Search NASA⌕ Search

SEARCH · Search NASA

Results for “Photovoltaic Module”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 487 records · Page 27

Water-module interaction studies

Mechanisms by which moisture enters photovoltaic modules and techniques for reducing such interactions are reported. Results from a study of the effectiveness of various module sealants are given. Techniques for measuring the rate and quantity of moisture ingress are discussed. It is shown that scribe lines and porous frit bridging conductors provide preferential paths for moisture ingress and that moisture diffusion by surface/interfacial paths is considerably more rapid than diffusion by bulk paths, which implies that thin-film substrate and supersubstrate modules are much more vulnerable to moist environments than are bulk-encapsulated crystalline-silicon modules. Design approaches that reduce moisture entry are discussed.

Mon, G.↗

Model Development of Degradation of PV Modules Backsheet with Locating Place of Module

Performance of a photovoltaic (PV) module is related to the micro-environment around the module. The position of photovoltaic modules in an array row have a large effect on the yellowing and gloss of PV module backsheet exposed in Dfa climatic zone (Gaithersburg, MD) with a polyethylene naphthalate (PEN) outer layer. Stress/Response models of yellowing and gloss-losing as function of location parameters of module, including the shed, row, measurement position in a same module and the distance of module location to the row center, are under development. The module installation height had the greatest influence on degradation of PEN PV backsheet in the Dfa climatic zone. The module backsheets at the end of an array have higher degradation rate (edge effect). The edge effect decreases with increasing of module installation heights.

14 SOLAR ENERGY↗

A New UV Spot Test for Quality Control

Here, we present a fast, low-cost ultraviolet (UV) spot test to screen photovoltaic modules for UV-induced degradation (UVID). The measurement is based on a fiber-coupled arc lamp that delivers a highly accelerated local UV dose-approximately five years of equivalent field exposure in less than a day. Spot-exposed areas are evaluated using electroluminescence imaging. We test a “known bad” product, which was observed to experience UVID in the field, and a “known good” product which did not exhibit UVID in the field. Results indicate that the method may be useful as a quick and relatively inexpensive quality control screening tool for customers and manufacturers.

14 SOLAR ENERGY↗

In-situ I-V measurement of a module in a PV array

In one respect, disclosed is an in-situ current-voltage (I-V) measurement device for photovoltaic modules in a photovoltaic array, comprising a variable load, wherein the variable load is configured to be connected in parallel with a module, wherein the module is connected in series with at least one other module in a string, such that the module supplies current simultaneously to the string and to the variable load, and wherein the variable load is controlled by a controller, and wherein the controller is configured to shift an I-V operating point of the module, based at least upon varying the variable load.

Gostein, Michael↗

Effects of PV Module Soiling on Glass Surface Resistance and Potential-Induced Degradation: Preprint

The sheet resistance of three soil types (Arizona road dust, soot, and sea salt) on glass were measured by the transmission line method as a function of relative humidity (RH) between 39% and 95% at 60 degrees C. Sea salt yielded a 3.5 order of magnitude decrease in resistance on the glass surface when the RH was increased over this RH range. Arizona road dust showed reduced sheet resistance at lower RH, but with less humidity sensitivity over the range tested. The soot sample did not show significant resistivity change compared to the unsoiled control. Photovoltaic modules with sea salt on their faces were step-stressed between 25% and 95% RH at 60 degrees C applying -1000 V bias to the active cell circuit. Leakage current from the cell circuit to ground ranged between two and ten times higher than that of the unsoiled controls. Degradation rate of modules with salt on the surface increased with increasing RH and time.

14 SOLAR ENERGY↗

Photovoltaic failure and degradation modes

The extensive photovoltaic field reliability literature was analyzed and reviewed. Future work is prioritized based upon information assembled from recent installations, and inconsistencies in degradation mode identification are discussed to help guide future publication on this subject. Reported failure rates of photovoltaic modules fall mostly in the range of other consumer products; however, the long expected useful life of modules may not allow for direct comparison. In general, degradation percentages are reported to decrease appreciably in newer installations that are deployed after the year 2000. However, these trends may be convoluted with varying manufacturing and installation quality world-wide. Modules in hot and humid climates show considerably higher degradation modes than those in desert and moderate climates, which warrants further investigation. Delamination and diode/j-box issues are also more frequent in hot and humid climates than in other climates. The highest concerns of systems installed in the last 10 years appear to be hot spots followed by internal circuitry discoloration. Encapsulant discoloration was the most common degradation mode, particularly in older systems. In newer systems, encapsulant discoloration appears in hotter climates, but to a lesser degree. Lastly, thin-film degradation modes are dominated by glass breakage and absorber corrosion, although the breadth of information for thin-film modules is much smaller than for x-Si.

