and relies on shear and normal stresses to form the complex shapes. Friction stir welding pin tool with shoulder is plunged at high revolutions per minute (rpm) into the sample to heat it to the desired temperature and enable plastic flow. Then, the tool is forged at high plunge rate to form the desired structurally-sound and defect free complex shapes. To better visualize the process the experiments are complemented by a 3D thermomechanically coupled, smoothed particle hydrodynamics (SPH) model to understand the material flow pattern both radially and through thickness in the gear teeth, plastic strain distribution, and temperature profile. We have demonstrated application of I-FSF to inherently poor formable AZ31 Mg, AA 7075-T6, and AA5083–10 vol% TiB 2 composite and fabricated 14-tooth spur gears from these materials with minimal farther machining. In conclusion, microstructure of the forged gears exhibited a directional material flow pattern due to the normal forging action and refinement of grains to 6–13 μm through dynamically recrystallization across the radial, through-thickness direction, which is in good agreement with the corresponding SPH simulation results.

42 ENGINEERING↗

Microstructure and nanohardness distribution in a polycrystalline Zn deformed by high strain rate impact

Polycrystalline Zn with an average grain size of about 300 {mu}m was deformed by direct impact Hopkinson pressure bar at a velocity of 29 m/s. An inhomogeneous grain structure was found consisting of a center region having large average grain size of 20 {mu}m surrounded by a fine-grained rim with an average grain size of 6 {mu}m. Transmission electron microscopy investigations showed a significant dislocation density in the large-grained area while in the fine-grained rim the dislocation density was negligible. Most probably, the higher strain yielded recrystallization in the outer ring while in the center only recovery occurred. The hardening effect of dislocations overwhelms the smaller grain size strengthening in the center part resulting in higher nanohardness in this region than in the outer ring. - Graphical Abstract: (a): EBSD micrograph showing the initial microstructure of polycrystalline Zn that was subsequently submitted to high strain rate impact. (b): an inhomogeneous grain size refinement was obtained which consists of a central coarse-grained area, surrounded by a fine-grained recrystallized rim. The black arrow points to the disc center. Research Highlights: {yields} A polycrystalline Zn specimen was submitted to high strain rate impact loading. {yields} Inhomogeneous grain refinement occurred due to strain gradient in impacted sample. {yields} A fine-grained recrystallized rim surrounded the coarse-grained center of specimen. {yields} The coarse-grained center exhibited higher hardness than the fine-grained rim. {yields} The higher hardness of the center was caused by the higher dislocation density.

36 MATERIALS SCIENCE↗

Structural characteristics and gasification reactivity of chars prepared from K{sub 2}CO{sub 3} mixed HyperCoals and coals

HyperCoal is a clean coal with mineral matter content <0.05 wt %. Oaky Creek (C = 82%), and Pasir (C = 68%) coals were subjected to solvent extraction method to prepare Oaky Creek HyperCoal, and Pasir HyperCoal. Experiments were carried out to compare the gasification reactivity of HyperCoals and parent raw coals with 20, 40, 50 and 60% K{sub 2}CO{sub 3} as a catalyst at 600, 650, 700, and 775{sup o}C with steam. Gasification rates of coals and HyperCoals were strongly influenced by the temperature and catalyst loading. Catalytic steam gasification of HyperCoal chars was found to be chemical reaction controlled in the 600-700{sup o}C temperature range for all catalyst loadings. Gasification rates of HyperCoal chars were found to be always higher than parent coals at any given temperature for all catalyst loadings. However, X-ray diffraction results showed that the microstructures of chars prepared from coals and HyperCoals were similar. Results from nuclear magnetic resonance spectroscopy show no significant difference between the chemical compositions of the chars. Significant differences were observed from scanning electron microscopy images, which showed that the chars from HyperCoals had coral-reef like structures whereas dense chars were observed for coals. 26 refs., 8 figs., 2 tabs.

01 COAL, LIGNITE, AND PEAT↗

Electromagnetic levitation containerless processing of metallic materials in microgravity: rapid solidification

Space levitation processing allows researchers to conduct benchmark tests in an effort to understand the physical phenomena involved in rapid solidification processing, including alloy thermodynamics, nucleation and growth, heat and mass transfer, solid/liquid interface dynamics, macro- and microstructural evolution, and defect formation. Supported by ground-based investigations, a major thrust is to develop and refine robust computational tools based on theoretical and applied approaches. This work is accomplished in conjunction with experiments designed for precise model validation with application to a broad range of industrial processes.

