Search NASA⌕ Search

SEARCH · Search NASA

Results for “recrystallization”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 487 records · Page 27

Hot forming of silicon sheet, silicon sheet growth development for the large area silicon sheet task of the low cost silicon solar array project

The hot workability of polycrystalline silicon was studied. Uniaxail stress-strain curves are given for strain rates in the range of .0001 to .1/sec and temperatures from 1100 to 1380 C. At the highest strain rates at 1380 C axial strains in excess of 20% were easily obtainable without cracking. After deformations of 36%, recrystallization was completed within 0.1 hr at 1380 C. When the recrystallization was complete, there was still a small volume fraction of unrecyrstallized material which appeared very stable and may degrade the electronic properties of the bulk materials. Texture measurements showed that the as-produced vapor deposited polycrystalline rods have a 110 fiber texture with the 110 direction parallel to the growth direction and no preferred orientation about this axis. Upon axial compression perpendicular to the growth direction, the former 110 fiber axis changed to 111 and the compression axis became 110 . Recrystallization changed the texture to 110 along the former fiber axis and to 100 along the compression axis.

Graham, C. D., Jr.↗

Progress towards high efficiency polycrystalline thin-film GaAs AMOS solar cells

Results of Ge film recrystallization using focused laser beams and GaAs film growth on such layers in the making of high efficiency thin-film AMOS solar cells are discussed. Since a conversion efficiency of 14% was obtained for an AMOS cell fabricated on sliced bulk polycrystalline GaAs, high efficiency cells are being developed by chemically vapor-depositing GaAs films on previously recrystallized evaporated Ge films to minimize the grain boundary (GB) effects. Schottky barrier solar cells made on sliced polycrystalline GaAs wafers were studied to investigate the effects of grain boundaries on cell properties and the potential efficiency of GaAs thin-film cells. Ge film recrystallization and the chemical vapor deposition (CVD) of the 2 to 3 micron thick GaAs films are described. AMOS solar cells with 100 Angstrom thick Ag metallization were made on CVD GaAs/recrystallized Ge/W substrates with an energy conversion efficiency of 8%.

Yeh, Y. C. M.↗

Holographic fabrication of gratings in metal substrates

A program for investigating the grain enlargement resulting from the laser recrystallization of a thin gallium arsenide film on a patterned substrate, a technique known as graphoepitaxy was evaluated. More specifically, the effects of recrystallizing an uncapped gallium arsenide film using a continuous wave neodymium YAG laser operating at 1.06 microns were studied. In an effort to minimize arsenic loss from the film, the specimens were held in an arsine atmosphere during recrystallization. Two methods for fabricating patterned substrates were developed, one using reactive ion etching of a molybdenum film on both sapphire and silicon substates and another by preferential wet etching of a silicon substrate onto which a film of molybdenum was subsequently deposited.

Fletcher, R. M.↗

Diffusion welding of MA 6000 and a conventional nickel-base superalloy

A feasibility study of diffusion welding the oxide dispersion strengthened (ODS) alloy MA 6000 to itself and to conventional Ni-base superalloy Udimet 700 was conducted. Butt joints between MA 6000 pieces and lap joints between Udimet 700 and the ODS alloy were produced by hot pressing for 1.25 hr at temperatures ranging from 1000 to 1200 C (1832-2192 F) in vacuum. Following pressing, all weldments were heat treated and machined into mechanical property test specimens. While three different combinations of recrystallized and unrecrystallized MA 6000 butt joints were produced, the unrecrystallized to unrecrystallized joint was most successful as determined by mechanical properties and microstructural examination. Failure to weld the recrystallized material probably related to a lack of adequate deformation at the weld interface. While recrystallized MA 6000 could be diffusion welded to Udimet 700 in places, complete welding over the entire lap joint was not achieved, again due to the lack of sufficient deformation at the faying surfaces. Several methods are proposed to promote the intimate contact necessary for diffusion welding MA 6000 to itself and to superalloys.

