Micro- and nano-scale characterization to study the thermal degradation of cement-based materials

The degradation of hydration products of cement is known to cause changes in the micro- and nano-structure, which ultimately drive thermo-mechanical degradation of cement-based composite materials at elevated temperatures. However, a detailed characterization of these changes is still incomplete. This paper presents results of an extensive experimental study carried out to investigate micro- and nano-structural changes that occur due to exposure of cement paste to high temperatures. Following heat treatment of cement paste up to 1000 °C, damage states were studied by compressive strength test, thermogravimetric analysis (TGA), scanning electron microscopy (SEM) atomic force microscopy (AFM) and AFM image analysis. Using experimental results and research from existing literature, new degradation processes that drive the loss of mechanical properties of cement paste are proposed. The development of micro-cracks at the interface between unhydrated cement particles and paste matrix, a change in C–S–H nano-structure and shrinkage of C–S–H, are considered as important factors that cause the thermal degradation of cement paste. - Highlights: • The thermal degradation of hydration products of cement is characterized at micro- and nano-scale using scanning electron microscopy (SEM) and atomic force microscopy (AFM). • The interface between unhydrated cement particles and the paste matrix is considered the origin of micro-cracks. • When cement paste is exposed to temperatures above 300 ºC, the nano-structure of C-S-H becomes a more loosely packed globular structure, which could be indicative of C-S-H shrinkage.

36 MATERIALS SCIENCE↗

Role of water in degradation of nitroplasticizer

The role of water in degradation of nitroplasticizer (NP) was studied using a set of NP samples aged inside confined containers between room temperature and 70°C with their water concentrations monitored during the aging course. For the first 42 days at the temperatures at 55°C and below, simple Fickian diffusion dominates the monotonic decreases of the water concentrations with time. After about 60 to 80 days depending on temperatures, diffusion alone can no longer explain the water decreases, despite no significant NP degradation detectable using the FTIR spectroscopy. Starting at about 80 to 160 days, also depending on temperatures, the measured water concentrations fluctuated around mean values that decrease with increasing temperature, and the onset of NP degradation was detected using FTIR and TGA. It was found that NP contains an irreducible amount of water on the order of a few hundred ppms, which decreases with increasing temperature. Pristine NP does not exist with a water concentration lower than this amount. The diffusivity, the irreducible amount of water in NP, and the mean water production rate due to NP degradation are calculated from the water concentrations of the first aging stage and the mean water concentrations during the onset of NP degradation. They all change with the temperature following Arrhenius laws with different prefactors and activation energies. This study shows that trace water formation is an intrinsic property of the NP while it ages with the mechanistic details to be resolved.

36 MATERIALS SCIENCE↗

Photovoltaic Cleaning Frequency Optimization Under Different Degradation Rate Patterns

Dust accumulation significantly affects the performance of photovoltaic modules and its impact can be mitigated by various cleaning methods. Optimizing the cleaning frequency is essential to minimize the soiling losses and, at the same time, the costs. However, the effectiveness of cleaning lowers with time because of the reduced energy yield due to degradation. Additionally, economic factors such as the escalation in electricity price and inflation can compound or counterbalance the effect of degradation on the soiling mitigation profits. The present study analyzes the impact of degradation, escalation in electricity price and inflation on the revenues and costs of cleanings and proposes a methodology to maximize the profits of soiling mitigation of any system. Here, the energy performance and soiling losses of a 1 MW system installed in southern Spain were analyzed and integrated with theoretical linear and nonlinear degradation rate patterns. The Levelized Cost of Energy and Net Present Value were used as criteria to identify the optimum cleaning strategies. The results showed that the two metrics convey distinct cleaning recommendations, as they are influenced by different factors. For the given site, despite the degradation effects, the optimum cleaning frequency is found to increase with time of operation.

