At least 469 records · Page 26

Phase Evolution and Mechanical Properties of AlCoCrFeNiSi{sub x} High-Entropy Alloys Synthesized by Mechanical Alloying and Spark Plasma Sintering

In the current investigation, AlCoCrFeNiSi{sub x} (x = 0, 0.3, 0.6 and 0.9 in atomic ratio) high-entropy alloy systems are prepared by mechanical alloying and subsequently consolidated by spark plasma sintering. The microstructural and mechanical properties were analyzed to understand the effect of Si addition in AlCoCrFeNi alloy. The x-ray diffraction analysis reveals the supersaturated solid solution of the body-centered cubic structure after 20 h of ball milling. However, the consolidation promotes the transformation of body-centered phases partially into the face-centered cubic structure and sigma phases. A recently proposed geometric model based on the atomic stress theory has been extended for the first time to classify single phase and multi-phases on the high-entropy alloys prepared by mechanical alloying and spark plasma sintering process. Improved microhardness and better wear resistance were achieved as the Si content increased from 0 to 0.9 in the present high-entropy alloy.

36 MATERIALS SCIENCE↗

Sliding Wear of Spark Plasma Sintered CrFeCoNiCu High-Entropy Alloy Coatings: Effect of Aluminum Addition

High-entropy alloys (HEAs) are considered as attractive coating materials due to their high hardness, good wear and corrosion resistance. Al{sub x}CrFeCoNiCu (x = 0, 1, 2, 3) high-entropy alloy coatings were fabricated on carbon steel substrate using spark plasma sintering. The microstructure evolved from FCC to FCC–BCC mixed structure. Al{sub 3}CrFeCoNiCu coating possesses an average hardness of approximately 682 HV{sub 0.2}, which is the highest hardness in all of the HEA coatings. The dry sliding wear behavior of the HEA coatings was investigated using a ball-on-disk sliding tribo-meter with a silicon nitride ball. In all of the HEA coatings, Al{sub 3}CrFeCoNiCu presents the lowest wear rate 8.81 × 10{sup −5} mm{sup 3} m{sup −1} and Al{sub 2}CrFeCoNiCu has the lowest coefficient of friction 0.195 during 1000 m sliding distance at 0.1 m s{sup −1} sliding velocity under 20 N normal load. Comparing with AISI 52100 steel, spark plasma sintered Al{sub 2}CrFeCoNiCu and Al{sub 3}CrFeCoNiCu HEA coatings exhibit outstanding sliding wear resistance and extremely low friction coefficient. The wear resistance of Al{sub 3}CrFeCoNiCu HEA coating is approximately four times better than the bearing steel, showing a promising application as a wear-resistant material.

36 MATERIALS SCIENCE↗

Effect of Strain Rate on the Plastic Deformation and Fracture of 90W-7Ni-3Fe Alloy Prepared by Liquid-Phase Sintering

In this study, the effect of the strain rates on the plastic deformation behavior and fracture mechanism of 90W-7Ni-3Fe heavy alloy prepared by liquid-phase sintering was investigated. Stress–strain tests were carried out in tensile and compression under quasi-static condition with the strain rate ranging from 10{sup −3} to 1 s{sup −1}. Dynamic test was examined using a compression split Hopkinson bar at strain rates ranging from 1000 to 1700 s{sup −1} in order to evaluate the effects of high strain rate on dynamic plastic deformation behavior. Quasi-static tests results show that the strength and hardness of this alloy increase with increasing strain rate. Results indicate that the as-sintered 90W-7Ni-3Fe heavy alloy has obvious strain-hardening characteristic under tensile or compression deformation under quasi-static condition. At this time, strain hardening is the main factor. Nevertheless, strain-hardening and strain-softening behaviors of the specimens occur simultaneously under dynamic compression condition. The effect of compressive stress on the work hardening is more obvious. A strong relevance of work-hardening effect on strain rate is also found. And the fracture mode of quasi-static and dynamic compression samples is also different.

