Search NASA⌕ Search

SEARCH · Search NASA

Results for “STRESS CORROSION”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 487 records · Page 27

Gap Analysis to Support Modeling the Long-Term Degradation of Used Nuclear Fuel Canisters

Welded stainless steel canisters are being used worldwide for dry storage of used nuclear fuel (UNF) assemblies, and the number of canisters in use is steadily increasing. In support of work currently being pursued at Pacific Northwest National Laboratory to understand the atmospheric corrosion behavior of spent fuel dry storage systems, a gap analysis is underway to assess the state of knowledge for modeling of the long-term degradation of a UNF canister. The fundamental aim of this work is to inform research and development (R&D) efforts to establish a sound technical basis to support the extended dry storage of UNF for 100+ years. The analysis is considering all major components of the atmosphere corrosion degradation processes, ranging from contaminant sources and climatic interactions to regional conditions of particle transport and deposition, to microscale effects leading to stress corrosion cracking. The results of this gap analysis will be used to define the R&D pathway to develop an integrated multi-scale atmospheric corrosion modeling capability for UNF in dry storage canisters that can support the safe and reliable performance of these structures for more than 100 years.

Nuclear Fuel Canisters↗

Advanced Characterization Capabilities for Nuclear Materials via Nuclear Science User Facilities (NSUF)

Advanced post-irradiation examination (PIE) techniques are required to design new or improved nuclear materials, characterize, and understand in-core behavior of fuel and materials, and support the qualification of new reactor materials. The Nuclear Science User Facilities (NSUF) is the U.S. Department of Energy Office of Nuclear Energy's only designated nuclear science user facility. NSUF provides researchers access to PIE capabilities at Idaho National Laboratory and at a diverse mix of university, national laboratory and industrial partner institutions. The PIE capabilities include novel destructive and non-destructive techniques for radiation damage characterization, such as advanced diffraction techniques (X-ray, electron, or neutron) coupled to extreme environments; in-situ observation of microstructural evolution under irradiation; in-situ irradiation to monitor corrosive attack in coolant environments; in-situ irradiation and mechanical testing; and test methods for synergistic effects of superimposed extreme environments (temperature, irradiation, stress, corrosion) on materials behaviors. This talk will provide an overview of NSUF PIE capabilities.

36 MATERIALS SCIENCE↗

CISCC Countermeasures for Spent Fuel Canisters in Concrete Casks

Aging management of spent fuel is an important issue worldwide. Chloride-induced stress corrosion cracking (CISCC) of welded canisters is particularly important for concrete casks, where it occurs in response to a combination of environmental, material, and residual stress factors. In this paper, we introduce a countermeasure to prevent the occurrence of CISCC by adjusting the flow rate of the cooling air into the concrete cask so that the canister surface temperature does not decrease below 100°C, which is a conservative deliquesce temperature threshold for CISCC occurrence. The flow adjustment device was installed in a cask model, and two tests were conducted under the heat rate conditions corresponding to those of an actual canister. In the first test, the device was operated under a condition where the canister surface temperature was below 100°C to verify whether it could increase the canister surface temperature to above 100°C. In the second test, the heat rate was decreased from a state where the canister surface temperature was above 100°C, to verify whether the device could maintain the canister surface temperature above 100°C. Good results were obtained in both cases. However, in the case of a low decay heat rate of spent fuel after extended dry storage, the temperature of the canister surface may decrease below 100°C even if no air supply is provided. Therefore, in this case, it may be necessary to take measures such as blocking air outlets.

Takeda, Hirofumi↗

SNF Interim Storage Canister Corrosion and Surface Environment Investigations (FY22 Status Update)

High-level purpose of this work: This report summarizes work carried out by Sandia National Laboratories (SNL) in the fiscal year 2022 (FY22) to evaluate the potential occurrence of stress corrosion cracking (SCC) on spent nuclear fuel (SNF) dry storage canisters. The U.S. currently lacks a repository for permanent disposal of SNF; thus, dry storage systems will be in use for much longer time periods than originally intended. Gap analyses by the US Department of Energy (DOE), the Nuclear Regulatory Commission (NRC), the Nuclear Waste Technical Review Board (NWTRB), and the Electric Power Research Institute (EPRI) have all determined that an improved understanding of the occurrence and risk of canister SCC is critical to demonstrating the safety of long-term dry storage. Should canister penetration by SCC occur, the containment boundary represented by the canister would be breached. A loss of the inert environment (helium) within the canister could occur and intrusion of air and moisture could react with and damage the fuel within the canister. For this reason, the DOE is funding an effort to evaluate the potential occurrence and consequences of dry storage canister SCC and to develop prevention, mitigation, and repair technologies for this degradation mechanism.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Preliminary Deposition Modeling: For Determining the Deposition of Corrosive Contaminants on SNF Canisters