14 SOLAR ENERGY↗

Forest structure and solar-induced fluorescence across intact and degraded forests in the Amazon

Tropical forest degradation (e.g., anthropogenic disturbances such as selective logging and fires) alters forest structure and function and influences the forest's carbon sink. In this study, we explored structure-function relationships across a variety of degradation levels in the southern Brazilian Amazon by 1) investigating how forest structural properties vary as a function of degradation history using airborne lidar data; 2) assessing the effects of degradation on solar-induced chlorophyll fluorescence (SIF) seasonality using TROPOMI data; and 3) quantifying the contribution of structural variables to SIF using multiple regression models with stepwise selection of lidar metrics. Forest degradation history was obtained through Landsat time-series classification. We found that fire, logging, and time since disturbance were major determinants of forest structure, and that forests affected by fires experienced larger variability in leaf area index (LAI), canopy height and vertical structure relative to logged and intact forests. Moreover, only recently burned forests showed significantly depressed SIF during the dry season compared to intact forests. Canopy height and the vertical distribution of foliage were the best predictors of SIF. Unexpectedly, we found that wet-season SIF was higher in active regenerating forests (~ 4 years after fires or logging) compared with intact forests, despite lower LAI. Furthermore, our findings help to elucidate the mechanisms of carbon accumulation in anthropogenically disturbed tropical forests and indicate that they can capture large amounts of carbon while recovering.

54 ENVIRONMENTAL SCIENCES↗

An efficient Chlorella sp.-Cupriavidus necator microcosm for phenol degradation and its cooperation mechanism.

In this work, a Chlorella sp.-Cupriavidus necator (C. necator) microcosm was artificially established for phenol degradation. Additionally, the cooperation relationship between Chlorella sp. and C. necator was initially demonstrated, and then the effects of Chlorella sp./C. necator inoculation ratio, light intensity, temperature and pH on the performance of this microcosm were systematically evaluated and optimized. The optimal conditions for phenol degradation were as follows: a Chlorella sp./C. necator inoculation ratio of 1:1, a light intensity of 110 μmol m -2 s -1 , a temperature in the range of 25-32 °C and a pH in the range of 5.5-7.5. Under optimal conditions, this microcosm could degrade phenol with a maximum concentration of 1200 mg L -1 within 60 h. It was found that only when the phenol concentration was reduced to the tolerance concentration of microalgae, that is, the last stage of phenol degradation, the cooperation effect could be generated, indicating that the tolerance of microalgae to phenol may be more important than its degradation performance. Comparative transcriptomic analysis was conducted to discuss the cooperation mechanism of this microcosm subject to high phenol concentrations. The up-regulation of genes involved in photosynthesis and carbon fixation of Chlorella sp. demonstrated the CO 2 and O 2 exchange between Chlorella sp. and C. necator and their cooperation relationship. This study suggests that this microcosm has great potential for the bioremediation of phenol contaminants.

59 BASIC BIOLOGICAL SCIENCES↗

Potential induced degradation in c-Si glass-glass modules after extended damp heat stress

Traditional Glass-Backsheet (GB) photovoltaic (PV) modules have been the industry standard for a long time, but the Glass-Glass (GG) modules are quickly rising in popularity. PV modules installed in hot-humid climates with high string voltages can undergo potential induced degradation (PID). So far, to the best of our knowledge, only fresh modules with strong interfacial adhesion have been investigated for PID. However, in reality, the PV modules have weak interfacial adhesion after a few years of field exposure. Therefore, it is essential to evaluate PV modules with weakened interfaces. In this study, we investigated the PID susceptibility of PV modules with weakened interfaces after subjecting them to 2000 hours of damp heat (DH2000) at 85°C/85% relative humidity (RH) in an accelerated environmental chamber. Fresh GG modules were also stressed for PID to compare with PID degradation of DH-stressed modules. Pre- and post-characterization tests were done before, between, and after each stress method to determine the changes in electrical performance, cell metallization properties, and hotspot properties. It is observed that fresh GG modules showed little/no degradation (less than 1%) in maximum power (Pmax), whereas the GG modules that underwent sequential DH and PID degraded by 11% to 12%. Potential mechanisms for these degradations are also presented. Furthermore, the results presented in this study are critical for the industry, considering that the bifacial modules with GG construction will be dominant in the next 10 years.

