A Coordinated-Anion-Enriched Electrolyte for Lean-Electrolyte Li–S Batteries

The solid electrolyte interphase (SEI) on Li and cathode electrolyte interphase (CEI) at sulfurized polyacrylonitrile (SPAN) formed in the commonly used liquid electrolytes cannot accommodate the large volume change of both Li anode and SPAN cathode, resulting in severe electrolyte and Li consumption and fast capacity decay under high mass loading and lean electrolyte condition. Herein, a LiF-rich SEI and a LiF-Li x N y O z co-enriched CEI are simultaneously formed by adding ionic liquid (Py 13 TFSI) in the localized high-concentration electrolyte (LHCE), which forms a coordinated-anion-enriched solvation structure. In this study, the LiF-rich interphase results in less stress/strain during large volume changes of Li and SPAN and therefore achieving obviously improved stability even at a high areal capacity. Consequently, Li (50 μm)||SPAN (6 mg cm -2 ) pouch cells under the lean electrolyte condition (E/S ratio of 5 mL g SPAN -1 ) delivers a stable cycle life of 120 cycles with 79.2% capacity retention, demonstrating great promise for high-energy-density lithium-sulfur batteries.

25 ENERGY STORAGE↗

Selective NMR observation of the SEI–metal interface by dynamic nuclear polarisation from lithium metal

While lithium metal represents the ultimate high-energy-density battery anode material, its use is limited by dendrite formation and associated safety risks, motivating studies of the solid–electrolyte interphase layer that forms on the lithium, which is key in controlling lithium metal deposition. Dynamic nuclear polarisation enhanced NMR can provide important structural information; however, typical exogenous dynamic nuclear polarisation experiments, in which organic radicals are added to the sample, require cryogenic sample cooling and are not selective for the interface between the metal and the solid–electrolyte interphase. Here we instead exploit the conduction electrons of lithium metal to achieve an order of magnitude hyperpolarisation at room temperature. We enhance the 7 Li, 1 H and 19 F NMR spectra of solid–electrolyte interphase species selectively, revealing their chemical nature and spatial distribution. These experiments pave the way for more ambitious room temperature in situ dynamic nuclear polarisation studies of batteries and the selective enhancement of metal–solid interfaces in a wider range of systems.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Production of fast-charge Zn-based aqueous batteries via interfacial adsorption of ion-oligomer complexes

Abstract Aqueous zinc batteries are attracting interest because of their potential for cost-effective and safe electricity storage. However, metallic zinc exhibits only moderate reversibility in aqueous electrolytes. To circumvent this issue, we study aqueous Zn batteries able to form nanometric interphases at the Zn metal/liquid electrolyte interface, composed of an ion-oligomer complex. In Zn||Zn symmetric cell studies, we report highly reversible cycling at high current densities and capacities (e.g., 160 mA cm −2 ; 2.6 mAh cm −2 ). By means of quartz-crystal microbalance, nuclear magnetic resonance, and voltammetry measurements we show that the interphase film exists in a dynamic equilibrium with oligomers dissolved in the electrolyte. The interphase strategy is applied to aqueous Zn||I 2 and Zn||MnO 2 cells that are charged/discharged for 12,000 cycles and 1000 cycles, respectively, at a current density of 160 mA cm −2 and capacity of approximately 0.85 mAh cm −2 . Finally, we demonstrate that Zn||I 2 -carbon pouch cells (9 cm 2 area) cycle stably and deliver a specific energy of 151 Wh/kg (based on the total mass of active materials in the electrode) at a charge current density of 56 mA cm −2 .

