Search NASA⌕ Search

SEARCH · Search NASA

Results for “Light Emitting Diode”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 523 records · Page 29

Effect of molecular permanent dipole moment on guest aggregation and exciton quenching in phosphorescent organic light emitting diodes

This study explores the effect of molecular permanent dipole moment (PDM) on aggregation of guest molecules in phosphorescent host–guest organic light-emitting diodes (OLEDs). Through a combination of photoluminescence measurements, high-angle annular dark-field scanning transmission electron microscopy analysis, and an Ising model based physical vapor-deposition simulation, we show that higher PDM of tris[2-phenylpyridinato-C2,N]iridium(III) guest can actually lead to a reduced aggregation relative to tris[bis[2-(2-pyridinyl-N)phenyl-C] (acetylacetonato)iridium(III) when doped into a non-polar host 1,3,5-tris(carbazol-9-yl)benzene. This study further explores the effect of host polarity by using a polar host 3′,5′-di(carbazol-9-yl)-[1,1′-biphenyl]-3,5-dicarbonitrile, and it is shown that the polar host leads to reduced guest aggregation. In conclusion, this study provides a comprehensive understanding of the impact of molecular PDM on OLED material efficiency and stability, providing insights for optimizing phosphorescent OLED materials.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Quantitative analysis of leakage current in III-nitride micro-light-emitting diodes

In this study, the electrical characteristics under forward- and reverse-bias conditions of III-nitride blue and green micro-light-emitting diodes (μLEDs) are analyzed. A fitting model is proposed to determine the contributions of reverse leakage current and the effectiveness of sidewall treatments. Moreover, the forward-bias currents of the μLEDs are examined using the extracted ideality factor to examine the impacts of sidewall defects. The results show that sidewall treatments are highly effective for suppression of leakage currents. From the efficiency perspective, higher wall-plug efficiency (WPE) than external quantum efficiency (EQE) is observed when the operating voltage is lower than the photon voltage in both blue and green 20 × 20 μm 2 devices. This enhancement of the WPE over the EQE is due to the suppression of Shockley–Read–Hall (SRH) nonradiative recombination. These observations indicate that μLEDs with sidewall treatments not only improve optical performance but also further enhance the electrical performance of devices by suppressing the leakage current paths due to SRH nonradiative recombination processes.

42 ENGINEERING↗

Cavity Light-Emitting Diode for Durable, High-Brightness and High-Efficiency Lighting Applications: First Budget Period Technical Report

A COLED device consists of a top electrode (anode) and a bottom electrode (cathode) separated by a thin dielectric layer. In this metal/dielectric stack, numerous small wells, or cavities, are etched through the top electrode and the dielectric layer. These cavities are subsequently filled with LEP molecules. When a voltage is applied between the top and bottom electrodes, holes (from the top electrode) and electrons (from the bottom electrode) are injected into the polymer. Light emission is generated upon recombination of holes and electrons within the polymer along the perimeters of cavities. Figure 1 compares the structures of the COLED and the traditional OLED. The existing COLED fabrication process flow is illustrated in Figure 2. A COLED can potentially be 5 times more efficient and can operate at as much as 100 times higher current density with much longer lifetime than an OLED. To fully realize these potential advantages, the COLED technology must overcome the following technical barriers, which were the technical focused points for Years 1 and 2 (Phase I) of this project: (1) Construct optimum thickness dielectric layer: In the traditional OLED structure, the optimal thickness of the LEP film is approximately 80-100 nm. In a COLED device, the effective LEP thickness roughly equals the thickness of the dielectric layer. Therefore, the optimal dielectric thickness for a COLED should also be roughly equal to 80-100 nm. Generally speaking, it is technically challenging to produce a defect-free dielectric layer at this thickness with high uniformity, especially over a large area. (2) Develop low-work-function cathode: A desired cathode should have a low work function that matches the lowest unoccupied molecular orbital (LUMO) level of the LEP molecules. This is usually achieved by using a low-work-function metal such as calcium, barium, lithium, or magnesium as the cathode. However, these metals are very vulnerable to oxygen and water. Since the cathode of the COLED will be exposed to air and processing chemicals during the COLED fabrication process, these low-work-function metals cannot be used directly in the COLED structure. Thus, new materials with low work function and better chemical stability are needed for the COLED cathode. (3) Increase active device area: Since photons are only generated from perimeters of the cavities, the actual active area in a COLED device is smaller than the device surface area. The cavity diameter and cavity spacing of the COLED devices previously produced at SRI by conventional photolithography processing are typically in the range of 3 to 7 μm with an estimated active area of 2-3%. To achieve the same brightness of a traditional OLED at the same applied voltage, the active device area of a COLED should be at least 20% (1/5) of the device surface area, provided the COLED has 5 times higher EQE. This requires reducing the cavity diameter and cavity spacing to the sub-micrometer region, which can be achieved by electron-beam lithography or nanoimprint lithography. (4) Improve metal/polymer interfaces: The polymer/metal interfaces are critical issues to improve and optimize since they directly affect the effectiveness and balance of hole and electron injection, and consequently the device performance. Conventional approaches for improving a metal/polymer interface include deposition of a special interfacial material on the selected electrode surface or applying a proper surface treatment prior to deposition of the LEP. Since these approaches are generally nonselective to the cathode and anode, they cannot be directly adopted for COLED devices. Generally, the interface integration in current OLED technology still needs a better chemical approach. Hence, advanced methodology developed for the COLED technology as promoted in this project may be also suitable for other OLED devices.

