Joining AA7099 to Ni-Cr-Mo Steel using Friction Stir Dovetailing
Friction stir dovetailing (FSD) was used to join 0.5 inch (12.7 mm) AA7099 to 0.5 inch (12.7 mm) Ni-Cr-Mo steel in a lap configuration. Two new FSD approaches are reported that significantly reduce zinc embrittlement of Fe-Al intermetallic compounds (IMCs) which form during conventional friction stir welding (FSW). The first method uses the general FSD approach where a custom designed tool is employed to extrude the AA7099 into the pre-machined dovetail groove of underlying steel by forming mechanical interlocking and metallurgical bonding simultaneously. The second method uses a two-step approach where FSD of AA6061 is first used to form a silicon-rich Fe-Al IMC within the dovetail groove. AA7099 plate is then joined to the AA6061 within the dovetail using conventional FSW. A discussion of the new FSD technique, joint configurations, and process parameters are provided along with joint microstructural analyses and mechanical performance.