36 MATERIALS SCIENCE↗

Large-scale production of (GeTe) x (AgSbTe 2 ) 100$-$x (x=75, 80, 85, 90) with enhanced thermoelectric properties via gas-atomization and spark plasma sintering

(GeTe) x (AgSbTe 2 ) 100$-$x : TAGS thermoelectrics are an attractive class of materials due to their combination of non-toxicity and good conversion efficiency at mid-temperature ranges. Here in the present work, we have utilized energy and time efficient high-pressure gas atomization and spark-plasma sintering techniques for large-scale preparation of samples with varying composition (i.e., (GeTe) x (AgSbTe 2 ) 100$-$x where x = 75, 80, 85, and 90). High-temperature x-ray diffraction was used to understand the phase transformation mechanism of the as-atomized powders. Detailed high-resolution transmission electron microscopy of the sintered samples revealed the presence of nanoscale precipitates, antiphase, and twin boundaries. The nanoscale twins and antiphase boundaries serve as phonon scattering centers, leading to the reduction of total thermal conductivity in TAGS-80 and 90 samples. The maximum ZT obtained was 1.56 at 623 K for TAGS-90, which was ~94% improvement compared to values previously reported. The presence of the twin boundaries also resulted in a high fracture toughness (K IC ) of the TAGS-90 sample due to inhibition of dislocation movement at the twin boundary.

36 MATERIALS SCIENCE↗

Sintering inhibition enables hierarchical porosity with extreme resistance to degradation during redox cycling of Fe-Mo foams

High-temperature (800 ºC) steam-hydrogen redox cycling, relevant to grid-scale energy storage, is studied for iron-based freeze-cast lamellar foams. In contrast to previously studied Fe, Fe-Ni, and Fe-Co foams that rapidly degrade, Fe-25Mo foams feature a much-enhanced structural damage resistance. Utilizing in-situ x-ray diffraction, microscopy, and x-ray tomography, strong sintering inhibition is observed in Fe-Mo foams, creating a hierarchically porous lamellar structure. This leads to (i) wide channels between lamellae, enabling high macroscopic porosity (~78%) which can accommodate gas flow as well as volumetric expansion without lamellar contact, and (ii) microporosity within lamellae, providing additional free volume to accommodate expansion during oxidation, limiting both swelling of the lamellae and the formation of Kirkendall pores. Finally, these combined effects enable a near-complete reversibility of the microstructure during cycling, preventing damage produced via internal lamellar buckling, cracking, contacting and sintering, with a remarkably high porosity (65%) remaining after 50 consecutive redox cycles.

36 MATERIALS SCIENCE↗

Influence of strontium on structure, sintering and biodegradation behaviour of CaO-MgO-SrO-SiO2-P2O5-CaF2 glasses

The present study investigates the influence of SrO on structure, apatite forming ability, physico-chemical degradation and sintering behaviour of melt-quenched bioactive glasses with composition: mol.% (36.07 – x) CaO – x SrO - 19.24 MgO – 5.61 P2O5 – 38.49 SiO2 – 0.59 CaF2, where x varies between 0 – 10. The detailed structural analysis of glasses has been made by infra red spectroscopy (FTIR) and magic angle spinning-nuclear magnetic resonance spectroscopy (MAS-NMR). Silicon was predominantly present as Q2 (Si) species while phosphorus was found in orthophosphate type environment in all the investigated glasses. The apatite forming ability of glasses was investigated by immersion of glass powders in simulated body fluid (SBF) for time durations varying between 1 h – 7 days. While increasing Sr2+/Ca2+ ratio in glasses did not affect the structure of glasses significantly, their apatite forming ability was decreased considerably. Further, physico-chemical degradation of glasses has been studied in accordance with ISO 10993-14 “Biological evaluation of medical devices – Part 14: Identification and quantification of degradation products from ceramics” in Tris HCl and citric acid buffer and the possible implications of ion release profile from glasses in different solutions has been discussed. The addition of strontium in glasses led to a 7-fold decrease in chemical degradation of glasses in Tris-HCl. The sintering of glass powders rendered glass-ceramics (GCs) with varying degree of crystallinity and good flexural strength (98-131 MPa) where the mechanical properties depend on the nature and amount of crystalline phases present in GCs.

