Search NASA⌕ Search

SEARCH · Search NASA

Results for “DEGRADATION”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 487 records · Page 27

Control blade degradation test under temperature gradient in steam atmosphere

The core of a boiling water reactor (BWR) consists of an array of fuel assemblies with cross-shaped control blades located between these assemblies. The typical control blade consists of a control blade sheath made of 316L-type S.S., a center pole made of 316L-type S.S., and control rods. In order to understand the degradation process of the control blade channel, control blade degradation tests were performed under various atmospheres with a temperature increase condition and in the presence of a temperature gradient. A test device was built. Four carbon heaters are set on both sides at the upper and the middle parts of the test device. The bottom ceramic part of the test device is cooled by water. Heating in the upper region and cooling at the bottom of the test piece give rise to the temperature gradient in the test piece. Temperatures of the test piece are measured by five W-Re type thermocouples placed close to the test piece. Steam carried by the argon gas is supplied from the bottom of the device and flows to the top inside a square carbon muffle in which the test piece is set. Three windows for visual observations are installed, with one located above the furnace and the others located at the back of the furnace. In the steam atmosphere with a steam flow rate of 0.0125 g/s/rod, the control blade, channel box, and fuel rods were degraded, especially at the upper part of the test piece. This result was similar to that observed in the argon atmosphere test. However, the observed degradation was rather different at a higher steam flow rate of 0.0417 g/s/rod. At the upper part of the test piece, only the control blade was degraded preferentially and did not react with the channel box wall. In contrast, the eutectic reaction of the stainless steel/boron carbide melt and zircaloy occurred at the lower part by coexisting with the relocated melt from the top part. These observations suggested the existence of a threshold condition for the control rod degradation between 0.0125 and 0.0417 g/s/rod which is significantly affected by the thickness of the oxide layer on zircaloy.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Results from an international interlaboratory study on light‐ and elevated temperature‐induced degradation in solar modules

Abstract This paper reports the results of an international interlaboratory comparison study on light‐ and elevated temperature‐induced degradation (LETID) on crystalline silicon photovoltaic (PV) modules. A large global network of PV module manufacturers and PV testing laboratories collaborated to design a protocol for LETID detection and screen a large and diverse set of prototype modules for LETID. Results across labs indicate the reproducibility of LETID testing is likely within ±1% of maximum power (P MP ). In intentionally engineered LETID‐sensitive modules, mean degradation after the prescribed detection stress is roughly 6% P MP . In other module types the LETID sensitivity is smaller, and in some we observe essentially negligible degradation attributable to LETID. In LETID‐sensitive modules, both open‐circuit voltage (V OC ) and short‐circuit current (I SC ) degrade by a roughly similar magnitude. We observe, as do previous studies, that LETID affects each cell in a module differently. An investigation of the potential mismatch losses caused by nonuniform LETID degradation found that mismatch loss is insignificant compared to the estimated loss of cell I SC , which drives loss of module I SC . Overall, this work has helped inform the creation of a forthcoming standard technical specification for LETID testing of PV modules, IEC TS 63342 ED1, and should aid in the interpretation of results from that and other LETID tests.

14 SOLAR ENERGY↗

Field retrieved photovoltaic backsheet survey from diverse climate zones: Analysis of degradation patterns and phenomena

