Search NASA⌕ Search

SEARCH · Search NASA

Results for “electrode interface”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 487 records · Page 27

Enabling High-Energy-Density Cathode for Lithium-Sulfur Batteries

High-loading sulfur electrode is critical for high energy Lithium-sulfur (Li-S) batteries used for practical applications. Unfortunately, dense and high-loading sulfur electrodes usually suffer from low sulfur utilization rate and limited cycle life. In this work, effects of electrode porosity on the electrode energy density, cell cycling stability, Li anode interface, and electrolyte/sulfur ratio were systematically investigated using high loading sulfur electrodes. The reduced electrode porosity increases volumetric energy density but also hinders electrode wetting process. To solve this problem, polysulfide (Li2S6) is selected as an electrolyte additive to enhance electrolyte penetration into dense sulfur cathodes. As a result, a high energy density of 1300 Wh L-1 (at electrode level) has been obtained for a dense sulfur cathode with a sulfur loading of 4 mg cm-2 at a compressed thickness of 60 µm. Li-S batteries with dense electrodes and Li2S6 additive also demonstrate promising cycling stability (~80 % capacity retention for 200 cycles). These significant improvements are contributed by synergistic effects of the dense sulfur cathode, improved electrolyte penetration, and suppressed growth of passivation layer on Li metal anode. This study sheds light on rational sulfur cathode structure design as well as control of electrode porosity for balanced energy density and cycling life.

Lu, Dongping↗

Electron Inversion and Tunneling at Silicon Thermal Oxide Interfaces for Solar-Driven Molecular Catalysis to Syngas

Semiconductor photoelectrodes are regularly coupled to solid-state heterogeneous catalysts to perform solar-driven reduction of CO 2 . Less frequently, molecular catalysts are employed to better control the reactivity toward desired products, yet the development of robust semiconductor/molecule interfaces has proven challenging. Here, we demonstrate that a 2–3 nm thermal oxide layer on Si exhibits stability in aqueous solution, high photovoltage, and a photocurrent density of ∼10 mA/cm 2 for the solar-driven photoelectrochemical reduction of a homogeneous molecular catalyst, producing syngas with an ∼2:1 H 2 to CO ratio. Because of a low defect density, the oxide interface forms an electron inversion layer with metal-like electron density at cathodic potentials. This inversion layer facilitates electron transfer to redox-active molecules via tunneling even if the molecule’s reduction potential is beyond the semiconductor’s conduction band edge. Using an electrolyte solution composed of a homogeneous cobalt bis(terpyridine) catalyst in a water/organic solvent mixture, stable photoelectrochemistry was observed under 1-sun illumination, exhibiting an ∼30% Faradaic efficiency for CO that was similar to a glassy carbon electrode under comparable conditions. Furthermore, the results demonstrate that an ultrathin thermal oxide interface is a robust platform for development of aqueous-stable, molecule-driven photoelectrocatalysis.

Catalysts↗

High-Spatial-Resolution Quantitative Chemomechanical Mapping of Organic Composite Cathodes for Sulfide-Based Solid-State Batteries

Understanding the chemo-mechanical behaviors of electrodes, particularly at the electrode/electrolyte interfaces, is critical for improving the performance of all-solid-state batteries. However, due to the instability of electrolyte materials under ambient conditions, such characterizations are challenging, particularly for sulfide-based all-solid-state batteries. Herein, by combining time-of-flight secondary-ion mass spectroscopy (ToF-SIMS) and in-SEM nanoindentation measurements, a systematic quantitative investigation of the chemo-mechanical behaviors of pyrene-4,5,9,10-tetraone (PTO) /Li 6 PS 5 Cl composite cathodes is carried out. Chemical and quantitative mechanical information of the composite cathode were collected with high spatial resolution after developing and implementing an air-free characterization protocol. By directly connecting the Young’s modulus and hardness with the Li distribution in the composite cathode, a comprehensive chemo-mechanical mapping of the PTO/ Li 6 PS 5 Cl composite cathode has been established. Furthermore, this work improves our knowledge of the critical chemo-mechanical phenomena that occur at the cathode/electrolyte interfaces in all-solid-state batteries.

