Search NASA⌕ Search

SEARCH · Search NASA

Results for “Impact testing”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 505 records · Page 28

DE-NE0000724 - Research Performance Final Report - Investigation of Thermal Aging Effects on the Evolution of Microstructure and Mechanical Properties of Cast Duplex Stainless Steels

This report details the research activities carried out under DOE-NEUP award number DE-NE0000724 concerning the evolution of structural and mechanical properties during thermal aging of CF–3 and CF–8 cast duplex stainless steels (CDSS). The overall objective of this project was to use state-of-the-art characterization techniques to elucidate trends and phenomena in the mechanical and structural evolution of cast duplex stainless steels (CDSS) during thermal aging. These steels are commonly used as structural materials in commercial light water nuclear power plants, undergoing aging for decades in operation as cooling water pipes, pump casings, valve bodies, etc. During extended exposure to these conditions, CDSS are known to undergo a change in mechanical properties resulting in a loss of ductility, i.e. embrittlement. While it is generally accepted that structural changes within the ferrite phase, such as decomposition into iron (Fe)-rich and chromium (Cr)-rich domains, lead to the bulk embrittlement of the steels, many questions remain as to the mechanisms of embrittlement at multiple length scales. This work is intended to shed insight into the atomic level composition changes, associated kinetic mechanisms, and effects of changing phase structure on micro- and nano-scale deformation that lead to loss of impact toughness and tensile ductility in these steels. In general, this project provides a route to answer some of these major questions using techniques such as 3-dimensional (3-D) atom probe tomography (APT) and real-microstructure finite element method (FEM) modeling, which were not readily available when these steels were originally selected for service in light water reactors. Mechanical properties evaluated by Charpy V-notch impact testing (CVN), tensile testing, and microhardness and nanohardness measurements were obtained for each condition and compared with the initial baseline properties to view trends in deformation behavior during aging. Concurrent analysis of the microstructure and nanostructure by atom probe tomography (APT) and transmission electron microscopy (TEM) provide mechanistic insight into the kinetic and mechanical behavior occurring on the nano-scale. The presence and morphology of the ferrite, austenite, and carbide phases have been characterized, and formation of new phases during aging, including spinodal decomposition products (α- and α'-ferrite) and G-phase, have been observed. The mechanical and structural characterization have been used to create accurate FEM models based on the real micro- and nano-structures of the systems. These models provide new insight into the local deformation behavior of these steels and the effects of each individual phase (including ferrite, austenite, carbides, and spinodal decomposition products) on the evolving bulk mechanical behavior of the system. The project was divided into three major tasks: 1. Initial Microstructure and Mechanical Property Survey and Initiate Heat Treatment; 2. Microstructural Characterization and Mechanical Property Testing During Aging; and 3. Microstructure-based Finite Element Modeling. Each of these tasks was successfully executed, resulting in reliable data and analysis that add to the overall body of work on the CDSS materials. Baseline properties and aging trends in mechanical data confirm prior observations and add new insights into the mechanical behavior of the steels. Structural characterization on multiple length scales provides new information on phase changes occurring during aging and sheds light on the kinetic processes occurring at the atomic scale. Furthermore, a combination of mechanical testing and microstructural characterization techniques was utilized to design FEM models of local deformation behavior of the ferrite and austenite phases, providing valuable new information regarding the effects of each of the microstructural components on the hardening and embrittlement processes. The data and analysis presented in this report and the publication associated with this project (§V) increase the understanding of aging and deformation in CF–3 and CF–8 steels. These results provide valuable information that can be utilized to aid in making informed decisions regarding the ongoing use of these steels in commercial nuclear infrastructure.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

