At least 487 records · Page 27

Production of Nanoscale Detonation Carbon using a Pulse Gas-Detonation Device

Combustion and thermal decomposition of hydrocarbon fuels are used to produce different forms of carbon. Combustion in the detonation mode is of particular interest, as nanocarbon obtained under these conditions differs in properties from products synthesized by other techniques. A pulsed gas-detonation device designed on the basis of a CCDS2000 detonation spraying facility opens up new possibilities for manufacturing of nanocarbon. The device operates in a flow mode of gas supply into the reactor at the atmospheric pressure, which ensures high productivity and industrial safety of this method. Using detonation of acetylene-oxygen mixtures rich in acetylene, nanoscale carbon was obtained with particle morphology depending on the ratio of the components in the gaseous mixture.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Shuttle active thermal control system development testing. Volume 7: Improved radiator coating adhesive tests

Silver/Teflon thermal control coatings have been tested on a modular radiator system projected for use on the space shuttle. Seven candidate adhesives have been evaluated in a thermal vacuum test on radiator panels similar to the anticipated flight hardware configuration. Several classes of adhesives based on polyester, silicone, and urethane resin systems were tested. These included contact adhesives, heat cured adhesives, heat and pressure cured adhesives, pressure sensitive adhesives, and two part paint on or spray on adhesives. The coatings attached with four of the adhesives, two silicones and two urethanes, had no changes develop during the thermal vacuum test. The two silicone adhesives, both of which were applied to the silver/Teflon as transfer laminates to form a tape, offered the most promise based on application process and thermal performance. Each of the successful silicone adhesives required a heat and pressure cure to adhere during the cryogenic temperature excursion of the thermal-vacuum test.

Reed, M. W.↗

Monitoring Delamination of Plasma-Sprayed Thermal Barrier Coatings by Reflectance-Enhanced Luminescence

Highly scattering plasma-sprayed thermal barrier coatings (TBCs) present a challenge for optical diagnostic methods to monitor TBC delamination because scattering attenuates light transmitted through the TBC and usually degrades contrast between attached and delaminated regions of the TBC. This paper presents a new approach where reflectance-enhanced luminescence from a luminescent sublayer incorporated along the bottom of the TBC is used to identify regions of TBC delamination. Because of the higher survival rate of luminescence reflecting off the back surface of a delaminated TBC, the strong scattering exhibited by plasma-sprayed TBCs actually accentuates contrast between attached and delaminated regions by making it more likely that multiple reflections of luminescence off the back surface occur before exiting the top surface of the TBC. A freestanding coating containing sections designed to model an attached or delaminated TBC was prepared by depositing a luminescent Eu-doped or Er-doped yttria-stabilized zirconia (YSZ) luminescent layer below a plasma-sprayed undoped YSZ layer and utilizing a NiCr backing layer to represent an attached substrate. For specimens with a Eu-doped YSZ luminescent sublayer, luminescence intensity maps showed excellent contrast between unbacked and NiCr-backed sections even at a plasma-sprayed overlayer thickness of 300 m. Discernable contrast between unbacked and NiCr-backed sections was not observed for specimens with a Er-doped YSZ luminescent sublayer because luminescence from Er impurities in the undoped YSZ layer overwhelmed luminescence originating form the Er-doped YSZ sublayer.

Eldridge, Jeffrey I.↗

Nanostructured Cathodes for Solid Oxide Fuel Cells by a Solution Spray-Coating Process

