At least 523 records · Page 29

Toward practical 3D radiography of pipeline girth welds

Digital radiography has made its way into in-the-field girth weld testing. With recent generations of detectors and x-ray tubes it is possible to reach the image quality desired in standards as well as the speed of inspection desired to be competitive with film radiography and automated ultrasonic testing. This paper will show the application of these technologies in the RTD Rayscan system. The method for achieving an image quality that complies with or even exceeds prevailing industrial standards will be presented, as well as the application on pipeline girth welds with CRA layers. A next step in development will be to also achieve a measurement of weld flaw height to allow for performing an Engineering Critical Assessment on the weld. This will allow for similar acceptance limits as currently used with Automated Ultrasonic Testing of pipeline girth welds. Although a sufficient sizing accuracy was already demonstrated and qualified in the TomoCAR system, testing in some applications is restricted to time limits. The paper will present some experiments that were performed to achieve flaw height approximation within these time limits.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Integrated modeling of cracking during deep penetration laser welding of nickel alloys

During deep penetration laser welding of nickel alloys, interactions between composition and processing conditions can lead to the formation of defects. Inconel 740H, for example, has demonstrated a susceptibility to horizontal fusion zone cracking at locations between 70% and 80% of the weld depth during laser welding at powers above 5 kW. Coupling three-dimensional heat transfer, fluid flow, and stress modeling tools allowed that both the strain rate and stress normal to the solidification direction to be calculated. In the Inconel 740H welds, cracks formed at locations where the strain rate and stress simultaneously reached critical levels. No cracking was observed in the Inconel 690 welds, since the strain rate and stress did not simultaneously reach these critical levels.

36 MATERIALS SCIENCE↗

Neutron diffraction measurements of residual stresses in friction stir welding: a review

Significant amounts of residual stresses are often generated during welding and result in critical degradation of the structural integrity and performance of components. Neutron diffraction has become a well established technique for the determination of residual stresses in welds because of the unique deep penetration, three-dimensional mapping capability, and volume averaged bulk measurements characteristic of the scattering neutron beam. Friction stir welding has gained prominence in recent years. The authors reviewed a number of neutron diffraction measurements of residual stresses in friction stir welds and highlighted examples addressing how the microstructures and residual stresses are correlated with each other. An example of in situ neutron diffraction measurement result shows the evolution of the residual stresses during welding.

36 MATERIALS SCIENCE↗

Temporarily alloying titanium to facilitate friction stir welding

While historically hydrogen has been considered an impurity in titanium, when used as a temporary alloying agent it promotes beneficial changes to material properties that increase the hot-workability of the metal. This technique known as thermohydrogen processing was used to temporarily alloy hydrogen with commercially pure titanium sheet as a means of facilitating the friction stir welding process. Specific alloying parameters were developed to increase the overall hydrogen content of the titanium sheet ranging from commercially pure to 30 atomic percent. Each sheet was evaluated to determine the effect of the hydrogen content on process loads and tool deformation during the plunge phase of the friction stir welding process. Two materials, H-13 tool steel and pure tungsten, were used to fabricate friction stir welding tools that were plunged into each of the thermohydrogen processed titanium sheets. Tool wear was characterized and variations in machine loads were quantified for each tool material and weld metal combination. Thermohydrogen processing was shown to beneficially lower plunge forces and stabilize machine torques at specific hydrogen concentrations. The resulting effects of hydrogen addition to titanium metal undergoing the friction stir welding process are compared with modifications in titanium properties documented in modern literature. Such comparative analysis is used to explain the variance in resulting process loads as a function of the initial hydrogen concentration of the titanium.

08 HYDROGEN↗

Uncertainty Quantification and Comparison of Weld Residual Stress Measurements and Predictions.