25 ENERGY STORAGE↗

Coupling of Adhesion and Anti-Freezing Properties in Hydrogel Electrolytes for Low-Temperature Aqueous-Based Hybrid Capacitors

Solid-state zinc-ion capacitors are emerging as promising candidates for large-scale energy storage owing to improved safety, mechanical and thermal stability and easy-to-direct stacking. Hydrogel electrolytes are appealing solid-state electrolytes because of eco-friendliness, high conductivity and intrinsic flexibility. However, the electrolyte/electrode interfacial contact and anti-freezing properties of current hydrogel electrolytes are still challenging for practical applications of zinc-ion capacitors. Here, we report a class of hydrogel electrolytes that couple high interfacial adhesion and anti-freezing performance. The synergy of tough hydrogel matrix and chemical anchorage enables a well-adhered interface between hydrogel electrolyte and electrode. Meanwhile, the cooperative solvation of ZnCl 2 and LiCl hybrid salts renders the hydrogel electrolyte high ionic conductivity and mechanical elasticity simultaneously at low temperatures. More significantly, the Zn||carbon nanotubes hybrid capacitor based on this hydrogel electrolyte exhibits low-temperature capacitive performance, delivering high-energy density of 39 Wh kg –1 at –60 °C with capacity retention of 98.7% over 10,000 cycles. With the benefits of the well-adhered electrolyte/electrode interface and the anti-freezing hydrogel electrolyte, the Zn/Li hybrid capacitor is able to accommodate dynamic deformations and function well under 1000 tension cycles even at –60 °C. This work provides a powerful strategy for enabling stable operation of low-temperature zinc-ion capacitors.

25 ENERGY STORAGE↗

Solid electrolytes and interfaces in all-solid-state sodium batteries: Progress and perspective

All-solid-state sodium batteries are promising candidates for the next generation of energy storage with exceptional safety, reliability and stability. The solid electrolytes are key components for enabling all-solid-state sodium batteries with high electrochemical performances. This Review discusses the current developments on inorganic and organic sodium ions solid electrolytes, including β/β’’-alumina, NASICON, sulfides, polymers and others. In particular, the structures, ionic conductivities and fabrications as well as electrochemical/chemical stabilities of solid electrolytes are discussed. Furthermore, the effective approaches for forming intimate interfaces between solid electrolytes and electrodes are also reviewed. And perspectives on future developments in the field of solid electrolytes and possible directions to improve interfacial contacts for future practical applications of all-solid-state sodium batteries are included.

25 ENERGY STORAGE↗

Combined Cr and S poisoning behaviors of La 1-x Sr x MnO 3±δ and La 1-x Sr x Co 1-y FeyO 3-δ cathodes in solid oxide fuel cells

Although the individual effects of airborne Cr and S contaminants on SOFC cathode performance degradation have been extensively studied, the combined effects of Cr and S contaminants remain largely unexplored. Under the real SOFC operating condition where the Cr and S species coexist, their effects may compete, affecting the poisoning behavior. Here, our investigation reveals that the combined Cr and S poisoning behavior of LSCF remains different from those of individual Cr and S poisonings, while the combined poisoning mechanism of LSM is equivalent to the sum of those of individual Cr and S effects. For LSCF electrode, gaseous Cr species are deposited mainly at the LSCF/GDC interface by electrochemical reduction, rather than forming SrCrO 4 on LSCF surfaces (as in the case of Cr-only poisoning), indicating no reaction between Cr vapors and SrO on the LSCF surface. Thermodynamic analysis demonstrates that the SrO on LSCF surface absorbs SO 2 (g) and thereby loses the Cr-gettering effect, allowing Cr vapors to flow through LSCF and to reach the LSCF/GDC interface where the Cr deposition occurs. Unlike LSCF, LSM electrode shows cumulative effects of Cr and S, as Cr accumulation occurs at the triple-phase boundary and S absorption takes place at localized Sr-rich regions.