Composite nano-cathodes containing Sr-doped LaMnO 3 (LSM) and Gd 2 O 3 -doped CeO 2 (GDC) were deposited on yttria-stabilized zirconia (YSZ) discs and YSZ/NiO + YSZ bi-layer discs using an aqueous solution. The samples were heated over a range of temperatures from 700°C to 1200°C to form LSM + GDC porous films. The crystallite size was estimated using X-ray diffraction (XRD) Scherrer formula. The crystallite size was in the ~3 nm to ~80 nm range. Polarization resistance was measured by electrochemical impedance spectroscopy (EIS) from 400°C to 700°C. Nano-cathodes of ~70 nm thickness fired at 700°C exhibited polarization resistance of ~0.23 Ωcm 2 at 700°C. By contrast, LSM + YSZ cathodes made by a conventional process exhibited polarization resistance of ~2 Ωcm 2 . Fuel cell tests were conducted at 700°C on cells with nano-cathodes and conventional LSM + YSZ cathode. The maximum power density was ~0.51 Wcm –2 with nano-cathodes. By contrast, the corresponding power density with conventional LSM + YSZ cathodes was ~0.11 Wcm –2 . Here, the present work shows that very thin cathode functional layers can be deposited on sintered YSZ/NiO + YSZ bi-layer discs by using an aqueous solution. This approach in principle could be extended to large area cells.

36 MATERIALS SCIENCE↗

Ditching Tests of a 1/18-Scale Model of the Lockheed Constellation Airplane

Tests were made of a 1/18-scale dynamically similar model of the Lockheed Constellation airplane to investigate its ditching characteristics and proper ditching technique. Scale-strength bottoms were used to reproduce probable damage to the fuselage. The model was landed in calm water at the Langley tank no. 2 monorail. Various landing attitudes, speeds, and fuselage configuration were simulated. The behavior of the model was determined from visual observations, by recording the longitudinal decelerations, and by taking motion pictures of the ditchings. Data are presented in tabular form, sequence photographs, and time-history deceleration curves. It was concluded that the airplane should be ditched at a medium nose-high landing attitude with the landing flaps full down. The airplane will probably make a deep run with heavy spray and may even dive slightly. The fuselage will be damaged and leak substantially but in calm water probably will not flood rapidly. Maximum longitudinal decelerations in a calm-water ditching will be about 4g.

Fisher, Lloyd J.↗

Natural chlorine and fluorine in the atmosphere, water and precipitation

The geochemical cycles of chlorine and fluorine are surveyed and summarized as framework for the understanding of the global natural abundances of these species in the atmosphere, water, and precipitation. In the cycles the fluxes into and out of the atmosphere can be balanced within the limits of our knowledge of the natural sources and sinks. Sea salt from the ocean surfaces represent the predominant portion of the source of chlorine. It is also an important source of atmospheric fluorine, but volcanoes are likely to be more important fluorine sources. Dry deposition of sea salt returns about 85 percent of the salt released there. Precipitation removes the remainder. Most of the sea salt materials are considered to be cyclic, moving through sea spray over the oceans and either directly back to the oceans or deposited dry and in precipitation on land, whence it runs off into rivers and streams and returns to the oceans. Most of the natural chlorine in the atmosphere is in the form of particulate chloride ion with lesser amounts as gaseous inorganic chloride and methyl chloride vapor. Fluorine is emitted from volcanoes primarily as HF. It is possible that HF may be released directly form the ocean surface but this has not been confirmed by observation. HCl and most likely HF gases are released into the atmosphere by sea salt aerosols. The mechanism for the release is likely to be the provision of protons from the so-called excess sulfate and HNO3. Sea salt aerosol contains fluorine as F(-), MgF(+), CaF(+), and NaF. The concentrations of the various species of chlorine and fluorine that characterize primarily natural, unpolluted atmospheres are summarized in tables and are discussed in relation to their fluxes through the geochemical cycle.