42 ENGINEERING↗

In situ synchrotron diffraction and modeling of non-equilibrium solidification of a MnFeCoNiCu alloy

The solidification mechanism and segregation behavior of laser-melted Mn 35 Fe 5 Co 20 Ni 20 Cu 20 was firstly investigated via in situ synchrotron x-ray diffraction at millisecond temporal resolution. The transient composition evolution of the random solid solution during sequential solidification of dendritic and interdendritic regions complicates the analysis of synchrotron diffraction data via any single conventional tool, such as Rietveld refinement. Therefore, a novel approach combining a hard-sphere approximation model, thermodynamic simulation, thermal expansion measurement and microstructural characterization was developed to assist in a fundamental understanding of the evolution of local composition, lattice parameter, and dendrite volume fraction corresponding to the diffraction data. This methodology yields self-consistent results across different methods. Via this approach, four distinct stages were identified, including: (I) FCC dendrite solidification, (II) solidification of FCC interdendritic region, (III) solid-state interdiffusion and (IV) final cooling with marginal diffusion. It was found out that in Stage I, Cu and Mn were rejected into liquid as Mn 35 Fe 5 Co 20 Ni 20 Cu 20 solidified dendritically. During Stage II, the lattice parameter disparity between dendrite and interdendritic region escalated as Cu and Mn continued segregating into the interdendritic region. After complete solidification, during Stage III, the lattice parameter disparity gradually decreases, demonstrating a degree of composition homogenization. The volume fraction of dendrites slightly grew from 58.3 to 65.5%, based on the evolving composition profile across a dendrite/interdendritic interface in diffusion calculations. Postmortem metallography further confirmed that dendrites have a volume fraction of 64.7 ± 5.3% in the final microstructure.

36 MATERIALS SCIENCE↗

Interactive microstructural phenomena during non-isothermal annealing of an Al-Mg-Si-Cu alloy

Highlights: • A non-isothermal annealing process that is concurrent with precipitation is investigated. • The mechanism of grain refinement through the interactions of precipitation, recovery and recrystallization is identified. • The combination of non-isothermal annealing and proper pre-deformation temper condition tetrads recovery. • Massive recrystallization nucleation is achieved by delaying recovery. • The growth of recrystallized grains is controlled by coarsening of precipitates that pin the grain boundaries. - Abstract: Interactions between precipitation, recovery and recrystallization during a non-isothermal annealing process in an Al-Mg-Si-Cu alloy have been investigated through a comprehensive experimental analysis. Non-isothermal annealing with a slow heating rate that starts from a low temperature is found to promote homogeneous nucleation of precipitates. The uniformly distributed precipitates limit the extent of recovery, which in turn facilitates extensive nucleation of new grains within the deformed microstructure. The growth of the recrystallized grains is strongly controlled through pinning of grain boundaries by precipitates. During the final stages of annealing, enhanced diffusion at the recrystallization front leads to preferential precipitate coarsening, release of grain boundaries from precipitates pinning, and completion of recrystallization. These interactive microstructural phenomena explain the effectiveness of a non-isothermal annealing route combined with an adequate level of deformation in obtaining a fine-grained recrystallized structure.

36 MATERIALS SCIENCE↗

Ferrite grain refinement in low carbon Cu–P–Cr–Ni–Mo weathering steel at various temperatures in the (α + γ) region

Self-designed Cu–P–Cr–Ni–Mo weathering steel was subjected to compression test to determine the mechanism of ferrite grain refinement from 750 °C to 925 °C. Optical microscopic images showed that ferrite grain size declined, whereas the ferrite volume fraction increased with increasing compression temperature. Electron backscatter diffraction patterns revealed that several low-angle boundaries shifted to high-angle boundaries, thereby generating fine ferrite grains surrounded by high-angle boundaries. Numerous low-angle boundaries were observed within ferrite grains at 750 °C, which indicated the existence of pre-eutectoid ferrite. Results showed that ferrite grain refinement could be due to continuous dynamic recrystallization at 750 °C and 775 °C, and deformation-induced ferrite transformation could be the main mechanism at 800 °C and 850 °C. Fine equiaxed ferrite grains with size ranging from 1.77 μm to 2.69 μm were produced in the (α + γ) dual-phase region. - Graphical abstract: There is a close relationship between the microstructure evolution and flow curves during deformation. Fine equiaxed ferrite grains with size ranging from 1.77 μm to 2.69 μm were achieved in the (α + γ) dual-phase region. Ferrite grain refinement could be due to continuous dynamic recrystallization at 750 °C and 775 °C, and deformation-induced ferrite transformation at 800 °C and 850 °C. The occurrence of deformation-induced ferrite transformation and continuous dynamic recrystallization can be monitored by analysis of flow curves and microstructures. Deformation-induced ferrite transformation leads to the dynamic softening in flow curve when temperature just below A{sub r3}, while the dynamic softening in flow curve is ferrite continuous dynamic recrystallization (Special Fig. 5b). - Highlights: • Compression deformation was operated at temperatures from 750 °C to 925 °C at a strain rate of 0.1 s–1, and a strain of 1.2. • Fine equiaxed ferrite grains of ~1.77–2.19 μm were obtained at 750 °C and 775 °C via continuous dynamic recrystallization. • Ferrite grain size of ~2.31–2.69 μm at 800 °C and 850 °C can be obtained by deformation-induced ferrite transformation. • With decreasing deformation temperature the average grain size of ferrite decreased while volume fraction increased. • Ferrite refinement was from deformation-induced ferrite to continuous dynamic recrystallization as temperature reduced.

