Search NASA⌕ Search

SEARCH · Search NASA

Results for “Tensile Strain”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 505 records · Page 28

Nanomechanical testing of freestanding polymer films: in situ tensile testing and Tg measurement

Abstract A method for small-scale testing and imaging of freestanding, microtomed polymer films using a push-to-pull device is presented. Central to this method was the development of a sample preparation technique which utilized solvents at cryogenic temperatures to transfer and deposit delicate thin films onto the microfabricated push-to-pull devices. The preparation of focused ion beam (FIB)-milled tensile specimens enabled quantitative in situ TEM tensile testing, but artifacts associated with ion and electron beam irradiation motivated the development of a FIB-free specimen preparation method. The FIB-free method was enabled by the design and fabrication of oversized strain-locking push-to-pull devices. An adaptation for push-to-pull devices to be compatible with an instrumented nanoindenter expanded the testing capabilities to include in situ heating. These innovations provided quantitative mechanical testing, postmortem TEM imaging, and the ability to measure the glass transition temperature, via dynamic mechanical analysis, of freestanding polymer films. Results for each of these mentioned characterization methods are presented and discussed in terms of polymer nanomechanics. Graphic Abstract

36 MATERIALS SCIENCE↗

Micro-tensile testing of neutron-irradiated Al/Zr and Zr/U-Mo diffusion bonds

This study focuses on micro-tensile testing of neutron-irradiated Al/Zr and Zr/U-Mo diffusion bonds, which are integral to the structure and performance of nuclear fuel plates used in the fuel being developed for U.S. high-power research reactors. During fabrication, two distinct diffusion bonds occur—one at the Zr/U-10Mo interface via roll bonding, and the Zr/Al interface via hot isostatic pressing at 833 K. This work utilizes micro-tensile testing specimens approximately 7 × 7 × 18 μm 3 , which are sufficiently large to encompass the identified diffusion zones to evaluate the failure strength and identify the failure location. For the Zr/Al interface, all failures occurred in the bulk aluminum. The average yield strength, ultimate strength, and strain at failure for the two parent samples were: 125 ± 10 MPa, 139 ± 24 MPa, 156 ± 21 MPa, 185 ± 14 MPa, 37.9 ± 5.6 %, and 29.7 ± 3.4 %, respectively. For specimens across the Zr/U-Mo interface, failures occurred either in the bulk Zr or U-Mo, with no failures observed in the diffusion region. For specimens that failed in the bulk Zr the failure strength and strain for the two parent samples were 570 MPa, 710 ± 131 MPa, and 43.3 %, 27.3 ± 6.6 % respectively. The specimens that failed in the bulk U-Mo had failure strengths and strains of 596 ± 32 MPa, 548 ± 124 MPa, and 2.2 ± 1.3 %, 1.5 ± 0.6 % respectively. In conclusion, these findings support the development of accurate thermo-mechanical models for irradiated fuel performance by identifying the mechanical limits and failure locations within the bonded regions.

11 - NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

In-situ investigation of strengthening and strain hardening mechanisms of Cu-added medium-Mn steels by synchrotron-based high-energy X-ray diffraction

A novel Cu-added medium-Mn steel with a chemical composition of Fe–0.27C–9.1Mn–1.86Al–3.3Cu (wt.%) was designed and subjected to intercritical annealing (IA) temperature range from 620 °C to 680 °C for 1 h. The ultimate tensile strength (UTS) increases and the yielding strength (YS) decreases with the IA temperature increasing. The YS of 824 MPa, UTS of 1222 MPa, total elongation (TE) of 55%, and product of strength and elongation (PSE) of 67.2 GPa·% are achieved after IA at 660 °C. Transmission electron microscopy confirmed that Cu-rich nanoparticles precipitate in the ferrite. The in-situ high-energy X-ray diffraction (HE-XRD) experiments show that at the beginning of plastic deformation, both austenite and ferrite bear the applied load. The load is mainly undertaken by martensite with effective transformation-induced plasticity (TRIP) effect triggered. The YS of ferrite is significantly higher than that of austenite. The individual contribution of solid solution strengthening, grain refinement strengthening, dislocation strengthening, and precipitation strengthening in ferrite and austenite is analyzed. The discrepancy between the YS of ferrite and austenite is mainly attributed to the precipitation strengthening due to the Cu-rich nanoparticles precipitation. The moderate mechanical stability and the collaboration of TRIP and twinning-induced plasticity (TWIP) effects of austenite contributed to the enhanced strain hardening capability and resulted in large ductility.