Friend, James P.↗

ADVANCED TEST REACTOR (ATR) CONVERSION TO LOW ENRICHED URANIUM (LEU) FUEL

The United States Department of Energy (DOE), National Nuclear Security Administration (NNSA), Office of Material Management and Minimization (MMM) is working to convert research reactors globally from highly enriched uranium (HEU) fuel to low-enriched uranium (LEU) fuel. MMM and its predecessor programs have converted or verified the shutdown of 88 HEU research reactors and isotope production facilities, using LEU fuel developed in the 1980s. However, there is a small set of high performance research reactors which require a new high density LEU fuel for conversion, including six U.S. high performance research reactors (USHPRRs), which include the Advanced Test Reactor (ATR) and the ATR Critical (ATRC) Facility at the Idaho National Laboratory (INL) near Idaho Falls, ID; University of Missouri Research Reactor (MURR) at Columbia, MO; Massachusetts Institute of Technology Reactor (MITR) at MIT in Cambridge, MA; High Flux Isotope Reactor (HFIR) at Oak Ridge National Laboratory (ORNL) near Oak Ridge, TN; and National Bureau of Standards Reactor (NBSR) at the National Institute of Standards and Technology (NIST) Center for Neutron Research (NCNR) in Gaithersburg, MA. These reactors will share the same uranium-molybdenum (U-Mo) fuel plate design. The U-Mo fuel meat foil will have a zirconium (Zr) diffusion barrier with aluminum cladding. Three different application methods for the Zr diffusion barrier layer are being pursued – co-rolled, electroplating and plasma spraying. Fabrication of the higher density LEU U-Mo fuel has presented several challenges. Because the U-Mo fuel fabrication process uses the existing stockpile of 93% highly enriched uranium (HEU) to be blended with molybdenum and depleted uranium (DU) to form 19.75% LEU, cost benefits of enriching to 19.75% will not be realized. Homogeneity of the U-235 and molybdenum in the metal foil is a challenge due to U-Mo casting process results in variations between adjacent cast U-Mo plates. LEU will not require less U-235 as previously believed due to self-shielding properties of U-238 requiring additional U-235 to be loaded in each fuel element. Although the overall dimensions of the ATR fuel element remain unchanged, the weight of the LEU ATR fuel element is 72% greater than a HEU ATR fuel element. During waste recovery and recycling efforts, separation of aluminum cladding from the HEU fuel meat is a relatively simple chemical dissolution, however, separation of the Zr diffusion barrier from the U-Mo fuel meat is significantly more challenging.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

High-Temperature Erosive Behavior of Plasma Sprayed Cr{sub 3}C{sub 2}-NiCr/Cenosphere Coating

This research examines the deposition of Cr{sub 3}C{sub 2}-NiCr/cenosphere and Cr{sub 3}C{sub 2}-NiCr coatings on MDN 321 steel through the process of plasma spray. In this process, the solid particle erosion test is established at 200, 400, 600 °C with 30° and 90° impact angles. Alumina erodent is adopted to investigate the erosive behavior of the coating at higher temperatures. The properties of the Cr{sub 3}C{sub 2}-NiCr/cenosphere coating are established based on the microhardness, the adhesive strength, the fracture toughness, and the ductility. To quantify volume loss as a result of erosion, an optical profilometer is used. At higher temperature, decrease in the erosion volume loss of Cr{sub 3}C{sub 2}-NiCr/cenosphere and Cr{sub 3}C{sub 2}-NiCr coatings is observed. The erosion-resistive property of Cr{sub 3}C{sub 2}-NiCr/cenosphere coating is higher than that of MDN 321 steel by 76%. This property is influenced by high-temperature stability of mullite, alumina, and protective oxide layer that is formed at elevated temperatures. The morphology of eroded coating discloses a brittle mode of material removal.

36 MATERIALS SCIENCE↗

Degradation of Thermal Barrier Coatings from Deposits and Its Mitigation

Ceramic thermal barrier coatings (TBCs) used in gas-turbine engines afford higher operating temperatures, resulting in enhanced efficiencies and performance. However, in the case of syngas-fired engines, fly ash particulate impurities that may be present in syngas can melt on the hotter TBC surfaces and form glassy deposits. These deposits can penetrate the TBCs leading to their failure. In experiments using lignite fly ash to simulate these conditions we show that conventional TBCs of composition 93wt% ZrO 2 + 7wt% Y 2 O 3 (7YSZ) fabricated using the air plasma spray (APS) process are completely destroyed by the molten fly ash. The molten fly ash is found to penetrate the full thickness of the TBC. The mechanisms by which this occurs appear to be similar to those observed in degradation of 7YSZ TBCs by molten calcium-magnesium-aluminosilicate (CMAS) sand and by molten volcanic ash in aircraft engines. In contrast, APS TBCs of Gd 2 Zr 2 O 7 composition are highly resistant to attack by molten lignite fly ash under identical conditions, where the molten ash penetrates ~25% of TBC thickness. This damage mitigation appears to be due to the formation of an impervious, stable crystalline layer at the fly ash/Gd 2 Zr 2 O 7 TBC interface arresting the penetrating molten-fly-ash front. Additionally, these TBCs were tested using a rig with thermal gradient and simultaneous accumulation of ash. Modeling using an established mechanics model has been performed to illustrate the modes of delamination, as well as further opportunities to optimize coating microstructure. Transfer of the technology was developed in this program to all interested parties.