58 GEOSCIENCES↗

Inkless, dry printing nanographene via in-Situ Coordinated laser ablation and sintering processes

Printing carbon, such as graphene and other carbon structures, for flexible and printed electronics currently relies on either ink-based printing, laser-induced forward transfer (LIFT), or laser-induced graphitization (LIG) to convert carbon-rich precursor materials, such as polymers, to graphene-like carbon structures. Liquid inks contain toxic solvents, surfactants, and stabilizing additives that degrade electrical conductivity and require high-temperature post-processing. On the other hand, LIG is limited by the substrate. Here, this study introduces an additive manufacturing method for dry-printing carbon nanomaterials, ranging from amorphous carbon to crystalline graphene-like structures, on various substrates. The system utilizes laser ablation of a solid graphite target to create pure carbon nanoparticles in situ and on demand. An inert gas carries the nanoparticles onto the substrate, where they can be deposited either as amorphous structures or laser-sintered in real time to form various graphitic structures. The study of laser processing parameters, specifically fluence and pulse repetition frequency, revealed three unique regimes of nanostructure evolution that influence the morphological and electrical properties of these printed structures. Raman spectroscopy confirmed graphitization with a resistivity slightly higher than that of the bulk graphite target. The conductivity/resistivity could be tuned as a function of sintering laser power. Scanning transmission electron microscopy (STEM) revealed that turbostratic nanographene formed with an interlayer spacing of 0.40 nm. Despite ink-based printing methods, such as screen printing, inkjet printing (IJP), and aerosol jet printing (AJP), this eco-friendly and green manufacturing technique could eliminate toxic chemicals, reduce environmental impact, and enable single-step fabrication of carbon-based devices for applications in wearable sensors, energy storage, flexible electronics, and Internet of Things (IoT) devices.

Additive nanomanufacturing↗

Coarse-grained computation for particle coagulation and sintering processes by linking Quadrature Method of Moments with Monte-Carlo

The study of particle coagulation and sintering processes is important in a variety of research studies ranging from cell fusion and dust motion to aerosol formation applications. These processes are traditionally simulated using either Monte-Carlo methods or integro-differential equations for particle number density functions. In this paper, we present a computational technique for cases where we believe that accurate closed evolution equations for a finite number of moments of the density function exist in principle, but are not explicitly available. The so-called equation-free computational framework is then employed to numerically obtain the solution of these unavailable closed moment equations by exploiting (through intelligent design of computational experiments) the corresponding fine-scale (here, Monte-Carlo) simulation. We illustrate the use of this method by accelerating the computation of evolving moments of uni- and bivariate particle coagulation and sintering through short simulation bursts of a constant-number Monte-Carlo scheme.

97 MATHEMATICS AND COMPUTING↗

Reaction-bond composite synthesis of SiC-TiB 2 by spark plasma sintering/field-assisted sintering technology (SPS/FAST)

High-density SiC-TiB 2 composites were fabricated using the displacement reaction spark plasma sintering/field-assisted sintering technology (SPS/FAST) and SiC, B 4 C, TiC, and Si powders. The reaction process was performed in a narrow time frame compared hot pressing. The SiC-TiB 2 composites were sintered with precursor SiC at various pressures to determine the effects of processing with SPS/FAST. The composites completed synthesis during SPS/FAST processing, which occurs more quickly than hot pressing. SEM, STEM, and Raman spectroscopy are used to show the conversion and microstructure. Finally, the composite of 53.6 wt.% SiC and 46.4 wt.% TiB 2 has 99 % theoretical density, hardness of 26.4 GPa, and fracture toughness of 5.12 MPa m 1/2 .