This report fulfills the M3 milestone M3SF-20PN010207045. During fiscal year (FY) 2019, Pacific Northwest National Laboratory (PNNL) worked to develop initial deposition and particle tracking models which could be used to better understand how corrosive contaminants deposit on the surfaces of spent nuclear fuel (SNF) canisters during dry storage. These models may be useful in understanding the likelihood of chloride induced stress corrosion cracking (CISCC) on SNF canisters

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Influence of Glycolate Anion on Aqueous Corrosion in DWPF and Downstream Facilities – SCC Testing

Glycolic acid is being evaluated as an alternate reductant in the preparation of High Level Waste for the Defense Waste Processing Facility (DWPF) at the Savannah River Site (SRS). During processing, the glycolic acid may not be completely consumed with small quantities of the glycolate anion being carried forward to waste facilities. The SRS liquid waste contractor requested an assessment of the influence of the glycolate anion on the corrosion of the materials of construction (MoC) throughout the waste processing system since this concern had not been previously evaluated. The influence of glycolic acid on the occurrence of stress corrosion cracking (SCC) had not been evaluated specifically in the previous testing. The present testing used electrochemical and coupon immersion testing to assess this influence. Additionally, the primary guidance on corrosion for operating DWPF with a formate-based flowsheet is based on testing that utilized test solutions with a small number of constituents. Recent testing used more complex solutions based on flowsheet development for DWPF. Additional electrochemical tests were also conducted to assess the influence of this difference on test results.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Fracture toughness evaluation for thin-shell stainless steel weldment

Integrity of spent nuclear fuel (SNF) interim storage canisters are very important to the safety of the back-end nuclear fuel cycle. Stress corrosion cracking (SCC) potential of interim storage canister has been considered as a high priority. Because no post-weld heat treatment was required for forming these canisters, the high tensile residual stress existed within these canister welds. This can change the fracture resistance capacity significantly as well as increase SCC potential. Due to relative thin shell thickness of a canister weldment, the spiral notch torsion test (SNTT) method of small specimen approach was used to estimate the canister weldment fracture toughness. Most SNTT weldment samples fracture initiation sites are at heat-affected zone (HAZ) regions. The estimated fracture toughness $J_Q'$ for the baseline SS304 steel is at 283 kJ/m 2 . The estimated $J_Q'$ for the SS304/308 weld from HAZ and weld specimens are 126 kJ/m 2 and 148.9 kJ/m 2 , respectively.

36 MATERIALS SCIENCE↗

Fracture toughness evaluations for spent nuclear fuel dry storage canister welds and spent nuclear fuel clad-pellet structures

Integrity of spent nuclear fuel (SNF) interim storage canisters is very important to the safety of the back-end nuclear fuel cycle. Stress corrosion cracking (SCC) potential of interim storage canister has been considered as a high priority. Because no post-weld heat treatment was required for forming these canisters, the high tensile residual stress existed within these canister welds. This can change the fracture resistance capacity significantly as well as increase SCC potential. Due to relative thin shell thickness of a canister weldment, the spiral notch torsion test (SNTT) method was used to estimate the canister weldment fracture toughness. SNTT was developed to measure the intrinsic fracture toughness of structural materials using small specimens. The SNTT method has been applied to a wide variety of structural materials, such as low-alloy steels, stainless steel, aluminum alloy, ceramics, concrete, and composites. The SNTT system operates by applying pure torsion to cylindrical specimens with a notch line that spirals around the specimen at a 45° pitch. In order to carry out pure torsion load mode, biaxial tension/torsion tester was developed accordingly to perform SNTT protocol. Moreover, applying fracture mechanics approach to SNF system reliability investigation is warranted due to the inherent flaws and hydride structures existed in a SNF system after nuclear reactor operation. However, none of the existing fracture toughness data deal with fuel cladding specific geometry or spent fuel material conditions, such as cladding structure with the pellet-inserts and the associated pellet clad mechanical interactions induced mixed-mode damage mechanisms. Thus, the development of an intrinsic fracture mechanics approach that is suitable for SNF materials is needed. Furthermore, due to thin wall and small dimension of clad tubing structure, the SNTT method was used to estimate the clad tubing structure fracture toughness. Fracture testing were performed on the received stainless steel canister weldment, most SNTT weld samples fracture initiation sites are at heat-affected zone (HAZ) regions. The estimated fracture toughness J Q ’ for the baseline SS304 steel is at 283 kJ/m². The estimated JQ’ for the SS304/308 weld and baseline metals are 148 kJ/m 2 and 459 kJ/m 2 , respectively. Out of cell fracture testing for spent fuel structure were carried out on the surrogate rods made of Zr-4 clad and alumina inserts, the estimated fracture toughness values for baseline Zr-4 cladding with alumina-pellet inserts are: (1) For SNTT samples with a short or medium crack length, between 5.4-mm and 8-mm, the estimate J IQ upon fracture initiation for the baseline Zr-4 cladding is at 50 kJ/m 2 with 2-sigma uncertainty of 3.26 kJ/m 2 , and the associated K IQ is at 67.46 MPa$\sqrt{m}$; and (2) For SNTT samples with a long crack length, around 13-mm, the crack initialization is deviated from that of the Mode-I tensile fracture and appears to be a mixed-mode fracture of Mode I - tensile stress and Mode III - out of plane shear stress; the estimated J MQ is at 18.9 kJ/m 2 , the associated K MQ is at 41.4 MPa$\sqrt{m}$.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Microtructure and Low-Cycle Fatigue Behavior of Additively Manufactured 316L Stainless Steel at 300°C