14 SOLAR ENERGY↗

Stabilization of light-induced effects in Si modules for IEC 61215 design qualification

Standardized testing of commercial photovoltaic modules is widely used around the world and decreases risks of module failures. Such testing also reduces financial risks for module manufacturers and customers. This work examines the expected impact of certain defects in silicon (Si) modules during standardized accelerated testing. Specifically, the behavior of boron-oxygen (BO) light-induced degradation (LID) and light- and elevated temperature-induced degradation (LeTID) are simulated during some of the stress tests in IEC 61215. LID and LeTID reaction rates at qualification temperatures are estimated from earlier published data. It is demonstrated the BO-related LID may cause some false positives and false negatives when IEC 61215 tests are performed as prescribed in the 2016 published version. Possible stabilization steps to avoid these false results are suggested. State changes for the defects causing LeTID occur much more slowly than those causing BO LID, and therefore LeTID is predicted to have a lesser impact on the IEC 61215 stress tests results.

14 SOLAR ENERGY↗

Automatic Detection and Evaluation of Solar Cell Micro-Cracks in Electroluminescence Images Using Matched Filters

A method for detecting micro-cracks in solar cells using two dimensional matched filters was developed, derived from the electroluminescence intensity profile of typical micro-cracks. We describe the image processing steps to obtain a binary map with the location of the micro-cracks. Finally, we show how to automatically estimate the total length of each micro-crack from these maps, and propose a method to identify severe types of micro-cracks, such as parallel, dendritic, and cracks with multiple orientations. With an optimized threshold parameter, the technique detects over 90 % of cracks larger than 3 cm in length. The method shows great potential for quantifying micro-crack damage after manufacturing or module transportation for the determination of a module quality criterion for cell cracking in photovoltaic modules.

14 SOLAR ENERGY↗

Nanocomposite barrier films for photovoltaic applications

Polymer-clay nanocomposites thin film coatings have improved water vapor and oxygen permeability, in addition to improved corrosion resistance, while retaining high transparency, high electrical resistivity, and excellent fire-retardant properties for use as encapsulants for photovoltaic module assemblies and barrier coatings in other photovoltaic applications.

Spoerke, Erik David↗

Mismatch losses in a PV system due to shortened strings

Numerous events may require intentional removal of one or more photovoltaic modules from a string, shortening the length of the string relative to others within the array, resulting in a string length mismatch. The impact of such a mismatch is not well understood either in measurable operational effects (voltage, current, power) or in the potential effects on long-term module health. It is impractical to solely approach this problem experimentally due to the size and complexity of arrays that may experience string length shortening. Here this work presents simulations, validated through limited field experiments on a two string array, providing a basis from which more complex arrays and scenarios may be explored. Refinement of the simulation achieves an overall error in IMPP for the nominal (S 1 ) and test strings (S 2 ) between the simulation and experimental values, through all test conditions, of +0.35 ± 1.46% and -0.36 ± 1.58% respectively. Shortening one of two strings by one module results in a power loss greater than the power contribution of the module alone (1.29 module equivalents); the impact increases through the maximum test case of a six module mismatch with a power loss equivalent to more than 11 modules. The impact of using string-end blocking diodes is presented with an emphasis at the array maximum power point and at open circuit. Implications are discussed for arrays of higher complexity.

14 SOLAR ENERGY↗

Systematic Operating Temperature Differences Between Al-BSF, PERC, and PERT-With-Optimized-Rear-Reflector Solar Mini-Modules Due to Rear Reflectance

Reflecting sub-bandgap light from photovoltaic modules has the potential to improve lifetime energy generation of fielded systems by reducing operating temperature. In this article, the temperature of fielded aluminum back-surface field (Al-BSF) and passivated emitter and rear contact (PERC) mini-modules was monitored every 5 minutes for 75 days along with corresponding meteorological data. Additionally, passivated emitter rear totally diffused (PERT) mini-modules with high-performance sub-bandgap rear reflectors were tested and compared to the state-of-the-art industrial modules. These reflectors consisted of a >300-nm-thick silicon dioxide nanoparticle film with a low refractive index. The impact of reflectance on measured operating temperature was isolated with a previously developed thermal model and quantified as the reflectance-induced median temperature difference between each tested module at representative outdoor conditions (1000 W m -2 , 25 degrees C ambient temperature, and 1.43 m s -1 wind speed). We found that, because of their reflectance differences, PERC modules ran systematically cooler than Al-BSF modules by 1.0 degrees C, whereas the PERT-with-optimized-rear-reflector systematically operated 1.4 degrees C cooler than the Al-BSF module and 0.4 degrees C than the PERC module. We also found that the rear reflector provided the greatest temperature benefit during periods of highest irradiance.