14 SOLAR ENERGY↗

Understanding interfacial chemistry of positive bias high-voltage degradation in photovoltaic modules

Photovoltaic module degradation from a high system voltage is a prevalent degradation mode in the field, where the enabling degradation mechanisms are inherently dependent on the voltage bias polarity of the installed system. In this study, the effects of positive bias on module performance are confirmed and the underlying chemical degradation processes are more thoroughly investigated to reveal different degradation pathways from those previously reported in negative bias studies. When cells are under +1000 V stress, crystalline silicon mini-modules with poly(ethylene-co-vinyl acetate) (EVA) encapsulant demonstrated a significant photocurrent loss due to EVA discoloration and delamination from increased chemical reactivity at the front-side EVA/cell metallization interface. Brown discoloration of the EVA encapsulant near the cell gridlines is linked to an electrochemical reaction at the Ag gridlines under hot and humid conditions (85 °C, 85% relative humidity). Chemical compositional analysis using X-ray photoelectron spectroscopy (XPS) confirmed that the discoloration is attributed to the formation of silver sulfide (Ag 2 S) and/or silver oxide (Ag 2 O) species at the EVA/Ag gridline interface. The subsequent migration of Ag ions from the cell gridlines into the bulk of the EVA was evident from XPS depth profiling and optical microscopy. However, the Ag signal was not detected at the EVA/glass interface, inferring limited ionic transport through the nominally 0.45 mm thick encapsulant. For the samples studied herein, the sulfur is believed by the process of elimination to come from the ambient air, diffusing into the module through the permeable polymer backsheet.

14 SOLAR ENERGY↗

Microstructure degradation of YSZ in Ni/YSZ anodes of SOFC operated in phosphine-containing fuels

The interaction of trace (ppm) phosphine with the nickel/yttria stabilized zirconia (YSZ) anode of commercial solid oxide fuel cells has been investigated and evaluated for both synthesis gas and hydrogen fuels in an effort to examine P–Y reactions. The Ni poisoning effects reported in literature were confirmed and degradation was examined by electrochemical methods and post-test microstructural and chemical analyses. The results indicate that P-induced degradation rates and mechanisms are fuel dependent and that degradation of cells operated in synthesis gas (syngas) with phosphine is more severe than that of cells operated in hydrogen with phosphine. As reported in published literature, a cell operated in syngas containing 10 ppm phosphine demonstrated significant microstructural degradation within the Ni phase, including formation of Ni–P phases concentrated on the outer layer of the anode and significant pitting corrosion in the Ni grains. In this research, a previously undetected YPO{sub 4} phase is observed at the YSZ/YSZ/Ni triple grain junctions located at the interface with the YSZ electrolyte. Tetragonal YSZ (t-YSZ) and cubic-YSZ (c-YSZ) domains with sizes of several tens of nanometers are also newly observed along the Ni/YSZ interface. These observations contrast with data obtained for a cell operated in dry hydrogen with phosphine, where no YPO{sub 4} phase is observed and the alternating t-YSZ and c-YSZ domains at the Ni/YSZ interface are smaller with typical sizes of 5–10 nm. The data imply that electrolyte attack by P is a potentially debilitating mode of degradation in SOFC anodes, and that the associated reaction mechanisms and rates are worthy of further examination.

