Thermal annealing induced structural and optical properties of Se{sub 72}Te{sub 25}In{sub 3} thin films
Thin films of a- Se{sub 72}Te{sub 25}In{sub 3} were prepared by vacuum evaporation technique in a base pressure of 10{sup -6} Torr on to well cleaned glass substrate. a-Se{sub 72}Te{sub 25}In{sub 3} thin films were annealed at different temperatures below their crystallization temperatures for 2h. The structural analysis of the films has been investigated using X-ray diffraction technique. The optical absorption spectra of these films were measured in the wavelength range 400-1100 nm in order to derive the absorption coefficient of these films. The optical band gap of as prepared and annealed films as a function of photon energy has been studied. It has been found that the optical band gap decreases with increasing annealing temperatures in the present system.