EBR-II Superheater Duplex Tube Examination

After 30 years of operation, the Experimental Breeder Reactor II (EBR-II) Superheater 710 at Argonne National Laboratory-West (now Idaho National Laboratory) was decommissioned. As part of its post-service examination, four duplex tube sections were removed and Charpy impact testing was performed to characterize the crack arresting ability of nickel-bonded tube interfaces. Scanning electron microscopy (SEM) examination was also performed to characterize and identify changes in bond material microstructure. From room temperature to 400 degrees C, all samples demonstrated ductility and crack-stopping ability similar to that exhibited by beginning-of-life samples. However, at low temperature (-5 degrees C), samples removed from the lower region of the superheater (near the sodium inlet) failed while those from the upper region (near the sodium outlet) did not. SEM analysis revealed that all the tube-tube interfaces showed evidence of iron diffusion into the nickel braze, which resulted in the formation of a multiphase diffusion structure. Yet, significant void formation was only observed in the bond layer of the tubes removed from the lower region. This may be due to a change in the crystal microstructure of one of the phases within the bond layer that occurs in the 350 to 450 degrees C temperature range, which results in a lower density and the formation of porosity. Apparently, only the samples from the higher temperature region were exposed to this transition temperature, and the resulting large voids that developed acted as stress concentrators that led to low-temperature embrittlement and failure of the Charpy impact specimens.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Formation of Lamellar Carbides in Alloy 617-HAZ and Their Role in the Impact Toughness of Alloy 617/9%Cr Dissimilar Welded Joint

The relationship between the microstructure and impact toughness, especially the formation of the lamellar carbides and its effect on the impact toughness of the heat-affected zone of Alloy 617 (Alloy 617-HAZ), was systematically investigated. Impact test was performed on Alloy 617/9%Cr dissimilar welded joints aged for different time at 620 °C. The results showed that the characteristic zones of the whole welded joint revealed decreased impact toughness with increasing the aging time. The impact energies in weld metal showed high stability despite the aging process, while the Alloy 617-HAZ for all testing specimens presented the lowest impact toughness with various aging time. Meanwhile, the mixed grains were found in the base metal (BM) and heat-affected zone of Alloy 617, together with the twins with different widths located in the interior of the large grains. The columnar and equiaxed grain zones appear alternately due to the multilayer and multi-pass welding technique. In particular, compared with Alloy 617-BM, coarsened and even lamellar carbides were observed in Alloy 617-HAZ. These special carbides can separate the grains and therefore result in the formation of intergranular fracture morphology in Alloy 617-HAZ. Besides, the microhardness distribution was tested with a proper load, and the results exhibited that the weld possessed the highest hardness for all specimens with various aging time. The higher microhardness in Alloy 617-HAZ compared with that in Alloy 617-BM was attributed to the high density of the dislocations, which could be detected by transmission electron microscope. As a result, the coarsened carbides aggregated in the grain boundaries to form the lamellar layer are deemed as the main factor to reduce the impact toughness in Alloy 617-HAZ.

36 MATERIALS SCIENCE↗

Single particle impact explorations on the role of powder heat treatments in cold spray: Effects of strength and oxide structure

In cold spray, the optimization of the powder feedstock for improving the final properties of the coating and for improving the process itself are two different objectives. This paper explores the latter, studying the relationship between powder pre-heat treatment and the kinetic bonding between the individual particles and the substrate. Using a laser-induced particle impact test (LIPIT), we investigate the effect of different heat treatments on the critical adhesion velocity of Al 6061. Although heat treatments change the strength of the powders as well as the thickness of the native oxide layer each by as much as ∼50 %, the critical adhesion velocity remains constant to within only ∼10 %. A deeper analysis reveals that these two factors change in somewhat complementary ways for the heat treatments explored here, leading to counteracting effects. By quantitatively evaluating these two microstructural factors in tandem, we find that they are roughly equally important in determining the critical adhesion velocity. These observations thus provide insight for the development of new heat treatment regimens that might lower the adhesion velocity.

