Long-Term Effects of Humidity on Stainless Steel Pitting in Sea Salt Exposures

Ground 304 stainless steel (SS) samples were exposed to sea salt particles at 35 °C and two relative humidity (RH) levels for durations ranging from 1 week to 2 years. For all exposure times, pit number density and total pit volume at 40% RH were observed to be considerably greater than those at 76% RH. Statistical analysis of distributions of pit populations for both RH conditions showed that pit number density and total pit volume increased rapidly at first but slowed as exposure time increased. Cross-hatched features were observed in the 40% RH pits while ellipsoidal, faceted pits were observed at 76% RH. Optical profilometry indicated that most pits were not hemispherical. X-ray tomography provided evidence of undercutting and fissures. Piecewise curve fitting modeled the 40% RH data closely, predicting that corrosion damage would eventually plateau. However, a similar treatment of the 76% RH data suggested that corrosion damage would continuously increase, which implied that the piecewise power-law fit was limited in its ability to model atmospheric corrosion generally. Based on these observations, the operative mechanisms determining long-term corrosion behavior were hypothesized to be different depending on the RH of exposure.

36 MATERIALS SCIENCE↗

Update on Investigations of Viability of Cold Spray and FSW as a Spent Nuclear Fuel Dry Storage Canister Mitigation Tool

The purpose of this work is to investigate the use of cold spray and friction stir welding or processing (FSW/P) for repair and mitigation of chloride-induced stress corrosion cracking (CISCC) in dry cask storage system (DCSS) canisters to ensure integrity far beyond their original license period. This report provides a viability analysis of cold spray and friction stir welding for repair and fabrication of DCSS canisters. This report presents experimental work and a research strategy to optimize and evaluate cold spray and FSW/P for CISCC resistance. The literature reports that the following three conditions must exist for CISCC to occur: tensile stress, corrosive environment, and susceptible material. These conditions must be understood and accounted for while evaluating CISCC susceptibility. Furthermore, non-obvious factors, such as surface conditions and geometric confinement, can dramatically increase the intensity of one or more of the three listed conditions for CISCC. Arc welding should be considered for either temporary or permanent repair when combined with a mitigation technology. It is known that alloys used in the existing inventory of spent nuclear fuel storage canisters become sensitized in areas around fusion welds. Technologies, such as cold spray or FSW, can mitigate the sensitization caused by fusion welds. FSW/P and cold spray, potential alternatives for fabrication and repair, are solid-phase processes. No melting occurs and the energy input can be controlled such that no harm is done to the base metal during these processes. FSW/P should be considered for use in new fabrication of canisters and repair of existing canisters. Low heat input and grain refinement result in material with improved mechanical properties and comparable generalized corrosion performance relative to base metal. FSW/P offers the potential of through-thickness CISCC resistance. Cold spray should be considered for production, mitigation, and repair of canisters. Cold spray has demonstrated the ability to deposit stainless steel, Inconel alloys, and other alloys on stainless steel 304L such that galvanic potential is matched and resistance to pitting is improved. The technical basis for cold spray mitigation and repair within the overpack using remote robotic equipment is established. A non-obvious application to the research community is the sealing of crevices. All reported instances of CISCC in the fielded nuclear applications were associated with crevice corrosion. This can be avoided by cold spraying to seal crevices. The bulk of the work planned for FY 2020 will be generating coupons for CISCC testing by collaborative projects at Pacific Northwest National Laboratory and Sandia National Laboratories. First an exploratory study will be executed that will include screening studies and process optimization. This task will identify the effect of process parameters on microstructure and CISCC resistance. Optimized parameters will be used to produce a smaller number of coupons for full testing and evaluation. Test methods for evaluating CISCC resistance must meet the following criteria: (1) normalized surface geometry and exposed process microstructure, (2) account for residual stresses, (3) be in a controlled and appropriate test environment, and (4) be numerically quantifiable and repeatable. Failure to meet these criteria could lead to results that cannot be used for comparative analysis of processes and materials.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Impact of Permanganate Oxidation of Glycolate on Corrosion of the Defense Waste Processing Facility (DWPF) Recycle Collection Tank (RCT), Transfer-line and Waste Tank Materials of Construction (MoC)