30 DIRECT ENERGY CONVERSION↗

A Structurally Dynamic Region of the HslU Intermediate Domain Controls Protein Degradation and ATP Hydrolysis

The I domain of HslU sits above the AAA+ ring and forms a funnel-like entry to the axial pore, where protein substrates are engaged, unfolded, and translocated into HslV for degradation. The L199Q I-domain substitution, which was originally reported as a loss-of-function mutation, resides in a segment that appears to adopt multiple conformations as electron density is not observed in HslU and HslUV crystal structures. The L199Q sequence change does not alter the structure of the AAA+ ring or its interactions with HslV but increases I-domain susceptibility to limited endoproteolysis. Notably, the L199Q mutation increases the rate of ATP hydrolysis substantially, results in slower degradation of some proteins but faster degradation of other substrates, and markedly changes the preference of HslUV for initiating degradation at the N or C terminus of model substrates. As such, a structurally dynamic region of the I domain plays a key role in controlling protein degradation by HslUV.

59 BASIC BIOLOGICAL SCIENCES↗

Degradation of Adsorbed Bisphenol A by Soluble Mn(III)

Bisphenol A (BPA), a high production volume chemical and potential endocrine disruptor, is found to be associated with sediments and soils due to its hydrophobicity (log K OW of 3.42). Here, we used superfine powdered activated carbon (SPAC) with a particle size of 1.38 ± 0.03 μm as a BPA sorbent and assessed degradation of BPA by oxidized manganese (Mn) species. SPAC strongly sorbed BPA, and desorption required organic solvents. No degradation of adsorbed BPA (278.7 ± 0.6 mg BPA g –1 SPAC) was observed with synthetic, solid α-MnO 2 with a particle size of 15.41 ± 1.35 μm; however, 89% mass reduction occurred following the addition of 0.5 mM soluble Mn(III). Small-angle neutron scattering data suggested that both adsorption and degradation of BPA occurred in SPAC pores. The findings demonstrate that Mn(III) mediates oxidative transformation of dissolved and adsorbed BPA, the latter observation challenging the paradigm that contaminant desorption and diffusion out of pore structures are required steps for degradation. Soluble Mn(III) is abundant near oxic-anoxic interfaces, and the observation that adsorbed BPA is susceptible to degradation has implications for predicting, and possibly managing, the fate and longevity of BPA in environmental systems.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Influence of Codeposition on Methylammonium Iodide Degradation during Vapor Transport Deposition

Vapor transport deposition (VTD) is one manufacturing-compatible technique for large-scale deposition of perovskite films. However, to date, little understanding has been given to degradation products formed by perovskites grown under vacuum. Here, we use methylammonium iodide (MAI) as an example organic precursor to identify degradation patterns through both the sublimation process and transport through a zone with temperatures much higher than MAI can thermodynamically survive. We show that degradation due to sublimation effects MAI powders and subsequent integration into methylammonium lead iodide (MAPbI3) films differently than degradation solely due to material transport through a very high-temperature zone. Additionally, we categorize common post-deposition treatments by their influence on the degradation products seen in MAPbI3 films. Furthermore, with these results we give recommendations for VTD reactor design and the feasibility of co-deposition as a film growth technique.

14 SOLAR ENERGY↗

Degradation of Alkali-Based Photocathodes from Exposure to Residual Gases: A First-Principles Study

Photocathodes are a key component in the production of electron beams in systems such as X-ray free-electron lasers and X-ray energy-recovery linacs. Alkali-based materials display high quantum efficiency (QE), however, their QE undergoes degradation faster than metal photocathodes even in the high vacuum conditions where they operate. The high reactivity of alkali-based surfaces points to surface reactions with residual gases as one of the most important factors for the degradation of QE. In order to advance the understanding on the degradation of the QE, we investigated the surface reactivity of common residual gas molecules (e.g., O 2 , CO 2 , CO, H 2 O, N 2 , and H 2 ) on one of the best-known alkali-based photocathode materials, cesium antimonide (Cs 3 Sb), using first-principles calculations based on density functional theory. Furthermore, the reaction sites, adsorption energy, and effect in the local electronic structure upon reaction of these molecules on (001), (110), and (111) surfaces of Cs 3 Sb were computed and analyzed. The adsorption energy of these molecules on Cs3Sb follows the trend of O 2 (-4.5 eV) > CO 2 (-1.9 eV) > H 2 O (-1.0 eV) > CO (-0.8 eV) > N 2 (-0.3 eV) ≈ H 2 (-0.2 eV), which agrees with experimental data on the effect of these gases on the degradation of QE. The interaction strength is determined by the charge transfer from the surfaces to the molecules. The adsorption and dissociation of O containing molecules modify the surface chemistry such as the composition, structure, charge distribution, surface dipole, and work function of Cs 3 Sb, resulting in the degradation of QE with exposure to O 2 , CO 2 , H 2 O, and CO.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Investigation of the Degradation Mechanisms of a Variety of Organic Photovoltaic Devices by Combination of Imaging Techniques - The ISOS-3 Inter-Laboratory Collaboration