Al 6061↗

Scaling of impact damage in fiber composites

Impact damage in fiber composite structures remains of much concern, and is often the limiting factor in establishing allowable strain levels. The complexity of impact damage formation usually dictates that experiments are required, but scaling of results from small laboratory scale specimens to large structures introduces additional uncertainty into the analysis. This presentation gives the results of an analytical and experimental investigation intended to develop procedures for prediction of damage formation and subsequent strength loss, with particular emphasis on scaling of results with respect to structure size. The experimental investigation involved both drop-weight and airgun impact on carbon/epoxy plates and cylinders. Five sizes of plates ranging from 50 by 50 by 1.072 mm to 250 by 250 by 5.36 mm, and two sizes of cylinders with diameters of 96.5 and 319 mm, were employed in the experimental program. Impact tests were carried out over a range of impact conditions, and specimens were inspected for damage by C-scan and deplying. Analysis procedures were developed for both quasistatic and dynamic impacts for both the plates and cylinders. As has been reported previously, comparison of predicted structural response and measured surface strains was quite good over the entire range of sizes employed in the program. The damage formation and strength loss after impact showed a number of interesting features that are significant with respect to scaling of size. The extent of delamination was observed to increase with specimen size more than would be expected if stresses controlled the delamination extent. This was explained on the basis that delamination is controlled by energy release rates, and thus incorporates the usual dependence on the absolute size characteristic of fracture mechanics. Additionally, the experiments indicated that delamination initiated at matrix cracks and is dependent on the absolute size of the ply group thicknesses. Both the initiation and propagation of delamination are seen to be controlled by fracture mechanics parameters, and thus show specific dependence on size that must be accounted for in extrapolating results from laboratory scale tests to full size structures.

Swanson, Stephen R.↗

Data Reduction and Its Impact on Test-Analysis Correlation

A research project has been initiated to improve crash test and analysis correlation. The research has focused on two specimen types: simple metallic beams and plates; and a representative composite fuselage section. Impact tests were performed under carefully controlled conditions. In addition, the specimens were densely instrumented to enable not only correlation with finite element simulations, but to also assess the repeatability of the data. Simulations utilizing a detailed finite element model were executed in a nonlinear transient dynamic code. The results presented in this paper concentrate on the effect of several data reduction processes, to include filtering frequency and sampling rate, on the correlation accuracy.

Lyle, Karen H.↗

A Wear Model for Diesel Engine Exhaust Valves

The work summarized here comprises the concluding effort of a multi-year project, funded by the U.S. Department of Energy, Office of Vehicle Technologies. It supports the development of a better understanding of advanced diesel engine designs in which enhanced power density, energy efficiency, and emissions control place increasing demands upon the durability of engine materials. Many kinds of metallic alloys are used in engines depending on the operating stresses, temperatures, and chemical environments. Exhaust valves, for example, are subjected to high temperatures and repetitive surface contacts that place demands on durability and frictional characteristics of the materials. Valves must continue to seal the combustion chamber properly for thousands of hours of cyclic engine operation and under varying operating conditions. It was the focus of this effort to understand the wear processes in the valve-seat area and to develop a model for the surface deformation and wear of that important interface. An annotated bibliography is provided to illustrate efforts to understand valve wear and to investigate the factors of engine operation that affect its severity and physical manifestation. The project for which this modeling effort was the final task, involved construction of a high-temperature repetitive impact test system as well as basic tribology studies of the combined processes of mechanical wear plus oxidation at elevated temperatures. Several publications resulted from this work, and are cited in this report. The materials selected for the experimental work were high-performance alloys based on nickel and cobalt. In some cases, engine-tested exhaust valves were made available for wear analysis and to ensure that the modes of surface damage produced in experiments were simulative of service. New, production-grade exhaust valves were also used to prepare test specimens for experimental work along with the other alloy samples. Wear analysis of valves and seats run for hundreds of hours in heavy-duty diesels provided insights into the kinds of complexity that the contact conditions in engines can produce, and suggested the physical basis for the current approach to modeling. The model presented here involves four terms, two representing the valve response and two for its mating seat material. The model's structure assumes that wear that takes place under a complex combination of plastic deformation, tangential shear, and oxidation. Tribolayers form, are removed, and may reform. Layer formation affects the friction forces in the interface, and in turn, the energy available to do work on the materials to cause wear. To provide friction data for the model at various temperatures, sliding contact experiments were conducted from 22 to 850 C in a pin-on-disk apparatus at ORNL. In order to account for the behavior of different materials and engine designs, parameters in all four terms of the model can be adjusted to account for wear-in and incubation periods before the dominant wear processes evolve to their steady-state rates. For example, the deformation rate is assumed to be maximum during the early stages of operation, and then, due to material work-hardening and the increase in nominal contact area (which reduces the load per unit area), decreases to a lower rate at long times. Conversely, the rate of abrasion increases with time or number of cycles due to the build-up of oxides and tribo-layers between contact surfaces. The competition between deformation and abrasion results in complex, non-linear behavior of material loss per cycle of operation. Furthermore, these factors are affected by valve design features, such as the angle of incline of the valve seat. Several modeling scenarios are presented to demonstrate how the wear profile versus number of cycles changes in response to: (a) different relative abrasion rates of the seat and valve materials, (b) the friction coefficient as a function of temperature, (c) the relative deformation contribution of valve and seat materials, and (d) an interruption in the dominant wear process.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Oxygen Compatibility Testing of Composite Materials

