Search NASA⌕ Search

SEARCH · Search NASA

Results for “improved microstructures and properties”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 523 records · Page 29

Study of microstructure, dielectric and ferromagnetic properties of the (1-x)Ba{sub 0.95}Sr{sub 0.05}TiO{sub 3}-(x)CoFe{sub 1.8}Mn{sub 0.2}O{sub 4} multiferroic composites

In the present work, (1-x)Ba{sub 0.95}Sr{sub 0.05}TiO{sub 3}-(x)CoFe{sub 1.8}Mn{sub 0.2}O{sub 4} composites are prepared by standard solid state reaction method. The X-ray diffraction measurement of the composites shows that both the phases coexist in the composite, individually. The morphology of the composites were examined by field emission scanning electron microscopy and reveals homogeneous microstructure with two types of grains, smaller grains of the Ba{sub 0.95}Sr{sub 0.05}TiO{sub 3} (BST) and bigger grains of the CoFe{sub 1.8}Mn{sub 0.2}O{sub 4} (CFM). The dielectric studies show that all the composites exhibit dispersion in the lower frequency region attributable to the interfacial polarization. In addition, at lower frequencies, the dielectric constant (ε´) is found to increase with increase in CFM content in the composites. The ferromagnetic properties of the composites improve with the increase in the CFM content.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Effects of Pouring Temperature and Electromagnetic Stirring on Porosity and Mechanical Properties of A357 Aluminum Alloy Rheo-Diecasting

Semisolid slurry of A357 aluminum alloy was prepared using a temperature-controllable electromagnetic stirrer and rheo-diecast at different temperatures. The effects of pouring temperature and electromagnetic stirring (EMS) on the porosity in rheo-diecast samples, as well as the relation between porosity and mechanical properties, were investigated. The results show that pouring temperature and EMS had minor influences on rheo-diecast microstructure but marked influence on the porosity. With decreasing slurry pouring temperature, the porosity decreased first and then increased, whereas the maximum pore ratio (ratio of shape factor to diameter of the largest pore) increased first and then decreased. The maximum pore ratio determines the level of tensile strength and elongation, and higher mechanical properties can be obtained with smaller and rounder pores in samples. The mechanical properties of the rheo-diecast samples increased linearly with increasing maximum pore ratio. The maximum pore ratio was 1.43 µm{sup −1}, and the minimum porosity level was 0.37% under EMS condition for the rheo-diecast samples obtained at a pouring temperature of 608 °C. With this porosity condition, the maximum tensile strength and elongation were achieved at 274 MPa and 4.9%, respectively. It was also revealed that EMS improves mechanical properties by reduction in porosity and an increase in maximum pore ratio.

36 MATERIALS SCIENCE↗

Effect of Multiple Reflow Cycles and Al{sub 2}O{sub 3} Nanoparticles Reinforcement on Performance of SAC305 Lead-Free Solder Alloy

The effect of Al{sub 2}O{sub 3} nanoparticles reinforcement on melting behavior, microstructure evolution at the interface and joint shear strength of 96.5Sn3Ag0.5Cu (SAC305) lead-free solder alloy subjected to multiple reflow cycles was investigated. The reinforced SAC305 solder alloy compositions were prepared by adding Al{sub 2}O{sub 3} nanoparticles in different weight fractions (0.05, 0.1, 0.3 and 0.5 wt.%) through mechanical dispersion. Cu/solder/Cu micro-lap-shear solder joint specimens were used to assess the shear strength of the solder joint. Differential scanning calorimetry was used to investigate the melting behavior of SAC305 solder nanocomposites. The solder joint interfacial microstructure was studied using scanning electron microscopy. The results showed that the increase in melting temperature (T{sub L}) and melting temperature range of the SAC305 solder alloy by addition of Al{sub 2}O{sub 3} nanoparticles were not significant. In comparison with unreinforced SAC305 solder alloy, the reinforcement of 0.05-0.5 wt.% of Al{sub 2}O{sub 3} nanoparticles improved the solder wettability. The addition of nanoparticles in minor quantity effectively suppressed the Cu{sub 6}Sn{sub 5} IMC growth, improved the solder joint shear strength and ductility under multiple reflow cycles. However, the improvement in solder properties was less pronounced on increasing the nanoparticle content above 0.1 wt.% of the solder alloy.