The investigation of degradation of seven distinct sets (with a number of individual cells of n {>=} 12) of state of the art organic photovoltaic devices prepared by leading research laboratories with a combination of imaging methods is reported. All devices have been shipped to and degraded at Riso DTU up to 1830 hours in accordance with established ISOS-3 protocols under defined illumination conditions. Imaging of device function at different stages of degradation was performed by laser-beam induced current (LBIC) scanning; luminescence imaging, specifically photoluminescence (PLI) and electroluminescence (ELI); as well as by lock-in thermography (LIT). Each of the imaging techniques exhibits its specific advantages with respect to sensing certain degradation features, which will be compared and discussed here in detail. As a consequence, a combination of several imaging techniques yields very conclusive information about the degradation processes controlling device function. The large variety of device architectures in turn enables valuable progress in the proper interpretation of imaging results -- hence revealing the benefits of this large scale cooperation in making a step forward in the understanding of organic solar cell aging and its interpretation by state-of-the-art imaging methods.

14 SOLAR ENERGY↗

Stability of push–pull small molecule donors for organic photovoltaics: spectroscopic degradation of acceptor endcaps on benzo[1,2- b :4,5- b ′]dithiophene cores

High efficiency organic photovoltaic devices have relied on the development of new donor and acceptor materials to optimize opto-electronic properties, promote free carrier generation, and suppress recombination losses. With single junction efficiencies exceeding 15%, materials development must now target long-term stability. This work focuses on the photobleaching dynamics and degradation chemistries of a class of small molecule donors inspired by benzodithiophene terthiophene cores (BDT-3T) with rhodanine endcaps, which have demonstrated 9% efficiency in single junction devices and >11% in ternary cells. Density functional theory was used to design three additional molecules with similar synthetic pathways and opto-electronic properties by simply changing the electron accepting endcap to benzothiazoleacetonitrile, pyrazolone, or barbituric acid functional groups. This new class of semiconductors with equivalent redox properties enables systematic investigation into photobleaching dynamics under white light illumination in air. Degradation chemistries are assessed via unique spectroscopic signatures for the BDT-3T cores and the endcaps using photoelectron spectroscopies. We show that the pyrazolone undergoes significant degradation due to ring opening, resulting in complete bleaching of the chromophore. The barbituric and rhodanine endcap molecules have moderate stability, while the benzothiazoleacetonitrile group produces the most stable chromophore despite undergoing some oxidative degradation. Collectively, our results suggest the following: (i) degradation is not just dependent on redox properties; (ii) core group stability is not independent of the endcap choice; and (iii) future design of high efficiency materials must consider both photo and chemical stability of the molecule as a whole, not just individual donor or acceptor building blocks.