36 MATERIALS SCIENCE↗

Understanding and Advancing Bifacial Thin Film Solar Cells under Dual Illumination

There is a great deal of interest in increasing the energy yield from thin film solar cells by implementing bifacial operation. However, deleterious band bending and high interface recombination at the back transparent electrode can cause problems. Herein, it is investigated how bifacial thin film devices perform when illuminated through the front, back, and simultaneously through both interfaces using numerical modeling. It is shown that the downward band bending near the back interface is reduced during illumination when the carrier concentration is low. This effect is not found when the doping is relatively high, but the minority carrier distribution is still modified. Under either condition, the power generated under bifacial illumination exceeds the sum of the power generated when the illumination is solely from the back or the front. It is also shown that the back-illuminated device performance is independent of the angle at which the light enters the back of the device, which provides accommodation for scattered light. Finally, the power enhancement is calculated for bifacial devices relative to front-illuminated devices, and is shown that any significant loss in frontside power generation is difficult to overcome with back illumination under real-world albedo conditions.

CdTe↗

Mesoscopic Elastic Distortions in GaAs Quantum Dot Heterostructures

Quantum devices formed in high-electron-mobility semiconductor heterostructures provide a route through which quantum mechanical effects can be exploited on length scales accessible to lithography and integrated electronics. The electrostatic definition of quantum dots in semiconductor heterostructure devices intrinsically involves the lithographic fabrication of intricate patterns of metallic electrodes. The formation of metal/semiconductor interfaces, growth processes associated with polycrystalline metallic layers, and differential thermal expansion produce elastic distortion in the active areas of quantum devices. Understanding and controlling these distortions present a significant challenge in quantum device development. In this paper, we report synchrotron X-ray nanodiffraction measurements combined with dynamical X-ray diffraction modeling that reveal lattice tilts with a depth-averaged value up to 0.04° and strain on the order of 10 –4 in the two-dimensional electron gas (2DEG) in a GaAs/AlGaAs heterostructure. Elastic distortions in GaAs/AlGaAs heterostructures modify the potential energy landscape in the 2DEG due to the generation of a deformation potential and an electric field through the piezoelectric effect. Finally, the stress induced by metal electrodes directly impacts the ability to control the positions of the potential minima where quantum dots form and the coupling between neighboring quantum dots.

36 MATERIALS SCIENCE↗

Self-Supporting, Hydrophobic, Ionic Liquid-Based Reference Electrodes Prepared by Polymerization-Induced Microphase Separation

Interfaces of ionic liquids and aqueous solutions exhibit stable electrical potentials over a wide range of aqueous electrolyte concentrations. This makes ionic liquids suitable as bridge materials that separate in electroanalytical measurements the reference electrode from samples with low and/or unknown ionic strengths. However, methods for the preparation of ionic liquid-based reference electrodes have not been explored widely. We have designed a convenient and reliable synthesis of ionic liquid-based reference electrodes by polymerization-induced microphase separation. This technique allows for a facile, single-pot synthesis of ready-to-use reference electrodes that incorporate ion conducting nanochannels filled with either 1-octyl-3-methylimidazolium bis(trifluoromethylsulfonyl)imide or 1-dodecyl-3-methylimidazolium bis(trifluoromethyl sulfonyl)imide as ionic liquid, supported by a mechanically robust cross-linked polystyrene phase. This synthesis procedure allows for the straightforward design of various reference electrode geometries. These reference electrodes exhibit a low resistance as well as good reference potential stability and reproducibility when immersed into aqueous solutions varying from deionized, purified water to 100 mM KCl, while requiring no correction for liquid junction potentials.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Degradation Effects at the Porous Transport Layer/Catalyst Layer Interface in Polymer Electrolyte Membrane Water Electrolyzer