Metal additive manufacturing (AM) or 3D printing has the potential to transform the nuclear industry by producing high quality components faster and cheaper, thus enhancing the operating performance of current plants and advanced reactors. Two AM 316L tubes - intended to act as surrogates for complex components where nuclear equipment vendors are more likely to consider AM technologies - were printed using a Renishaw AM400 Laser Powder Bed Fusion (L-PBF) system. The porosity of the as-built material was found to be small, 0.06%. In prior research, the fatigue and corrosion fatigue crack growth rate (CGR) response of the AM specimens in the as-built condition was found to be similar to that expected for conventional alloys, and extremely resistant to stress corrosion cracking (SCC). The present research demonstrates that the low-cycle fatigue behavior of the AM material in air is similar to that of wrought stainless steel at LWR temperature. The data suggest that low porosity levels do not have a significant effect on the fatigue performance of AM materials. Taken together, all data generated to date demonstrate that the use of AM alloys in a nuclear environment is plausible. Additional research on environmental fatigue, crack initiation, and SCC needs to be conducted to provide the performance information needed to qualify AM materials for LWR applications.

36 MATERIALS SCIENCE↗

SNF Canister Coatings for Corrosion Prevention and Mitigation (FY21 Status Report)

This report summarizes the current actives in FY21 related to the effort by Sandia National Laboratories to identify and test coating materials for the prevention, mitigation, and repair of spent nuclear fuel dry storage canisters against potential chloride-induced stress corrosion cracking. This work follows up on the details provided in Sandia National Laboratories FY20 report on the same topic, which provided a detailed description of the specific coating properties desired for application and implementation on spent nuclear fuel canisters, as well as provided detail into several different coatings and their applicability to coat spent nuclear fuel canisters. In FY21, Sandia National Laboratories has engaged with private industry to create a Memorandum of Understanding and established a collaborative R&D program building off the analytical and laboratory capabilities at Sandia National Laboratories and the material design and synthesis capabilities of private industry. The resulting Memorandum of Understanding included four companies to date (Oxford Performance Materials, White Horse R&D, Luna Innovations, and Flora Coating) proposing six different coating technologies (polyetherketoneketone, modified polyimide/polyurea, modified phenolic resin, silane-based polyurethane hybrid with and without a Znrich primer, and a quasi-ceramic sol-gel polyurethane hybrid) to be tested, evaluated, and optimized for their potential use for this application. This report provides a detailed description of each of the coating systems proposed by the participating industry partners. It also provides a description of the planned experimental actives to be performed by Sandia National Laboratories including physical tests, electrochemical tests, and characterization methods. These analyses will be used to identify specific ways to further improve coating technologies toward their application and implementation on spent nuclear fuel canisters. In FY21, Sandia National Laboratories began baseline testing of the base metal material in according with activities of the Memorandum of Understanding. In FY22, Sandia National Laboratories will receive coated coupons from each of the participating industry partners and begin characterization, physical, and electrochemical testing following the test plan described herein.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Intergranular corrosion of Ni-30Cr in high-temperature hydrogenated water after removing surface passivating film