25 ENERGY STORAGE↗

Corrosion of lithium metal anodes during calendar ageing and its microscopic origins

Rechargeable lithium (Li) metal batteries must have long cycle life and calendar life (retention of capacity during storage at open circuit). Particular emphasis has been placed on prolonging the cycle life of Li metal anodes, but calendar ageing is less understood. Here, we show that Li metal loses at least 2–3% of its capacity after only 24 hours of ageing, regardless of the electrolyte chemistry. These losses of capacity during calendar ageing also shorten the cycle life of Li metal batteries. Cryogenic transmission electron microscopy shows that chemical corrosion of Li and the continuous growth of the solid electrolyte interphase—a passivation film on Li—cause the loss of capacity. Electrolytes with long cycle life do not necessarily form a solid electrolyte interphase with more resistance to chemical corrosion, so functional electrolytes must simultaneously minimize the rate of solid electrolyte interphase growth and the surface area of electrodeposited Li metal.

36 MATERIALS SCIENCE↗

Characterization of the structure and chemistry of the solid–electrolyte interface by cryo-EM leads to high-performance solid-state Li-metal batteries

Solid-state lithium-metal (Li 0 ) batteries are gaining traction for electric vehicle applications because they replace flammable liquid electrolytes with a safer, solid-form electrolyte that also offers higher energy density and better resistance against Li dendrite formation. Solid polymer electrolytes (SPEs) are highly promising candidates because of their tunable mechanical properties and easy manufacturability; however, their electrochemical instability against lithium metal (Li 0 ), mediocre conductivity, and poorly understood Li 0 /SPE interphases have prevented extensive application in real batteries. In particular, the origin of the low Coulombic efficiency (CE) associated with SPEs remains elusive, as the debate continues as to whether it originates from unfavored interfacial reactions or lithium dendritic growth and dead lithium formation. In this work, we use state-of-the-art cryo-electromicroscopy (cryoEM) imaging and spectroscopic techniques to characterize the structure and chemistry of the interface between Li 0 and a polyacrylate-based SPE. Contradicting the conventional knowledge, we find that no protective interphase forms, owing to the sustained reactions between deposited Li dendrites and polyacrylic backbones and succinonitrile plasticizer. Due to the reaction induced volume change, large amounts of cracks form inside the Li dendrites with a stress corrosion-cracking behavior, indicating that Li0cannot be passivated in this SPE system. Based on this observation, we then introduce additive engineering leveraging on the knowledge of liquid electrolytes, and demonstrate that the Li 0 surface can be effectively protected against corrosion using fluoroethylene carbonate (FEC), leading to densely packed Li 0 domes with conformal and stable solid-electrolyte interphases (SEIs) films. Owing to the high room temperature ionic conductivity of 1.01 mS/cm -1 , the high transference number of 0.57 and the stabilized lithium electrolyte interface, this improved new SPE delivers an excellent lithium plating/stripping CE of 99% and 1800 hours of stable cycling in Li||Li symmetric cells (0.2 mA/cm -2 , 1mAh/cm -2 ). Furthermore, this improved cathodic stability along with the high anodic stability enables record high cycle life of >2000 cycles for Li||LiFePO 4 and >400 cycles for Li||LiCoO 2 full cells.

25 ENERGY STORAGE↗

Aqueous electrolyte solutions with anion-bridged secondary solvation sheaths for highly efficient zinc metal batteries

Aqueous zinc metal batteries are low-cost electrochemical devices suitable for safe grid energy storage. However, water decomposition and Zn dendrite formation detrimentally affect their coulombic efficiency. Conventional aqueous electrolyte solutions, with a concentration around 1 M, are cost-effective and exhibit high bulk ionic conductivity but cannot form a stable solid electrolyte interphase. Water-in-salt and aqueous-organic hybrid electrolyte solutions can form robust solid electrolyte interphases, but they are not kinetically efficient and cost-effective. Here, to circumvent these issues, we design variously concentrated aqueous electrolyte solutions using several salts with different donor numbers to extend anion coordination into the secondary solvation sheath. We show that salt-derived anions with donor number > 18 enter the Zn2+ first solvation sheath, and ensure a strong binding energy between the Zn2+(H2O)5-anion nanometric clusters and water molecules in the secondary solvation sheath. In particular, 2 M aqueous electrolyte solutions containing fluorinated anions exhibit bulk ionic conductivities of 26-35 mS cm−1 at 25 °C and form a ZnF2-rich solid electrolyte interphase. When tested in Zn||NaV3O8·1.5H2O Swagelok cells, the best-performing electrolyte solution enables an average coulombic efficiency of 99.99% for 1,000 cycles at 1.5 mA cm−2, corresponding to an initial specific energy of 130 Wh kg−1 (based on the combined weight of the positive and negative electrodes).