36 MATERIALS SCIENCE↗

Effect of micron-scale manufacturing flaws on the tensile response of centimeter sized two-photon polymerization microlattices

Two-photon polymerization (TPP) is a unique fabrication technique that enables sub-micron scale resolution. Herein, we report on uniaxial tensile tests on millimeter-sized TPP log-pile structures that were fabricated using a recently developed interdigitated stitching strategy. As expected, the Young’s modulus increased with laser intensity, however elastic modulus, ultimate strength and strain-at-failure varied widely, even for nominally identical samples. Post-mortem analysis revealed a series of print defects resulting from various sources including misalignments, resin shrinkage, laser beam shadowing, and local depletion of the oxygen inhibitor. While some of the defects can be eliminated, such as misalignments due to insufficient precision of the mechanical stage, others are more intrinsic to TPP and thus more difficult to address.

36 MATERIALS SCIENCE↗

Ultra-grain refinement creates FCC pure cobalt with high strength and high ductility

Although pure cobalt is generally known to have a hexagonal close-packed (HCP) structure at room temperature, we show that its high-temperature face-centered cubic (FCC) phase can be strongly stabilized through grain refinement, resulting in FCC pure cobalt at room temperature. Ultrafine-grained (UFG) FCC cobalt exhibits a hierarchical microstructure consisting of dense stacking fault (SF) networks in the dominant FCC grains and numerous SFs and thin FCC layers within a few HCP plates. This unique microstructure leads to a high tensile strength exceeding 1 GPa, together with a tensile elongation of over 35%, thereby surpassing the well-known strength–ductility trade-off of pure metals. In-situ synchrotron X-ray diffraction revealed that the UFG FCC cobalt exhibited a markedly enhanced deformation-induced FCC→HCP martensitic transformation, which provided sustained strain hardening through the transformation-induced plasticity (TRIP) effect. Furthermore, ultra-grain refinement dramatically suppressed premature void and crack formation, causing a transition in the fracture mode from brittle to ductile. These findings advance the fundamental understanding of the phase stability and TRIP-assisted deformation in elemental cobalt and offer new guidelines for the microstructure-driven design of high-performance cobalt-based structural alloys.

Metastability↗

The influence of thermomechanical treatment pathways on texture and mechanical properties in ARB Cu/Nb nanolaminates

Accumulative roll-bonded Cu/Nb nanolaminates (ARB Cu/Nb) possess high strength, thermal stability, and radiation tolerance arising from a high content of heterophase interfaces at fine layer thicknesses. These properties can be tailored by processing parameters used in the ARB Cu/Nb fabrication process, in which layer thickness, thermal history, and strain pathway determine the interface types and resultant properties found in the material. In this work, we subject ARB Cu/Nb to annealing, and then two different rolling pathways – one where rolling direction is held constant (longitudinal rolling, or LR), and one where rolling direction is rotated by 90º and held constant thereafter (cross rolling, or CR). Rolling is performed on ARB Cu/Nb over a targeted range of layer thicknesses from 193 to 25 nm and resultant bulk textures measured by neutron diffraction are correlated with mechanical properties measured by miniaturized tensile tests. The annealing procedure sharpens texture in both phases. We find that Cu mostly develops the same texture in LR and CR. In contrast, Nb develops a distinct texture along the CR pathway that is distinct from the LR texture. The composite texture of Cu/Nb is thus distinct between LR and CR pathways. This difference in texture development between Cu and Nb as a function of strain after change in rolling direction demonstrates the viability for deliberate pairing of Cu LR and Nb CR textures at a desired layer thickness. For mechanical properties, we find that differences in texture do not result in yield or flow stress differences above a layer thickness of 25 nm. Below a layer thickness of 25 nm, despite similar Taylor factors, yield and flow stress and are significantly different. In conclusion, this indicates texture only influences mechanical behavior at low layer thickness, where interface structure dominates mechanical properties.

36 MATERIALS SCIENCE↗

On the Mechanical Behavior of LP-DED C103 Thin-Wall Structures

Laser Powder Directed Energy Deposition (LP-DED) can produce thin-wall features on the order of 1 mm. These features are essential for large structures operating in extreme environments such as regeneratively cooled nozzles and heat exchangers, which often make use of refractory metals. In this work, the mechanical behavior of LP-DED C103 was investigated via quasi-static tensile testing and low cycle fatigue (LCF) testing. The effects of vacuum stress relief (SR) and hot isostatic pressing (HIP) heat treatments were investigated for specimens in the vertical and horizontal build orientations during tensile testing. The AB and SR properties were lower than literature values for wrought and laser powder bed fusion (L-PBF) bulk components but higher than electron beam powder bed fusion (EB-PBF). The application of a HIP cycle improved strength by 7% and ductility by 27% past the initial as-built condition. Fracture images reveal that interlayer stress concentration sites are responsible for fracture in specimens in the vertical orientation. Meanwhile, fracture in the horizontal specimens mainly propagates at a slanted angle typical of plane stress conditions. The LCF results show cycles to failure ranging from 100 cycles to 8000 cycles for max strain levels of 2% and 0.5%, respectively. Fractography on the fatigue specimens reveals an increasing propagation zone as max strain levels are increased. The impact of these findings and future work are discussed in detail.