20 FOSSIL-FUELED POWER PLANTS↗

Probing early parton emissions in heavy ion collisions using the Lund jet plane

In scattering experiments, high-virtuality partons, i.e., quarks and gluons, initiate a series of additional parton emissions to create collimated sprays of particles known as jets. This paper presents a measurement of the Lund jet plane (LJP) of high-energy jets produced in lead-lead (PbPb) collisions and compares the results to data for proton-proton (pp) collisions. The LJP is formed by iteratively declustering the constituents of a jet into consecutive emissions and recording the relative transverse momentum ($k_\mathrm{T}$) and angle of the resulting emission with respect to its emitter. The angular distributions of two different $k_\mathrm{T}$ slices of the LJP are investigated for jets with radius parameter of 0.4 and transverse momentum in the range 200$-$1000 GeV. The PbPb (pp) data were recorded by the CMS experiment in 2018 (2017) and correspond to an integrated luminosity of 1.7 nb$^{-1}$ (301 pb$^{-1}$) at a nucleon-nucleon center-of-mass energy of 5.02 TeV. The measurement was designed to test whether the earliest jet emissions are produced before the formation of the quark-gluon plasma (QGP) in PbPb collisions. Within the experimental uncertainties, no significant difference is observed between the angular distribution of high-$k_\mathrm{T}$ emissions in \pp and PbPb collisions, which is consistent with these emissions occurring early in the jet evolution, before substantial interaction with the QGP.

Belyaev, Andrey [Yerevan Phys. Inst.] (ORCID:00000↗

Residual stress analysis of multilayer environmental barrier coatings.

Silicon-based ceramics (SiC, Si{sub 3}N{sub 4}) are promising materials systems for high-temperature structural applications in gas turbine engines. However, the silica layer that forms on these materials is susceptible to attack from water vapor present in combustion environments. To protect against this degradation, environmental barrier coatings (EBCs) have been developed to shield the underlying substrate and prevent degradation. Here we report on elastic and thermal properties, as well as internal stresses of candidate multilayer coatings, as measured in situ using microfocused high-energy X-rays in a transmission diffraction geometry. Doped aluminosilicate coatings were investigated for their stability on a SiC/SiC melt-infiltrated substrate. The coatings consisted of a Ba{sub 1-x}Sr{sub x}Al{sub 2}Si{sub 2}O{sub 8} topcoat with a mullite or mullite+SrAl{sub 2}Si{sub 2}O{sub 8} interlayer, and a silicon bond coat. A numerical model was used to compare the stress results with an ideal coating system. Experiments were carried out on as-sprayed and heat-treated samples in order to analyze the strain and phase evolution as a function of multilayer depth and temperature. The phase transformation of the topcoat promoted healing of cracks in the EBC and reduced stresses in the underlying layers and the addition of SAS to the interlayer reduced stresses in thermally cycled coatings, but did not stop cracks from forming.