25 ENERGY STORAGE↗

Regulating electrodeposition morphology of lithium: towards commercially relevant secondary Li metal batteries

Lithium, the lightest and most electronegative metallic element, has long been considered the ultimate choice as a battery anode for mobile, as well as in some stationary applications. The high electronegativity of Li is, however, a double-edged sword—it facilitates a large operating voltage when paired with essentially any cathode, promising a high cell-level energy density. It is also synonymous with a high chemical reactivity and low reduction potential. The interfaces a Li metal anode forms with any other material (liquid or solid) in an electrochemical cell are therefore always mediated by one or more products of its chemical or electrochemical reactions with that material. The physical, crystallographic, mechanical, electrochemical, and transport properties of the resultant new material phases (interphases) regulate all interfacial processes at a Li metal anode, including electrodeposition during battery recharge. This Review takes recent efforts aimed at manipulating the structure, composition, and physical properties of the solid electrolyte interphase (SEI) formed on an Li anode as a point of departure to discuss the structural, electrokinetic, and electrochemical requirements for achieving high anode reversibility. An important conclusion is that while recent reports showing significant advances in the achievement of highly reversible Li anodes, e.g. as measured by the coulombic efficiency (CE), raise prospects for as significant progress towards commercially relevant Li metal batteries, the plateauing of achievable CE values to around 99 ± 0.5% apparent from a comprehensive analysis of the literature is problematic because CE values of at least 99.7%, and preferably >99.9% are required for Li metal cells to live up to the potential for higher energy density batteries offered by the Li metal anode. On this basis, we discuss promising approaches for creating purpose-built interphases on Li, as well as for fabricating advanced Li electrode architectures for regulating Li electrodeposition morphology and crystallinity. Considering the large number of physical and chemical factors involved in achieving fine control of Li electrodeposition, we believe that achievement of the remaining ~0.5% in anode reversibility will require fresh approaches, perhaps borrowed from other fields. We offer perspectives on both current and new strategies for achieving such Li anodes with the specific aim of engaging established contributors and newcomers to the field in the search for scalable solutions.

25 ENERGY STORAGE↗

Designing better electrolytes

Electrolytes and the associated interphases constitute the critical components to support the emerging battery chemistries that promise tantalizing energy but involve drastic phase and structure complications. Designing better electrolytes and interphases holds the key to the success of these batteries. As the only component that interfaces with every other component in the device, an electrolyte must satisfy multiple criteria simultaneously. These include transporting ions while insulating electrons between the electrodes and maintaining stability against electrodes of extreme chemical natures: the strongly oxidative cathode and the strongly reductive anode. In most advanced batteries, the two electrodes operate at potentials far beyond the thermodynamic stability limits of electrolytes, so the stability therein has to be realized kinetically through an interphase formed from the sacrificial reactions between electrolyte and electrodes.

Meng, Y. Shirley↗

Properties of GaN(SiC)-(Ti, Zr)B{sub x} contacts subjected to rapid thermal annealing