14 SOLAR ENERGY↗

Prediction of Climate-Specific Degradation Rate for Photovoltaic Encapsulant Discoloration

Encapsulant discoloration is a well-known field degradation mode of crystalline-silicon photovoltaic modules, particularly in the hot climate zones. The discoloration rate is influenced by several weathering factors, such as UV light, module temperature, and humidity, as well as the permeability of oxygen into the module. Here, a rate dependence model employing the modified Arrhenius equations to predict the degradation rate for encapsulant discoloration in different climates is presented. Two modeling approaches are introduced, which utilize the field and accelerated UV testing degradation data in conjunction with the field meteorological data to determine the acceleration factor for encapsulant browning. A novel method of accelerated UV stress testing at three simultaneous module temperatures in a single environmental chamber test run is implemented to estimate the activation energy for browning. The test was performed on three field-retrieved modules to capture the wear-out failure mechanism. The degradation in short-circuit current Isc rather than maximum power is used as a decisive parameter for the discoloration analysis. Furthermore, the developed model has been used to predict the Isc degradation rate for the Arizona field characterized by a hot and dry climate and is validated against the field-measured value. It has also been applied to other climate types, e.g., the cold and dry climate of New York.

14 SOLAR ENERGY↗

Use of non-contact voltmeter to quantify potential induced degradation in CdTe modules

Potential induced degradation (PID) is a significant reliability issue for photovoltaic modules in the field. Conventionally, to detect the PID-affected modules, all the modules in a string are individually disconnected and measured using I-V (current–voltage) tracers. It is extremely time-consuming, expensive and unsafe (if the module connectors are field aged) approach. In our approach, we aim detecting the PID-affected modules quickly, inexpensively and safely without disconnecting individual modules in the string. In this study, contactless electrostatic voltmeter’s (ESV) strength was explored to detect the PID-affected cadmium telluride (CdTe) modules in a string. These contactless measurements on high-voltage PV strings could make this technique unique and preferable to detect PID-affected modules in a string compared to the I-V curve method. In this work, a CdTe module was stressed for PID using the Aluminum (Al) foil method in a walk-in environmental chamber, which resulted in a reduction of module's peak current (I max ), peak voltage (Vmax), and fill factor (FF), and hence power (Pmax). Outdoor light I-V, EL, and ESV measurements were performed pre- and post-PID to determine the effectiveness of the non-contact ESV technique. Further, the ESV technique successfully detected the change in V max , and hence Pmax, compared to the pre-and post-PID conditions. A difference of less than 2% was observed in the results of the non-contact and non-interruptive method compared to the conventionally used interruptive voltmeter or I-V tracer method. This technique and the test results demonstrate a significant promise to identify poor-performing modules in PV string without disconnection of individual modules in the string.

14 SOLAR ENERGY↗

Nishati Prototype 72-Cell Endurance Modules (Test Report)

US Manufacturer Nishati provided three prototype, 72-cell photovoltaic modules to Sandia for characterization under the US Department of Energy Small Business Voucher program. Nishati is developing the Endurance © product to address the stringent requirements associated with PV system installations sited near airports and military bases. These prototype modules are uniquely constructed of a polymeric matrix and an internal honeycomb structural element. Target features of the module design are reduced reflectivity from the front surface and reduced weight. Sandia applied a variety of in-house characterization methods to these modules with the goal of validating performance and identifying any areas for improvement. Reflectance testing revealed extremely low specular reflection, dramatically surpassing the performance of industry standard PV panels. Electrical performance testing validated performance in line with expectations for similar size and power class modules. Complimentary to reflection testing, outdoor angle of incidence testing indicated performance far exceeding expectations for industry standard PV panels. It is possible that the extremely low reflectance properties of these modules will convey an advantage in annual energy production in comparison to industry standard modules. Detailed performance modeling and experimental field validation would be required to verify this possible advantage. During the course of this testing, no obvious deficiencies in this module design were discovered. It is recommended that Nishati and Sandia proceed to the final Task associated with the SBV award. This final task will involve fielding modules at Sandia for reliability and energy production validation.