36 MATERIALS SCIENCE↗

Microstructure and mechanical properties of NiCoCrAlYTa alloy processed by press and sintering route

Nickel-based superalloys such as NiCoCrAlY are widely used in high-temperature applications, such as gas turbine components in the energy and aerospace industries, due to their strength, high elastic modulus, and high-temperature oxidation resistance. However, the processing of these alloys is complex and costly, and the alloys are currently used as a bond coat in thermal barrier coatings. In this work, the effect of cold press and sintering processing parameters on the microstructure and mechanical properties of NiCoCrAlY alloy were studied using the powder metallurgy route as a new way to obtain NiCoCrAlYTa samples from a gas atomized prealloyed powder feedstock. High mechanical strength and adequate densification up to 98% were achieved. The most suitable compaction pressure and sintering temperature were determined for NiCoCrAlYTa alloy through microstructure characterization. Scanning electron microscopy (SEM), transmission electron microscopy (TEM), X-ray diffraction (XRD), and energy dispersive spectroscopy microanalysis (EDS) were performed to confirm the expected γ-Ni matrix and β-NiAl phase distribution. Additionally, the results demonstrated the unexpected presence of carbides and Ni–Y-rich zones in the microstructure due to the powder metallurgy processing parameters used. Thus, microhardness, nanoindentation and uniaxial compression tests were conducted to correlate the microstructure of the alloy samples with their mechanical properties under the different studied conditions. The results show that the compaction pressure did not significantly affect the mechanical properties of the alloy samples. In this work, the compaction pressures of 400, 700 and 1000 MPa were used. The sintering temperature of 1200 °C for NiCoCrAlYTa alloy was preferred; above this temperature, the improvement in mechanical properties is not significant due to grain coarsening, whereas a lower temperature produces a decrease in mechanical properties due to high porosity and poor solid-state diffusion. - Graphical abstract: Display Omitted - Highlights: • We made NiCoCrAlYTa alloy by a conventional powder metallurgy route. • High densification and adequate strength were observed. • The presence of unexpected carbides found along γ/γ and γ/β grain boundaries was detected. • The effect of cold press and sintering processing parameters on the microstructure and mechanical properties were studied.

36 MATERIALS SCIENCE↗

Effect of mechanical alloying synthesis process on the dielectric properties of (Bi{sub 0.5}Na{sub 0.5}){sub 0.94}Ba{sub 0.06}TiO{sub 3} piezoceramics

Highlights: • MA samples show higher dielectric permittivity and Curie temperature. • In MA samples, dielectric loss is almost 27% less than conventional ones. • In MA samples, sintering time and temperature are lower than conventional ones. • In MA samples, particle morphology is more homogeneous conventional ones. • In MA samples, crystallite size is smaller conventional ones. - Abstract: In present work, in order to study the effects of synthesis techniques on dielectric properties, the BNBT lead-free piezoceramics with (Bi{sub 0.5}Na{sub 0.5}){sub 0.94}Ba{sub 0.06}TiO{sub 3} stoichiometry (called as BNBT6) were synthesized by mechanical alloying (MA) and conventional mixed oxides methods. The structural, microstructural, and dielectric properties were carried out by X-ray diffractometer (XRD), scanning electron microscope (SEM), and impedance analyzer LCR meter, respectively. Based on results, the density of MA samples is considerably higher than conventional samples owning to smaller particles size and more uniformity of particle shape of MA samples. Moreover, the dielectric properties of MA samples are comparatively improved in which the dielectric loss of these samples is almost 27% less than conventional ones. Furthermore, MA samples exhibit obviously higher dielectric permittivity and Curie temperature compared to the conventional samples.

36 MATERIALS SCIENCE↗

Fabrication of Al-Zn solid solution via friction stir processing

Highlights: • Thermomechanical nature of FSP was utilized for mechanical alloying. • Zn particles dissolved in Al during FSP to form solid solution. • Second pass of FSP lead to homogenization and partial decomposition of the solid solution. • Processed alloy exhibited improved hardness over base and FSPed metal. • The process can be adopted for site specific property enhancement. - Abstract: The present study demonstrates that friction stir processing (FSP) can be used as a mechanical alloying tool to process solid solution. Zn was incorporated in commercially pure aluminium by multi-pass FSP leading to its dissolution and formation of supersaturated solid solution which was confirmed by X-ray diffraction and scanning electron microscopy. The hardness across the stir zone matched with the distribution of Zn and was significantly improved compared to the base metal. The supersaturated solid solution that formed in the first pass, partially decomposed during the second pass, leading to the formation of fine Al-Zn precipitates. Thermal stability of the microstructure against abnormal grain growth was also improved after the second pass due to the pinning effect of the grain boundary precipitates. FSP also caused grain refinement of the alloy yielding fine equiaxed grains in the range of 4–6 μm with a high fraction (> 67%) of high angle grain boundaries. Such microstructure is conducive for isotropic properties and the fact that the microstructure is stable against thermal cycles make the process suitable for selective alloying for location specific property enhancement.

