Search NASA⌕ Search

SEARCH · Search NASA

Results for “recrystallization”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 523 records · Page 29

Effect of microstructure on exfoliation corrosion resistance in an Al-Zn-Mg alloy

Highlights: • A quantitative method was proposed to characterize EXCO resistance. • The EXCO product lead to strain in ND and elongation in RD on nearby grains. • Recrystallized grains are more susceptible to EXCO than fibrous grains. • High fraction of high-angle grain boundaries reduces EXCO resistance. • High coverage ratio of η phases on high-angle grain boundaries reduces EXCO resistance. - Abstract: In this work, the effect of microstructure on exfoliation corrosion (EXCO) resistance in an Al-Zn-Mg alloy were investigated using standard EXCO test, together with detailed microstructural examinations mainly by scanning electron microscopy (SEM) and high-angle annular detector dark-field scanning transmission electron microscopy (HAADF-STEM). An EXCO product model was built based on morphologies of EXCO product on longitudinal section and cross section for further measurement and analysis. A quantitative characterization of EXCO resistance by measuring average thickness of EXCO product was conducted, showing average results of 6.94 μm, 10.21 μm and 18.14 μm, which are corresponding to EXCO ratings of P, EA and EB under ASTM G34 standard, respectively. It was concluded that recrystallization, high fraction of high-angle grain boundaries (HAGBs) and high coverage ratio of η phases on HAGBs reduced EXCO resistance.

36 MATERIALS SCIENCE↗

Effects of friction stir processing and minor Sc addition on the microstructure, mechanical properties, and damping capacity of 7055 Al alloy

Highlights: • Good mechanical and damping properties were obtained in the 7055 after FSP and Sc addition. • The strengthening and damping mechanisms of FSP 7055(-Sc) were analyzed. • FSP and Sc addition were found to be strategy of preparing 7xxx alloys with well damping and mechanical properties. - Abstract: This study investigated the effects of friction stir processing (FSP) and addition of 0.25% (mass ratio) Sc on the microstructure, mechanical properties, and damping capacity of AA 7055 alloy. Microstructure analyses revealed that a low tool rotation rate of 300 rpm effectively inhibited the grain coarsening in the recrystallization of the alloy during FSP. Sc addition prevented the coarsening of grains and precipitated η phase and the annihilation of dislocations in the FSP AA 7055 alloy. After being subjected to FSP at 300 rpm, the AA 7055 alloy containing Sc exhibited good mechanical and damping properties, which were mainly attributed to the fine recrystallized grain structure, fine precipitated η phase, and large number of nano-sized Al{sub 3}(Sc, Zr) particles located at the grain boundaries and dislocations. This work provides an effective strategy for preparing commercial Al alloys with excellent damping capacity and mechanical properties.

36 MATERIALS SCIENCE↗

Precipitation behavior of ωo phase and texture evolution of a forged Ti-45Al-8.5Nb-(W, B, Y) alloy during creep

Highlights: • The morphology of ω{sub o} and residual β{sub o} phases depends on creep temperature and stress. • Stress can increase the tendency of the α{sub 2} to ω{sub o} phase transformation. • The strength of the texture components depend on temperature and stress. • β{sub o}(ω{sub o}) precipitation retards the growth of recrystallized γ grains. • ω{sub o} precipitation resists and deflects the crack during the crack propagation. - Abstract: Creep rupture tests of the as-forged Ti-45Al-8.5Nb-(W,B,Y) alloy with a duplex microstructure were carried out at 750–850 °C and 130–300 MPa. An investigation was performed to study the effects of temperature and stress on the microstructure and texture evolution, as well as on the creep properties of the forged high Nb-containing TiAl alloy with a duplex microstructure. The results show that the stress exponent n = 2.8–3.3, and the creep activation energy values are in the range of 300–400 kJ/mol. After creep, a regular arrangement of ω{sub o} precipitations was observed in the β{sub o} region. The un-transformed β{sub o} phase, which remained in the ω{sub o} interval, was examined using high resolution transmission electron microscope (HRTEM). It is shown that the growth of ω{sub o} precipitations and the morphology of residual β{sub o} phases are related to the creep temperature and stress. Certain β{sub o} stabilizer elements, such as Nb, segregate into α{sub 2} plates and cause ω{sub o} precipitation during dissolution of α{sub 2} plates at high temperature. The interfacial structure between the ω{sub o} and α{sub 2} phases was studied in detail using HRTEM. Meanwhile, texture evolution and dynamic recrystallization of the γ phase were studied using electron backscatter diffraction (EBSD). Observations on the deformation structure also demonstrate that ω{sub o} precipitation acts as an obstacle inhibiting crack propagation and growth of the γ phase. The corresponding formation mechanism and possible effects on creep are discussed.