Moore, T. J.↗

Petrology and classification of the Garraf, Spain chondrite

Microscopic and electron microprobe studies indicate that the Garraf meteorite is a highly-recrystallized chondrite of petrologic type 6. Olivine (Fa24.7; PMD 1.1) and low-Ca pyroxene (Fs20.9; PMD 1.1) compositions indicate that it belongs to the L-group. Based on contents of noble gases, pervasive fracturing of silicates, common undulose extinction of olivine and plagioclase, and the lack of melt pockets and maskelynite, Garraf is placed into shock facies b. It is concluded that Garraf is a highly recrystallized L6b chondrite that, after recrystallization, was cataclased and comminuted by shock.

Keil, K.↗

Cellular monotectic model solidification

Succinonitrile (sn) was purified to a superior level using a fractional recrystallization method. The melting point of the best twice recrystallized sn was not raised by following with double distillation. This was tested using differential scanning calorimetry. The peak shape on melting also proved that double distillation after double recrystallization did not improve the quality. Stability and phase diagrams for succinonitrile and glycerol are presented.

Kaukler, William F.↗

In situ irradiation of spent nuclear fuels

To improve the economics of commercial nuclear reactors, nuclear vendors and utilities are seeking approval for increased burnup usage of the existing nuclear fleet. This is especially critical for meeting the clean energy initiative by the United States Government, Department of Energy (DOE). However, one of the key challenges the nuclear industry faces in this regard is that the regions exposed to high burnup and low temperatures exhibit a fine-grained microstructure with large bubbles known as high-burnup structure (HBS) [1]. The formation of HBS has been correlated to the diminished performance of the reactor, as well as fuel fragmentation and pulverization during transient and accidental conditions [2]. Therefore, it is paramount to understand the mechanisms for HBS formation along with its impact on the properties and performance of nuclear fuels. While existing programs, such as Nuclear Energy Advanced Modeling and Simulation (NEAMS) and Advanced Fuel Campaign (AFC) are focusing on evaluating the performance impact of HBS, the physical mechanisms contributing to HBS formation are still not fully understood. In addition, having predictive capabilities and sound understanding of the microstructural evolution of nuclear fuel is essential for accelerated development, qualification, and deployment of new nuclear materials and novel reactor designs for advanced nuclear reactors. There is a lack of consensus among researchers regarding the mechanisms leading to such restructuring observed in HBS. Grain subdivision due to polygonization versus recrystallization, continuous versus discrete recrystallization occurring in tandem or conjunction, etc., have been proposed and debated. In general, it is hypothesized that defect accumulation and dislocation interaction within the grains cause the realignment of dislocations into grain boundaries, leading to the new subgrain formation, which over time transforms into new grains. However, due to the lack of transient data, the importance of fission rate, irradiation, thermal, and stress history of the fuel on the restructuring could not be assessed. In situ microstructural evolution under various irradiation conditions is desired to bridge this gap. Alternatively, phase-field-based models have been developed to capture HBS formation via discrete recrystallization utilizing the classical nucleation approach [3–5]. However, in these models, the grain nucleation criteria are often defined based on empirical relations for burnup and fission gas density leading to dislocation density change. A mechanistic approach to capture the dislocation interaction with the microstructural features leading to grain subdivision is lacking.

11 - NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Activatino of Erbium Films for Hydrogen Storage

Hydriding of metals can be routinely performed at high temperature in a rich hydrogen atmosphere. Prior to the hydrogen loading process, a thermal activation procedure is required to promote facile hydrogen sorption into the metal. Despite the wide spread utilization of this activation procedure, little is known about the chemical and electronic changes that occur during activation and how this thermal pretreatment leads to increased rates of hydrogen uptake. This study utilized variable kinetic energy X-ray photoelectron spectroscopy to interrogate the changes during in situ thermal annealing of erbium films, with results confirmed by time-of-flight secondary ion mass spectrometry and low energy ion scattering. Activation can be identified by a large increase in photoemission between the valence band edge and the Fermi level and appears to occur over a two stage process. The first stage involves desorption of contaminants and recrystallization of the oxide, initially impeding hydrogen loading. Further heating overcomes the first stage and leads to degradation of the passive surface oxide leading to a bulk film more accessible for hydrogen loading.