Savannah River Remediation (SRR) is evaluating the use of glycolic acid to replace formic acid as an alternate reductant for the Defense Waste Processing Facility (DWPF) at Savannah River Site (SRS). The replacement is aimed at reducing facility hazards, improving pH stability and rheological control, and lowering off gas production. Glycolate, which is the product that may remain, can also be carried downstream to High-Level Waste and Low-Level Waste facilities. Complete oxidation of glycolate and other organic species from the Sludge Receipt and Adjustment Tank (SRAT) may be necessary to minimize thermolytic hydrogen generation that can cause flammability issues. The glycolate oxidation may be performed in the Recycle Collection Tank (RCT). The RCT heel would be adjusted with sodium hydroxide to maintain the solution caustic and sodium nitrite as corrosion inhibitor prior to the addition of condensate that can be from the contents of the Slurry Mix Evaporator Condensate Tank (SMECT) or Offgas Condensate Tank (OGCT). The RCT tank collects the waste to be transferred via the Low Point Pump Pit – Recycle Pump Tank (LPPP-RPT) through a jacketed transfer-line to the Tank Farm facility. Scoping studies were performed to evaluate an oxidizing agent and sodium permanganate was selected as the best option for glycolate destruction. Testing was recommended to determine the impact on the Materials of Construction (MoC) due to the addition of sodium permanganate. The targeted concentration of sodium permanganate used equated to a 7:1 molar permanganate to glycolate ratio (nominally 0.002 M permanganate). However, to conservatively maximize the permanganate corrosivity, in some cases no glycolate was added.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

The stress-corrosion behavior of Al-Li-Cu alloys: A comparison of test methods

Two powder metallurgy processed (Al-Li-Cu) alloys with and without Mg addition were studied in aqueous 3.5% NaCl solution during the alternate immersion testing of tuning fork specimens, slow crack growth tests using fracture mechanics specimens, and the slow strain rate testing of straining electrode specimens. Scanning electron microscopy and optical metallography were used to demonstrate the character of the interaction between the Al-Li-Cu alloys and the selected environment. Both alloys are susceptible to SC in an aqueous 3.5% NaCl solution under the right electrochemical and microstructural conditions. Each test method yields important information on the character of the SC behavior. Under all conditions investigated, second phase particles strung out in rows along the extrusion direction in the alloys were rapidly attacked, and played principal role in the SC process. With time, larger pits developed from these rows of smaller pits and under certain electrochemical conditions surface cracks initiated from the larger pits and contributed directly to the fracture process. Evidence to support slow crack growth was observed in both the slow strain rate tests and the sustained immersion tests of precracked fracture mechanics specimens. The possible role of H2 in the stress corrosion cracking process is suggested.

Rizzo, P. P.↗

Effects of Laser Etching on the Corrosion Susceptibility of SAVY 4000 and Hagan Containers

Since the late 1990’s, the Hagan container was used as the primary container for packaging of plutonium-bearing materials. The Hagan design consisted of a threaded closure, a Viton® ORing, a carbon-carbon filter, and a 304L stainless steel (SS) body. Over the years, Hagans have shown vulnerability in their design [1]. In 2008, The Department of Energy (DOE) issued DOE M 441.1-1, Nuclear Material Packaging Manual, which detailed an approach to obtain highconfidence in containers by including specific design requirements, material contents and an approach to determine life span from said contents, and surveillance techniques [2]. In response to both the vulnerability issues with the Hagan and DOE M 441.1-1, the SAVY 4000 container with its twist style closure, Viton® O-Ring, Fiberfrax-Gortex filter, and annealed 316L SS body, was designed as the replacement for Hagan containers, but only for a short term lifespan of 5 years [1]. However, both the Hagan and SAVY 4000 are being pushed to maintain a lifespan of 40 years. Therefore, proper confidence must be placed on each component of each container to last a minimum of 40 years. So far, the biggest concern found during surveillance of these containers is corrosion and the potential for failure by corrosion. One concern is that the containers fail due to stress corrosion cracking (SCC), especially around the weld between the collar and the body as welds leave residual stresses. One advantage the SAVY 4000 has is that the body is annealed, but its weld is still susceptible as it was welded after annealing [3, 4]. Moreover, 316L SS is known to have a higher pitting resistance (pits are a precursor to SCC and can also lead to extensive failure of the material), than 304L SS [4]. During recent surveillance activities, two SAVY 4000’s containing Solution Assay Instrument (SAI) solutions were opened. The SAI SAVY 4000’s contained plutonium (Pu) in 3M HCl solution in plastic volumetric flasks placed inside of polyethylene bags. Historically, a SAVY 4000 containing an SAI solution is packaged for 3 weeks, however, these particular containers were not reopened until 14 months later. When opened, brown-red corrosion product was found all over the inside of the container as shown in Figure 1.