36 MATERIALS SCIENCE↗

Photoluminescent and thermal properties of (Sr{sub 0.995−x−y−z}Ca{sub x}Ba{sub y}Mg{sub z}){sub 2}SiO{sub 4}:0.01Eu{sup 2+} phosphors for warm white light-emitting diodes

Highlights: • The photoluminescent property of Sr{sub 2}SiO{sub 4}:Eu{sup 2+} is improved by doping Ca{sup 2+} and Ba{sup 2+}. • The emission spectra red-shift obviously by doping Ca{sup 2+} into Sr{sub 2}SiO{sub 4}:Eu{sup 2+}. • The thermal stability is enhanced by doping Ba{sup 2+} into (Sr,Ca){sub 2}SiO{sub 4}:Eu{sup 2+}. • The improved phosphors can combine blue-LED chips to generate warm white light. - Abstract: A series of phosphors (Sr{sub 0.995−x−y−z}Ca{sub x}Ba{sub y}Mg{sub z}){sub 2}SiO{sub 4}:0.01Eu{sup 2+} (0 ≤ x ≤ 0.45, 0 ≤ y ≤ 0.015, 0 ≤ z ≤ 0.35) were synthesized by solid state reaction. Their phase compositions and photoluminescent properties were investigated in detail. The X-ray diffraction analysis indicates the impurity phase of SrSiO{sub 3} is formed only when z ≥ 0.25. A photoluminescence investigation shows, with x increasing the emission spectra of the phosphors (0 ≤ x ≤ 0.45, 0 ≤ y ≤ 0.015, z = 0) obviously red-shift, the corresponding color tones shift from yellow to orange–yellow and their CCTs reduce from 2875 to 2237 K. All the results are beneficial for the phosphors to combining blue light-emitting diode chips to generate warm white light. Besides, the thermal stability of the phosphor (x = 0.36, y = z = 0) is enhanced by doping Ba{sup 2+}, due to the greater activation energy for the compounds containing barium.

36 MATERIALS SCIENCE↗

Indium tin oxide modified transparent nanotube thin films as effective anodes for flexible organic light-emitting diodes

Sn-doped In{sub 2}O{sub 3} (ITO) modified single-walled carbon nanotube (SW-CNT) transparent electrodes are fabricated on flexible polyethyleneterephthalate (PET) substrates by stamp printing SW-CNT films, followed by room temperature ion-assisted deposition of ITO. Polymer light-emitting diodes (PLEDs) using such film as anodes exhibit superior performance versus CNT-only controls. Flexible PLEDs with the following structure: PET/CNT(30 nm)-ITO(45 nm)/poly (3,4-ethylenedioxythiophene) poly (styrenesulfonate)/[poly(9,9-dioctyl-fluorene-co-N- (4-butylphenyl)diphenylamine)]+(4,4{sup '}-bis[(p-trichlorosilyl propylphenyl)-phenylamino]biphenyl)/[poly (9,9-dioctylfluorene-co-benzothiadiazole)]/CsF/Al, achieve a maximum light output of 8900 cd/m{sup 2} with a current efficiency of 4.5 cd/A. Bending test comparisons with ITO/PET show the ITO modified CNT/PET electrodes to be far more mechanically flexible.