In pressurized water reactors, the prevention, detection, and repair of cracks within dissimilar metal welds is essential to ensure proper plant functionality and safety. Weld residual stresses, which are difficult to model and cannot be directly measured, contribute to the formation and growth of cracks due to primary water stress corrosion cracking. Additionally, the uncertainty in weld residual stress measurements and modeling predictions is not well understood, further complicating the prediction of crack evolution. The purpose of this document is to develop methodology to quantify the uncertainty associated with weld residual stress that can be applied to modeling predictions and experimental measurements. Ultimately, the results can be used to assess the current state of uncertainty and to build confidence in both modeling and experimental procedures. The methodology consists of statistically modeling the variation in the weld residual stress profiles using functional data analysis techniques. Uncertainty is quantified using statistical bounds (e.g. confidence and tolerance bounds) constructed with a semi-parametric bootstrap procedure. Such bounds describe the range in which quantities of interest, such as means, are expected to lie as evidenced by the data. The methodology is extended to provide direct comparisons between experimental measurements and modeling predictions by constructing statistical confidence bounds for the average difference between the two quantities. The statistical bounds on the average difference can be used to assess the level of agreement between measurements and predictions. The methodology is applied to experimental measurements of residual stress obtained using two strain relief measurement methods and predictions from seven finite element models developed by different organizations during a round robin study.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Status Report on Pressure Resistance Weld Development for FeCrAl Thin-Wall Cladding

This report summarizes the recent development on the weld techniques of joining the thin walled FeCrAl cladding to the endplug as a part of accident tolerant fuels (ATF) program for advanced light water reactor (LWR) systems. The FeCrAl alloy has been considered as the top candidate cladding materials for ATF fuels largely due to its high oxidation resistance in high temperature steam relevant to the loss of coolant accident (LOCA) conditions. The two primary techniques for the thin-walled cladding weld development are laser beam weld (fusion based) and pressure resistance weld (solid state without melting). This report focuses on the progress made on the pressure resistance weld (PRW) development for a commercial FeCrAl alloy.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

A Solution to Asymmetric Marangoni GTA Weld Behavior in a Dissimilar Chemistry Stainless Steel Joint [Slides]

Asymmetric and irregular weld morphology is an issue with the 9516 shipping container GTA weld. Observation of the weld puddle and cross sections showed the weld was biased toward the body side of the joint. This issue is attributed to a difference in the sulfur content and Marangoni fluid flow characteristics of the lid (150 ppm) and body (10 ppm) components of the weld joint. An additional contributing factor in this issue is the large difference in mass between the ½” thick lid and 1/8” thick body. A solution was developed comprised of a preliminary partial penetration weave pass across the joint intended to homogenize the sulfur content prior to the full penetration pass.

42 ENGINEERING↗

Development of Fiber Laser Weld Parameters for Stainless Steel and Refractory Metals

Laser welds were made in 21-6-9 stainless steel, vanadium and tantalum using LLNL's new 6kW fiber laser to target 1 mm penetration depths. The materials were machined into flat coupon samples with standard step-joint geometries, and were welded in a continuous wave mode. The laser was characterized using the Primes laser beam diagnostic system so that the beams can be reproduced in the future. The optical configuration consisted of a 200 {micro}m fiber, 200 mm collimator and 250 mm focusing lens, which delivered electron-beam level power densities in the 5 to 20 kW/mm2 range. The three different materials required different power densities to produce the desired penetration, and this report summarizes the results of this screening study that was directed at developing a first approximation to the proper welding parameters for future work. The results show that 1 mm penetrations can be achieved using a 400W beam for 21-6-9 stainless steel, a 600W beam for vanadium, and a 1,100W beam for tantalum using sharp focus and a travel speed of 40 inch/min. Future welds should incorporate a trailing gas shield to prevent discoloration of the surface and to prevent oxygen and nitrogen pickup in the welds.