36 MATERIALS SCIENCE↗

Experimental methodology and theoretical framework in describing constrained plastic flow of FCC microscale tensile specimens

Small scale mechanical testing (SSMT) allows for the quantification of the mechanical responses for microscale and nanoscale material volumes. It has significant potential in improving our fundamental understanding of plastic deformation and in providing an engineering solution for testing complex and/or critical materials. Importantly, previous studies have revealed that plastic intermittency, manifested as strain bursts, are characteristic of the plastic flow behavior at the small length scale. In this work, interfacial constraint has been utilized to suppress strain bursts in order to stabilize plasticity. A new parameter, blocked volume ratio (BVR), is introduced to quantify the degree of constraint for a microscale specimen due to an interface. Here, we showed that the plastic flow behavior in FCC Ni-based metals is highly dependent on the BVR of the specimen.

36 MATERIALS SCIENCE↗

Achieving superior mechanical properties: Tailoring multicomponent microstructure in AISI 9254 spring steel through a two-stage Q&P process and nanoscale carbide integration

In the pursuit of lightweight, durable steel, we have successfully developed a multicomponent structure in AISI 9254 spring steel using a two-stage quenching and partitioning (Q&P) process. The primary objective of this process was to engineer an optimized microstructure consisting of nanobainite, martensite, and nano-carbides. Utilizing the insights gained from the results of advanced techniques such as X-ray diffraction (XRD), scanning electron microscopy (SEM), transmission electron microscopy (TEM), and atom probe tomography (APT) performed on the as-received AISI 9254 spring steel, we refined the quenching and partitioning (Q&P) path, leading to the successful establishment of a bainitic transformation for superior mechanical properties. Our tensile tests revealed a high yield strength (≈ 1600 ± 25 MPa) and ultimate tensile strength (≈ 1850 ± 50 MPa), along with considerable elongation (≈ 11.15 ± 0.25%). We also identified that pre-formed martensite lath defects and high silicon content play crucial roles during the Q&P process, preventing carbide coalescence and increasing strain-hardening capacity. Finally, this study demonstrates the potential of a Q&P process to generate high-strength, ductile steel for automotive and aerospace applications.

36 MATERIALS SCIENCE↗

Amorphous complexions alter the tensile failure of nanocrystalline Cu-Zr alloys

Grain boundary-based mechanisms are known to control the plastic deformation and failure of nanocrystalline metals, with manipulation of the boundary structure a promising path for tuning this response. In this study, the role of interfacial structural disorder on plasticity and failure of nanocrystalline Cu-Zr alloys is investigated with in situ scanning electron microscopy tensile deformation experiments. Two model materials are created, one with only the typical ordered grain boundaries and another with amorphous intergranular films interspersed into the boundary network, while the microstructures are otherwise identical. Hence, the importance of complexion type on plasticity and failure is isolated by only varying complexion structure. Here, the tensile experiments show that failure of the samples containing amorphous films is significantly retarded, as evidenced by an increase in the cross-sectional area reduction, a decrease in the occurrence of shear-dominated failure, a decrease in strain localization, and fracture surfaces with more elongated dimple features. As a whole, this study provides direct evidence that structural disorder at the grain boundaries can be beneficial for improving the ductility of nanocrystalline metals.

36 MATERIALS SCIENCE↗

Ribbon Wrinkling Origin and Its Effect on Tape-Wound Core Shape

Improved understanding of advanced manufacturing techniques is needed to fabricate next- generation soft magnetic tape-wound cores. These utilize metal amorphous nano-composites (MANCs) in the form of long thin ribbons. MANCs exhibit attractive soft magnetic properties for use in high frequency and high power density magnetic components. Of particular interest here, the permeability and hysteresis of MANC ribbons can be tuned in a strain annealing process. An unexpected consequence is that wider ribbons develop longitudinal wrinkle patterns. This can substantially reduce the tape-wound core stacking factor. However, when winding a wrinkled ribbon into a toroidal core, the wrinkles can completely flatten, or crinkle. By this phenomenon, the stacking factor can be recovered. To understand the crinkling effect we have developed analytical and finite element analysis (FEA) models. Experiments with known boundary conditions demonstrate the transition from wrinkled to crinkled versus winding curvature. The models utilize an elastic modulus measured via ribbon tensile testing and a ribbon thickness value measurement made by profilometry. The analytical model provides insight into the crinkling effect but cannot explain the length of the transition region from wrinkling to crinkling. With FEA, we successfully predict the transition region and depending on wrinkling amplitude can determine when a ribbon will wind into a useable core. Such mechanics-based insight provides critical feedback for allowable processing parameters in the strain annealing process.