08 HYDROGEN↗

Microstructural Evolution of Al-1Fe (Weight Percent) Alloy During Accumulative Continuous Extrusion Forming

As a new microstructure refining method, accumulative continuous extrusion forming (ACEF) cannot only refine metal matrix but also refine the phases that exist in it. In order to detect the refinements of grain and second phase during the process, Al-1Fe (wt pct) alloy was processed by ACEF, and the microstructural evolution was analyzed by electron backscatter diffraction (EBSD) and transmission electron microscopy (TEM). Results revealed that the average grain size of Al-1Fe (wt pct) alloy decreased from 13 to 1.2 μm, and blocky Al{sub 3}Fe phase with an average length of 300 nm was granulated to Al{sub 3}Fe particle with an average diameter of 200 nm, after one pass of ACEF. Refinement of grain was attributed to continuous dynamic recrystallization (CDRX), and the granulation of Al{sub 3}Fe phase included the spheroidization resulting from deformation heat and the fragmentation caused by the coupling effects of strain and thermal effect. The spheroidization worked in almost the entire deformation process, while the fragmentation required strain accumulation. However, fragmentation contributed more than spheroidization. Al{sub 3}Fe particle stimulated the formation of substructure and retarded the migration of recrystallized grain boundary, but the effect of Al{sub 3}Fe phase on refinement of grain could only be determined by the contrastive investigation of Al-1Fe (wt pct) alloy and pure Al.

36 MATERIALS SCIENCE↗

Evolution of Residual Stress and Distortion of Cold-Rolled Bearing Ring from Annealing to Quenched-Tempered Heat Treatment

This study investigates the correlation between the residual stress and distortion behavior of a cold-rolled ring from the annealing to quenching-tempering (QT) process. Due to the cold-rolled process, the external periphery of the bearing ring experiences a compressive residual stress. To relieve the residual stress, cold-rolled rings are annealed at 700 °C which is higher than the starting temperature of recrystallization. When cold-rolled rings are annealed at 700 °C for 15 min, the compressive residual stress is reduced to zero and the outer diameter of the annealed ring becomes larger than that of a non-annealed sample, which is unrelated to annealing time. Simultaneously, the roundness and taper deviation do not obviously change compared with those of non-annealed sample. The stress relaxation during the annealing process was attributed to the recovery and recrystallization of ferrite. Annealing has a genetic influence on the following QT heat treatment, wherein the lowest residual stress is in the non-annealed cold-rolled ring. From the annealing to QT process, the deviation of the outer diameter, roundness, and taper increased with annealing time, a large extend than that of non-annealed samples.

36 MATERIALS SCIENCE↗

Adiabatic Shear Localization and Microstructure in Ultrafine Grained Aluminum Alloy at Cryogenic Temperature

Adiabatic shear localization plays an important role in the deformation and failure of ultrafine grained 6061 aluminum alloy processed by friction stir processing. To understand the effects of temperature and strain on adiabatic shear localization in the ultrafine grained 6061 aluminum alloy, it has been investigated dynamic mechanical behavior of ultrafine grained 6061 aluminum alloy under the controlled shock loading experiments. Deformation characteristics and microstructures in the shear band were performed by optical microscopy and transmission electron microscopy. The shear band in the ultrafine grained aluminum alloy is a long and straight band distinguished from the matrix. The width of the shear band decreases with increasing nominal strain. The results show that the grains in the boundary of the shear band are highly elongated along the shear direction and form the elongated cell structures (0.2 μ in width), and the core of the shear band consists of a number of recrystallized equiaxed grains 0.2-0.3 μ in diameters and the second phases distribute in both the boundary and the inner of the equiaxed new grains. The calculated temperature in the shear band is about 692 K. Rotational dynamic recrystallization mechanism is responsible for the formation of the microstructure in the shear band.

36 MATERIALS SCIENCE↗

In Situ Apparatus to Study Gas–Metal Reactions and Wettability at High Temperatures for Hot-Dip Galvanizing Applications