36 MATERIALS SCIENCE↗

High-power low-droop violet semipolar (303{sup ¯}1{sup ¯}) InGaN/GaN light-emitting diodes with thick active layer design

Devices grown on nonpolar and semipolar planes of GaN offer key performance advantages over devices grown on the conventional c-plane, including reduced polarization fields. This allows for a wider design space on semipolar planes for light emitting diodes (LEDs) to address the problem of efficiency droop at high current densities. LED structures with very thick (10–100 nm) InGaN single-quantum-well/double heterostructure active regions were grown using conventional metal organic chemical vapor deposition on semipolar (303{sup ¯}1{sup ¯}) free-standing GaN substrates and processed and packaged using conventional techniques. Simulated band diagrams showed reduced polarization fields on the (303{sup ¯}1{sup ¯}) plane. The calculated critical thickness for misfit dislocation formation is higher on the (303{sup ¯}1{sup ¯}) plane than on other semipolar planes, such as (202{sup ¯}1{sup ¯}), allowing for thicker active regions than our previous work to further reduce droop. The higher critical thickness was confirmed with defect characterization via cathodoluminescence. A trend is demonstrated in lower efficiency droop for devices with thicker active regions. Thermal droop characteristics of these devices are also presented. These observed results were utilized to demonstrate over 1 W of output power at a current density of 1 kA/cm{sup 2} from a single 0.1 mm{sup 2} LED device.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Thermal Inspection of Low Emissivity Surfaces Using a Pulsed Light Emitting Diodes (PLED) Heat Source

Thermal inspections of a structure typically utilize a flash or quartz lamp heat source located on the same side of an infrared camera. The heat source provides light energy for heating while the infrared camera measures the surface transient temperature response. The inspection can be difficult for low emissivity surfaces for several reasons. First, the high intensity light can reflect off the surface and cause “burn-in” to the camera’s detector. The “burn-in” can take time for the sensors to recover and potentially damage the detector. Secondly, the heat source after pulsing, has a transient cool down component. The cool down component can be reflected and therefore superimposed over the structure’s thermal response which can cause an error (false defect indications) in the inspection. Lastly, the heat source is spectrally broad and therefore while heating, infrared components of the heat source can produce non-uniformity in the measured temperature field. Typically for the inspection of reflective surfaces, paint or other emissivity enhancing coatings are applied before inspection. In this paper, a pulsed light emitting diodes (PLED) heat source is used. The PLED heat source is spectrally narrow, contained within the visible band, and therefore not detectable by the infrared camera. The PLED heat source is configured to reduce any transient cool down components that could produce false defect indications. The PLED thermal inspections are compared to commercially available flash thermography inspections on unpainted aluminum samples with simulated corrosion and additively manufactured Ti-6AL-4V metal specimens.

thermal nondestructive evaluation↗

Thermal Inspection of Low Emissivity Surfaces Using a Pulsed Light Emitting Diodes (PLED) Heat Source

Thermal inspections of a structure typically utilize a flash or quartz lamp heat source located on the same side of an infrared camera. The heat source provides light energy for heating while the infrared camera measures the surface transient temperature response. The inspection can be difficult for low emissivity surfaces for several reasons. First, the high intensity light can reflect off the surface and cause “burn-in” to the camera’s detector. The “burn-in” can take time for the sensors to recover and potentially damage the detector. Secondly, the heat source after pulsing, has a transient cool down component. The cool down component can be reflected and therefore superimposed over the structure’s thermal response which can cause an error (false defect indications) in the inspection. Lastly, the heat source is spectrally broad and therefore while heating, infrared components of the heat source can produce non-uniformity in the measured temperature field. Typically for the inspection of reflective surfaces, paint or other emissivity enhancing coatings are applied before inspection. In this paper, a pulsed light emitting diodes (PLED) heat source is used. The PLED heat source is spectrally narrow, contained within the visible band, and therefore not detectable by the infrared camera. The PLED heat source is configured to reduce any transient cool down components that could produce false defect indications. The PLED thermal inspections are compared to commercially available flash thermography inspections on unpainted aluminum samples with simulated corrosion and additively manufactured Ti-6AL-4V metal specimens.

thermal nondestructive evaluation↗

Changes in the performance characteristics of a GaAs near infrared light emitting diode when exposed to various current and thermal stresses

The changes that occurred in the optical and electrical characteristics of a near infrared, GaAs light emitting diode, when operated under various levels and combinations of current and thermal stresses are discussed. A total of forty parts were operated for two thousand hours under eight different sets of dc current and ambient temperature conditions. Degradation in the radiant optical power of these devices was thirty-four percent when operated at their rated current and an ambient temperature of 298K (25 C). Derating the current and/or the thermal stress reduced the degradation of this parameter in approximately a linear manner. All degraded devices behaved similarly, exhibiting rapid nonlinear degradation followed by a gradual linear degradation and finally a period of stable operation. An attempt was made to correlate initial device condition to degradation during stress testing, but met with little success.