20 FOSSIL-FUELED POWER PLANTS↗

Origin, parameters, and underlying deformation mechanisms of propagating deformation bands in irradiated 316L stainless steel

Lüders-type propagating deformation bands were observed in specimens of irradiated 316L stainless steel samples removed from Spallation Neutron Source target vessels after service. Mechanical testing with digital image correlation (DIC) and in-situ tensile testing with scanning electron microscopy electron backscatter diffraction showed that the observed Lüders-type behavior was not related to the known transformation-induced plasticity or twinning-induced plasticity behavior. Instead, the phenomenon occurs at small local strain values before a significant amount of martensite or deformation twins appear in the microstructure. Microstructural analysis and in-situ mechanical test results suggest Lüders-type band formation and propagation were related to the appearance and evolution of defect-free channels—analogous to slip bands. A modified Swift equation with a Ludwigson-like component was offered to rationalize the phenomenon and model the strain-softening processes at small strain values. Finally, the results indicate complex microstructural processes and deformation mechanisms were active at small strain values and underline the benefits of advanced mechanical test approaches such as DIC.

36 MATERIALS SCIENCE↗

Residual elastic strain evolution due to thermal cycling of a ceramic-metal composite (WC-Cu) via high energy X-ray diffraction and analytical modeling

Residual stress, when superimposed with in-service loading, can significantly reduce the lifetime and performance of a component. Ceramic-metal composites are susceptible to residual stresses due to the thermal expansion mismatch of the ceramic and metallic phases. The WC-Cu composite explored in the present study provides a promising combination of thermal conductivity and strength properties, while exhibiting counterintuitive improvements in strength and ductility after thermal cycling. Further, this work quantifies the evolution of the residual elastic strains as a result of processing and cyclic thermal loading in a co-continuous WC-Cu composite through experimental high energy X-ray diffraction and kinetics-based modeling. Both analyses indicate that processing-induced residual tensile stress in the copper phase is relieved upon subsequent thermal cycling, with kinetics modeling revealing the cyclic-dependent nature of the active power-law creep mechanisms. The results indicate that, through stress relaxation, this material system maintains structural stability during thermal cycling. The illustrated kinetics of relaxation can inform general material processors and designers of ceramic-metal composites to minimize detrimental residual stress and improve performance of these material systems.

36 MATERIALS SCIENCE↗

On the exceptionally high ductility of Mg–2Zn-0.3Ca-0.2Ce-0.1Mn alloy

A newly developed Mg–2Zn-0.3Ca-0.2Ce-0.1Mn (in weight %, ZXEM2000) wrought alloy exhibits an exceptionally high tensile ductility (29% ± 1.4% tensile elongation) along the rolling direction at room temperature. In this work, we investigated the fundamental plastic deformation mechanisms that can contribute to the high ductility of ZXEM2000. Scanning electron microscopy and transmission electron microscopy were carried out at selected strain levels to characterize the microstructural evolution. Compared with the deformed microstructures from the hot-rolled pure Mg and Mg–3Al–1Zn alloy at similar conditions, our results revealed that the high ductility of ZXEM2000 could be attributed to four key factors: weaker texture, fine grain size, reduced twinning, and increased cross-slip frequency of < c +a > dislocation. Furthermore, these direct observations offer a key insight into improving ductility of magnesium alloys for future alloy design and development.