Composite materials offer significant weight-saving potential for aerospace applications in propellant and oxidizer tanks. This application for oxygen tanks presents the challenge of being oxygen compatible in addition to complying with the other required material characteristics. This effort reports on the testing procedures and data obtained in examining and selecting potential composite materials for oxygen tank usage. Impact testing of composites has shown that most of these materials initiate a combustion event when impacted at 72 ft-lbf in the presence of liquid oxygen, though testing has also shown substantial variability in reaction sensitivities to impact. Data for screening of 14 potential composites using the Bruceton method is given herein and shows that the 50-percent reaction frequencies range from 17 to 67 ft-lbf. The pressure and temperature rises for several composite materials were recorded to compare the energy releases as functions of the combustion reactions with their respective reaction probabilities. The test data presented are primarily for a test pressure of 300 psia in liquid oxygen. The impact screening process is compared with oxygen index and autogenous ignition test data for both the composite and the basic resin. The usefulness of these supplemental tests in helping select the most oxygen compatible materials is explored. The propensity for mechanical impact ignition of the composite compared with the resin alone is also examined. Since an ignition-free composite material at the peak impact energy of 72 ft-lbf has not been identified, composite reactivity must be characterized over the impact energy level and operating pressure ranges to provide data for hazard analyses in selecting the best potential material for liquid tank usage.

Engel, Carl D.↗

Inhibited Shaped Charge Launcher Testing of Spacecraft Shield Designs

This report describes a test program in which several orbital debris shield designs were impact tested using the inhibited shaped charge launcher facility at Southwest Research Institute. This facility enables researchers to study the impact of one-gram aluminum projectiles on various shielding designs at velocities above 11 km/s. A total of twenty tests were conducted on targets provided by NASA-MSFC. This report discusses in detail the shield design, the projectile parameters and the test configuration used for each test. A brief discussion of the target damage is provided, as the detailed analysis of the target response will be done by NASA-MSFC.

Grosch, Donald J.↗

Inhibited Shaped Charge Launcher Testing of Spacecraft Shield Designs

This report describes a test program in which several orbital debris shield designs were impact tested using the inhibited shaped charge launcher facility at Southwest Research Institute. This facility enables researchers to study the impact of one-gram aluminum projectiles on various shielding designs at velocities above 11 km/s. A total of twenty tests were conducted on targets provided by NASA-MSFC. This report discusses in detail the shield design, the projectile parameters and the test configuration used for each test. A brief discussion of the target damage is provided, as the detailed analysis of the target response will be done by NASA-MSFC.

Grosch, Donald J.↗

Simulation of dynamic crystal plasticity with a Lagrangian discontinuous Galerkin hydrodynamic method