The understanding of gas–metal reactions and related surface wettability at high temperatures is often limited due to the lack of in situ surface characterization. Ex situ transfers at low temperature between annealing furnace, wettability device, and analytical tools induce noticeable changes of surface composition distinct from the reality of the phenomena.Therefore, a high temperature wettability device was designed in order to allow in situ sample surface characterization by x-rays photoelectron spectroscopy after gas/metal and liquid metal/solid metal surface reactions. Such airless characterization rules out any contamination and oxidation of surfaces and reveals their real composition after heat treatment and chemical reaction. The device consists of two connected reactors, respectively, dedicated to annealing treatments and wettability measurements. Heat treatments are performed in an infrared lamp furnace in a well-controlled atmosphere conditions designed to reproduce gas–metal reactions occurring during the industrial recrystallization annealing of steels. Wetting experiments are carried out in dispensed drop configuration with the precise control of the deposited droplets kinetic energies. The spreading of drops is followed by a high-speed CCD video camera at 500-2000 frames/s in order to reach information at very low contact time. First trials have started to simulate phenomena occurring during recrystallization annealing and hot-dip galvanizing on polished pure Fe and FeAl8 wt.% samples. The results demonstrate real surface chemistry of steel samples after annealing when they are put in contact with liquid zinc alloy bath during hot-dip galvanizing. The wetting results are compared to literature data and coupled with the characterization of interfacial layers by FEG-Auger. It is fair to conclude that the results show the real interest of such in situ experimental setup for interfacial chemistry studies.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Characterization of Friction-Stir-Welded Dual-Phase Brass

Friction stir welding (FSW) is an ideal process to join brass to avoid the evaporation of zinc. In the present investigation, 6-mm-thick dual-phase brass plates were joined efficiently using FSW at various tool rotational speeds. The microstructures were studied using optical microscopy, electron backscattered diffraction and transmission electron microscopy. The optical micrographs revealed the evolution of various zones across the joint line. The microstructure of the heat-affected zone was similar to that of base metal. The weld zone exhibited finer grains due to dynamic recrystallization. The recrystallization was inhomogeneous and the inhomogeneity reduced with increased tool rotational speed. The dual phase was preserved in the weld zone due to the retention of zinc. The severe plastic deformation created a lot of dislocations in the weld zone. The weld zone was strengthened after welding. The role of tool rotational speed on the joint strength is further reported.

36 MATERIALS SCIENCE↗

Annealing Effects on Microstructure and Mechanical Properties of Ultrafine-Grained Al Composites Reinforced with Nano-Al{sub 2}O{sub 3} by Rotary Swaging

Microstructure evolution and variations in mechanical properties of Al-Al{sub 2}O{sub 3} nanocomposite produced by powder metallurgy were investigated and compared with commercially pure aluminum (Al-1050) after furnace annealing. Fine gas-atomized Al powder compacts were first sintered in flowing nitrogen, subsequently consolidated into wires by rotary swaging and eventually annealed at 300 and 500 °C for 24 h each. Scanning and transmission electron microscopy with energy-dispersive spectroscopy was utilized to document the microstructure evolution. Rotary swaging was proven to lead to a marked decrease in grain size. After heavy swaging to true deformation degree of φ = 6 and annealing at 500 °C, obvious recrystallization was observed at Al-1050’s existing grain boundaries and the crystals began to grow perpendicular to the flow direction. In the Al-Al{sub 2}O{sub 3} nanocomposite, fabricated from d{sub 50} = 6 μm Al powder, recrystallization partially occurred, while grains were still extremely fine. Due to the dual role of fine-grained Al{sub 2}O{sub 3} dispersion strengthening, the nanocomposite showed improved mechanical performance in terms of tensile strength, approximately twice higher than Al-1050 after annealing at 500 °C.

36 MATERIALS SCIENCE↗

Phase-Field Modeling of Nugget Zone for a AZ31-Mg-Alloy Friction Stir Weld

This work presents simulation of microstructure evolution in the nugget zone (NZ) of a AZ31-Mg-alloy friction stir weld. The process parameters (tool geometrical characteristics, rotational speed, travel speed, applied load) have been correlated with the resulting microstructural features in the NZ of the weld (grain size and population) with the aid of the MICRESS software, which provides the ability to simulate both nucleation and grain growth during dynamic recrystallization phenomena evolving in the NZ during the weld thermal cycle. The input parameters of the developed model include the tool geometry, the welding conditions as well as the recrystallization energy, the grain boundary mobility and specific material properties. NZ microstructure obtained by simulation shows good agreement with experimental measurements for both grain population and size.