33 ADVANCED PROPULSION SYSTEMS↗

Coke Deposition and Smoke Formation in Turbojet Engines

In the early development of jet engines, it was occasionally found that excessive amounts of coke or other carbonaceous deposits were formed in the combustion chamber. Sometimes a considerable amount of smoke was noted in the-exhaust gases. Excessive coke deposits may adversely affect jet-engine performance in several ways. The formation of excessive amounts of coke on or just downstream of a fuel nozzle (figs. 116(a) and (b)) changes the fuel-spray pattern and possibly affects combustor life and performance. Similar effects on performance can result from the deposition of coke on primary-air entry ports (fig. 116(c)). Sea-level or altitude starting may be impaired by the deposition of coke on spark-plug electrodes (fig. 116(b)), deposits either grounding the electrodes completely or causing the spark to occur at positions other than the intended gap. For some time it was thought that large deposits of coke in turbojet combustion chambers (fig. 116(a)) might break away and damage turbine blades; however, experience has indicated that for metal blades this problem is insignificant. (Cermet turbine blades may be damaged by loose coke deposits.) Finally, the deposition of coke may cause high-temperature areas, which promote liner warping and cracking (fig. 116(d)) from excessive temperature gradients and variations in thermal-expansion rates. Smoke in the exhaust gases does not generally impair engine performance but may be undesirable from a tactical or a nuisance standpoint. Appendix B of reference 1 and references 2 to 4 present data obtained from full-scale engines operated on test stands and from flight tests that indicate some effects on performance caused by coke deposits and smoke. Some information about the mechanism of coke formation is given in reference 5 and chapter IX. The data indicate that (1) high-boiling fuel residuals and partly polymerized products may be mixed with a large amount of smoke formed in the gas phase to account for the consistency, structure, and chemical composition of the soft coke in the dome and (2) the hard deposits on the liner are similar to petroleum coke and may result from the liquid-phase thermal cracking of the fuel. During the early development period of jet engines, it was noted that the excessive coke deposits and exhaust smoke were generally obtained when fuel-oil-type fuels were used. Engines using gasoline-type fuels were relatively free from the deposits and smoke. These results indicated that some type of quality control would be needed in fuel specifications. Also noted was the effect of engine operating conditions on coke deposition. It is possible that, even with a clean-burning fuel, an excessive amount of coke could be formed at some operating conditions. In this case, combustor redesign could possibly reduce the coke to a tolerable level. This chapter is a summary of the various coke-deposition and exhaust-smoke problems connected- with the turbojet combustor. Included are (1) the effect of coke deposition on combustor life or durability and performance; (2) the effect of combustor design, operating conditions, inlet variables, and fuel characteristics on coke deposition; (3) elimination of coke deposits; (4) the effect of operating conditions and fuel characteristics on formation of exhaust smoke; and (5) various bench test methods proposed for determining and controlling fuel quality.

Hibbard, R. R.↗

Characterization of Ceramic Plasma-Sprayed Coatings, and Interaction Studies Between U-Zr Fuel and Ceramic Coated Interface at an Elevated Temperature

Candidate coating materials for re-usable metallic nuclear fuel crucibles, HfN, TiC, ZrC, and Y2O3, were plasma-sprayed onto niobium substrates. The coating microstructure and the thermal cycling behavior were characterized, and U-Zr melt interaction studies carried out. The Y2O3 coating layer had a uniform thickness and was well consolidated with a few small pores scattered throughout. While the HfN coating was not well consolidated with a considerable amount of porosity, but showed somewhat uniform thickness. Thermal cycling tests on the HfN, TiC, ZrC, and Y2O3 coatings showed good cycling characteristics with no interconnected cracks forming even after 20 cycles. Interaction studies done on the coated samples by dipping into a U-20wt.%Zr melt indicated that HfN and Y2O3 did not form significant reaction layers between the melt and the coating while the TiC and the ZrC coatings were significantly degraded. Y2O3 exhibited the most promising performance among HfN, TiC, ZrC, and Y2O3 coatings.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

High density tape casting system

A system is provided for casting thin sheets (or tapes) of particles bound together, that are used for oxygen membranes and other applications, which enables the particles to be cast at a high packing density in a tape of uniform thickness. A slurry contains the particles, a binder, and a solvent, and is cast against the inside walls of a rotating chamber. Prior to spraying the slurry against the chamber walls, a solvent is applied to a container. The solvent evaporates to saturate the chamber with solvent vapor. Only then is the slurry cast. As a result, the slurry remains fluid long enough to spread evenly over the casting surface formed by the chamber, and for the slurry particles to become densely packed. Only then is the chamber vented to remove solvent, so the slurry can dry. The major novel feature is applying solvent vapor to a rotating chamber before casting slurry against the chamber walls.