The porous transport layer (PTL)/catalyst layer (CL) interface plays a crucial role in the achievement of high performance and efficiency in polymer electrolyte membrane water electrolyzers (PEMWEs). This study investigated the effects of the PTL/CL interface on the degradation of membrane electrode assemblies (MEAs) during a 4000 h test, comparing the MEAs assembled with uncoated and Ir-coated Ti PTLs. Our results show that compared to an uncoated PTL/CL interface, an optimized interface formed when using a platinum group metal (PGM) coating, i.e., an iridium layer at the PTL/CL interface, and reduced the degradation of the MEA. The agglomeration and formation of voids and cracks could be found for both MEAs after the long-term test, but the incorporation of an Ir coating on the PTL did not affect the morphology change or oxidation of IrO x in the catalyst layer. In addition, our studies suggest that the ionomer loss and restructuring of the anodic MEA can also be reduced by Ir coating of the PTL/CL interface. Optimization of the PTL/CL interface improves the performance and durability of a PEMWE.

30 DIRECT ENERGY CONVERSION↗

Root Cause Analysis of Degradation in Protonic Ceramic Electrochemical Cell with Interfacial Electrical Sensors Using Data‐Driven Machine Learning

Abstract Protonic ceramic electrochemical cells (PCECs) offer promising paths for energy storage and conversion. Despite considerable achievements made, PCECs still face challenges such as physiochemical compatibility between componenets and suboptimal solid–solid contact at the interfaces between the electrolytes and electrodes. In this study, a novel approach is proposed that combines in situ electrochemical characterization of interfacial electrical sensor embedded PCECs and machine learning to quantify the contributions of different cell components to total degradation, as well as to predict the remaining useful life. The experimental results suggest that the overpotential induced by the oxygen electrode is 48% less than that of oxygen electrode/electrolyte interfacial contact for up to 1171 h. The data‐driven machine learning simulation predicts the RUL of up to 2132 h. The root cause of degradation is overpotential increase induced by oxygen electrode, which accounts for 82.9% of total cell degradation. The success of the failure diagnostic model is demonstrated by its consistency with degradation modes that do not manifest in electrolysis fade during early real operations. This synergistic approach provides valuable insights into practical failure diagnosis of PCECs and has the potential to revolutionize their development by enabling improved performance prediction and material selection for enhanced durability and efficiency.

25 ENERGY STORAGE↗

Autonomous Strategies for Improved Performance and Reliability of Li‐Ion Batteries

Abstract The battery community has devoted significant effort to improve the performance and reliability of Li‐ion batteries through the development of new materials. The integration of autonomous function provides an alternative strategy to further extend performance. Autonomous material systems mimic the ability of biological systems to self‐protect, sense, regulate, and heal in response to damage and other environmental changes. When incorporated in batteries, these materials enable autonomic restoration of battery performance upon degradation, as well as autonomic shutdown or extinguishment in response to thermal runaway. Successful strategies for improving Li‐ion battery performance include controlled release of microencapsulated functional additives and the integration of self‐healing or adaptive interlayers and binders. These methods have been effective for stabilizing the solid electrolyte interface, preventing battery fires, restoring electrode conductivity, and suppressing Li dendrite growth. Challenges and opportunities exist in the further application of autonomous strategies in the battery environment. A greater variety of encapsulated additives with precise triggered‐release are needed to address specific battery degradation mechanisms. Incorporation of self‐healing polymers in solid‐state batteries facilitates improvement in interfacial and mechanical stability. The integration of autonomous strategies with battery management systems potentially enables enhanced control over multiple battery cycling parameters.

Zhao, Lihong↗

Electrochemical Structure of the Plasma–Liquid Interface

Nonthermal atmospheric pressure plasma in contact with a liquid yields a variety of energetic photons, ions, and electrons, which can be transported into the plasma–liquid interface (PLI). Similar to the electrochemical interface formed between a solid electrode and electrolyte in conventional electrochemical systems, the charge-transfer process across the PLI is able to promote reduction–oxidation (redox) reactions. However, in the case of free plasma jets in contact with liquids, the absence of solid electrodes obscures the spatial locations of the electrochemical half-reactions. Herein, we present a spatial electrochemical measurement technique used to characterize an aqueous solution in contact with an atmospheric pressure plasma jet. The technique is based on measuring the potential difference between two identical Ag/AgCl electrochemical electrodes positioned at different locations within the solution. More specifically, electrochemical maps were made by measuring the potential of one electrochemical electrode positioned at different locations near the PLI with respect to the other electrochemical electrode positioned far away from the PLI in the bulk solution. Regions in the map with negative and positive potential differences between these electrochemical electrodes were used to identify the electrodeless cathode and anode, respectively. Here, visualization of the spatial distribution of molecular colorimetric redox indicators by multispectral imaging revealed that reduction was occurring near the plasma jet centerline while oxidation was occurring further away in solution, which constitutes an independent confirmation of the electrochemical maps.