36 MATERIALS SCIENCE↗

Cold rolling texture evolution of TiB2 particle reinforced Al-based composites by Neutron Diffraction and EBSD analysis

Highlights: • Texture development of in-situ TiB{sub 2} particle reinforced Al matrix composites after cold rolling were characterized. • The sum of rolling texture volume fractions has been significantly reduced by the weak texture in particle deformation zone. • Recrystallization nuclei with the Cube and Rotated-Cube orientations were observed in the particle deformation zones. • Small TiB{sub 2} particles within Al grains kept the parallel relationship with surrounding matrix during the deformation. - Abstract: Texture development of particle-reinforced metal matrix materials (P-MMCs) has not been understood well, especially the effects of second-phase particles during the deformation. In this work, we have investigated the texture evolution of TiB{sub 2}/Al composites during cold rolling by Neutron Diffraction and EBSD analysis. Two forms of TiB{sub 2} particles influenced the texture evolution in different ways. The particle-clusters aggregated along grain boundaries led to a reduction of texture volume fraction; recrystallization nuclei with weak texture appeared around these particle-clusters. Small non-shearable TiB{sub 2} particles dispersed inside Al matrix contributed to strong Copper texture component at high strains; the individual particles rotated together with Al matrix during the deformation. These revealed effects of particles on the texture development in TiB{sub 2}/Al composites provide a reference for the texture control of P-MMCs.

36 MATERIALS SCIENCE↗

Effect of high content of manganese on microstructure, texture and mechanical properties of magnesium alloy

Highlights: • Extremely refined Mg-3.0Mn alloys are prepared by conventional extrusion process. • Mn addition can effectively weaken the basal texture of the alloys. • Strength, yield anisotropy and ductility have been obviously improved. - Abstract: In the present investigation, microstructure, texture and mechanical properties of Mg-3Mn alloys fabricated by hot extrusion process with the extrusion temperatures of 250 °C and 300 °C were investigated. The results revealed that the samples exhibited the refined microstructure and weakened basal texture. Refined microstructure of the samples was attributed to the dynamic precipitates suppressing the recrystallization grain growth during extrusion process. Weakened basal texture of the samples was explained as a result of particle stimulated nucleation (PSN) promoted by coarsened Mn precipitates altering the texture of extruded profiles during recrystallization by orienting the c-axis of grains at an angle that favors basal slip activity. As a result, the samples exhibited the high tensile elongation and good yield strength at room temperature.

36 MATERIALS SCIENCE↗

Microstructure evolution and mechanical properties of the compressively deformed AgInCd alloy during annealing treatment

Highlights: • The microstructure of AgInCd alloy during annealing treatment is investigated. • Nanoscale deformation twins are formed in the deformed AgInCd alloy. • Deformation twins are transformed into stacking faults by detwinning mechanism. • Annealing twins show higher thermal stability than deformation twins. - Abstract: The microstructure evolution and mechanical properties of the compressively deformed AgInCd alloy during annealing treatment have been investigated in the present study. In the deformed AgInCd alloy, many deformation markings are formed and these deformation markings are mainly composed of nanoscale deformation twins. The AgInCd alloy exhibits a significant work hardening capability because of the formation of deformation twins. The recrystallization temperature of the deformed AgInCd alloy is between 300 °C and 350 °C. In the AgInCd alloy annealed at 300 °C, the deformation twins are eliminated and a large number of dark strips consisting of stacking faults are presented in the un-recrystallized regions, indicating that the deformation twins are transformed into stacking faults by the detwinning mechanism. The annealing twins show higher thermal stability than the deformation twins. The strength and microhardness of the deformed AgInCd alloy gradually decrease with the increase of annealing temperature.