36 MATERIALS SCIENCE↗

REAL TIME ULTRASONIC ALUMINUM SPOT WELD MONITORING SYSTEM

Aluminum alloys pose several properties that make them one of the most popular engineering materials: they have excellent corrosion resistance, and high weight-to-strength ratio. Resistance spot welding of aluminum alloys is widely used today but oxide film and aluminum thermal and electrical properties make spot welding a difficult task. Electrode degradation due to pitting, alloying and mushrooming decreases the weld quality and adjustment of parameters like current and force is required. To realize these adjustments and ensure weld quality, a tool to measure weld quality in real time is required. In this paper, a real time ultrasonic non-destructive evaluation system for aluminum spot welds is presented. The system is able to monitor nugget growth while the spot weld is being made. This is achieved by interpreting the echoes of an ultrasound transducer located in one of the welding electrodes. The transducer receives and transmits an ultrasound signal at different times during the welding cycle. Valuable information of the weld quality is embedded in this signal. The system is able to determine the weld nugget diameter by measuring the delays of the ultrasound signals received during the complete welding cycle. The article presents the system performance on aluminum alloy AA6022.

36 MATERIALS SCIENCE↗

Postirradiation Examination of the ATF-1 Experiments - 2019 Status

A collaborative effort of the Advanced Fuels Campaign together with industry consortia is focused on the development of enhanced accident tolerant fuels for Light Water Reactors (LWRs). The scoping studies, referred to as ATF-1 irradiations, are being performed in the Advanced Test Reactor of Idaho National Laboratory using drop-in style irradiations. The Post-Irradiation Examinations (PIEs) of ATF-1 began in 2017 and continued in 2019. This report describes the results of examinations on ATF-1 irradiations designed to test the performance of advanced iron-based cladding, including compatibility of FeCrAl with UO2, and ATF-1 irradiation of U3Si5. Two rodlets with commercial iron-based cladding and UO2 pellets have been irradiated to low burnup (i.e., < 20 GWd/tHM). The first rodlet had an Alloy33 cladding, while the other had a Kanthal APMT® cladding. The performed PIEs were focused on the determination of fuel microstructure, evaluation of fuel-cladding interaction and irradiation-induced variations of cladding mechanical properties. For both rodlets, no significant changes in the cladding hardness were measured, and the cladding hoop strain remained limited. Gamma tomography revealed no Cs axial migration as expected for LWR fuel, but significant cesium radial migration, which was induced by thermal migration consequent to high irradiation temperatures. Microstructure analyses revealed formation of secondary phases along the pellet rim of samples from both rodlets. No wastage or extensive chemical interaction between the fuel and the internal wall of the cladding was observed, suggesting that the secondary phases accumulated at the pellet rim might be due to formation of Cs-U-O compounds. However, further advanced PIEs are necessary to finally confirm this hypothesis. Optical microscopy analysis of the rodlet designed by Oak Ridge National Laboratory to evaluate the interaction between UO2 and various FeCrAl alloys revealed no extensive interaction in all the samples irradiated in the rodlet. Localized defects, namely circular pitting and cracks of a few tents of microns, were observed on the FeCrAl disc surfaces in some of the diffusion couples. These defects might be surface fabrication defects rather than irradiation-induced localized corrosion, but chemical analyses are needed to determine whether accumulation of corrosive fission products are causing enhanced interaction. Both non-destructive and destructive PIEs were collected on a rodlet containing U3Si5 fuel. The rodlet had extremely low fission gas release, similar to previously analyzed U3Si2 rodlets. Gamma tomography revealed thermo-migration of fission product ruthenium toward the center of the fuel pellet. The fuel microstructure resembles the as-fabricated microstructure, showing extensive microcracking related to the phase transition at 450°C. Two types of secondary phases were observed, which could either be due to segregation and precipitation of fission products or to UN impurities from fabrication. Finally, the current status of PIE on other ATF-1 irradiations will be discussed. These irradiations include UN-U3Si5 rodlets, UN-U3Si2 rodlets and an additional test with U3Si2 fuel.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