The effect of rapid thermal annealing on the structural and physical properties of Au-(Ti, Zr)B{sub x}-GaN(SiC) contacts and diode structures on their basis is investigated. The X-ray-diffraction investigations and the layer-by-layer Auger analysis showed that the phase composition and structure of the GaN and SiC contacts are retained to the temperatures as high as 900 and 1000 deg. C, respectively. The stability of interphase boundaries is confirmed by almost constant physical properties of contacts before and after the rapid thermal treatments. The Schottky-barrier height {phi}{sub b} amounts to 0.89-0.9 eV for the contacts with GaN and 0.79-0.83 eV for SiC; the ideality factor n of the I-V characteristic amounts to n = 1.2 for the Au-TiB{sub x}(ZrB{sub x})-n-GaN(SiC) contacts and n {approx} 1.12 for the Au-ZrB{sub x}-n-n{sup +}-4HSiC contacts. The structural investigations indicate that there are glass-forming boron and metal oxides at an interphase boundary, which form a thin amorphous vitreous layer resistant against rapid thermal annealing and represent the diffusion barrier for the interphase transport.

36 MATERIALS SCIENCE↗

Shape Effect in Layering of Solid Solutions in Small Volume: Bismuth–Antimony Alloy

The regularities of the effect of the shape of interphase boundaries in small volume systems on the separation of solutions with an upper critical solution temperature (UCST) are described by the example of Bi–Sb alloy particles with a core–shell configuration. The change in the shape of interphase boundaries is simulated in general by introducing a parameter corresponding to the degree of deviation of the shape of the boundaries from the spherical one. An analysis of the extrema of the Gibbs function revealed regularities in the effect of the shape of the core and shell phases on phase equilibria, the thermodynamic stability of heterogeneous states, and the phase separation diagram. The deviation of the shape of the interphase boundaries from the spherical shape changes the UCST and the mutual solubility of the components. The deformation of the shell of a core–shell particle increases the thermodynamic stability of the heterogeneous state, which contributes to the separation of the solution. The deformation of the core lowers the thermodynamic stability of the heterogeneous state and expands the range of metastable states.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Influence of Wetting and Mass Transfer Properties of Organic Chemical Mixtures in Vadose Zone Materials on Groundwater Contamination by Nonaqueous Phase Liquids

Previous studies have found that organic acids, organic bases, and detergent-like chemicals change surface wettability. The wastewater and NAPL mixtures discharged at the Hanford site contain such chemicals, and their proportions likely change over time due to reaction-facilitated aging. The specific objectives of this work were to (1) determine the effect of organic chemical mixtures on surface wettability, (2) determine the effect of organic chemical mixtures on CCl4 volatilization rates from NAPL, and (3) accurately determine the migration, entrapment, and volatilization of organic chemical mixtures. Five tasks were proposed to achieve the project objectives. These are to (1) prepare representative batches of fresh and aged NAPL-wastewater mixtures, (2) to measure interfacial tension, contact angle, and capillary pressure-saturation profiles for the same mixtures, (3) to measure interphase mass transfer rates for the same mixtures using micromodels, (4) to measure multiphase flow and interphase mass transfer in large flow cell experiments, all using the same mixtures, and (5) to modify the multiphase flow simulator STOMP in order to account for updated P-S and interphase mass transfer relationships, and to simulate the impact of CCl4 in the vadose zone on groundwater contamination. Results and findings from these tasks and summarized in the attached final report.

54 ENVIRONMENTAL SCIENCES↗

Chemical compatibility issues associated with use of SiC/SiC in advanced reactor concepts