Here we present a new Lagrangian modal discontinuous Galerkin (DG) hydrodynamic method that supports a dynamic dislocation based crystal plasticity model for simulating the mechanical behavior of crystallographic materials, both single crystal and polycrystalline, under dynamic conditions. A modal DG approach is used to evolve fields relevant to conservation laws. These fields are approximated by Taylor series polynomials of varying degree. These polynomials describe macro-scale hydrodynamic behavior while their evolution is determined by evaluating the dynamic crystal plasticity model at material points within the element. The dynamic crystal plasticity model is sensitive to the time increment size, with too large of time increments leading to instability in the model. To mitigate this, the temporal evolution of the dynamic crystal plasticity model is achieved with the combination of a sub-incrementing scheme with Heun’s third-order time integration scheme, which is also used to temporally evolve the governing equations. The implementation of the dynamic crystal plasticity model within the DG framework is tested using a 2D approximation of the Taylor impact test with a single crystal material, using quadratic elements that have faces that can bend. In addition to the standard continuous material modeling, we propose a new simulation method that would represent the heterogeneous behavior of polycrystalline microstructures within an element by varying the position and material properties of the material points within the element. This method is demonstrated using random orientation distributions on materials points that are arranged in both structured and random configurations.

42 ENGINEERING↗

Correlating Mechanical Sensitivity with Spin Transition in the Explosive Spin Crossover Complex [Fe(Htrz) 3 ] n [ClO 4 ] 2 n

Spin crossover complexes are known to undergo bond length, volume, and enthalpy changes during spin transition. In an explosive spin crossover complex, these changes could affect the mechanical and initiation sensitivity of the explosive and lead to the development of a new class of sensitivity switchable materials. To explore this relationship, the well-known spin crossover compound [Fe(Htrz) 3 ] n [ClO 4 ] 2n (1) was re-evaluated for its explosive properties, and its mechanical impact sensitivity was correlated to spin transition. A variable temperature impact test was developed and used to evaluate the impact sensitivity of 1 in the low spin (LS, S = 0), thermally accessed high spin (HS, S = 2), and mixed LS and HS states. For comparison, the structurally similar Ni compound, [Ni(Htrz) 3 ] n [ClO 4 ] 2n (2), which does not undergo a spin transition at accessible temperatures, was synthesized and characterized, and its explosive properties and variable temperature impact sensitivity measured. These results reveal a correlation between impact sensitivity and spin transition, where 1 exhibits lower impact sensitivity in the LS state and increases in sensitivity upon transition to the HS state. Here, density functional theory was used to predict structural changes that occur upon spin transition that correlate to the change in sensitivity. This demonstrates, for the first time, an explosive spin crossover compound (ExSCO) that exhibits switchable impact sensitivity with a fully reversible internal switching mechanism.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Investigation of Orbital Debris Impacts on Shuttle Radiator Panels

This paper documents the data collected from two hypervelocity micro-meteoroid orbital debris (MMOD) impact events where the shuttle payload bay door radiator sandwich panel was completely perforated. Scanning Electron Microscope/Energy-Dispersive x-ray Spectroscopy (SEM/EDS) analysis of impact residue provided evidence to identify the source of each impact. Impact site features that indicate projectile directionality are discussed, along with hypervelocity impact testing on representative samples conducted to simulate the impact event. The paper provides results of a study of impact risks for the size of particles that caused the MMOD damage and the regions of the orbiter vehicle that would be vulnerable to an equivalent projectile

Hyde, James L.↗

Evaluation of Material Models within LS-DYNA(Registered TradeMark) for a Kevlar/Epoxy Composite Honeycomb

The performance of material models to simulate a novel composite honeycomb Deployable Energy Absorber (DEA) was evaluated using the nonlinear explicit dynamic finite element code LS-DYNA(Registered TradeMark). Prototypes of the DEA concept were manufactured using a Kevlar/Epoxy composite material in which the fibers are oriented at +/-45 degrees with respect to the loading axis. The development of the DEA has included laboratory tests at subcomponent and component levels such as three-point bend testing of single hexagonal cells, dynamic crush testing of single multi-cell components, and impact testing of a full-scale fuselage section fitted with a system of DEA components onto multi-terrain environments. Due to the thin nature of the cell walls, the DEA was modeled using shell elements. In an attempt to simulate the dynamic response of the DEA, it was first represented using *MAT_LAMINATED_COMPOSITE_FABRIC, or *MAT_58, in LS-DYNA. Values for each parameter within the material model were generated such that an in-plane isotropic configuration for the DEA material was assumed. Analytical predictions showed that the load-deflection behavior of a single-cell during three-point bending was within the range of test data, but predicted the DEA crush response to be very stiff. In addition, a *MAT_PIECEWISE_LINEAR_PLASTICITY, or *MAT_24, material model in LS-DYNA was developed, which represented the Kevlar/Epoxy composite as an isotropic elastic-plastic material with input from +/-45 degrees tensile coupon data. The predicted crush response matched that of the test and localized folding patterns of the DEA were captured under compression, but the model failed to predict the single-cell three-point bending response.