LIQUID AIR INTERFACE CORROSION TESTING FOR FY2010

An experimental study was undertaken to investigate the corrosivity to carbon steel of the liquid-air interface of dilute simulated radioactive waste solutions. Open-circuit potentials were measured on ASTM A537 carbon steel specimens located slightly above, at, and below the liquid-air interface of simulated waste solutions. The 0.12-inch-diameter specimens used in the study were sized to respond to the assumed distinctive chemical environment of the liquid-air interface, where localized corrosion in poorly inhibited solutions may frequently be observed. The practical inhibition of such localized corrosion in liquid radioactive waste storage tanks is based on empirical testing and a model of a liquid-air interface environment that is made more corrosive than the underlying bulk liquid due to chemical changes brought about by absorbed atmospheric carbon dioxide. The chemical changes were assumed to create a more corrosive open-circuit potential in carbon in contact with the liquid-air interface. Arrays of 4 small specimens spaced about 0.3 in. apart were partially immersed so that one specimen contacted the top of the meniscus of the test solution. Two specimens contacted the bulk liquid below the meniscus and one specimen was positioned in the vapor space above the meniscus. Measurements were carried out for up to 16 hours to ensure steady-state had been obtained. The results showed that there was no significant difference in open-circuit potentials between the meniscus-contact specimens and the bulk-liquid-contact specimens. With the measurement technique employed, no difference was detected between the electrochemical conditions of the meniscus versus the bulk liquid. Stable open-circuit potentials were measured on the specimen located in the vapor space above the meniscus, showing that there existed an electrochemical connection through a thin film of solution extending up from the meniscus. This observation supports the Hobbs-Wallace model of the development of the pitting susceptibility of carbon steel in alkaline solutions.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Uncertainty Quantification of Environmentally Assisted Stress Corrosion Cracking in Used Fuel Canisters (Status Report)

This study was initiated to quantify and characterize the uncertainty associated with the degradation mechanisms impacting normal dry storage operations for used nuclear fuel (UNF) and normal conditions of transport in support of the Spent Fuel and Waste Science & Technology Campaign (SFWST) and its effectiveness to rank the data needs and parameters of interest. This report describes the technical basis and guidance resulting from the development of software to perform uncertainty quantification (UQ) by developing and describing a holistic model that integrates the various processes controlling Atmospheric Stress Corrosion Cracking (ASCC) in the specific context of Interim Spent Fuel Storage Installations (ISFSIs). These processes include the daily and annual cycles of temperature and humidity associated with the environment, the deposition of chloride-containing aerosol particles, pit formation, pit-to-crack transition, and crack propagation.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Atomic-scale understanding of oxide growth and dissolution kinetics of Ni-Cr alloys

Aqueous corrosion of metals is governed by formation and dissolution of a passivating, multi-component surface oxide. Unfortunately, a detailed atomistic description is challenging due to the compositional complexity and the need to consider multiple kinetic factors simultaneously. To this end, we combine experiments with a first-principles-derived, multiscale computational framework that transcends thermodynamic descriptions to explicitly simulate the kinetic evolution of surface oxides of Ni-Cr alloys as a function of composition, temperature, pH, and applied voltage. In the absence of pitting, we identify three distinct voltage regimes, which are kinetically dominated by oxide growth, dissolution, and competitive dissolution and reprecipitation. Evolving compositional gradients and oxide thickness are revealed, including a transition between a metastable Ni-Cr mixed oxide and a thick, porous Ni-dominated oxide. Beyond elucidating the underlying physics, we highlight the need for competing kinetics in models to properly predict the transition from passivation to corrosion. Our results provide a key step towards co-design of alloy composition alongside environmental conditions for sustainable use across a variety of critical energy and infrastructure applications.

36 MATERIALS SCIENCE↗

Selective oxidation and nickel enrichment hinders the repassivation kinetics of multi-principal element alloy surfaces

