Self-Forming Thin Interphases and Electrodes Enabling 3-D Structured High Energy Density Batteries

An electrolytically in-situ formed fluoride/lithium based battery has been developed to offer a pathway to scalable reconfigurable solid state batteries of high energy density. Research into the development of novel in-situ formed chemistries encompassing the negative and positive reactive current collectors, and the bi-ion glass conductor along with electrode structure was accomplished with a focused attention on transport. The solid state in-situ batteries were fabricated with a maskless scalable patterning technique to offer a pathway to high throughput, low material loss and fabrication of complex architectures. Such development and integration enabled to achieve the 12 V bipolar batteries at > 1000 Wh/L energy density based on electrode pairs and current collectors.

25 ENERGY STORAGE↗

In situ Diagnostics of Coupled Electrochemical-Mechanical Properties of Solid Electrolyte Interphases on Lithium Metal Rechargeable Batteries (Final Technical Report)

The fundamental understanding of the coupled mechanical/chemical degradation of the SEI layer during lithium cycling will enable the project to identify the desirable mechanical properties on SEI/lithium as a system and the specific transport properties that enable the homogenous lithium stripping/plating while avoiding the mossy structure. Furthermore, it will allow the project to develop a highly impactful strategy to protect lithium metal and achieve dendrite free high cycle efficiency, which can dramatically increase the energy density of lithium batteries for EV applications. During past three years, four coherent steps have been taken to solve the coupled mechanical and electrochemical degradation: (1) Developed a comprehensive set of in-situ diagnostic techniques to investigate the coupled mechanical/chemical properties of SEI layer and its impact on lithium striping/plating. (2) Identified failure mechanisms of SEI/Li as a whole electrode system using in-situ electrochemical tools. (3) Established a design strategy of protective coatings on Li metal to extend the cycle life Li meal electrode. (4) Developed novel surface coatings as the artificial SEI layer to protect Li metal and significantly extend cycle life. During past 3-year budget period, we have published over 16 peer-reviewed paper, filed 7 patents, and given over 30 invited talks. 5 graduated students and 2 postdocs were supported by this project.

36 MATERIALS SCIENCE↗

Atomistic Modeling of the Interphase Structure between Alumina and Al12Fe2Cr Quasicrystal Approximant

Molecular dynamics simulations are performed to study the stability of an fcc metallic interlayer phase between an iron aluminide quasicrystal approximant (QCA) phase (84.2 Al, 5.7 Fe, 5.4 Ni, and 4.7 at.% Cr) and aluminum oxides (α-Al 2 O 3 and γ-Al 2 O 3 ). The presence of the interlayer phase was experimentally observed in some regions of the inner diameter surface of a TPBAR cladding tube. The simulations employed existing many-body (MEAM and EAM) interatomic potentials to describe atomic interactions in the interlayer and QCA phases, and Buckingham+Coulomb pair interactions for the alumina and between the alumina and the QCA (or fcc). Interface systems of QCA/alumina, fec/alumina, and QCA/fcc are modeled and the fracture energy of the interfaces is calculated. Based on the fracture energies, for the γ-Al 2 O 3 , both MEAM and EAM suggest that the fcc interlayer phase would not form. For the α-Al 2 O 3 , the MEAM predicts that the fcc phase would form, however, the EAM predicts that it forms only if the α-Al 2 O 3 is Al-terminated at the interface. For the O-terminated α-Al 2 O 3 , the EAM predicts the fcc phase would not form, consistent with the results for γ-Al 2 O 3 .

36 MATERIALS SCIENCE↗

Glassy interphases reinforce elastomeric nanocomposites by enhancing percolation-driven volume expansion under strain

For nearly a century, introduction of nanoparticles to elastomers has yielded extraordinarily tough nanocomposites that are critical to technologies from actuators to tires. The mechanisms by which this reinforcement occurs have nevertheless remained a central open question in material science. One widely debated hypothesis posits that strong interactions between polymer and particles induce "glassy bridges" that cement particles into a cohesive percolating network that resists elongation. Here, molecular dynamics simulations show that glassy particle shells do not primarily provide elongational cohesion. Instead, they amplify an underlying mechanism wherein competition between filler and elastomer networks causes the elastomer's volume to increase on deformation. This induces contributions from the elastomer's bulk modulus, which is of order 1000 times larger than its Young's modulus. These findings establish a unified understanding of low-strain reinforcement in filled elastomers as emanating from volumetric competition between coexisting particulate and elastomeric networks. This reframes and unifies our understanding of low-strain reinforcement, provides a clear-cut diagnostic for the presence of glassy bridging, and offers a new design principle for tough elastomeric nanocomposites.

Computational Physics (physics.comp-ph)↗

Methods for solid electrolyte interphase formation and anode pre-lithiation of lithium ion capacitors

A method of pre-doping an anode of an energy storage device can include immersing the anode and a dopant source in an electrolyte, and coupling a substantially constant current between the anode and the dopant source. A method of pre-doping an anode of an energy storage device can include immersing the anode and a dopant source in an electrolyte, and coupling a substantially constant voltage across the anode and the dopant source. An energy storage device can include an anode having a lithium ion pre-doping level of about 60% to about 90%.

25 ENERGY STORAGE↗

Three-Dimensional Resistivity vs. Depth Profiling for Advanced Characterization of the Lithium-Ion Battery Solid Electrolyte Interphase

In this work, we investigate the evolution of SEI formed from a standard electrolyte (1.2 M LiPF6 in EC:EMC (3:7 wt%)) through various points in cycling on several model Si surfaces. We also examine the solubility of SEI by resting the anode in the cell at varied temperatures then characterizing the residual SEI. Evolution of the SEI surface is also analyzed with atomic force microscopy (AFM) measurements. AFM and SSRM-derived results are presented in combination with chemical characterization, including time-of-flight secondary ion mass spectrometry (TOF-SIMS).