Polanco, Michael A.↗

Recent Shuttle Post Flight MMOD Inspection Highlights

Four significant micro-meteoroid orbital debris (MMOD) impact events on the shuttle are documented: two perforations of the payload bay door radiator sandwich panel along with craters in a crew module window and a wing leading edge reinforced carbon-carbon panel. Results from Scanning Electron Microscope/Energy-Dispersive x-ray Spectroscopy (SEM/EDS) analysis of impact residue are provided in an attempt to identify the source of each impact. Particle sizes that could produce the observed damage are discussed, along with hypervelocity impact testing on representative samples conducted to simulate the impact event.

Hyde, James L.↗

Orbital Debris Impact Damage to Reusable Launch Vehicles

In an effort by the National Aeronautics and Space Administration (NASA), hypervelocity impact tests were performed on thermal protection systems (TPS) applied on the external surfaces of reusable launch vehicles (RLV) to determine the potential damage from orbital debris impacts. Three TPS types were tested, bonded to composite structures representing RLV fuel tank walls. The three heat shield materials tested were Alumina-Enhanced Thermal Barrier-12 (AETB-12), Flexible Reusable Surface Insulation (FRSI), and Advanced Flexible Reusable Surface Insulation (AFRSI). Using this test data, predictor equations were developed for the entry hole diameters in the three TPS materials, with correlation coefficients ranging from 0.69 to 0.86. Possible methods are proposed for approximating damage occurring at expected orbital impact velocities higher than tested, with references to other published work.

Robinson, Jennifer H.↗

A Summary of Test and Analysis Results from a Second Lift+Cruise Full-Scale Drop Test

The realization of advanced air mobility markets is enabling new forms of transportation to take shape in the United States and around the world. Though currently in development, as these markets mature, new types of vertical take-off and landing (VTOL) vehicles have been undergoing development for use. There are many factors which must be addressed prior to these types of vehicles becoming viable alternative forms of transportation in these markets. These factors include incorporation into the existing airspaces, the logistics of operating in urban environments, along with numerous factors associated with safety and reliability. To address some of the safety aspects associated with the development of these new types of vehicles, NASA has been conducting research into the performance of an example electric VTOL (eVTOL) aircraft as a part of the Revolutionary Vertical Lift Technology (RVLT) project. Over the course of this research, many aspects including the development of energy absorbing components, the evaluation of seating systems, the development of advanced finite element material model systems and the acquisition of full-scale vehicle impact data were investigated. The report will discuss aspects related to the acquisition of full-scale vehicle data which occurred in the form of a full-scale impact test conducted in the Summer of 2025. This test was on a NASA designed Lift+Cruise composite cabin test article and represented a partial capstone in the entirety of previous eVTOL research conducted for the project. In this test, a variety of experiments were included in order to investigate the effect of a full-scale environment on the experiment results. In parallel, the development of a computational impact model to simulate the full-scale test will be discussed in this report. A model of the Lift+Cruise test article was developed utilizing data collected from previous sub- and full-scale test data and then simulated in the current test environment. The model development, its use in pre-test predictions, and its use in post-test correlation will all be presented. This report will present the test data acquired from the Lift+Cruise test and document several of the results obtained. One intended result is to determine the effect of a complex full-scale crash impact on the identification of occupant injury risk within seat and vehicle designs. A second intended result is to determine whether high-fidelity models can be used with some confidence in the prediction of test events and can allow for additional test cases to be simulated without the need of having to conduct additional tests. The overall goal of the test is to provide the community with data that can be used for design, development or certification efforts, along with providing data on what an example eVTOL crash incident could entail.

energy storage systems↗