Abstract High-resolution transmission electron microscopy and atom probe tomography are used to characterize the initial passivation and subsequent intergranular corrosion of degraded grain boundaries in a model Ni-30Cr alloy exposed to 360 °C hydrogenated water. Upon initial exposure for 1000 h, the alloy surface directly above the grain boundary forms a thin passivating film of Cr 2 O 3 , protecting the underlying grain boundary from intergranular corrosion. However, the metal grain boundary experiences severe Cr depletion and grain boundary migration during this initial exposure. To understand how Cr depletion affects further corrosion, the local protective film was sputtered away using a glancing angle focused ion beam. Upon further exposure, the surface fails to repassivate, and intergranular corrosion is observed through the Cr-depleted region. Through this combination of high-resolution microscopy and localized passive film removal, we show that, although high-Cr alloys are resistant to intergranular attack and stress corrosion cracking, degradation-induced changes in the underlying metal at grain boundaries make the material more susceptible once the initial passive film is breached.

(S)TEM↗

Adaptation of Crack Growth Detection Techniques to US Material Test Reactors

A key component in evaluating the ability of Light Water Reactors to operate beyond 60 years is characterizing the degradation of materials exposed to radiation and various water chemistries. Of particular concern is the response of reactor materials to Irradiation Assisted Stress Corrosion Cracking (IASCC). Some materials testing reactors (MTRs) outside the U.S., such as the Halden Boiling Water Reactor (HBWR), have deployed a technique to measure crack growth propagation during irradiation. This technique incorporates a compact loading mechanism to stress the specimen during irradiation. A crack in the specimen is monitored using the Direct Current Potential Drop (DCPD) method. A project is underway to develop and demonstrate the performance of a similar type of test rig for use in U.S. MTRs. The first year of this three year project was devoted to designing, analyzing, fabricating, and bench top testing a mechanism capable of applying a controlled stress to specimens while they are irradiated in a pressurized water loop (simulating PWR reactor conditions). During the second year, the mechanism will be tested in autoclaves containing high pressure, high temperature water with representative water chemistries. In addition, necessary documentation and safety reviews for testing in a reactor environment will be completed. In the third year, the assembly will be tested in the Massachusetts Institute of Technology Reactor (MITR) and Post Irradiation Examinations (PIE) will be performed.

36 MATERIALS SCIENCE↗

Grain boundary damage evolution and SCC initiation of cold-worked alloy 690 in simulated PWR primary water

Long-term grain boundary (GB) damage evolution and stress corrosion crack initiation in alloy 690 are being investigated by constant load tensile testing in high-temperature, simulated PWR primary water. Six commercial alloy 690 heats are being tested in various cold work conditions loaded at their yield stress. This paper reviews the basic test approach and detailed characterizations performed on selected specimens after an exposure time of ~1 year. Intergranular crack nucleation was observed under constant stress in certain highly cold-worked (CW) alloy 690 heats and was found to be associated with the formation of GB cavities. Somewhat surprisingly, the heats most susceptible to cavity formation and crack nucleation were thermally treated materials with most uniform coverage of small GB carbides. Microstructure, % cold work and applied stress comparisons are made among the alloy 690 heats to better understand the factors influencing GB cavity formation and crack initiation.

Alloy 690↗

The Nuclear Fuel Cycle: Safe Management of Spent Nuclear Fuel

The aim for storage of spent nuclear fuel (SNF) either in wet or in dry storage systems is to ensure general safety objective s are met throughout a desired storage period. Staff at the Savannah River National Laboratory (SRNL), in collaborations with partners at other national laboratories, industry research organizations, and the University of South Carolina (UofSC), have performed materials aging testing and analyses, and have established nuclear materials aging management programs to support extended periods of safe storage of research reactor (RR) SNF and of commercial power reactor (PR) SNF pending ultimate disposal. Several example challenges include susceptibility of aluminum SNF from research reactors to corrosion in poor quality water (wet storage). In dry storage, aluminum SNF can release hydrogen via radiolysis of the hydrated oxides on the aluminum cladding. Austenitic stainless steel canisters used for dry storage are susceptible to chloride-induced stress corrosion cracking (outside-in attack) that threaten the confinement boundary provided by the canister. This paper further describes these challenges, among others, and the formulated solutions to support extended safe storage of SNF.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

THERMAL STRESS ANALYSIS OF A SPENT NUCLEAR FUEL CANISTER

The potential for chloride induced stress corrosion cracking (CISCC) in spent nuclear fuel dry storage canisters is a current topic of research by the US Department of Energy Spent Fuel and Waste Science and Technology program. One of the important prerequisites for CISCC is a tensile residual stress state. This study utilizes computational models to provide an initial analysis of thermal stresses in a generic spent nuclear fuel canister. A STAR-CCM+ thermal fluid model provides a temperature profile analysis of the canister based on four different ambient temperature conditions. An ANSYS APDL finite element model incorporates the temperature profiles to analyze the thermal stresses in the canister. The calculated thermal stress magnitudes are in the range of 10 MPa to 80 MPa, which could be significant for crack propagation through the canister wall. The maximum thermal stress is not a concern for the structural failure of the canister, but it is high enough that it is a significant contribution to the total stress state of the canister wall, which also includes residual stress from fabrication, internal pressure from helium cover gas, and potential transient mechanical loads, such as earthquakes. This paper describes the initial finite element thermal stress analysis that was completed in 2020, reports the initial findings, and identifies areas where model refinement is still needed to complete this work in the future.