14 SOLAR ENERGY↗

Understanding and Overcoming Water-induced Interfacial Degradation in Si Modules (Final Technical Report)

Moisture ingress is an established issue for photovoltaic module durability. Durability studies probing moisture effects typically evaluate performance losses at the module level, attributing global power losses to the overall humidity condition of the test environment while leaving local module behavior unknown. This project successfully develops an in situ short-wave infrared probe of moisture content in PV modules with demonstrated detection limits better than 100 ppm in EVA-encapsulated Al-BSF and PERC architectures (66 µg/cm3) and applicability across the range of terrestrial conditions. Combining this optical moisture quantification method (water reflectometry detection, WaRD) with peel testing of interfaces, biased photoluminescence imaging of performance, and first principles computation, we correlate module moisture content and cell performance over the course of accelerated damp heat tests. By performing multi-level humidity and thermal accelerated testing over thousands of hours (0, 65 and 85% RH and 25, 65, and 85°C), we are able to attribute effects of individual environmental stresses and the dependence on module architecture. Using first-principles computational chemistry, we find that the decomposition of EVA to acetic acid (Norrish II) is thermodynamically preferred over a pathway to acetaldehyde (Norrish I), elucidating the underlying chemistry of encapsulant degradation. We also find it is likely that water segregates to the stable interfaces of the cell, especially the SiNx/EVA interface. We find that moisture is strongly correlated with reduction in adhesion at the interfaces of the cells, particularly at Ag fingers. We show uniquely that the peel strength required to delaminate the encapsulant from the front of the cell depends not only on the exposure to a high heat and humid environment, but also to the moisture content during the mechanical testing, indicating an important interaction between when mechanical stresses are faced in terms of the moisture content of the module and its durability. We find that the background sheet resistance (that is, the sheet resistance rise not attributable to finger interruptions or cracks) is substantially higher in the backsheet mini-modules vs glass-glass packages when humidity and temperature are faced. This increase in power loss due to the background resistance increase over time in damp heat in glass-backsheet modules resulted in ~3-4% larger decrease in relative PCE compared to glass-glass modules. In glass-backsheet modules, the effect of the moisture dose alone is comparable or greater than that of the combined temperature and water term, suggesting that glass-backsheet modules are overall more susceptible to moisture induced performance loss. Finally, we show that thin film PV modules are amenable to WaRD measurement, based on the ability to detect moisture in POE encapsulants or in the cell stack itself. The ease of WaRD measurement and its few requirements on the bill of materials should enable broad applicability of this technique for studying the effects of moisture in PV.

14 SOLAR ENERGY↗

A Module Experimental Process System Development Unit (MEPSDU)

Design work for a photovoltaic module, fabricated using single crystal silicon dendritic web sheet material, resulted in the identification of surface treatment to the module glass superstrate which improved module efficiencies. A final solar module environmental test, a simulated hailstone impact test, was conducted on full size module superstrates to verify that the module's tempered glass superstrate can withstand specified hailstone impacts near the corners and edges of the module. Process sequence design work on the metallization process selective, liquid dopant investigation, dry processing, and antireflective/photoresist application technique tasks, and optimum thickness for Ti/Pd are discussed. A noncontact cleaning method for raw web cleaning was identified and antireflective and photoresist coatings for the dendritic webs were selected. The design of a cell string conveyor, an interconnect feed system, rolling ultrasonic spot bonding heat, and the identification of the optimal commercially available programmable control system are also discussed. An economic analysis to assess cost goals of the process sequence is also given.

Source record↗

Thin film module development

The design of ARCO Solar, Inc.'s Genesis G100 photovoltaic module was driven by several criteria, including environmental stability (both electrical and mechanical), consumer aesthetics, low materials costs, and manufacturing ease. The module circuitry is designed as a 12 volt battery charger, using monolithic patterning techniques on a glass superstrate. This patterning and interconnect method proves amenable to high volume, low cost production throughput, and the use of glass serves the dual role of handling ease and availability. The mechanical design of the module centers on environmental stability. Packaging of the glass superstrate circuit must provide good resistance to thermal and humidity exposure along with hi-pot insulation and hailstone impact resistance. The options considered are given. Ethylene vinyl acetate (EVA) is chosen as the pottant material for its excellent weatherability.

Jester, T.↗