Thomas, E. F., Jr.↗

Amber light-emitting diode comprising a group III-nitride nanowire active region

A temperature stable (color and efficiency) III-nitride based amber (585 nm) light-emitting diode is based on a novel hybrid nanowire-planar structure. The arrays of GaN nanowires enable radial InGaN/GaN quantum well LED structures with high indium content and high material quality. The high efficiency and temperature stable direct yellow and red phosphor-free emitters enable high efficiency white LEDs based on the RGYB color-mixing approach.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Enhancement of electrical property by oxygen doping to copper phthalocyanine in inverted top emitting organic light emitting diodes

We reported the evidence of oxygen doping to copper-phthalocyanine (CuPc) by O{sub 2}-plasma treatment to inverted top-emitting organic light-emitting diodes (ITOLEDs). In situ synchrotron-radiation photoelectron spectroscopy results showed that a new Cu-O bond appeared and the energy difference between the highest-occupied molecular orbital and E{sub F} is lowered by 0.15 eV after plasma treatment. The oxygen ions chemically interacted with Cu atoms and transferred charges to the CuPc. Thus the hole injection barrier was lowered, enhancing the electroluminescent property of ITOLEDs.

36 MATERIALS SCIENCE↗

Effects of Mg-doped AlN/AlGaN superlattices on properties of p-GaN contact layer and performance of deep ultraviolet light emitting diodes

Mg-doped AlN/AlGaN superlattice (Mg-SL) and Mg-doped AlGaN epilayers have been investigated in the 284 nm deep ultraviolet (DUV) light emitting diodes (LEDs) as electron blocking layers. It was found that the use of Mg-SL improved the material quality of the p-GaN contact layer, as evidenced in the decreased density of surface pits and improved surface morphology and crystalline quality. The performance of the DUV LEDs fabricated using Mg-SL was significantly improved, as manifested by enhanced light intensity and output power, and reduced turn-on voltage. The improved performance is attributed to the enhanced blocking of electron overflow, and enhanced hole injection.

36 MATERIALS SCIENCE↗

Highly efficient inverted top emitting organic light emitting diodes using a transparent top electrode with color stability on viewing angle

We report a highly efficient phosphorescent green inverted top emitting organic light emitting diode with excellent color stability by using the 1,4,5,8,9,11-hexaazatriphenylene-hexacarbonitrile/indium zinc oxide top electrode and bis(2-phenylpyridine)iridium(III) acetylacetonate as the emitter in an exciplex forming co-host system. The device shows a high external quantum efficiency of 23.4% at 1000 cd/m{sup 2} corresponding to a current efficiency of 110 cd/A, low efficiency roll-off with 21% at 10 000 cd/m{sup 2} and low turn on voltage of 2.4 V. Especially, the device showed very small color change with the variation of Δx = 0.02, Δy = 0.02 in the CIE 1931 coordinates as the viewing angle changes from 0° to 60°. The performance of the device is superior to that of the metal/metal cavity structured device.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Control of circular polarization of electroluminescence in spin light-emitting diodes based on InGaAs/GaAs/δ〈Mn〉 heterostructures

Circularly polarized luminescence of light-emitting InGaAs/GaAs structures with a delta-doped Mn layer in a GaAs barrier was studied. The structural parameters were varied by different ways, among them are homogeneous and delta-doping with acceptor impurity, and removal of donor doping from the technological process. As it was found, the magnitude and polarity of the degree of circular polarization of luminescence strongly depend on the technological mode chosen. Simultaneous modeling of wave functions of structures highlights a good agreement between the parameters of circularly polarized luminescence and spatial distribution of wave functions of heavy holes relative to the Mn delta-layer.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Unexpected origin of the quantum efficiency reduction in long-wavelength (In,Ga)⁢N light-emitting diodes