Jensen, Ben J.↗

Crack Initiation Behavior of Cold-Worked Alloy 690 in Simulated PWR Primary Water - Role of Starting Microstructure, Applied Stress and Cold Work on Precursor Damage Evolution

Long-term stress corrosion crack (SCC) initiation behavior in Alloy 690 is being evaluated by constant load tensile testing in simulated pressurized water reactor primary water. Seven commercial Alloy 690 heats with different starting microstructures and cold-work levels are being tested at either 90% or 100% of the material yield stress. Previous studies have revealed grain boundary (GB) cavity formation after 7,110 to 9,220 hours of exposure in certain thermally treated (TT) Alloy 690 heats in highly cold-worked (CW) conditions, serving as precursors to intergranular cracks. This paper summarizes the new characterization results for the evolution of GB cavities in four Alloy 690TT heats in 21% and 31%CW conditions loaded at yield stress after 18,400 hours of exposure. Link-up of GB cavities has led to formation of long internal creep cracks, resulting in crack initiation detected by direct current potential drop in a highly CW Alloy 690TT heat with uniform, semi-continuous distribution of small GB carbides. In comparison, highly CW materials featuring larger and more widely spaced GB carbides did not show a significant increase in GB cavity density or size. Quantitative assessments were performed on GB cavity evolution in highly CW specimens for two Alloy 690TT heats demonstrating the strong dependence of GB cavity evolution on applied stress and starting GB microstructure.

Zhai, Ziqing↗

Residual Stresses and Other Properties of Teardrops

The Department of Energy’s 3013 Standard for packaging plutonium-bearing materials for storage up to fifty years specifies a minimum of two individually welded, nested containers herein referred to as the 3013 outer and the 3013 inner.1 Stress corrosion cracking (SCC) is a potential failure mechanism for 3013 inner containers.2,3 The bagless transfer container (BTC), a 3013 inner container used by Hanford and Savanna River Site (SRS) made from 304L stainless steel (SS), poses the greatest concern for SCC.4,5 The Surveillance and Monitoring Program (SMP) use stressed metal samples known as teardrops as screening tools in SCC studies to evaluate factors that could result in cracks in the 3013 containers.6,7 This report provides background information on the teardrops used in the Los Alamos National Laboratory (LANL) SMP studies including method of construction, composition and variability. In addition, the report discusses measurements of residual stresses in teardrops and compares the results with residual stresses in BTCs reported previously.4 Factors affecting residual stresses, including teardrop dimensions and surface finish, are also discussed.

36 MATERIALS SCIENCE↗

Residual Stresses in SAVY 4000 and Hagan Container Bodies

Chloride-induced stress corrosion cracking (SCC) has been investigated as a potential failure mechanism for the SAVY 4000 and the Hagan containers used to store plutonium-bearing materials at Los Alamos National Laboratory. This report discusses the regions of the container bodies most susceptible to SCC and the magnitude of the residual stresses in those regions. Boiling MgCl2 testing indicated that for both containers the region near the top weld was most susceptible to SCC. The Hagan showed through wall cracking after 22-24 hours of exposure both parallel (axial stresses) and perpendicular (hoop stresses) to the weld. The SAVY 4000 container showed significant cracking above and below the weld after 47 hours of exposure but there was no visual evidence of a through wall crack and the cracks did not leak water. Two through wall holes formed in the bottom of the SAVY 4000 container after 44-46 hours of exposure. For both containers, average “through wall” residual stresses were determined from hole drilling data 4 mm below the weld. In the Hagan body, average tensile hoop stresses were 194 MPa and average compressive axial stresses were -120 MPa. In the SAVY 4000 body, average compressive hoop stresses were 11 MPa and average tensile axial stresses were 25 MPa. Results suggest that because the Hagan container exhibited through wall cracking in a shorter time in boiling MgCl2 and had the higher average tensile stress, 194 MPa hoop stress, it is more susceptible to SCC than the SAVY 4000 container.