Collins, Earl R., Jr.↗

Fire Protection Materials

Avco has drawn upon its heat shield experience to develop a number of widely-accepted commercial fire protection materials. Originating from NASA's space shuttle thermal protection system, one such material is Chartek 59 fireproofing, an intumescent epoxy coating specifically designed for outdoor use by industrial facilities dealing with highly flammable products such as oil refineries and chemical plants. The coating is applied usually by spray gun to exterior structural steel conduits, pipes and valves, offshore platforms and liquefied petroleum gas tanks. Fireproofing provides two types of protection: ablation or dissipation of heat by burn-off and "intumescence" or swelling; the coating swells to about five times its original size, forming a protective blanket of char which retards transfer of heat to the metal structure preventing loss of structural strength and possible collapse which would compound the fire fighting problem.

Source record↗

Computer Modeling and Analysis of Truck Generated Salt-Spray Transport Near Bridges

Bridge painting is very expensive. Over the lifetime of a bridge, painting to protect the steel from the elements can cost a large fraction of the original construction cost. In addition to monetary costs, maintenance workers face health risks if strict procedures are not in place to avoid exposure to hazardous dust when old paint is removed and the fumes of hazardous chemicals when new paint is applied. Use of weathering steel in bridge construction avoids the large cost of periodic painting and the hazards of paint removal and repainting because this type of steel is never painted. When exposed to weather, the initial corrosion of weathering steel forms a natural corrosion resistant layer that prevents further corrosion under a wide variety of conditions. Given the advantages of using weathering steel, the choice might appear to be obvious. However, the large potential savings in bridge maintenance costs in using weathering steel are not always realized because the protective patina layer fails to adhere when the steel is exposed to excessively salt-laden and moisture-laden environments. A multi-year study is underway by the FHWA to better quantify the conditions that lead to excessive corrosion in weathering steel bridges. This report documents work using computational fluid dynamics (CFD) analysis to study the conditions and mechanisms that lead from the salt spray thrown from truck tires to salt water droplets reaching bridge girders. Computer simulations use the advanced motion modeling capability called a “sliding mesh” in the CFD software to move one or more large trucks under bridges at 60 mph. The computations include multiphase spray droplet tracking of salt-laden water droplets coming off the tires.

Lottes, S. A.↗

Using Ambient Ion Beams to Write Nanostructured Patterns for Surface Enhanced Raman Spectroscopy

Electrolytic spray deposition was used to pattern surfaces with 2D metallic nanostructures. Spots that contain silver nanoparticles (AgNP) were created by landing solvated silver ions at desired locations using electrically floated masks to focus the metal ions to an area as little as 20 mm in diameter. The AgNPs formed are unprotected and their aggregates can be used for surface-enhanced Raman spectroscopy (SERS). The morphology and SERS activity of the NP structures were controlled by the surface coverage of landed silver ions. The NP structures created could be used as substrates onto which SERS samples were deposited or prepared directly on top of predeposited samples of interest. The evenly distributed hot spots in the micron-sized aggregates had an average SERS enhancement factor of 108. The surfaces showed SERS activity when using lasers of different wavelengths (532, 633, and 785 nm) and were stable in air.

Environmental Molecular Sciences Laboratory↗

Phase distributions in plasma-sprayed zirconia-yttria

The distribution of phases in plasma-sprayed zirconia-yttria has been determined over a range of yttria levels from 0 to 26.1 molpct YO(1.5) using room temperature X-ray diffractometry. Pure, plasma-sprayed zirconia is composed almost entirely of the monoclinic phase. At levels of yttria between 4 and 10 percent, a quenched-in tetragonal phase predominates, and at higher levels the cubic phase predominates. The phase distributions are compared with previously reported test lives of thermal barrier coatings formed from these materials. Regions of optimal lives were found to correlate with regions having high amounts of the tetragonal phase, small but nonzero amounts of the monoclinic phase, and little or none of the cubic phase. Possible relationships between phase composition and coating performance are discussed.