Understanding the impact of climate stressors on photovoltaic (PV) backsheet degradation in real-use conditions is critical to improve the accelerated testing exposures, extend the backsheet lifetime, and increase the confidence in PV reliability. Here, in this work, a total of 33 PV module backsheets were retrieved from six climatic zones worldwide with 2 - 28 years of exposure. These modules included five types of backsheet air-side materials (or outer layer): poly(vinylidene fluoride) (PVDF), poly(tetrafluoroethylene-co-hexafluoropropylene-co-vinylidene fluoride) (THV), poly(vinyl fluoride) (PVF), poly(ethylene terephthalate) (PET), and polyamide (PA). Attenuated total reflection Fourier-transform infrared spectroscopy (ATR-FTIR) was used to identify air-side materials. The degradation induced color change, gloss loss, and chemical material changes analyzed using optical microscopy, differential scanning calorimetry (DSC), scanning electron microscopy (SEM), colorimetry (yellowness index (YI)), and gloss measurements. PVDF, THV, and PVF air-side layer backsheets, in particular PVF, had minimal degradation in the air-side layer appearance and chemical structures after exposure in different climatic zones. The PET air-side backsheets exhibited obvious color increase (22.55 YI units after about 9 years exposure) and the PA/PA/PA backsheets showed large gloss loss (up to 76.4 %) relative to the unexposed backsheets. Severe cracks between cells that penetrated through the entire thickness of backsheets are observed on PA/PA/PA backsheets after 4-6 years of exposure in 6 climatic zones. The current indoor exposure standards were not sufficient to identify this degradation type. However, fluoropolymer based PV backsheets showed lower levels of degradation predictors and increased climatic resistance. Specific samples (PVF) showed little change from baseline after 28 years of outdoor exposure.

29 ENERGY PLANNING, POLICY, AND ECONOMY↗

Pool Boiling Reliability Tests and Degradation Mechanisms of Microporous Copper Inverse Opal (CuIOs) Structures

The rising power density in electronic systems requires thermal management solutions that are both high-performing and reliable. Porous materials such as Copper Inverse Opal (CuIOs) have unique structural features, including high permeability and high thermal conductivity, to enhance pool boiling performance. However, there is little understanding of the degradation mechanism of such porous materials under pool boiling conditions. In this study, samples of 10 ..mu..m thick CuIOs with 4.8 ..mu..m diameter, covering silicon substrate of area 11 mm x 11 mm, with various heated areas ranging from 2.5 mm x 2.5 mm to 10 mm x 10 mm, were tested in 100 degrees C deionized water at a constant heat flux of 110 Wcm -2 for 3-to-7 days. The combined effect of erosion and corrosion caused structural degradation of the CuIOs. The directly heated area had the most severe degradation while the edge of the heater and the unheated area showed progressively less degradation, maintaining some CuIOs structure even after the 7-day reliability test. Among all the tested samples with various heater sizes, the 2.5 mm x 2.5 mm heater sample - in which the heater size was designed to be comparable to the water bubble characteristic length - had the largest critical heat flux (CHF) up to 300 Wcm -2 with a superheat ~ 13 degrees C. Additionally, CuIOs with a smaller heated area performed better in terms of reliability. This study offers preliminary insights into CuIOs degradation mechanisms, contributing to the development of more robust thermal management solutions. We expect that electroless plating of CuIOs with gold (Au), nickel (Ni), and atomic layer deposition (ALD) aluminum oxide (Al 2 O 3 ) in combination with appropriate application-specific coolants will further improve the reliability and lifetime of the CuIOs.

boiling-induced degradation↗

Transmission Electron Microscopy Study on Microstructure of Degraded CdTe Mini-Modules

In this paper, we employ transmission electron microscopy coupled with energy-dispersive X-ray spectrometry (EDS) to study the structure and chemistry of cadmium telluride (CdTe) thin-film solar cells with different extents of degradation. The studied regions originate from the same photovoltaic mini-module, which was subjected to one-sun light exposure at a temperature of 100 degrees C for 400 h to induce light and heat degradation. EDS maps reveal a discontinuous CdS layer and particles rich in O and S but Te-depleted within the CdTe absorber layer after the light and heat stress. These features could act as enhanced recombination centers, resulting in decreased photovoltaic conversion efficiency. Additionally, the most degraded CdTe sample shows a strong accumulation of Na precisely localized in the discontinuous part of the CdS layer. The local Na concentration is determined to be ~16 at.%. In addition, appreciable Na accumulation is observed at the soda-lime glass/transparent conductive oxide interface in both degraded CdTe solar cells. The microstructure of the baseline CdTe mini-module with no stress was also investigated to demonstrate that the structure difference was caused by the light- and heat-induced degradation, instead of module fabrication. These results highlight the need to control the distribution of Na in fielded CdTe modules to sustain long-term high-power output.

