Antiferromagnetism in semiconducting SrMn 2 Sb 2 and BaMn 2 Sb 2 single crystals
Here, crystals of SrMn 2 Sb 2 and BaMn 2 Sb 2 were grown using Sn flux and characterized by powder and single-crystal x-ray diffraction, respectively, and by single-crystal electrical resistivity ρ, heat capacity C p , and magnetic susceptibility χ measurements versus temperature T, and magnetization versus field M(H) isotherm measurements. SrMn 2 Sb 2 adopts the trigonal CaAl 2 Si 2 -type structure, whereas BaMn 2 Sb 2 crystallizes in the tetragonal ThCr 2 Si 2 -type structure. The ρ(T) data indicate semiconducting behaviors for both compounds with activation energies of ≳0.35 eV for SrMn 2 Sb 2 and 0.16 eV for BaMn 2 Sb 2 . The χ(T) and C p (T) data reveal antiferromagnetic (AFM) ordering at T N = 110 K for SrMn 2 Sb 2 and 450 K for BaMn 2 Sb 2 . The anisotropic χ(T≤T N ) data also show that the ordered moments in SrMn 2 Sb 2 are aligned in the hexagonal ab plane, whereas the ordered moments in BaMn 2 Sb 2 are aligned collinearly along the tetragonal c axis. The ab-plane M(H) data for SrMn 2 Sb 2 exhibit a continuous metamagnetic transition at low fields 0 2 Sb 2 exhibits no metamagnetic transitions up to 5.5 T. The χ(T) and C p (T) data for both SrMn 2 Sb 2 and BaMn 2 Sb 2 indicate strong dynamic short-range AFM correlations above their respective T N up to at least 900 K within a local-moment picture, corresponding to quasi-two-dimensional magnetic behavior. The present results and a survey of the literature for Mn pnictides with the CaAl 2 Si 2 and ThCr 2 Si 2 crystal structures show that the T N values for the CaAl 2 Si 2 -type compounds are much smaller than those for the ThCr 2 Si 2 -type materials.