36 MATERIALS SCIENCE↗

Plasticity in irradiated FeCrAl nanopillars investigated using discrete dislocation dynamics

Here, in this paper, we investigate plasticity in irradiated FeCrAl nanopillars using discrete dislocation dynamics simulations (DDD), with comparisons to transmission electron microscopic (TEM) in situ tensile tests of ion- and neutron-irradiated commercial C35M FeCrAl alloy. The effects of irradiation-induced defects, such as a/2<111> and a<100> type loops and composition fluctuations representative of phase separation in irradiated FeCrAl alloys, are investigated separately as well as superposed together in simulations. We explore the effects of defects on the stress-strain behavior, specifically yield strength and hardening response, of FeCrAl nanopillars. Our simulations confirm the widely accepted fact that irradiated alloys exhibit a stress-strain response with higher yield strength as compared to unirradiated alloys. However, our DDD calculations reveal an atypical superposition of the hardening contributions due to composition inhomogeneity and irradiation loops wherein composition inhomogeneity annihilates the hardening due to irradiation loops at small scales. As a result, we observe that the yield strength in irradiated alloys, after taking into consideration the effects of both composition inhomogeneity and irradiation loops, is smaller than the yield strength of the alloys with only irradiation loops and is approximately same for the alloy with composition inhomogeneity alone. This is referred to as “destructive interference” between the hardening contributions due to composition fluctuations and irradiation loops in the paper. We also identify this destructive interference in the superposition in our parallel TEM in situ tensile tests on unirradiated, ion-irradiated, and neutron-irradiated C35M FeCrAl alloy. This destructive interference in the hardening contributions contrasts with the dispersed barrier hardening (DBH) models widely utilized by the experimental community to model the hardening contributions due to different irradiation induced defects. The effects of the loading orientations on the yield strength and hardening are investigated and the mechanisms for the hardening in irradiated FeCrAl alloys are also reported.

36 MATERIALS SCIENCE↗

Plastic homogeneity in nanoscale heterostructured binary and multicomponent metallic eutectics: An overview

Heterostructured materials comprised of relatively soft/hard disparate phases typically exhibit composite strengthening but lack plastic deformability at ambient temperatures. However, heterostructured systems comprised of nanoscale phases can simultaneously enhance yield strength and strain hardening, thereby promoting uniform distribution of plastic flow. In this review, the atomic-scale deformation mechanisms in model systems of eutectic alloys, Al-Al 2 Cu and Al-Si, refined to nanoscales via laser rapid solidification are discussed, and compared with literature on multi-component (high entropy) eutectics such as Ni-Al-Fe-based with Cr and/or Co additions. The nano-lamellar Al-Al 2 Cu structures exhibit unit defect mechanisms not reported in monolithic Al 2 Cu intermetallic: localized shear on {0 1 1} and shear-induced faults on {1 2 1} planes, constrained by closely-spaced dislocation arrays in Al confined by Al/Al 2 Cu interfaces. The unexpected plasticity mechanisms are enabled by slip continuity in nanoscale Al-Al 2 Cu eutectics associated with the orientation relationship and interface habit planes. In nano-fibrous Al-Si eutectic, tensile ductility at strength approaching 600 MPa is observed resulting from dislocation plasticity in the nano-Al channels and cracking in Si nanofibers. Molecular dynamics simulations show that Al dislocations easily cross-slip (screw) or climb (edge) along Al-Si interfaces, making slip transmission difficult. The propagation of nano-cracks is suppressed by surrounding strain hardening Al, retaining good ductility of the sample, in spite of lack of direct slip transmission. Finally, the critical unit mechanisms of slip transmission and interface-enabled plasticity observed in nanoscale eutectic binary systems can also explain the strength-ductility relationship in multi-component eutectics and homogeneously distributed plastic flow with increasing microstructural heterogeneity.

36 MATERIALS SCIENCE↗

Performance of hybrid Innegra-carbon fiber composites

Abstract In this work material synergy with high stiffness carbon fiber with ductile high strength polypropylene fiber (Innegra S), (referred to as Innegra, herein) have been evaluated in a range of laminate designs. Both woven and discontinuous carbon fiber have been considered. The discontinuous fibers are based on three-dimensional deposition (3DEP) (referred to as 3DEP, herein) carbon fiber preform process. Eleven (11) variants of Innegra-carbon fiber hybrid laminates were investigated for tensile, flexure, compression, in-plane shear and low velocity impact response. The effect of position of Innegra within the laminate was studied and found to influence strength and stiffness properties. In terms of overall trends, Innegra provides upward of 18% improvement in strain (ductility) to the composite and eliminates brittle fracture of carbon fiber. The moduli trends follow the proportionality of Innegra fiber to carbon fiber plies. However, the strength is controlled by the interface between Innegra and carbon fiber. The primary failure mode in tension and compression is via onset of debonding between Innegra and carbon fiber. The 3DEP carbon fiber constituents provided highest values of in-plane shear indicating that three-dimensional (3D) network of carbon fiber provides higher shear resistance. The Innegra intensive variants exhibited superior energy absorption under low velocity impact, at energy levels 15–60 J. This work provides insight for designers to incorporate Innegra and carbon fiber hybrids in composite structures.

36 MATERIALS SCIENCE↗