36 MATERIALS SCIENCE↗

Microstructure and Electromagnetic Shielding Properties of Mg-Zn-Ce-Y-Zr Alloys

Microstructure and electromagnetic interference shielding properties of extruded Mg-Zn-Ce-Y-Zr alloys were systematically investigated. A bimodal grain structure of fine recrystallized grains and deformed grains was observed in the alloys. Yttrium (Y) and cerium (Ce) refined the recrystallized grains. Mg-Zn-Ce phase, Mg{sub 3}Zn{sub 3}Y{sub 2} phase and a few precipitates containing Zn and Zr were observed. Y and Ce additions changed the texture of the alloys. When the total rare earth content reached 4 wt.%, the texture was remarkably weaker than other studied alloys. The shielding capacity increased first and then decreased with Y contents. The value of shielding effectiveness for the extruded Mg-5Zn-1Ce-2Y-0.6Zr alloys reached 79-118 dB in the frequency range of 30 MHz-1.5 GHz, which was significantly higher than that of some aluminum alloys. The addition of Y and Ce is effective in improving the shielding capacity in Mg alloys. The electrical conductivity and second phases in the alloys were important in enhancing shielding effectiveness. The texture and precipitation exerted significant effect on electrical conductivity. In addition, subsequently aging treatment evidently improved shielding effectiveness.

36 MATERIALS SCIENCE↗

Correlating thermoelectric properties with microstructure in Bi 0.8 Sb 0.2 thin films

The room temperature electronic transport properties of 100 nm-thick thermoelectric Bi 0.8 Sb 0.2 films, sputter-deposited onto quartz substrates and post-annealed in an ex-situ furnace, systematically correlate with the overall microstructural quality, improving with increasing annealing temperature until close to the melting point for the alloy composition. Furthermore, the optimized films have high crystalline quality with ~99% of the grains oriented with the trigonal axis perpendicular to the substrate surface. Film resistivities and Seebeck coefficients are accurately measured by preventing deleterious surface oxide formation via a SiN capping layer and using Nd-doped Al for contacts. Our resulting values are similar to single crystals and significantly better than previous reports from films and polycrystalline bulk alloys.

36 MATERIALS SCIENCE↗

Effects of Heat Treatment on Microstructure, Thermal Transport and Stability in SRF Niobium

Efficient heat transfer and thermal stability are critical for preventing thermal quench and ensuring the high performance and reliability of superconducting radiofrequency (SRF) cavities, especially under high RF fields. In this article, we investigate thermal conductivity and heat capacity of high-purity cold-worked niobium used in SRF applications, with a particular focus on the effects of high-temperature heat treatments. Our measurements reveal a pronounced sensitivity of thermal transport and thermodynamic properties to the underlying microstructure such as grain size and dislocation density. The results show the critical role of controlled heat treatment processes in optimizing the thermal performance of SRF niobium, providing valuable insights for improving cavity fabrication and processing.

36 MATERIALS SCIENCE↗

Development of HPC based phase field simulations tool for modification of alloy morphology to enhance material properties during additive manufacturing (AM) process