36 MATERIALS SCIENCE↗

Effect of non-axisymmetric arc on microstructure, texture and properties of variable polarity plasma arc welded 5A06 Al alloy

Highlights: • Variable polarity plasma arc welding of 5A06 Al alloy was carried out under the condition of non-axisymmetric arc. • Deformation bands formed in the weld joint were due to microstructural inhomogeneities. • Tensile fracture occurred along the deformation bands in the TZ/HAZ fusion boundary on the side of “lower arc”. • The weld zones are harder than the BM due to dislocation sub-structure, deformation bands and ultrafine subgrain. - Abstract: Microstructure, texture and mechanical properties in the weld joint of variable polarity plasma arc welding of 5A06 Al alloy under the condition of non-axisymmetric arc have been investigated. The weld joint are characterized by elongated structure in the base material (BM), the heat affected zone (HAZ) and the transition zone (TZ) and equiaxed structure in the fusion zone (FZ). Microstructure of the weld joint is asymmetrical and inhomogeneous leading to deformation bands. Deformation texture and recrystallization texture were developed in the weld zones. The FZ center was dynamic recrystallized due to severe deformation. Materials in the TZ have undergone dynamic recovery. The weld zones are harder than the BM due to dislocation sub-structure, deformation bands and ultrafine subgrains. Microhardness distribution was homogeneous in the regions without deformation bands. Tensile fracture occurred along the deformation bands on the side of “lower arc” exhibiting ductile fracture, while the BM is less ductile.

36 MATERIALS SCIENCE↗

Characterization of Alloy 600 joints exposed to a high-temperature supercritical-carbon dioxide environment

Highlights: • Diffusion-bond showed similar corrosion and carburization behavior as parent matrix. • Diffusion-bond line migrated due to the Cr-depletion induced recrystallization. • Alloy 182 fusion-weld showed larger weight gains with outer Mn-rich oxides. • The presence of SiO{sub 2} in chromia suppressed carburization at the oxide/matrix interface. • Despite larger weight gains, Alloy 182 fusion-weld showed negligible tensile property changes. - Abstract: Two types of Alloy 600 joints, such as diffusion-bonded joint and Alloy 182 fusion-weld, were exposed to supercritical-CO{sub 2} environment at 550 and 650 °C (20 MPa) for 1000 h. The diffusion-bond region showed similar oxidation characteristics as parent Alloy 600, but the migration of diffusion bond line below oxide layer was observed due to the Cr-depletion induced recrystallization. For Alloy 182 fusion-weld, outer Mn-rich oxides (Mn{sub 3}O{sub 4} and MnCr{sub 2}O{sub 4}) and a small amount of inner SiO{sub 2} mixed with chromia were formed due to high Mn and Si contents. The presence of SiO{sub 2} in chromia suppressed carburization at the oxide/matrix interface, which resulted in the formation of an amorphous C layer between the outer Mn-rich oxide and inner Cr-rich oxide. For Alloy 182 fusion-weld, tensile property changes after exposure to supercritical-CO{sub 2} environment were negligible.

36 MATERIALS SCIENCE↗

The effect of finish rolling temperature and tempering on the microstructure, mechanical properties and dislocation density of direct-quenched steel

Highlights: • The effect of thermomechanical treatment and tempering on direct-quenched steel has been studied. • Dislocation density of direct-quenched and tempered martensite is evaluated using both TEM and Williamson-Hall method. • Statistical analysis has been performed to study the effect of different factors on toughness of direct-quenched martensite. - Abstract: A unique batch tempering treatment for industrial scale direct-quenched steel coils has been studied using laboratory simulations. The tempering treatment was non-isothermal with slow heating to 570 °C and slow cooling to simulate the tempering of large steel coils. The paper presents the effect of finishing rolling temperature (FRT) relative to the non-recrystallization temperature (T{sub NR}) and the effect of long time tempering on the microstructure, dislocation density and mechanical properties of direct-quenched coiled strips. Conditioning austenite below the recrystallization stop temperature resulted in a finer effective grain size distribution, which correlated strongly with the impact toughness of the final product. Furthermore low finish rolling temperature resulted in partially ferritic microstructures while higher finishing rolling temperatures led to mixtures of bainite and martensite. Dislocation densities determined with TEM and XRD showed somewhat different trends regarding the effect of tempering: intra-lath dislocation density, as measured with TEM, showed a statistically significant drop in only one case, while XRD analysis indicated a drop in all cases. Furthermore, no significant correlation between finishing rolling temperature and dislocation density existed in XRD studies. The XRD results indicate that the decrease in dislocation density corresponds to about 100 MPa lower dislocation strengthening. However, precipitation hardening and potential internal micro stress relief compensates this as yield strength remains unchanged or even increases during tempering.