Absorption↗

Addressing the Challenge of Electrochemical Ionomer Oxidation in Future Anion Exchange Membrane Water Electrolyzers

Hydrogen production through anion-exchange membrane water electrolyzers (AEMWEs) offers cost advantages over proton-exchange membrane counterparts, mainly due to the good oxygen evolution reaction (OER) activity of platinum-group-metal-free catalysts in alkaline environments. However, the electrochemical oxidation of ionomers at the OER catalyst interface can decrease the local electrode pH, which limits AEMWE performance. Various strategies at the single-cell-level have been explored to address this issue. Here, this work reviews the current understanding of electrochemical ionomer oxidation and strategies to mitigate it, providing our perspective on each approach. Our analysis highlights the competitive adsorption strategy as particularly promising for mitigating ionomer oxidation. This Perspective also outlines future directions for advancing high-performance alkaline AEMWEs and other energy devices using hydrocarbon ionomers.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Understanding resistances in capacitive deionization devices

The desalination characteristics of capacitive deionization (CDI) are significantly impacted by the cell resistance. Here we apply electrochemical impedance spectroscopy (EIS) to analyze the resistive properties of a CDI device, which include EIS measurements on a complete assembled cell (in two wire mode) and EIS measurements with additional contacts to decouple electrode/electrolyte and contact impedances (four wire mode). These measurements shed light on the interface between current collector and electrode as well as the internal capacitive and resistive elements of the cell. With two-wire and four-wire EIS measurements, we find that the often observed high-frequency arc(s) in the impedance spectra can be due to contact effects and/or an internal ionic-transfer resistance that is locally in parallel with macropore wall capacitance. In some cases, the two associated arcs in the Nyquist plot are overlapping and present simultaneously, making their identification in the EIS spectra difficult unless both two-wire and four-wire measurements are made. Despite causing a large high-frequency arc in the Nyquist plot, we find that the apparent internal ionic-transfer resistance is negligible compared to the resistances of the electrode, separator, and external electronic components. Here, an investigation of the contact impedance between the electrode and current collector reveals a parallel RC arc that can grow over time if an improper material is used (e.g., titanium). In our system, the electrode ionic resistance dominates the total Ohmic power dissipation, which has implications for scale-up of CDI systems and future improvements of cell design.

36 MATERIALS SCIENCE↗

Solid-state polymer-particle hybrid electrolytes: Structure and electrochemical properties

Solid-state electrolytes (SSEs) are challenged by complex interfacial chemistry and poor ion transport through the interfaces they form with battery electrodes. Here, we investigate a class of SSE composed of micrometer-sized lithium oxide (Li 2 O) particles dispersed in a polymerizable 1,3-dioxolane (DOL) liquid. Ring-opening polymerization (ROP) of the DOL by Lewis acid salts inside a battery cell produces polymer-inorganic hybrid electrolytes with gradient properties on both the particle and battery cell length scales. These electrolytes sustain stable charge-discharge behavior in Li||NCM811 and anode-free Cu||NCM811 electrochemical cells. On the particle length scale, Li 2 O retards ROP, facilitating efficient ion transport in a fluid-like region near the particle surface. On battery cell length scales, gravity-assisted settling creates physical and electrochemical gradients in the hybrid electrolytes. By means of electrochemical and spectroscopic analyses, we find that Li 2 O particles participate in a reversible redox reaction that increases the effective CE in anode-free cells to values approaching 100%, enhancing battery cycle life.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