Silicon carbide/silicon carbide (SiC/SiC) composites are of interest for components that will experience high radiation fields in the High Temperature Gas Cooled Reactor (HTGR), the Very High Temperature Reactor (VHTR), the Sodium Fast Reactor (SFR), or the Fluoride-cooled High-temperature Reactor (FHR). In all of the reactor systems considered, reactions of SiC/SiC composites with the constituents of the coolant determine suitability of materials of construction. The material of interest is nuclear grade SiC/SiC composites, which consist of a SiC matrix [high-purity, chemical vapor deposition (CVD) SiC or liquid phase-sintered SiC that is crystalline beta-phase SiC containing small amounts of alumina-yttria impurity], a pyrolytic carbon interphase, and somewhat impure yet crystalline beta-phase SiC fibers. The interphase and fiber components may or may not be exposed, at least initially, to the reactor coolant. The chemical compatibility of SiC/SiC composites in the three reactor environments is highly dependent on thermodynamic stability with the pure coolant, and on reactions with impurities present in the environment including any ingress of oxygen and moisture. In general, there is a dearth of information on the performance of SiC in these environments. While there is little to no excess Si present in the new SiC/SiC composites, the reaction of Si with O 2 cannot be ignored, especially for the FHR, in which environment the product, SiO 2 , can be readily removed by the fluoride salt. In all systems, reaction of the carbon interphase layer with oxygen is possible especially under abnormal conditions such as loss of coolant (resulting in increased temperature), and air and/ or steam ingress. A global outline of an approach to resolving SiC/SiC chemical compatibility concerns with the environments of the three reactors is presented along with ideas to quickly determine the baseline compatibility performance of SiC/SiC.

FHR↗

DC Electrical Conductivity of Silicon Carbide Ceramics and Composites for Flow Channel Insert Applications

High purity chemically vapor-deposited silicon carbide (SiC) and 2D continuous SiC fiber, chemically vapor-infiltrated SiC matrix composites with pyrocarbon interphases were examined for temperature dependent (RT to 800 C) electrical conductivity and the influence of neutron irradiation on it. In the 2D composites, trans-thickness electrical conductivity was dominated by bypass conduction via interphase network at relatively low temperatures, whereas conduction through SiC constituents dominated at higher temperatures. The Influence of neutron irradiation on electrical properties appeared very strong for SiC, resulting typically in by orders lower ambient conductivity and steeper temperature dependency. Through-thickness electrical conductivity of neutron-irradiated 2D SiC composites with thin PyC interphase will likely in the order of 10 S/m in the typical operating temperature range for flow channel inserts. Mechanisms of electrical conduction in the composites and irradiation-induced modification of electrical conductivity of the composites and their constituents are discussed.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Polysulfide-incompatible additive suppresses spatial reaction heterogeneity of Li-S batteries

Rational electrolyte engineering for practical pouch cells remains elusive because the correlation between the cathode/solid-electrolyte interphase layer and cell-level reaction behavior is poorly understood. Here, by combining multiscale characterization and computational modeling, we show that—counter to the conventional perception of polysulfide-incompatible additives—the spontaneous reaction of sparingly solvated polysulfides with Lewis acid additives (LAAs) can induce in situ formation of a homogeneous interphase on thick and tortuous S cathode. Multiscale synchrotron X-ray characterization consistently affirms that such interface design could effectively eliminate the notorious problems of polysulfide shuttle and lithium corrosion and, more importantly, provide an interconnected “ion transport highway” to alleviate the uneven ion transport within the tortuous S cathode. Hence, this design dramatically reduces the reaction heterogeneity of lithium-sulfur (Li-S) pouch cells under lean electrolyte conditions. Further, this work resolves controversy around the role of polysulfide-incompatible additives in high-energy Li-S pouch cells and highlights the importance of suppressing reaction heterogeneity for practical batteries.