Robust and sustained corrosion resistance in multi-principal element alloys (MPEA) requires rapid repassivation, i.e. regrowth of the passive layer once it is damaged or destroyed at the surface. In this study, we show that the repassivation of Al 0.1 CrCoFeNi MPEA in 0.6 M NaCl solution is hindered at pH of ~ 2.4 - 6.8 due to the formation of a Ni-enriched subsurface layer as a result of selective oxidation and dissolution of several principal elements, which can be fully restored at pH of ~ 14 from the oxidation of all principal elements. Specifically, surface characterization via X-ray photoelectron spectroscopy (XPS), high-angle annular dark-field (HAADF) imaging in scanning transmission electron microscopy (STEM), and atom probe tomography (APT), are coupled with density functional theory (DFT) calculations to determine surface composition, oxidation state, and electron work function to uncover the structural origin of the pH-dependent repassivation mechanisms. It was found that selective oxidation of Cr, Co, and Fe in the acidic to neutral solutions altered the surface composition to be significantly enriched in Ni as compared to the bulk. Once the original passive film is destroyed locally by either pitting or tribocorrosion, this altered surface composition exhibited a much poorer repassivation capability due to the increased electron work function and reduced surface reactivity at higher Ni concentration. Finally, these understandings could shed light on the future compositional design of non-equiatomic MPEAs towards sustained repassivation and corrosion resistance over a wide pH range.

36 MATERIALS SCIENCE↗

Sensitization of 316L Stainless Steel made by Laser Powder Bed Fusion Additive Manufacturing

Additively manufactured (AM) 316L stainless steel (SS) manufactured by laser powder bed fusion (L-PBF) and wrought 316L SS were subjected to sensitization heat treatments at 700°C up to 100 h. Using two evaluation methods, double-loop electrochemical potentiokinetic reactivation (DL-EPR) and ditching tests, degree of sensitization (DOS) and intergranular corrosion (IGC) susceptibility was evaluated. It was found that the wrought samples showed slightly lower IGC susceptibility compared to their AM counterpart. DOS and IGC attacks increased with sensitization time for all samples. Dislocation cellular structures were found to have little to no impact on DOS and IGC for the AM samples. Sensitized at 100 h, the AM sample showed significant Cr depletion along high-angle grain boundaries (12.35 wt% on average) and exhibited Cr carbide precipitation. Mo-rich particles along grain boundaries were also observed. The DL-EPR test attacks the surface oxide film and grain boundaries while the ditching test attacks the melt pool boundaries and grain boundaries (IGC and pitting). Changes to the DL-EPR and ditching standards for AM application have been proposed in this work.

316L stainless steel↗

Effect of tempering temperature on properties of 00Cr16Ni5Mo stainless steel

Specimens of 00Cr16Ni5Mo low carbon martensitic stainless steel were normalized at 1000 deg. C followed by tempering at 525 deg. C, 550 deg. C, 575 deg. C, 600 deg. C and 625 deg. C. After heat treatment, mechanical properties and pitting potential were determined through tensile, impact and electrochemical polarization tests. The results showed that the samples tempered at 550 deg. C and 600 deg. C for 2 h had an excellent combination of tensile strength, elongation, impact energy, hardness and corrosion resistance. Scanning electron microscopy, and X-ray diffraction examinations were conducted. These revealed that the properties of the steel were affected by the structure of the lath martensite, {delta}-ferrite, retained austenite and carbides.

36 MATERIALS SCIENCE↗

Friction Stir Processed Repair Welding of Dry Storage Canisters and Mitigation Strategies: Effect of Engineered Barrier Layer on Environmental Degradation

The proposed project aims to develop a friction sir based repair technique to heal cracks of stainless steel dry storage canisters (DSCs), created by the effect of stress corrosion cracking (SCC). In real service conditions, the welded parts of the canisters become prone to SCC under exposure to aggressive chemical environment. The focus of the project is on developing a mitigation strategy that can be implemented for countering SCC in DSCs following a two-pronged approach: (i) apply friction stir processing (FSP) as a crack repair technique while creating compressive residual stresses at the canister material surface, thus improving resistance against SCC; (ii) add molybdenum and/or nitrogen by friction stir based alloying process to create compositions that improve pitting resistance and thus enhance resistance against SCC. The specific project objectives are listed below: • Investigate FSW of 304L SS a potential repair welding technique of dry storage canisters; • Optimize the FSW parameters to introduce surface compressive stress profiles in the weldments; • Develop a FSP method to surface alloy the 304L with nitrogen and Mo by adding CrN and Mo powders; • Evaluate the surface compressive residual stress profile during FSW and FSP processes; • Evaluate the localized corrosion resistance of the FSW and FSP samples as a function of temperature, chloride concentration, and surface alloy composition; • Evaluate the SCC behavior of the FSW and FSP samples as a function of stress, chloride concentration, and temperature at different surface chemistries and induced residual stress profiles.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Magnetostrictive EMAT for Nuclear Spent Fuel Canisters