36 MATERIALS SCIENCE↗

Optimization of Hot Deformation Parameters and Constitutive Analysis for As-Cast Mg-5Li-3Zn-0.3Y Alloy Using Processing Maps

Hot deformation behavior of as-cast Mg-5Li-3Zn-0.3Y (wt.%) alloy has been studied by establishing processing maps covering the range of 200-450 °C in temperature and 0.001-10 s{sup −1} in strain rate. The map corresponding to the strain of 0.7 reveals that a domain of dynamic recrystallization occurred at 340-400 °C/0.01-0.158 s{sup −1} with its peak efficiency of approximately 31%. Analysis of the flow behaviors and microstructural observations indicated that dynamic recrystallization occurred in the domain, in which fine microstructure can be achieved. The above conditions represent the optimum processing parameters, and the flow instability regimes are also recognized from the maps. The average deformation in the deformed range was 136.414 kJ/mol which is close to that for lattice self-diffusion in magnesium and far smaller than that for as-cast Mg-5.75Zn-0.73Y-0.36Zr (wt.%) alloy. It is believed that a lower activation energy for Mg-5Li-3Zn-0.3Y alloy can partly result from both the weak particle pinning effects and adding Li into the Mg-Zn-Y-Zr alloy. Results of extrusion experiments conducted at 350 °C show that the alloy can be easily extruded with good mechanical properties of the yield strength of 132 MPa, the fracture strength of 215 MPa and the elongation of 20.9%, and the grains can be well refined.

36 MATERIALS SCIENCE↗

Effect of Heat Treatment and Combination of Cold Rolling and Heat Treatment on Microstructure and Mechanical Properties of Titanium Alloy Ti6Al2V2Zr1.5Mo

The heat treatment and cold rolling combinations have been carried out on titanium alloy Ti6Al2V2Zr1.5Mo, and microstructure evolution and mechanical behavior have been studied. Solution treatment below the β-transus temperature, followed by air cooling, resulted in higher microhardness/strength as compared to the same with water quenching. A sudden drop in microhardness/strength is observed in sample solution heat-treated above β-transus temperature followed by air cooling. The former is attributed to the additional presence of fine secondary α-phase formed by dynamic aging during air cooling as compared to water-quenched samples which did not have fine secondary α-phase. Solution treatment above β-transus temperature resulted in Widmanstatten microstructure with no significant fine secondary α in air-cooled samples. Among the studied conditions of cold rolling (CR), gain in strength of the alloy from annealed condition is significant with first 15% reduction and thereafter it is marginal for 30% reduction. Initiation of cracks at the edges has been observed in 30% CR. The microstructure of cold-rolled samples confirms the fragmentation of α-plates with the presence of high dislocation density. Heat treatment of cold-rolled samples resulted in significant reduction in strength from the as-cold-rolled conditions. The marginally lower strength than the as-received (annealed) or heat-treated alloy samples is due to the recrystallization in CR samples and the formation of Widmanstatten microstructure in air-cooled samples. The alloy does not have fine secondary α or regions with large dislocation density in this condition. The microstructure in the samples heat-treated (with air cooling) below as well as above β-transus temperature (after CR) is similar to air-cooled samples (without prior CR) with heat treatment above β-transus temperature. This indicates the reduction in recrystallization temperature with cold working, which is substantiated with the reduction in strength as well.

36 MATERIALS SCIENCE↗

Hot Deformation Characteristics and Processing Map of FV520B Martensitic Precipitation-Hardened Stainless Steel

Hot deformation characteristics of FV520B martensitic precipitation-hardened stainless steel were investigated in the temperature range of 850-1150 °C and strain rate range of 0.005-0.5 s{sup −1} with true strain 0.8 by using Gleeble-3500 thermo-mechanical simulator. Critical stress and corresponding critical strain for dynamic recrystallization initiation were calculated. The constitutive equation was developed by employing Arrhenius constitutive model to represent the nonlinear relationship of true stress and deformation parameters including temperature, strain rate and strain. The correlation coefficient and average absolute relative error are 0.9979 and 2.225%, which indicates the good predictive accuracy of the established constitutive equations. Processing maps were constructed at different plastic strains levels based on dynamic material model (DMM) and established constitutive equation. Combining the processing map with microstructure, the optimum region for good workability is designated as the temperature range of 1050-1125 °C and strain rate range of 0.027-0.23 s{sup −1} with peak efficiency of 0.32. Homogeneous fine and equiaxed dynamic recrystallization (DRX) grains can be found in this optimum according to the microstructure metallographic pictures.

36 MATERIALS SCIENCE↗