14 SOLAR ENERGY↗

Mitigation of Boiling-Induced Thermal Degradation Using Microporous Nickel Inverse Opals Structures

Engineered microporous structures have received much attention in high-heat-flux electronics cooling due to their high thermal conductivity and permeability, and large surface area for heat transfer, but are susceptible to boiling-induced thermal degradation. Here, this study investigates the efficacy of nickel inverse opals (NiIOs) in mitigating structural degradation caused by corrosion-assisted erosion during pool boiling with water as the working fluid. First, we compared the reliability of NiIOs to copper inverse opals (CuIOs) for a 3-day pool boiling test at constant heat flux. The NiIOs demonstrated superior resistance to thermal degradation due to their inherent corrosion resistance and mechanical strength. Subsequently, we conducted a more controlled experiment to show the effect of heat flux on the degradation of the NiIOs while excluding the effect of temperature variations. Pool boiling tests of 20-μm-thickness NiIOs covering an area of ∼11 × 11 mm 2 with a 2.5 × 2.5 mm 2 heater at the center were conducted at heat flux levels of 20%, 40%, and 60% of the critical heat flux (CHF) for 3 days. The NiIOs subjected to heat flux levels of 20% and 40% CHF showed minimal degradation, while the sample subjected to 60% CHF showed erosion on the top surface due to higher bubble formation and departure rate. These results show the potential of NiIOs as a promising solution for long-term thermal management in high-power electronic devices, although design considerations for maximum allowable heat flux are necessary for reliable operation.

36 MATERIALS SCIENCE↗

Statistical analysis and degradation pathway modeling of photovoltaic minimodules with varied packaging strategies

Degradation pathway models constructed using network structural equation modeling (netSEM) are used to study degradation modes and pathways active in photovoltaic (PV) system variants in exposure conditions of high humidity and temperature. This data-driven modeling technique enables the exploration of simultaneous pairwise and multiple regression relationships between variables in which several degradation modes are active in specific variants and exposure conditions. Durable and degrading variants are identified from the netSEM degradation mechanisms and pathways, along with potential ways to mitigate these pathways. A combination of domain knowledge and netSEM modeling shows that corrosion is the primary cause of the power loss in these glass/backsheet PV minimodules. We show successful implementation of netSEM to elucidate the relationships between variables in PV systems and predict a specific service lifetime. The results from pairwise relationships and multiple regression show consistency. This work presents a greater opportunity to be expanded to other materials systems.

electrical measurements↗

Automated Data Collection for Determining Statistical Distributions of Module Power Undergoing Potential-Induced Degradation: Preprint

We propose a method for increasing the frequency of data collection and reducing the time and cost of accelerated lifetime testing of photovoltaic modules undergoing potential-induced degradation (PID). This consists of in-situ measurements of dark current-voltage curves of the modules at elevated stress temperature, their use to determine the maximum power at 25 degrees C standard test conditions (STC), and distribution statistics for determining degradation rates as a function of stress level. The semi-continuous data obtained by this method clearly show degradation curves of the maximum power, including an incubation phase, rates and extent of degradation, precise time to failure, and partial recovery. Stress tests were performed on crystalline silicon modules at 85% relative humidity and 60 degrees C, 72 degrees C, and 85 degrees C. Activation energy for the mean time to failure (1% relative) of 0.85 eV was determined and a mean time to failure of 8,000 h at 25 degrees C and 85% relative humidity is predicted. No clear trend in maximum degradation as a function of stress temperature was observed.

14 SOLAR ENERGY↗

Pool Boiling Reliability Tests and Degradation Mechanisms of Microporous Copper Inverse Opal (CuIOs) Structures: Preprint