36 MATERIALS SCIENCE↗

Reactive flash sintering of TiZrN and TiAlN ternary metal nitrides

Here, this study demonstrated the reactive flash sintering (RFS) for two powder mixtures: TiN-ZrN (both conducting) and AlN-TiN (TiN conducting but AlN insulating), targeting ternary metal nitrides (TMN) of Ti 0.5 Zr 0.5 N and Ti 0.5 Al 0.5 N, respectively. A constant volage and pressure (e.g., 8 V DC, ∼15 MPa) at room temperature triggered the flash (current density up to 27 A/mm 2 ) without pre-heating, and the entire RFS process finished in a few minutes. For TiZrN, the flash was instantaneous whereas for TiAlN, there was a long incubation before the flash followed by a quick and dramatic flash. Both conventional ex situ XRD and in situ synchrotron study had been carried out. They showed a uniform Ti 0.57 Zr 0.43 N solution formed in RFS and persisted upon cooling, while (Ti, Al) N solid solution formed at high temperature was not stable and likely went through a very quick phase separation in the cooling process. The final products from RFS had been characterized using SEM/EDS for microstructure. Both TiZrN and TiAlN were dense. Distribution of Ti, Zr, and N was uniform for TiZrN; for TiAlN, Ti and N distribution was uniform, while association of Al with oxygen was observed. TGA-DSC revealed the onset oxidation temperature for TiZrN was comparable to TiN and ZrN, while it was higher by ∼200 °C for TiAlN, likely due to the formation of Al 2 O 3 . In terms of mechanical properties such as hardness or fracture toughness, forming a single-phase solid solution (like TiZrN) does not offer obvious benefits. while large grain size from RFS seemed to be unfavorable. Future optimization of RFS condition and in-depth study by both experiments and simulation are needed to fully understand the composition-processing-structure-property relationships for such TMN from the reactive flash sintering process.

Flash Sintering↗

Toughening Sm–Co sintered magnets via microstructure modification with additives

We report the mechanical properties of the brittle Smsingle bondCo permanent magnets are of great practical significance. However, studies on the magnets have mostly focused on their magnetic properties. This paper reports the modified microstructure and refined unimodal grain size, enhanced flexural strength, and magnetic properties of Sm 2 (Co,Fe,Cu,Zr) 17 sintered magnets doped with La 2 O 3 , MgO, and CaF 2 fine particulates. The correlations between microstructure, phase composition, and mechanical and magnetic properties were studied. Doping of a small amount (e.g., 0.5–3 wt%) of La 2 O 3 , MgO, or CaF 2 fine particulates could significantly refine the unimodal grain sizes of the Smsingle bondCo magnets via the Zener pinning effect. Moreover, doping significantly improved the flexural strengths σ of the magnets. For example, the σ values of the magnets with 0.5 wt% MgO, 1 wt% La 2 O 3 , and 1 wt% CaF 2 were approximately 65%, 63%, and 42% higher than that of the reference magnet, respectively. Micromechanical simulations revealed that the fine particles of La 2 O 3 could deflect crack growth, while the CaF 2 particles could attract or arrest cracks during the fracture process. The mechanical strengthening effect was mainly due to grain size refinement. The Smsingle bondCo magnets with 0.5–1.5 wt% CaF2 and 0.5 wt% La 2 O 3 exhibited excellent magnetic properties while doping 1–3 wt% La2O3 and 0.5–3 wt% MgO deteriorated magnetic performance. The rational design of CaF 2 - or La 2 O 3 -doped microstructure can be an economical and effective method for producing toughened Sm–Co sintered magnets with high magnetic performance.

36 MATERIALS SCIENCE↗

Spark Plasma Sintering of W-UO2 Cermets

About 50 vol.% 3 um depleted uranium dioxide (UO2) powder was encapsulated within a tungsten super alloy matrix produced from sub-micron tungsten powders using the Spark Plasma Sintering (SPS) process. An additive of 25 atom-percent (at.%) rhenium was included within the tungsten matrix to improve the ductility and fracture toughness of the ceramic–metallic (cermet) matrix. Cermet fabrication to 97.9% of the theoretical cermet density was achieved by sintering at 1500 degrees C with 40 MPa of applied pressure for 20 min. The results presented are from the first known trials of W–UO2 and nuclear cermet production via SPS.