Currently, additive manufacturing (AM) technology is extensively used to manufacture aerospace components because of the unique advantages of the technique in producing custom designs, complex geometries in a near-net fashion that significantly reduces the manufacturing cost, and improved energy efficiency. However, the thermodynamic properties of existing aerospace alloys and the thermal conditions that prevail in most of the powder-bed based additive manufacturing processes lead to undesirable columnar / columnar-dendritic microstructures that promote solidification cracking during the process, and the development of anisotropy in the mechanical properties of the as-built components. Time consuming, energy-intensive post AM treatments are required to recover the mechanical properties of the wrought components for which the existing alloy compositions were designed for. However, novel alloy compositions, that exploit the AM thermal conditions to produce fine, equiaxed grain structures in the as-built condition, with mechanical properties equal to or exceeding those of the wrought work-horse alloy, Ti-6Al-4V has recently been demonstrated in Ti-Cu alloys. Significant energy savings up to 66% can be obtained for a typical aerospace component through digitally designing the AM process, process parameters, and alloy composition. The current project focused on developing a fundamental understanding of the evolution of the columnar to equiaxed transition (CET) occurring during solidification under AM thermal conditions in Ti-Cu and Ti-Cu-X alloys using high-fidelity phase field (PF) simulations using the leadership class computing facilities that exist in the national laboratories. The simulations were able to capture the effect of alloy and process conditions on CET, and clearly showed the beneficial effect of a ternary solute addition to Ti-Cu binary alloys on CET. The simulations indicated that bulk nucleation in the liquid ahead of the solidifying epitaxial front was promoted by a large, transient, thermal undercooling promoted by the mismatch between the growth rate of the dendrite tips in the epitaxial front and the imposed solidification rate. AM experiments performed at Raytheon Technologies Research Center using the same thermal conditions used in the PF simulations indicated the formation of equiaxed grains, although the grain size was bigger than the ones reported in the literature. On the other hand, the equiaxed grain size predicted by PF simulations were smaller than the grain size of Ti-Cu alloys reported in the literature. The industry will follow up the existing work in a future program that would involve further optimization of the process for the Ti-Cu-X alloys to demonstrate the application of the process and the alloy to a specific aerospace component.

36 MATERIALS SCIENCE↗

Development of Stretch Flangeable Grade Steels by Inclusion Engineering Approach

The demand for good stretch flangeability in high-strength automotive steels has necessitated due attention on steel cleanliness and processes. The presence of elongated MnS stringers and centerline segregation of nonmetallic inclusions adversely affects the transverse mechanical property. In the present investigation, stretch flangeability of industrially produced steel, with and without Ca treatment, has been compared with Ti-added steel, produced at 40 kg scale without Ca treatment. The study brings out the influence of centerline segregation and modification of nonmetallic inclusions on HER performance. The microstructural analysis of industrial steel revealed that the method of hole formation (punching/drilling) determines crack initiation mechanism. The inclusions, along with the second phase present in the centerline, drive the crack propagation. An addition of Ti in liquid steel promotes formation of Al-Ti-O-based oxide, prior to MnS precipitation, during solidification and acts as nucleation site for MnS inclusion. This obviates the elongated stringer-type MnS inclusions. The centerline segregation-free Ti-modified steel, prepared at the laboratory scale, showed consistent HER property compared with industrial steel. It is also concluded that calcium treatment can be circumvented by modifying the sulfide stringer with the addition of Ti in the steel for further improvement in HER property.

36 MATERIALS SCIENCE↗

Effect of Partial Substitution of Mn for Ni on Mechanical Properties of Friction Stir Processed Hypoeutectic Al-Ni Alloys

In this study, the mechanical properties of as-cast and FSPed Al-2Ni-xMn alloys (x = 1, 2, and 4 wt pct) were investigated and compared with those of the as-cast and FSPed Al-4Ni alloy. According to the results, the substitution of 2 wt pct Mn for 2 wt pct Ni leads to the formation of fine Mn-rich intermetallics in the microstructure increasing the tensile strength, microhardness, fracture toughness, and specific strength of alloy by 22, 56, 45, and 35 pct, respectively. At higher Mn concentrations, the formation of large Mn-rich platelets in the microstructure reduces the tensile properties. Friction stir processing at 12 mm/min and 1600 rpm significantly enhances both the strength and ductility of the alloy. The tensile strength, yield strength, fracture strain, fracture toughness, microhardness, and specific strength of FSPed Al-2Ni-4Mn alloy improved by 97, 83, 30, 380, 152, and 110 pct, respectively, as compared to those of the as-cast Al-4Ni alloy. This can be attributed to dispersion strengthening of Ni- and Mn-rich dispersoids, formation of ultrafine grains, and elimination of casting defects. The fractography results also show that the brittle fracture mode of the as-cast Mn-rich alloys turns to a more ductile mode, comprising fine and equiaxed dimples in FSPed samples.