36 MATERIALS SCIENCE↗

Processing, As-Cast Microstructure and Wear Characteristics of a Monotectic Al-Bi-Cu Alloy

Ternary Al-based monotectic alloys have a good combination of wear resistance and mechanical strength. While self-lubricating soft elements guarantee an adequate wear resistance, the modification with third elements can increase the ability to support load. In the present investigation, a collection of microstructures is generated through transient directional solidification of the Al-3.2wt.%Bi-3.0wt.%Cu alloy. Samples with different Bi spacing have been subjected to micro-adhesive wear ball tests. A relationship linking the wear volume, V, the microstructural spacing and the test time is proposed for Bi spacing higher than 16 μm, according to which V decreases with the decrease in Bi spacing. It is observed that wider and deeper grooves emerged on the surface of the samples related to more refined Bi and Al{sub 2}Cu phases, that is, associated with Bi spacing and Bi diameter lower than 16 and 2.4 μm, respectively. A reverse trend is noted for these finer microstructures, for which V increases with further decrease in Bi spacing. This can be caused by the detachment of the very fine and less cohesive Al{sub 2}Cu lamellas as the Al{sub 2}O{sub 3} oxide breaks up forming debris, with the presence of these lamellas as loose debris at the interface acting as third-body abrasives.

36 MATERIALS SCIENCE↗

Effect of Heating Rate during Continuous Annealing on Microstructure and Mechanical Properties of High-Strength Dual-Phase Steel

The study concerns the influence of heating rate during continuous annealing on microstructure and mechanical properties of high-strength ferrite–martensite dual-phase (DP) steel. The study suggests that the superheat (ΔT), carbon diffusion and distribution were strongly influenced by increasing the heating rate, leading to different microstructure and mechanical properties of DP steel. The morphology of martensite was observed to shift from network along ferrite grain boundaries to banded structure to uniformly dispersed, and the average ferrite grain size was refined from 5.3 to 2.0 µm. When the heating rate was 300 °C/s, the steel exhibited excellent mechanical properties with tensile strength (UTS) of 982 MPa, total elongation (TEL) of 17.5%, strength–elongation balance (UTS × TEL) of 17.2 GPa%, because of finer microstructure, uniform martensite distribution and low carbon content of martensite. Moreover, the precipitation strengthening effect of NbC is an important reason for the high-strength DP steels. In addition, the variation in strain-hardening behavior and fracture mechanism of steel subjected to different heating rates is discussed in relation to the microstructure.

36 MATERIALS SCIENCE↗

In Vitro Degradation, Antibacterial Activity and Cytotoxicity of Mg-3Zn-xAg Nanocomposites Synthesized by Mechanical Alloying for Implant Applications

A class of biodegradable Mg-3Zn-xAg nanocomposites was presented in the present study with the assessments for implant application. The evaluations included the effects of increasing the Ag content from 0.5 to 3 wt.% on the corrosion behavior, mechanical properties, antibacterial activity and cytotoxicity of Mg-3Zn-xAg nanocomposite. Microstructural analysis revealed the secondary phase intermetallic Mg{sub 54}Ag{sub 17} along the grain boundaries, with grain refinement as a result of increasing the Ag concentration. 0.5 wt.% Ag results in increasing the compressive strength and elongation; however, further addition decreases the compressive strength. The nanocomposite samples were verified for the improved antimicrobial activity by utilizing both E. coli and S. aureus bacteria, the growth of which was suppressed around all Ag-containing nanocomposites, whereas bacterial proliferations were detected around the Mg-3Zn nanocomposite. The escalating levels of Ag in the nanocomposite resulted in the elevated antimicrobial effect. Cell adhesion and proliferation were not significantly influenced by the inclusion of 0.5-1 wt% Ag into Mg-3Zn nanocomposite; however, cell adhesion and proliferation were lower on the surfaces of the nanocomposite containing 2-3 wt.% Ag counterparts. According to the mechanical, corrosion and biological assessments in the current research, it can be concluded that the nanocomposite containing 0.5 wt.% Ag can be properly applied as an orthopedic implant biomaterial.