36 MATERIALS SCIENCE↗

High-temperature deformation behavior and microstructural characterization of high-Mn bearing titanium-based alloy

Highlights: • The hot deformation behavior of a biomedical low-cost Ti-10Mn alloys was studied. • The flow curves of the alloy display periodic serrations attributed to dynamic strain aging. • Mn alloying increases the activation energy to 243 kJ/mol compared to pure Ti. • The dynamic recovery is more effective than dynamic recrystallization at hot deformation. - Abstract: Ti-Mn alloys exhibit an excellent potential for biomedical applications as well as structural engineering applications, especially in the aerospace industry. In order to control and enhance grain structure during the manufacturing of Ti-Mn alloys and thereby help to enhance mechanical properties such as strength and toughness, we studied the hot-deformation behavior of βTi-10Mn alloys. Isothermal compression tests were conducted in the strain rate range of 0.01–10 s{sup −1} and temperatures in the range of 850–1000 °C using a Gleeble thermomechanical simulator. High-temperature flow stress curves exhibited discontinuous yielding and pronounced periodic serrations without any strain hardening during compression straining of these alloys. Such peculiar behavior of this alloy is due to active dynamic strain aging in its β-bcc structure. Metallographic observations by electron-backscattered diffraction (EBSD) analysis revealed that dynamic recovery (DRV) is more active than continuous dynamic recrystallization (CDRX) when the alloy is deformed at high strain rates, i.e. higher than 1 s{sup −1}. Furthermore, the constitutive behavior of the alloy was modeled and the apparent hot-deformation activation energy of the alloy was estimated to be 243 kJ/mol, which is ~60% higher than the self-diffusion energy in pure titanium.

36 MATERIALS SCIENCE↗

Optimization of hot workability and microstructure control in a 12Cr-10Ni precipitation hardenable stainless steel: An approach using processing maps

Highlights: • Deformation processing map was developed for a 12Cr10Ni precipitation hardenable martensitic stainless steel and optimized hot working parameters were suggested to obtain defect free products. • The ‘stable’ domain of the processing maps were correlated to the dynamic recrystallization in the austenite phase and further confirmed by detailed microstructural investigations. • The DRx domain showed a refinement of the martensite packet size and of the prior transformation austenite grain size, essential to obtain the desired mechanical properties. - Abstract: Optimization of hot working parameters and corresponding microstructure control were explored in a 12Cr-10Ni precipitation hardenable martensitic stainless steel. From hot compression tests, 1073–1373 K (800°–1100 °C) and five (0.001–10 s{sup −1}) different strain rates, processing maps were developed, and various domains of microstructure evolution (in the austenite phase) were identified. The stable domain of the processing maps appeared to indicate dynamic recrystallization (DRx) in the austenite phase: as evident by the appearance of inflection point in the strain hardening rate versus flow stress plots. The suspected DRx domain was further confirmed by detailed microstructural investigations of the respective water-quenched specimens. The DRx domain showed a refinement of the martensite packet size and of the prior transformation austenite grain size. The later was shown with optical microstructure and reconstructed (modelled) microtexture data of the prior austenite grains. Additionally, the DRx domain showed a significant difference in activation energy as estimated from appropriate constitutive modelling.

36 MATERIALS SCIENCE↗

Enhanced strength and toughness in ultra-fine grained 99.9% copper obtained by cryo-hydrostatic extrusion

Highlights: • Cryo-HE can increase the yield strength of Cu by more than threefold. • In cryo-HE of Cu, the grain refinement is stronger by 30% than in room-HE. • Cryo-HE with post-annealing effectively creates a bimodal microstructure in Cu. • Short-term post-annealing applied to cryo-HE-treated Cu can double its ductility. • Grain refinement with recrystallization results in a slight increase of Cu toughness. - Abstract: Ultrafine grained 99.9% Cu with enhanced strength and toughness was produced by hydrostatic extrusion conducted at the temperature of liquid nitrogen. The cryo-extruded Cu has a tensile yield strength of 490 MPa, hardness of 145 HV0.2, and tensile fracture toughness of 39.5 MPa m{sup 1/2}, which means that their values increased by 380%, 185% and ~10%, respectively, compared to those of the starting material. The significant strengthening is due to the strong grain refinement to 320 nm and the high energy of defects stored during the processing at liquid nitrogen temperature. The short term post deformation annealing doubles the ductility of material even by above 10% of the elongation to fracture at a slight expense of the yield strength (485 MPa). The observed behavior of Cu can be explained in terms of its low stacking fault energy, the susceptibility to dynamic recrystallization within the working zone of the extrusion die, and the triaxial strain components with the very large strain gradients, combined with the significant adiabatic heating effect active during the hydrostatic extrusion. The better homogeneity of the grain refinement and the higher efficiency of the distribution of defects and of the energy storage accompanied by the decreased dislocation mobility during the cryo hydrostatic extrusion contributed to the higher strength.