36 MATERIALS SCIENCE↗

F and N Rich Solid Electrolyte for Stable All-Solid-State Battery

We report the instability of sulfide solid electrolytes to Li anode and high-voltage LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) cathodes limits the cyclic performance of all-solid-state lithium battery (ASSLB). Herein, the stability of Li 6 PS 5 Cl against Li anode is enhanced by mixing a small amount (0.32 wt%) of CuF 2 -LiNO 3 (CL) into Li 6 PS 5 Cl electrolyte layer to in-situ form a mixed-conductive-lithiophobic and self-healing LiF-Li 3 N-Cu solid electrolyte interphase (SEI) at Li 6 PS 5 Cl-CL/Li interface. The critical current density (CCD) of Li 6 PS 5 Cl-CuF 2 -LiNO 3 increases to 1.4 mA cm –2 /1.4 mAh cm –2 at room temperature, which is much higher than that of pristine Li 6 PS 5 Cl (0.4 mA cm –2 /0.4 mAh cm –2 ) even though mixing 0.32 wt% CL into Li 6 PS 5 Cl slightly reduces the ionic conductivity from 2.9 × 10 –3 to 1.5 × 10 –3 S cm –1 . The compatibility of Li 6 PS 5 Cl-CL electrolyte to single-crystalline NMC811 (S-NMC811) is further enhanced by adding a small amount (0.02 wt%) of AlF 3 into Li 6 PS 5 Cl-CL forming Li 6 PS 5 Cl-CuF 2- LiNO 3 -AlF 3 (Li 6 >PS 5 Cl-CLA) as a cathode electrolyte and by doing Cl – on S-NMC811 (Cl@S-NMC811) surface. The Cl@S-NMC811-Li 6 PS 5 Cl-CLA|Li 6 PS 5 Cl-CL|Li cells with areal capacity of 2.55 mAh cm -2 achieve a capacity retention of 69.4% after 100 cycles at 1C (1C = 200 mAh g -1 ). Adding a small amount of SEI and cathode/electrolyte interphase (CEI) former into the sulfide electrolytes with minimal reduction (48.3%) of ionic conductivity is an effective method to enhance the performance of ASSLB.

36 MATERIALS SCIENCE↗

Effects of Propylene Carbonate Content in CsPF 6 -Containing Electrolytes on the Enhanced Performances of Graphite Electrode for Lithium-Ion Batteries

The effects Of propylene carbonate (PC) content in CsPF6-containing electrolytes on the performances of graphite electrode in lithium half cells and in graphite parallel to LiNi0.80Co0.15Al0.05O2 (NCA) full cells are investigated. It is found that the performance of graphite electrode is significantly-affected by PC content in the CsPF6-containing electrolytes. An optimal PC content of 20% by weight in the solvent mixtures is identified. The enhanced electrochemical performance of graphite electrode can be attributed to the synergistic effects of the PC solvent and the Cs+ additive. The synergistic effects of Cs+ additive and appropriate amount of PC enable the formation of a robust, ultrathin, and compact solid electrolyte interphase (SEI) layer on the surface of graphite electrode, which is only permeable for desolvated Li+ ions and allows fast Li+ ion transport through it. Therefore, this SEI layer effectively suppresses the PC cointercalation and largely alleviates the Li dendrite formation on graphite electrode during lithiation even at relatively high current densities. The presence of low-melting-point PC solvent improves the sustainable operation of graphite parallel to NCA full cells under a wide temperature range. The fundamental findings also shed light On the importance of manipulating/maintaining the electrode/electrolyte interphasial stability in various energy-storage devices.

25 ENERGY STORAGE↗

Surprising Relationship between Silicon Anode Calendar Aging and Electrolyte Components in a Localized High-Concentration Electrolyte System

Although localized high-concentration electrolytes (LHCEs) have been shown to improve the calendar lifetime of silicon anodes, the roles of the electrolyte constituents in calendar aging are not well understood. Here, in this work, we utilize a voltage hold protocol and an LHCE with varying molar ratios of lithium bis(fluorosulfonyl)imide (LiFSI), tetramethylene sulfone (TMS), and 1,1,2,2-tetrafluoroethyl-2,2,3,3-tetrafluoropropyl ether (TTE) to probe the component roles during aging. Interestingly, the estimated calendar lifetime and irreversible lithium losses from the V-hold experiments are independent of the electrolyte formulations. Contrarily, the solid electrolyte interphase (SEI) composition depends on the electrolyte formulation. X-ray photoelectron spectroscopy shows that TMS-coordinated species decompose to form insoluble alkanes and lithium hydroxide (LiOH), while lithium fluoride (LiF) originates from the anion-coordination complex. The SEI composition does not appear to play a significant role in the silicon anode passivity, as measured by parasitic current, suggesting that the SEI-electrolyte interactions dictate the calendar aging mechanisms.