36 MATERIALS SCIENCE↗

Electromagnetic wave absorption of multifunctional cementitious composites incorporating polyvinyl alcohol (PVA) fibers and fly ash: Effects of microstructure and hydration

Highlights: • The cementitious composite shows excellent wide-band electromagnetic wave absorption in a frequency range of 2–18 GHz. • The PVA fibers and the fly ash change the dielectric properties of the cementitious composite by Debye polarization. • The iron oxide of the cementitious binders contributes to the magnetic properties of the composites. • The impacts of the microstructure and the hydration of the cementitious composite on its microwave absorption are analyzed. This paper devises a novel method for the adjustment of the pore structure and the hydration of cement to improve the electromagnetic wave absorption of the cementitious composites incorporating polyvinyl alcohol (PVA) fibers and fly ash in a frequency range of 2–18 GHz. The underlying mechanism of the absorption is investigated to explore the possibility of the structural and functional integration of these composites. The electromagnetic parameters of the prepared cementitious composites and those of the raw materials are analyzed in a frequency range of 0.5–18 GHz. Moreover, the pore structure and the chemical environment of the cementitious composites are examined by mercury intrusion porosimetry (MIP), back-scattered electron detector (BSE), and X-ray photoelectron spectroscopy (XPS). The results indicate that the PVA fibers and the high-volume fly ash have a positive effect on electromagnetic wave absorption of the cementitious composites through the adjustment of their pore structure and hydration.

36 MATERIALS SCIENCE↗

Ensemble Manufacturing Techniques for Steam Turbine Components Across Length Scales

Faster design to manufacturing requirements were sought for steam turbine components to meet the changing demands of today’s power grid of improved efficiency through operating temperature increases and enhanced operational flexibility from baseload to cyclic operations. Advances in multiple advanced manufacturing (AM) process enabled redesign of turbine components for extreme environments with the potential to reduce cost. AM is of particular interest to improve component functionality, higher temperature capability, and superior durability in large scale steam turbine applications. AM methods have an immense potential to open-up the design space by working directly with the 3D model to produce near-net shapes, enable fast design-manufacturing iterations, thereby significantly reducing product cost and lead-time up to 25 % from current baseline. However, these benefits cannot be fully realized due to the potential for unknown AM processing defects and their resultant effect upon component performance in service. Siemens is partnering with Oak Ridge National Laboratory (ORNL), Electric Power Research Institute (EPRI), and Connecticut Center for Advanced Technology (CCAT) to advance the knowledge of complex process-material interactions for desired microstructures and properties that are closely interlinked to component geometries across different length scales. The proposed program utilized an ensemble of multidisciplinary technologies to accelerate the development of materials, high-throughput experiments for their qualification, and design flexibility/topology optimization for repair/redesign of components to address critical failure mechanisms for improved performance and increased reliability of existing power plant components. The proposed activities, if successfully demonstrated for identified components, will enable paradigm shift in customized manufacturing and accelerated qualification/certification towards increased steam turbine component durability, increased turbine efficiency, and reduced CO 2 emissions in load-following environments compared to today’s technology. Technology maturation is built into the project as successful research will include customized process-component down-selection enabling AM methodologies to be incorporated directly into the existing supply chain. The specific activities of the proposed effort are: 1. Topology optimization of down-selected steam turbine parts that are amenable to additive and hybrid manufacturing for cost/performance improvement. 2. Process-structure-property relationships for five AM processes for steam turbine materials of interest to compare with conventional materials. 3. Perform part/assembly build process using advanced additive/hybrid machine tools followed by quality inspection of the built components for insight into qualification for production scale-up. Steam turbine rig testing of printed components under targeted, well monitored and characterized environmental conditions of for performance comparison of baseline and redesigned components.

36 MATERIALS SCIENCE↗

Effect of Local Postweld Heat Treatments on Metal Inert Gas-Welded A7N01S-T5 Joints

T6, T7, and retrogression and reaging (RRA) postweld heat treatments (PWHTs) were redefined and deployed to restore MIG-welded A7N01-T5 aluminum alloy joints in train-body structures using an inductive heating device. After the PWHT, the microstructures and mechanical properties of the joints were studied by x-ray diffraction (XRD), electron backscattered diffraction (EBSD), and scanning electron microscopy (SEM). The results showed that the hardness and strength of the joints were improved by the T6 treatment, and the tensile strength of the joints reached 87.39% of the base metal. However, an improvement in the corrosion resistance was not observed. The T7-treated joints enhanced the toughness of the welded joints and improved their corrosion resistance. The RRA-treated joints improved the toughness and corrosion resistance and increased the strength and hardness. The RRA treatment had a more comprehensive effect on the improvement of the welded joint structure and performance and is more suitable for postweld heat treatment of the aluminum alloy welded joints in the body of high-speed trains.