36 MATERIALS SCIENCE↗

Flash microwave synthesis and sintering of nanosized La{sub 0.75}Sr{sub 0.25}Cr{sub 0.93}Ru{sub 0.07}o{sub 3-{delta}} for fuel cell application

Perovskite-oxide nanocrystals of La{sub 0.75}Sr{sub 0.25}Cr{sub 0.93}Ru{sub 0.07}O{sub 3-{delta}} with a mean size around 10 nm were prepared by microwave flash synthesis. This reaction was performed in alcoholic solution using metallic salts, sodium ethoxide and microwave autoclave. The obtained powder was characterised after purification by energy dispersive X-ray analysis (EDX), X-ray powder diffraction (XRD), BET adsorption technique, photon correlation spectroscopy (PCS) and transmission electron microscopy (TEM). The results show that integrated perovskite-type phase and uniform particle size were obtained in the microwave treated samples. At last the synthesised powder was directly used in a sintering process. A porous solid, in accordance with the expected applications, was then obtained at low sintering temperature (1000 deg. C) without use of pore forming agent. - Graphical abstract: TEM photograph of La{sub 0.75}Sr{sub 0.25}Cr{sub 0.93}Ru{sub 0.07}O{sub 3-{delta}} obtained by microwave flash synthesis. This picture confirms the nanometric size of the ceramic particles.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Structural and physical properties evolution of BaIr{sub 1-x}Mn{sub x}O{sub 3} solid solutions synthesized by high-pressure sintering

The BaIr{sub 1-x}Mn{sub x}O{sub 3} (0.0<=x<=1.0) solid solutions were synthesized by using the solid-state chemical method and high pressure sintering in the pressure range 0-5 GPa. According to the pressure-composition 'phase diagram' at 1000 deg. C, the 9M BaIr{sub 1-x}Mn{sub x}O{sub 3} transforms to the 6M form at 5 GPa and x<=1/6. In the x range 0.5-1.0, it transforms to the 9R form in a large pressure range. For the 9M BaIrO{sub 3}, the Mn ions substitution for Ir ions enhances the semiconducting property, and reduces the weak ferromagnetism. When x is larger than 1/3, the 9M/9R BaIr{sub 1-x}Mn{sub x}O{sub 3} behave spin-glass-like state at low temperature, with the glass transition temperature T{sub g} about 60 K. For the 6M BaIrO{sub 3}, the Mn ions doping results in that it transforms to insulator and spin-glass-like magnetism from the initial paramagnetic metal. - Graphical abstract: The BaRu{sub 1-x}Mn{sub x}O{sub 3} solid solutions were synthesized by using the solid-state chemical method and high-pressure sintering, and the pressure-composition 'phase diagram' at 1000 deg. C was obtained.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Sintering and characterization of SrBi{sub 2}Ta{sub 2}O{sub 9} obtained by high-pressure processing at low temperatures

High-pressure processing is a very attractive approach for the production of materials with new and/or improved properties. In this work, pressures in the order of 7.7 GPa and 2.5 GPa were induced in SrBi{sub 2}Ta{sub 2}O{sub 9} samples at different temperatures placed in a specific reaction cell and generated different effects on phase formation. The microstructural evolution during high-pressure processing was investigated by scanning electron microscopy in association with energy dispersion spectroscopy and with the support of an X-ray diffraction analyzer. Frequency response analysis was used to obtain the dielectric curves by electrochemical impedance spectroscopy. A SrBi{sub 2}Ta{sub 2}O{sub 9} single-phase sample, treated at 2.5 GPa and 900 °C, was used to evaluate the electrical properties, obtaining a dielectric response similar to SrBi{sub 2}Ta{sub 2}O{sub 9} samples sintered by conventional processes at temperatures above 1000 °C. In addition, by this method, it was possible to obtain ceramics with uniform microstructure and a relative density of 93%. - Highlights: • The first production of SrBi{sub 2}Ta{sub 2}O{sub 9} using the technique of high-pressure processing. • The ability to produce single-phase SrBi{sub 2}Ta{sub 2}O{sub 9} treated at 2.5 GPa and 900 °C. • The electrical properties are compatible with SBT sintered at high temperatures.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Macroporous glass monoliths prepared from powdered niobium phosphate glass by fast sintering

Macroporous monoliths were prepared by very fast sintering (between 3 and 15 min) of niobophosphate glass powders at low temperature (1018 K) using cellulose as a foaming agent. The porous materials were analyzed by thermal analysis, Raman spectroscopy, scanning electron microscopy and powder X-ray diffraction, and further investigated using X-ray microtomography, a non-destructive technique capable of reconstructing three-dimensional models of samples and providing structural measurements. The progression of the porosity of the monoliths depends on the sintering time (3 to 15 min) and the amount (up to 50% in mass) of cellulose used. The macroporous glass monoliths may find application in integrated chemical systems and in filtering processes.