36 MATERIALS SCIENCE↗

Impact of Plate Thickness and Joint Geometry on Residual Stresses in 347H Stainless Steel Welds

Weldments of 347H stainless steel are potentially susceptible to stress relaxation cracking at elevated service temperatures. Mitigation of stress relaxation cracking susceptibility within a multipass weld requires a good understanding of welding practices and manufacturing techniques to control high tensile residual stresses. Here in this work, the dependence of residual stress distribution in 347H stainless steel on base plate thickness, joint geometry design, and preheating condition was systematically investigated by using three-dimensional finite element models. The finite element models were validated through good agreement between neutron diffraction measurements and calculated elastic strains. The single-V-groove welds with and without a preheating step all produced similar peak von Mises residual stresses, above 450 MPa, within both the fusion zone and heat-affected zone (HAZ). In plates thicker than 0.5 in. (12.7 mm), high tensile residual stress could be observed in a relatively large area, from the middle of the plate thickness to underneath the top surface. A double-V groove shifted the high tensile stress area to the middle thickness of the weld. A single-J-groove weld was able to confine the residual stress to a very small region near the middle thickness within the fusion zone and suppressed the von Mises residual stress within the HAZ to below 400 MPa.

14 SOLAR ENERGY↗

Rotary Inertia Friction Welding of Dissimilar High-Strength 422 Martensitic Stainless Steel and 4140 Low Alloy Steel for Heavy-Duty Engine Piston Fabrication

AISI 422 martensitic stainless steel with superior high temperature performance (oxidation resistance and strength) is under evaluation for replacing current heavy-duty piston crown materials, AISI 4140 martensitic steel and micro alloyed steel (MAS) 38MnSiVS5, to fabricate a multimaterial piston. This multimaterial piston concept further improved power density and fuel economy by allowing heavyduty diesel engines to operate at higher temperatures and pressures. Joining AISI 422 steel piston crowns with AISI 4140 steel piston skirts is a key manufacturing step for this multimaterial piston. However, the significant differences in strength, elevated temperature flow stress, alloy chemistry, and temper resistance between these two martensitic steels cause some weldability issues (cracking) and metallurgical challenges (alloying element migration/segregation) when using conventional fusion-based welding processes. Rotary inertia friction welding (RIFW), a solid-state welding process, has been the preferred method to join 4140 crowns to 4140 skirts (and MAS crowns to MAS skirts) in high-volume production of current heavy-duty diesel engine pistons. It has been used to join these two materials with relatively comparable alloy chemistry to fabricate pistons with MAS skirts and 4140 crowns. Meanwhile, RIFW has also been a preferred method of dissimilar metal welding. However, RIFW of dissimilar high-strength martensitic steels has yet to be widely pursued. The interfacial microstructure complexities created by the thermomechanical process and highly nonequilibrium phase transformations during RIFW are a significant challenge for understanding and predicting their joining behavior and have not been reported in detail. Here, in this work, defect-free AISI 422 steel-AISI 4140 multimaterial pistons were successfully fabricated using the RIFW process. The interfacial microstructure and mechanical properties of dissimilar 422/4140 steel RIFW in the as-welded condition were experimentally studied in detail. The results provide critical baseline information for understanding RIFW mechanisms and guiding subsequent postweld heat treatment (PWHT) practice.

36 MATERIALS SCIENCE↗

Analysis of the Fatigue Strength of Welds in Terms of Local Stress

A local approach is developed for calculating the fatigue strength of welded metal structures, selecting the basic weld structure, and identifying the group of welded structures corresponding to that basic structure. To that end, the stress state of typical welded structures is analyzed on the basis of two-level stress concentrators. The results may be used to develop standards for calculating the fatigue strength of welded metal structures.