36 MATERIALS SCIENCE↗

High temperature deformation mechanism in hierarchical and single precipitate strengthened ferritic alloys by in situ neutron diffraction studies

Here, the ferritic Fe-Cr-Ni-Al-Ti alloys strengthened by hierarchical-Ni 2 TiAl/NiAl or single-Ni 2 TiAl precipitates have been developed and received great attentions due to their superior creep resistance, as compared to conventional ferritic steels. Although the significant improvement of the creep resistance is achieved in the hierarchical-precipitate-strengthened ferritic alloy, the in-depth understanding of its high-temperature deformation mechanisms is essential to further optimize the microstructure and mechanical properties, and advance the development of the creep resistant materials. In the present study, in-situ neutron diffraction has been used to investigate the evolution of elastic strain of constitutive phases and their interactions, such as load-transfer/load-relaxation behavior between the precipitate and matrix, during tensile deformation and stress relaxation at 973 K, which provide the key features in understanding the governing deformation mechanisms. Crystal-plasticity finite-element simulations were employed to qualitatively compare the experimental evolution of the elastic strain during tensile deformation at 973 K. It was found that the coherent elastic strain field in the matrix, created by the lattice misfit between the matrix and precipitate phases for the hierarchical-precipitate-strengthened ferritic alloy, is effective in reducing the diffusional relaxation along the interface between the precipitate and matrix phases, which leads to the strong load-transfer capability from the matrix to precipitate.

36 MATERIALS SCIENCE↗

Local polar structure and multiferroic properties of (1−x)Bi{sub 0.9}Dy{sub 0.1}FeO{sub 3}−xPbTiO{sub 3} solid solution

The multiferroic (1–x)[0.9BiFeO{sub 3}–0.1DyFeO{sub 3}]–xPbTiO{sub 3} (BDF–xPT) solid solution with compositions around the morphotropic phase boundary (x = 0.25, 0.28, 0.31, 0.34, and 0.37) has been synthesized in the form of ceramics. The phase symmetry, microstructure, ferroelectricity, piezoresponse, and ferromagnetic properties have been characterized by various techniques. It is found that, with increasing content of lead titanate from x = 0.25 to x = 0.37, the grain size increases and the ferroelectric property is improved. The ferroelectric performance is further enhanced by the introduction of an excess amount (2%) of TiO{sub 2} or by sintering in oxygen atmosphere, which reduces the leakage. The local polar structure is imaged by piezoresponse force microscopy. Both the out-of-plane and in-plane images reveal distinct ferroelectric domain structures, with the amplitude and the average domain size decreasing with the increase of lead titanate amount. Compared with the (1–x)BiFeO{sub 3}–xPbTiO{sub 3} binary solid solution of about the same concentration of PT, the magnetic properties are enhanced in BDF–xPT due to the presence of dysprosium, as demonstrated by the ferromagnetic hysteresis loops displayed at room temperature and at 10 K, but the remnant magnetization decreases with increasing PT content. The simultaneous presence of ferroelectricity and ferromagnetism entitles the BDF–xPT solid solution a room-temperature multiferroic material.

36 MATERIALS SCIENCE↗

Effect of Friction Stir Processing on the Microstructure, Damping Capacity, and Mechanical Properties of Al-Si Alloy

Friction stir processing (FSP) was conducted on an Al-Si casting alloy. The Si phase and Al grains of an Al-Si casting alloy were refined through FSP. Furthermore, FSP with high rotation rate led to the precipitation of Mg and Si atoms and the formation of Mg{sub 2}Si phase in the Al-Si alloy. Precipitation improved the low-strain damping capacity but deteriorates high-strain damping capacity of the FSP sample at room temperature. At low rotation rate, the FSP sample exhibited excellent high-temperature damping capacity mainly because of its fine grain structure and the low density of its pinning points. The plastic instability of the Al-Si alloy was eliminated by FSP because of the refinement of the Si phase. The increase in the strength of each FSP sample was attributed to the increase in second-phase and boundary strengthening effects. Thus, the mechanical properties and damping capacity of Al-Si were enhanced after FSP.

36 MATERIALS SCIENCE↗