14 SOLAR ENERGY↗

System-level performance and degradation of 21 GWDC of utility-scale PV plants in the United States

We assess the performance of a fleet of 411 utility-scale (i.e., >5 MWAC and ground-mounted) photovoltaic (PV) projects totaling 21.1 GWDC (16.3 GWAC) of capacity, which achieved commercial operations in the United States from 2007 to 2016. This fleet of projects contributed more than 50% of all solar electricity generated in the United States in 2017. Using detailed information on individual project characteristics, in conjunction with modeled irradiance data, we assess the extent to which actual first-year performance has lived up to both modeled and stated expectations. We then analyze system-level performance degradation in subsequent years by employing a “fixed effects” regression model to statistically isolate the impact of age on system performance. We find that this fleet of utility-scale PV projects has generally lived up to ex ante expectations for first-year performance but that subsequent system-level degradation—found to be −1.3%/year (±0.2%)—has, on average, been worse than both ex ante expectations (commonly −0.5%/year) and results from past studies (ranging from −0.8%/year to −1.0%/year). We emphasize that −1.3%/year is a system-level estimate that captures more than just module degradation (e.g., including soiling, balance of plant degradation, and downtime for maintenance and/or other events). A side analysis of a variety of project characteristics suggests that system-level degradation rates tend to be of lower magnitude among newer projects and larger projects and at sites with lower long-term average temperatures.

14 SOLAR ENERGY↗

An Investigation of Heuristic Control Strategies for Multi-Electrolyzer Wind-Hydrogen Systems Considering Degradation

With the growing demand for renewable-energy-powered hydrogen generation and the corresponding increase in plant capacity, individually controlling many electrolyzer stacks will be critical for increasing the plant's lifetime and efficiency. This paper introduces a rule-based controller framework targeting electrolyzer degradation to explore the opportunity space in multi-stack hydrogen plant control. A novel control-oriented degradation model is also presented in this work, which quantifies the impact of steady power input, fluctuating power input, and the number of startup/shutdown cycles on electrolyzer degradation. Using a wind power input signal, 13 controller configurations are tested on 5 MW hydrogen plants consisting of 2, 5, 10, and 25 stacks. These configurations are evaluated on their capability to mitigate electrolyzer degradation and efficiently produce hydrogen from the time-varying input power. The results show that multi-stack control for degradation can extend the plant's lifetime by more than a factor of 3 with minimal impact on instantaneous hydrogen production.

control↗

Light and Elevated Temperature Induced Degradation (LeTID) in a Utility-Scale Photovoltaic System

Here, we present a detailed case study of degradation in monocrystalline silicon photovoltaic modules operating in a utility-scale power plant over the course of approximately three years. We present the results of degradation analysis on arrays within the site, and find that five of the six arrays degraded faster than the best performing array, even though the arrays consist of modules of the same manufacturer and model. We also describe the results of extensive laboratory characterization of modules returned from the field, including module- and cell-level current–voltage characterization, luminescence imaging, and accelerated testing. The laboratory test results and the field performance are consistent with light and elevated temperature induced degradation (LeTID). Notably, we observe differences in back contact technology between affected and unaffected modules. This article also demonstrates a method to identify possible LeTID degradation in the field and confirm the result with laboratory testing of a small number of modules.

14 SOLAR ENERGY↗

Prediction of Climate-Specific Degradation Rate for Photovoltaic Encapsulant Discoloration

Encapsulant discoloration is a well-known field degradation mode of crystalline-silicon photovoltaic modules, particularly in the hot climate zones. The discoloration rate is influenced by several weathering factors, such as UV light, module temperature, and humidity, as well as the permeability of oxygen into the module. Here, a rate dependence model employing the modified Arrhenius equations to predict the degradation rate for encapsulant discoloration in different climates is presented. Two modeling approaches are introduced, which utilize the field and accelerated UV testing degradation data in conjunction with the field meteorological data to determine the acceleration factor for encapsulant browning. A novel method of accelerated UV stress testing at three simultaneous module temperatures in a single environmental chamber test run is implemented to estimate the activation energy for browning. The test was performed on three field-retrieved modules to capture the wear-out failure mechanism. The degradation in short-circuit current Isc rather than maximum power is used as a decisive parameter for the discoloration analysis. Furthermore, the developed model has been used to predict the Isc degradation rate for the Arizona field characterized by a hot and dry climate and is validated against the field-measured value. It has also been applied to other climate types, e.g., the cold and dry climate of New York.

14 SOLAR ENERGY↗