42 ENGINEERING↗

Friction Stir Welding of Line-Pipe Steels

Friction stir welding (FSW) offers both economic and technical advantages over conventional fusion welding practices for welding line-pipe. For offshore line-pipe construction, the economic savings has been shown to be considerable, approaching a calculated 25%. Offshore pipe is relatively small diameter but heavy wall compared to onshore pipe. One concern is the ability to achieve consistent full weld penetration in an on-site offshore FSW operation, e.g., on a lay-barge. In addition, depending on the size and morphology of the unwelded zone, lack of penetration at the weld root can be difficult if not impossible to detect by conventional NDE methods. Thus, an approach to assure consistent full penetration via process control is required for offshore line-pipe construction using FSW. For offshore construction, an internal structural mandrel can be used offering the opportunity to use a sacrificial anvil FSW approach. With this approach, a small volume of sacrificial material can be inserted into the structural anvil. The FSW tool penetrates into the sacrificial anvil, beyond the inner diameter of the pipe wall, thus assuring full penetration. The sacrificial material is subsequently removed from the pipe inner wall. In the work presented herein, FSW studies were completed on both 6 mm and 12 mm wall thickness line-pipe. Lastly, post-FSW evaluations including radiography, root-bend tests, and metallography demonstrated the merits of the sacrificial anvil approach to achieve consistent full penetration.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Influence of Alloy and Solidification Parameters on Grain Refinement in Aluminum Weld Metal due to Inoculation

The goals are: (1) Establish how much Ti/B grain refiner is need to completely refine aluminum weld metal for different alloys and different welding conditions; (2) Characterize how alloy composition and solidification parameters affect weld metal grain refinement; and (3) Apply relevant theory to understand observed behavior. Conclusions are: (1) additions of Ti/B grain refiner to weld metal in Alloys 1050, 5083, and 6082 resulted in significant grain refinement; (2) grain refinement was more effective in GTAW than LBW, resulting in finer grains at lower Ti content - reason is limited time available for equiaxed grain growth in LBW (inability to occlude columnar grain growth); (3) welding travel speed did not markedly affect grain size within GTAW and LBW clusters; and (4) application of Hunt CET analysis showed experimental G to be on the order of the critical G{sub CET}; G{sub CET} was consistently higher for GTAW than for LBW.

36 MATERIALS SCIENCE↗

Implementation of ASME Code, Section XI, Code Case N-770, on Alternative Examination Requirements for Class 1 Butt Welds Fabricated with Alloy 82/182

In May 2010, the NRC issued a proposed notice of rulemaking that includes a provision to add a new section to its rules to require licensees to implement ASME Code Case N-770, ‘‘Alternative Examination Requirements and Acceptance Standards for Class 1 PWR Piping and Vessel Nozzle Butt Welds Fabricated with UNS N06082 or UNS W86182 Weld Filler Material With or Without the Application of Listed Mitigation Activities, Section XI, Division 1,’’ with 15 conditions. Code Case N-770 contains baseline and inservice inspection (ISI) requirements for unmitigated butt welds fabricated with Alloy 82/182 material and preservice and ISI requirements for mitigated butt welds. The NRC stated that application of ASME Code Case N-770 is necessary because the inspections currently required by the ASME Code, Section XI, were not written to address stress corrosion cracking Alloy 82/182 butt welds, and the safety consequences of inadequate inspections can be significant. The NRC expects to issue the final rule incorporating this code case into its regulations in the spring 2011 time frame. This paper discusses the new examination requirements, the conditions that NRC is imposing , and the major concerns with implementation of the new Code Case.

alloy 82/182↗

Process Development of the Vaporizing Foil Actuator Welding Technique

The industrial focus on continuous improvement for products is leading design engineers to consider multi-material design concepts more frequently. The design concepts use the advantages of each material while simultaneously minimizing the drawbacks. It also allows for the overall weight of the products to be reduced. Some traditional joining methods, though, struggle to join dissimilar material combinations. A technique known as vaporizing foil actuator welding, which was developed around ten years ago, is a solid-state joining method that has the potential to overcome the barriers to dissimilar material joining. The biggest drawbacks of vaporizing foil actuator welding are that it is still exclusively used in laboratory settings and early in the technology development process. As such, there is not enough confidence in the process for it to be transitioned to manufacturing environments yet. This work begins by analyzing the current state of the technology and identifying a roadmap to achieve a transition to manufacturing. The analysis found that increased confidence in the technology requires sample to sample repeatability to be improved. Beyond that, the process also needs to be fully automated before it can be considered as a viable technique for mass production. In order to further develop the technique, a fully automated work cell was constructed. By removing the human element from the process, this cell helped identify iii the aspects which contribute to process variability. The positioning of the vaporizing foil actuator was identified as the most important factor in process stability. A small set of samples were made in the automated cell with the addition of one component epoxy adhesive around the perimeter of the weld. These samples showed improved process repeatability compared with the samples made without adhesive. This indicates that small amounts of adhesive may be critical in using the process in industrial settings. Additionally, work was performed with manual positioning and adhesive dispensing. This work found that a hybrid joint behaves like traditional weld bonding, where the addition of adhesive makes the joint stronger than if either of the two joining methods were used on their own. To realize this performance with vaporizing foil actuator welding, though, the adhesive needs to be protected from burning during the rapid compression of air during the impact process.