The rising power density in electronic systems requires thermal management solutions that are both high-performing and reliable. Porous materials such as Copper Inverse Opals (CuIOs) have unique structural features, including high permeability and high thermal conductivity, to enhance pool boiling performance. However, there is little understanding of the degradation mechanism of such porous materials under pool boiling conditions. In this study, samples of 10-micrometer-thick CuIOs with 4.8-micrometer diameter, covering silicon substrate of area 11-mm by 11-mm, with various heated areas ranging from 2.5-mm by 2.5-mm to 10-mm by 10-mm, were tested in 100 degrees C deionized water at a constant heat flux of 110 watts per square cm for 3-7 days. The combined effect of erosion and corrosion caused structural degradation of the CuIOs. The directly heated area had the most severe degradation while the edge of the heater and the unheated area showed progressively less degradation, maintaining some CuIOs structure even after the 7-day reliability test. Among all the tested samples with various heater sizes, the 2.5-mm by 2.5-mm heater sample - in which the heater size was designed to be comparable to the water bubble characteristic length - had the largest critical heat flux (CHF) up to 300 watts per square cm with a superheat of approximately 13 degrees C. Additionally, CuIOs with a smaller heated area performed better in terms of reliability. This study offers preliminary insights into CuIOs degradation mechanisms, contributing to the development of more robust thermal management solutions. We expect that electroless plating of CuIOs with gold (Au), nickel (Ni), and atomic layer deposition of aluminum oxide in combination with appropriate application-specific coolants will further improve the reliability and lifetime of the CuIOs.

boiling-induced degradation↗

Mapping of Heterogeneous Catalyst Degradation in Polymer Electrolyte Fuel Cells

Pt catalysts in polymer electrolyte fuel cells degrade heterogeneously as the catalyst particles are exposed to local variations throughout the catalyst layer during operation. State-of-the-art analytical techniques for studying degradation of Pt catalysts do not possess fine spatial resolution to elucidate such non-uniform degradation behavior at a large electrode level. A new methodology is developed to spatially resolve and quantify the heterogeneous Pt catalyst degradation over a large area (several cm ) of aged MEAs based on synchrotron X-ray microdiffraction. PEFC single cells are aged using voltage cycling as an accelerated stress test and the degradation heterogeneity at a micrometer length scale is visualized by mapping Pt catalyst particle size after voltage cycling. It is demonstrated in detail that the Pt catalyst particle size growth is non-uniform and follows the flow field geometry. The Pt particle size growth is greater in the area under the flow field land, while it is minimal in the area under the flow field channel. Additional non-uniformity is observed with the Pt particle size increasing more rapidly at the air outlet area than the Pt particle size at the inlet area.

36 MATERIALS SCIENCE↗

Photovoltaic failure and degradation modes

The extensive photovoltaic field reliability literature was analyzed and reviewed. Future work is prioritized based upon information assembled from recent installations, and inconsistencies in degradation mode identification are discussed to help guide future publication on this subject. Reported failure rates of photovoltaic modules fall mostly in the range of other consumer products; however, the long expected useful life of modules may not allow for direct comparison. In general, degradation percentages are reported to decrease appreciably in newer installations that are deployed after the year 2000. However, these trends may be convoluted with varying manufacturing and installation quality world-wide. Modules in hot and humid climates show considerably higher degradation modes than those in desert and moderate climates, which warrants further investigation. Delamination and diode/j-box issues are also more frequent in hot and humid climates than in other climates. The highest concerns of systems installed in the last 10 years appear to be hot spots followed by internal circuitry discoloration. Encapsulant discoloration was the most common degradation mode, particularly in older systems. In newer systems, encapsulant discoloration appears in hotter climates, but to a lesser degree. Lastly, thin-film degradation modes are dominated by glass breakage and absorber corrosion, although the breadth of information for thin-film modules is much smaller than for x-Si.

14 SOLAR ENERGY↗

UV-Induced Degradation and Associated Metastability in TOPCon Photovoltaic Modules: Understanding Kinetics and Cell Variance

Tunnel oxide passivated contact (TOPCon) silicon photovoltaic (PV) modules are dominating the PV market, but they may be susceptible to degradation under ultraviolet (UV)-containing light. Quantifying the impacts of UV-induced degradation (UVID) is complicated by an associated metastability causing further degradation under dark storage and rapid recovery under sunlight. Here, we study modules that have -2.3% to -3.2% nonrecoverable UVID loss after 60 kWh/m2 dose of 340 nm light and additional recoverable loss under dark storage. We use in situ electroluminescence (EL) imaging to characterize the post-UVID metastability at the module level. The cell-by-cell dark degradation and recovery kinetics span a wide range from +6% to -70% changes in EL intensity after 520 h of dark storage, which returns to +- 4% of the initial post-UVID EL intensity after illumination. The kinetics follow double exponential rates with dark storage degradation time constants of 345 and 45 h, and UV light recovery time constants of 5 min and 36 s. We propose that this is consistent with prior reports of kinetics for light-soaking metastability in Al2O3 passivation. Finally, we further show that cells having high UVID also have injection-dependent effective carrier lifetimes and significant intra-cell variance, suggesting possible origins of processing inconsistency.