One approach for mitigation of stainless steel (SS) spent fuel canisters (SFCs) is to coat the welds or even the entire SFC with a cold-sprayed nickel coating. The coating can serve as a magnetostrictive interface between an electromagnetic acoustic transducer (EMAT) and the SS plate material. The EMAT can send ultrasound into the canister and “listen” for reflections caused by chloride-initiated stress corrosion cracking (CISCC) or other damage mechanisms that may lead to leaks if undetected and unmitigated. Here, this project outlines an approach for monitoring the integrity of SFCs using magnetostrictive EMAT sensors, which emit and detect discontinuity-initiated reflections indicative of pits or cracks likely arising from CISCC. Flat 13 mm SS plates with welds similar to actual canister welds were prepared, with flat-bottom holes 3 mm and 6 mm deep and 6 mm in diameter placed within the weld heat-affected zone (HAZ). The most effective sensor configurations were able to detect critical discontinuities more than 2 m away. Although a single sensor could be robotically deployed, the large volume covered by each sensor could support a small number of permanently mounted sensors, equipped with an external connector for periodic interrogation. The HAZ of a hypothetical SFC cylindrical surface could be effectively monitored with just 16 sensors.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Magnetostrictive Cold Spray Sensor Feasibility Assessment

Ultrasound sensors and inspection systems are frequently used to generate acoustic waves in metal structures capable of detecting and characterizing cracks, pits, erosion, inclusions, weld anomalies, and other material and structural features. One significant problem with piezoelectric transducers is the difficulty to achieve good coupling between the transducer and the surface being examined. This is particularly true in harsh conditions with high temperatures, cyclical hot and cold temperatures, highly radioactive fields found near nuclear reactors or spent nuclear fuel, caustic or corrosive fluids, and other extreme environmental conditions, as well as in long-term monitoring applications where repair or replacement of the sensor is difficult or expensive. Typically, coupling between the surface and the transducer is achieved with water, gel, grease, viscous shear coupling material, or pressure, which might not be possible or appropriate for long-term applications in which the impedance -matching materials wear away, evaporate, or simply stop functioning due to changes in surface conditions. Fluid couplings can evaporate or drain away from the transducer-substrate interface; glue- based couplings may foul or fail and are notoriously unreliable at high temperatures and in radioactive environments. This work explores the behavior of a magnetostrictive cold-spray patch that is metallurgically bonded to a stainless steel inspection target surface, and compares it to the performance of a standard adhesively-bonded ferrous-cobalt magnetostrictive strip solution. Cold-spray is a coating process where 10 –100 micron diameter powdered metal is accelerated to Mach 2 to Mach 3 (2–3 × speed of sound) and impacted on the surface to be coated. Each powder particle forms a kinetic bond with the substrate or other coating particles to produce a metallurgically bonded layer. If the powder is nickel or cobalt with high magnetostrictive coefficients, this surface can serve as the base of a magnetostrictive sensor suitable for crack or pitting-damage inspection and monitoring that is not subject to temporal or environmental degradation.

47 OTHER INSTRUMENTATION↗

Hanford double-shell tank ultrasonic test examinations - 15287

Washington River Protection Solutions, LLC (WRPS) under contact from the US DOE is responsible for assessing the condition of the double-shell tanks (DSTs) of the Hanford Nuclear Site. WRPS contracted AVERA Federal Services, LLC to perform the ultrasonic testing inspections of the primary tank wall in 28 DSTs to access the condition of the tanks, judge the effects of past corrosion control practices, and satisfy a regulatory requirement to periodically (eight to ten year frequency) assess the integrity of the tanks per Brookhaven National Laboratory (BNL) guidelines for structural integrity programs for tank systems. The major requirements for the Ultrasonic Testing (UT) of each tank are to detect, characterize (identify, size and locate), and record measurements made of any wall thinning, pitting or cracks that might be present in the wall of the primary tank. The UT program examines representative areas of the primary tank and secondary liner by deploying equipment in the annulus of the tank through two 24-inch diameter risers approximately 180 deg. apart. From 1996 to 2006 the first-round of ultrasonic test inspections for all DSTs were completed utilizing a Pulse-Echo (P-Scan) system. The second round of ultrasonic test inspections have continued since 2007 and are complete for 26 of 28 tanks. The two remaining tanks will receive the second inspections during fiscal year 2015. Currently, the ultrasonic testing comparison results between the first and second rounds of inspection have identified no structural integrity concerns at action levels specified in the BNL guidelines. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