36 MATERIALS SCIENCE↗

Laser Welded Edge Seals for Polymer-Free Glass/Glass Modules

This presentation covers fs lasers which enable crack-free and stress-free glass/glass welds. Welds are nearly as strong as the glass (KI, weld ~ KI, glass) and static load test passed, enabling: 1) polymer-free; 2) hermetically sealed; and 3) recyclable modules. Next steps are: 1) follow-on funding; 2) develop feed throughs (metal/glass welds already achieved for other devices); and 3) weld mini modules for further IEC module testing.

DuraMAT↗

Remote In-bore Laser Cutting and Welding Tools for use in Future Nuclear Fusion Reactors - 18348

The maintenance, replacement and decommissioning of future nuclear fusion reactors will require quick and reliable cutting and joining of in-vessel pipework. Initial design studies for nuclear fusion reactors for power generation have estimated cutting and welding could account for up to 60% of the maintenance duration using conventional in-situ processing techniques (dry-mechanical cutting and arc welding) and that new methods are required to expedite the process. Additionally, the expected radioactivity and limited access at the cutting and welding sites mean that these processes cannot be done manually and robotic tools are required. To this end, remote in-bore laser cutting and welding tools have been developed for use in 90 mm internal diameter steel pipes. Here, we will present the designs of the remote in-bore laser cutting and welding tools, and how the tools fit within the overall remote maintenance strategy of a nuclear fusion reactor. Initial high-power laser trials were performed with prototype tools which successfully demonstrated their laser processing, thermal management and dust protection functionality. Although the tools described herein have been developed specifically for use within the fusion reactor environment, however the tool design and technology demonstrated here is readily transferable to many remote applications in challenging environments such as fission reactor maintenance, nuclear decommissioning and other in-accessible pipework. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

ELECTRIC FIELD-ASSISTED DIFFUSION WELDING TO FABRICATE ALLOY 617 COMPACT HEAT EXCHANGERS

Compact heat exchangers are of interest for a number of applications including advanced reactors. Alloy 617 is one of the top candidate materials for the gas-cooled reactor intermediate heat exchanger. Previous endeavors to diffusion weld Alloy 617 utilized hot pressing (HP). It was reported that grain boundary migration across the interface was hindered by extensive precipitation. Bonds of this nature have been observed to reduce the elevated-temperature mechanical properties compared to the wrought-product form. It was hypothesized that the electric current applied during electric-field-assisted sintering (EFAS) can overcome these challenges, resulting in improved diffusion welding (DW). This study investigated DW of Alloy 617 via EFAS. Stacks composed of three sheets that were 20 mm in diameter were welded using EFAS. Specimens were welded with an applied electric current, a pressure of 30 MPa, hold time of 30 min, and temperatures of 1050°C, 1100°C, and 1150°C. DW using HP as the zero-current analog of EFAS was also performed at the most promising EFAS conditions. Results revealed that both the applied electric current and temperature played a key role in precipitation and grain boundary migration in diffusion-welded Alloy 617. Precipitates were observed at the interface of the hot-pressed samples which limited grain boundary migration. Electric current was found to prevent precipitate formation along the interface at 1150°C. The electric current coupled with a temperature of 1150°C during EFAS resulted in significant grain boundary migration across the interface.

36 - MATERIALS SCIENCE↗