14 SOLAR ENERGY↗

Degradation mechanism of lead-vanado-iodoapatite in NaCl solution

Degradation mechanism of lead-vanado-iodoapatite (IAPT) in NaCl solution at 90 °C was investigated through systematic characterization of surface morphology, microstructure and microchemistry evolution of the alteration layer. Nano-scale characterization indicated that IAPT crystals degraded from grain boundaries toward inner grains, forming ultrafine Cl-bearing crystallites. A coupled interface dissolution-reprecipitation replacement mechanism and the ion exchange between Cl - and I - across the degradation zone may together play roles in determining the nano-scale degradation behavior of IAPT. This work highlights the degradation through multiple reactions and elemental transport across the liquid-solid and solid-solid interfaces at length scales from sub-millimeter to nanoscale.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Forecasting battery capacity and power degradation with multi-task learning

Lithium-ion batteries degrade due to usage and exposure to environmental conditions, which affects their capability to store energy and supply power. Accurately predicting the capacity and power fade of lithium-ion battery cells is challenging due to intrinsic manufacturing variances and coupled nonlinear ageing mechanisms. In this paper, we propose a data-driven prognostics framework to predict both capacity and power fade simultaneously with multi-task learning. The model is able to predict the degradation trajectory of both capacity and internal resistance together with knee-points and end-of-life points accurately at early-life stage. The validation shows an average percentage error of 2.37% and 1.24% for the prediction of capacity fade and resistance rise, respectively. The model's ability to accurately predict the degradation, facing capacity and resistance estimation errors, further demonstrates the model's robustness and generalizability. Compared with single-task learning models for forecasting capacity and power degradation, the model shows a significant prediction accuracy improvement and computational cost reduction. This work presents the highlights of multi-task learning in the degradation prognostics for lithium-ion batteries.

25 ENERGY STORAGE↗

A control oriented comprehensive degradation model for battery energy storage system life prediction

In order to ensure that stationary battery energy storage systems (BESSs) provide reliable energy buffering, both for power quality and economic purposes, the degradation must be considered. Cell degradation involves various side reactions and is highly dependent on its operating conditions. To accurately track cell degradation and predict its impact on battery behavior, a comprehensive physics-based degradation model based on an electrolyte phase-enhanced single particle (SP) model is developed. Key degradation physics, namely solid electrolyte interphase (SEI) layer formation and growth, Li plating on the graphite anode, and Mn dissolution on cathode of nickel-cobalt-manganese oxide (NMC622) are considered. The model is validated against experimental capacity data. The results reveal that the deposition rate of both SEI layer and Li metal increase as the charge voltage increases. At the cathode side, the solvent oxidation rate determines the Mn dissolution rate. As a result, the volume fraction of NMC622 in the cathode continually decreases at a gradually increasing rate.

25 ENERGY STORAGE↗

Degradation and fate of 2,4-dinitroanisole (DNAN) and its intermediates treated with Mg/Cu bimetal: Surface examination with XAS, DFT, and LDI-MS