Differential carrier lifetime (DCL) measurements were performed on c-plane In 𝑥 ⁢Ga 1−𝑥⁢ N/Ga⁢N single-quantum-well (QW) light-emitting diodes (LEDs) with varying indium-content QWs (x = 13.5%, 16%, 22%), emitting with violet, blue, and green wavelengths. The recombination lifetimes of LEDs were found to increase with increasing indium composition, resulting in increased carrier densities n measured by DCL. Extraction of the A coefficients, which are assumed to not vary with n, and of the effective B(n) and C(n) coefficients of the ABC model of the internal quantum efficiency (IQE) of QWs showed no significant changes in the A coefficient with increasing indium content [In] in the In 𝑥 ⁢Ga 1−𝑥 ⁢N QW, and a reduction in the B(n) and C(n) coefficients with increasing [In]. When looking at the Shockley-Read-Hall (SRH) recombination rate An, the radiative recombination rate B(n)𝑛 2 , and the Auger-Meitner (AM) recombination rate C(n)𝑛 3 , we observed that at any given n, the SRH rate is the same for the three [In] measured, while the radiative rate decreases (by up to approximately 9 times) and the AM rate decreases (by up to approximately 7 times) with increasing indium content. This shows that the larger reduction in radiative recombination rates relative to nonradiative recombination rates with increasing [In] is the largest contributor to the decreased quantum efficiencies of LEDs (the “green gap”) at any given n. While some of the reduction in the effective recombination coefficients B(n) and C(n) can be explained by the reduced wave-function overlaps of the QW with increasing indium content, the larger reduction of B(n) relative to C(n) motivates further study of the intrinsic recombination coefficients 𝐵 0 and 𝐶 0 of bulk In 𝑥 ⁢Ga 1−𝑥 ⁢N alloys and how they are related to the effective recombination coefficients B(n) and C(n) in QWs. The relative contributions of nonradiative recombination are enhanced at any given current density due to the sublinear relationship between the carrier density n and the current density. Thus, the solution to the green gap, up to any intrinsic limitations set by the indium content of the QW, from an IQE perspective, requires the design of long-wavelength (In,Ga)⁢N LEDs with improved wave-function overlaps that can operate with a lower carrier density at any given current density.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Al(0.3)Ga(0.7)As / Al(0.05)Ga(0.95)As light-emitting diodes on GaAs-coated Si substrates grown by liquid phase epitaxy

Al(0.3)Ga(0.7)As/Al(0.05)Ga(0.95)As double-heterostructure light-emitting diodes (LEDs) were successfully grown for the first time by liquid phase epitaxy on a GaAs-coated Si substrate that was prepared by a sequential process of migration-enhanced epitaxy and molecular beam epitaxy. The edge-emitting LEDs had diode ideality factors of 1.54 at a forward-biased voltage higher than 0.9 V and external quantum efficiencies of 0.0033 W/A per facet. This efficiency is 50 times higher than the previously reported value, and is on the same order as that of AlGaAs homojunction LEDs fabricated on the GaAs substrates by liquid phase epitaxy.

Sakai, Shiro↗

Anomalous hole injection deterioration of organic light-emitting diodes with a manganese phthalocyanine layer

Metal phthalocyanines (MPcs) are well known as an efficient hole injection layer (HIL) in organic devices. They possess a low ionization energy, and so the low-lying highest occupied molecular orbital (HOMO) gives a small hole injection barrier from an anode in organic light-emitting diodes. However, in this study, we show that the hole injection characteristics of MPc are not only determined by the HOMO position but also significantly affected by the wave function distribution of the HOMO. We show that even with the HOMO level of a manganese phthalocyanine (MnPc) HIL located between the Fermi level of an indium tin oxide anode and the HOMO level of a N,N′-bis(1-naphthyl)-N,N′-diphenyl-1,1′-biphenyl-4,4′-diamine hole transport layer the device performance with the MnPc HIL is rather deteriorated. This anomalous hole injection deterioration is due to the contracted HOMO wave function, which leads to small intermolecular electronic coupling. The origin of this contraction is the significant contribution of the Mn d-orbital to the MnPc HOMO.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Phosphorescent organic light emitting diodes with high efficiency and brightness

An organic light emitting device including a) an anode; b) a cathode; and c) an emissive layer disposed between the anode and the cathode, the emissive layer comprising an organic host compound and a phosphorescent compound exhibiting a Stokes Shift overlap greater than 0.3 eV. The organic light emitting device may further include a hole transport layer disposed between the emissive layer and the anode; and an electron transport layer disposed between the emissive layer and the cathode. In some embodiments, the phosphorescent compound exhibits a phosphorescent lifetime of less than 10 .mu.s. In some embodiments, the concentration of the phosphorescent compound ranges from 0.5 wt. % to 10 wt. %.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