36 MATERIALS SCIENCE↗

Nanostructured cobalt powders synthesised by polyol process and consolidated by Spark Plasma Sintering: Microstructure and mechanical properties

Bulk nanostructured cobalt was processed using a bottom-up strategy. Nanostructured particle agglomerates of about 50 and 240 nm in diameter were synthesised using a polyol route and subsequently consolidated by Spark Plasma Sintering (SPS). The microstructure of the starting powders and of the processed bulk samples was studied and characterised by X-ray diffraction (XRD) and transmission electron microscopy (TEM). The XRD patterns of the as-prepared powders showed predominantly a face centred cubic (fcc) crystalline phase, whereas both fcc and hexagonal close packed (hcp) phases were found within the consolidated samples. A sample with the highest relative mass density (94.5%) was obtained from the small powder particles. TEM observations revealed a lamellar substructure with a high density of nanotwins and stacking faults in every grain in the sample with the highest density. Brillouin light scattering (BLS) and quasistatic compression tests were used to investigate the mechanical properties of the consolidated samples. The two techniques yielded Young modulus values of 168 GPa and 130 GPa, respectively, in the sample with the highest density. This sample also exhibited a yield stress higher than 1 GPa after the compression test, which is mainly attributed to the lamellar-like structure occurring in almost every grain of the polycrystalline aggregate. - Highlights: Black-Right-Pointing-Pointer Cobalt nanoparticles produced by the polyol process present mainly the fcc metastable phase. Black-Right-Pointing-Pointer Bulk nanostructured cobalt is obtained from the nano-particles by Spark Plasma Sintering consolidation. Black-Right-Pointing-Pointer Nanotwins and stacking faults are present in every grain of the more dense sample. Black-Right-Pointing-Pointer Yield strength and plastic domain may be varied depending on the nanoparticle size and the porosity of the consolidated material.

36 MATERIALS SCIENCE↗

Development of an in-situ multi-component reinforced Al-based metal matrix composite by direct metal laser sintering technique — Optimization of process parameters

In the present investigation, an in-situ multi-component reinforced aluminum based metal matrix composite was fabricated by the combination of self-propagating high-temperature synthesis and direct metal laser sintering process. The different mixtures of Al, TiO{sub 2} and B{sub 4}C powders were used to initiate and maintain the self-propagating high-temperature synthesis by laser during the sintering process. It was found from the X-ray diffraction analysis and scanning electron microscopy that the reinforcements like Al{sub 2}O{sub 3}, TiC, and TiB{sub 2} were formed in the composite. The scanning electron microscopy revealed the distribution of the reinforcement phases in the composite and phase identities. The variable parameters such as powder layer thickness, laser power, scanning speed, hatching distance and composition of the powder mixture were optimized for higher density, lower porosity and higher microhardness using Taguchi method. Experimental investigation shows that the density of the specimen mainly depends upon the hatching distance, composition and layer thickness. On the other hand, hatching distance, layer thickness and laser power are the significant parameters which influence the porosity. The composition, laser power and layer thickness are the key influencing parameters for microhardness. - Highlights: • The reinforcements such as Al{sub 2}O{sub 3}, TiC, and TiB{sub 2} were produced in Al-MMC through SHS. • The density is mainly influenced by the material composition and hatching distance. • Hatching distance is the major influencing parameter on porosity. • The material composition is the significant parameter to enhance the microhardness. • The SEM micrographs reveal the distribution of TiC, TiB{sub 2} and Al{sub 2}O{sub 3} in the composite.

36 MATERIALS SCIENCE↗