In this article, a novel Mg-based bimetal reagent (Mg/Cu) was used as an enhanced reductive system to degrade insensitive munition 2,4-dinitroanisole (DNAN), a contaminant found in energetic-laden waste. Degradation of DNAN was significantly impacted by dissolved oxygen and studied in anoxic and oxic bimetal systems (i.e., purging with N 2 , air, or O 2 gas). Degradation occurred through sequential nitroreduction: first one nitro group was reduced (ortho or para) to form short-lived intermediates 2-amino-4-nitroanisole or 4-amino-2-nitroanisole (2-ANAN or 4-ANAN), and then subsequent reduction of the other nitro group formed 2,4-diaminoanisole (DAAN). The nitro-amino intermediates demonstrated regioselective reduction in the ortho position to 2-ANAN; Regioselectivity was also impacted by the anoxic/oxic environment. Under O 2 -purging DNAN degradation rate was slightly enhanced, but most notably O 2 significantly accelerated DAAN generation. DAAN also further degraded only in the oxygenated Mg/Cu system. Adsorption of DNAN byproducts to the reagent occurred regardless of anoxic/oxic condition, resulting in a partition of carbon mass between the adsorbed phase (27%-35%) and dissolved phase (59%-72%). Additional surface techniques were applied to investigate contaminant interaction with Cu. Density functional theory (DFT) calculations identified preferential adsorption structures for DNAN on Cu with binding through two O atoms of one or both nitro groups. X-ray absorption spectroscopy (XAS) measurements determined the oxidation state of catalytic metal Cu and formation of a Cu-O-N bond during treatment. Laser desorption ionization mass spectrometry (LDI-MS) measurements also identified intermediate 2-ANAN adsorbed to the bimetal surface.

54 ENVIRONMENTAL SCIENCES↗

A non-aqueous sodium hexafluorophosphate-based electrolyte degradation study: Formation and mitigation of hydrofluoric acid

Fundamental characterization of battery electrolyte is crucial for rechargeable batteries. This work reports the chemical stability of sodium hexafluorophosphate (NaPF6)-based non-aqueous electrolytes containing different solvent mixtures (e.g., cyclic and acyclic carbonates) in the presence of water for Na-ion batteries. A degradation study is conducted using NaPF 6 -based electrolytes, highlighting the effect of two electrolyte additives, 2,2,2-trifluoroethoxy-2,2,2-ethoxy phosphazene (FM2) and fluoroethylene carbonate (FEC), on degradation and cell performance of full-cell Na-ion batteries. Hydrolysis of this salt in acidic condition is particularly prone to form hydrofluoric acid (HF), and can be observed in electrolytes made with battery grade carbonate solvents (<20 ppm of water). Here, degradation mechanisms of NaPF 6 -based electrolytes are studied using liquid nuclear magnetic resonance (NMR). Noticeable degradation takes place in high purity electrolytes with the presence of moisture to form HF and organophosphates in timeframes below the current shelf-life of the Na electrolytes. FEC is not efficient to protect the electrodes from being exposed to HF. On the other hand, FM2 is revealed as a “scavenger” of HF, which helps stabilize the shelf life of electrolytes that might contain or become exposed to water. Our study underscores the importance to understanding the degradation of electrolyte and improving stability toward better shelf life for sodium ion batteries.

25 ENERGY STORAGE↗

Degradation and recovery of solid oxide fuel cell performance by control of cathode surface acidity: Case study – Impact of Cr followed by Ca infiltration

Solid oxide fuel cells (SOFC) have attracted attention as clean and efficient energy conversion devices with low emissions. However, several degradation mechanisms limit the electrochemical performance of current SOFCs, with cathode degradation due to Cr-poisoning from metal interconnects particularly problematic. The acidity/basicity of binary additives has been found to be a sensitive descriptor of the oxygen exchange kinetics, indicating that acidic Cr-species/basic Ca-species can be expected to deactivate/activate the cathode surface, respectively. Inspired by recent advances, the feasibility of relative acidity as a tool for reviving degraded SOFCs is demonstrated by neutralizing Cr-poisoned SOFCs by subsequent serial infiltration of Ca-species. Furthermore, a model mixed ionic and electronic conducting oxide, Pr 0.1 Ce 0.9 O 2-δ (PCO), is selected as the cathode material. Area-specific resistances (ASR) of symmetric cells obtained by electrochemical impedance spectroscopy show that Cr-infiltration results in a seven-fold increase in ASR, while subsequent infiltration of Ca-species leads to complete recovery. Performance degradation and recovery are attributed to depressed/enhanced redox properties at the PCO surface, as supported by XPS analysis. Experiments using anode-supported fuel cells show a reduction in peak power density by 26% upon Cr-infiltration, reversed following Ca-infiltration, after which no degradation is observed during subsequent operation for 100 h.

(Pr,Ce)O2-δ↗