36 MATERIALS SCIENCE↗

Low-Cost Production of Lithium-Ion Separator Membranes w/ Improved Safety

The purpose of this Cooperative Research and Development Agreement (CRADA) between Oak Ridge National Laboratory (ORNL) and Porous Power Technologies, LLC (PPT) was to validate the performance, durability, and safety of a new type of reinforced, composite lithium ion battery separator produced as either a free-standing product or by a method of direct coating after electrode fabrication. ORNL’s primary roles were to develop novel separator thermophysical and mechanical property characterization methods and assist with fundamental understanding of SYMMETRIX® HPX and HPX-F product line chemical makeup and microstructure. PPT’s primary roles were to implement the understanding gained from the ORNL developed characterization methods into a refined product line featuring nonwoven-reinforced, ceramic-filled composite HPX-F separators for the lithium ion battery industry and quantify long-term cell performance improvements associated with HPX-F separators. Over the course of this CRADA, the product line of PPT was expanded from a pure polyvinylidene fluoride (PVDF) HP and polyester nonwoven-reinforced HPX separator platform to one that includes a variety of ceramic-filled HPX-F separators. In addition, the laminating and direct coating technologies for HPX and HPX-F separators are now more developed and moving towards commercial licensing. PPT’s SYMMETRIX® production process will revolutionize the production of lithium ion batteries by eliminating one of the most expensive components (the free-standing separator membrane) while improving performance and safety. The performance and safety improvements are due primarily to replacement of the conventional polyethylene/polypropylene (PE/PP) separator material with polyvinylidene fluoride (PVDF), and to ceramic materials added to the PVDF to form a short-resistant, thermally-stable composite structure. Ultimately, lithium ion battery manufacturers will be able to produce PPT separators in-house through the laminating or direct coating methods such as those based on the SYMMETRIX® product line, giving them higher performance cells at a fraction of the cost required to purchase separators from existing vendors. Direct coating of separators onto electrodes eliminates the cost of a downstream thermal lamination step and requires little or no change to existing equipment. It is a clear path for lithium ion battery manufacturers to reach the <$1/m2 separator price target set by the U.S. Advanced Battery Consortium (USABC). The technology enabled by this project will have a substantial impact on energy efficiency required to produce cells and is anticipated to save up to $1B annually by 2014 in reduced manufacturing costs. In addition, it will contribute significantly to production energy savings associated with transporting free-standing polyolefin (PE/PP) separators from the vendor to the cell manufacturer locations. SYMMETRIX® separators have shown increased cell capacity, improved thermal stability, and longer cycle life over their PE/PP counterparts and have been repeatedly demonstrated to improve nearly all aspects of lithium ion battery performance Prior to the start of this CRADA, widespread adoption has been limited by three factors: 1) difficulty in handling the material on high-speed processing equipment due to lower tensile strength than oriented PE/PP materials; 2) cost concerns associated with the higher expense of PVDF as a raw material; and 3) questions regarding short resistance and durability. The first factor was addressed through thorough mechanical (ultimate tensile strength and dynamic mechanical analysis, etc.) property characterization of HPX and HPX-F materials against the commercial polyolefin baselines. The second factor was address by shifting the focus of PPT’s product line towards the HPX-F materials with low-PVDF (high ceramic filler) content to reduce overall separator cost. Concerns associated with the third factor were alleviated by evaluating the internal shorting resistance of the separators using a custom developed ORNL measurement method and obtaining long-term cycling data of the new HPX-F separator formulations. A materials emphasis was placed on polyester fiber mats for the nonwoven reinforcement (to boost overall separator tensile strength) and proprietary metal oxides for the HPX-F fillers (to improve thermomechanical properties of the separator and make it more resistant to overcharge and internal shorting).

batteries↗

Laser Weld Geometry and Microstructure of Cast Uranium-6 wt% Niobium Alloy

Laser welding was performed on a U6 wt% Nb uranium alloy using a 400W solid state laser with welding speeds from 20 to 2,500 mm/s. This speed range spanned melt pool sizes from traditional welding to surface modification and additive manufacturing. With increasing scan speed, the ratio of weld length relative to depth and width increased, with melt pool lengths being more than 5x greater than the width and 10x greater than the depth at the highest speeds. Keyhole mode welds were shown to occur at low speeds, while conduction mode welds occurred at 700 mm/s or higher as the weld depth dropped off more rapidly than width at higher speeds. Microstructures that form at the boundary between the fusion zone and base metal were observed to have a nonconventional appearance consisting of interpenetrating dark and light contrast phases before cells or dendrites appear. Dendrites with secondary arms form from this boundary in keyhole welds and refine to no visible secondary arms near the weld center. Primary and secondary dendrite arms, where present, were shown to refine in size inversely with cooling rate raised to the 0.465 and 0.376 powers respectively. Dendrites were largely absent from the conduction mode welds at higher speeds, and were replaced by a banded microstructure, that appears to form by an oscillatory solidification front mechanism.

36 MATERIALS SCIENCE↗