36 MATERIALS SCIENCE↗

Effect of niobium and phase transformation temperature on the microstructure and texture of a novel 0.40% C thermomechanically processed steel

Field emission scanning electron microscopy, electron backscatter diffraction (EBSD) and X-ray diffraction (XRD) have been employed to investigate the effect of niobium and phase transformation temperature on the evolution of microstructure and texture in a novel thermomechanically processed, medium‑carbon, low-alloy steel intended for slurry pipeline applications. Thermomechanical processing consisted of hot-rolling in the austenitic region with deformation both above the recrystallization limit temperature and below the recrystallization stop temperature. Immediately after rolling, specimens were directly quenched in water to two different temperatures of 560 °C and 420 °C and subsequently furnace cooled from those temperatures to simulate the cooling of coiled strip on a hot strip mill. The microstructure of samples quenched to 560 °C mostly comprised of upper bainite, whereas the samples quenched to 420 °C mainly consisted of lath-type lower bainite. The transformation texture of all samples at the mid-thickness position consisted of α, γ and ε-fibers with high intensities close to the transformed copper, transformed brass and rotated cube components. The addition of 0.013 wt% Nb refined the microstructure and sharpened the texture. The texture of the small fraction of retained austenite present in the final microstructures indicated that the main bcc texture components result from the brass and copper components in the parent austenite.

36 MATERIALS SCIENCE↗

Effect of annealing after strip casting on microstructure, precipitates and texture in non-oriented silicon steel produced by twin-roll strip casting

Highlights: • Non-oriented silicon steel with superior magnetic properties was produced by twin-roll strip casting. • The effect of annealing after strip casting on microstructure, precipitates and texture was investigated. • Role of precipitates in microstructure and texture evolution along the entire route was explored. • High magnetic induction and strong λ-fiber texture was obtained by optimizing strip annealing process. - Abstract: A 3.1 mm thick non-oriented Fe-1.0% Si steel as-cast strip was produced by twin-roll strip casting. Samples with/without strip annealing were cold rolled to 0.5 mm and then annealed. The development of microstructure, precipitate and texture was characterized along the entire processing route. It was found that annealing after strip casting had a minor influence on the average grain size and texture of the as-cast strip. A large number of particles precipitated and coarsened during the strip annealing process. Meanwhile, precipitates hindered dislocation slip and crystal rotation such that more significant in-grain shear bands were formed in cold rolled sheets. During recrystallization annealing process, the newly formed fine precipitates in directly cold-rolled sheets consumed stored strain energy and also hindered grain growth. But the initial precipitates in the annealed strip grew further and the effect of pinning of dislocations and grain boundary was lost. Therefore, annealed sheets with strip annealing process showed homogeneous equiaxed grains and the recrystallization texture was characterized by strong λ-fiber texture, which led to high permeability.

36 MATERIALS SCIENCE↗

Characteristics of martensite transformed from deformed austenite with various states of ultrahigh strength 300 M steel

Highlights: • Fractions of lath martensite and its packets decrease with the increasing of strain. • Length and width of blocks of lath martensite decrease with an increase in strain. • Severe work-hardening and completed DRX hamper transformation of lath martensite. • As for austenite with the state of work-hardening, the lath width changes little. • As for austenite with the state of DRX and subsequent growth, the lath width changes. - Abstract: 300 M steel was isothermally compressed on a Gleeble 1500 simulator at a deformation temperature of 1173 K, a strain rate of 0.1 s{sup −1} and strains ranging from 0.11 to 1.20. The morphologies and structure characteristics of martensite transformed from deformed austenite during water quenching were observed and analysed via scanning electron microscope and transmission electron microscope. Subsequently, effects of prior austenite state on martensitic transformation behavior of 300 M steel were analysed. The experimental results showed that predominant lath martensite and complemental twinned martensite and retained austenite coexisted in deformation-quenched 300 M steel at various strains. The volume fraction of lath martensite and packets of lath martensite decreased with the increasing of strain, and the length and width of the blocks in lath martensite concurrently decreased. Prior austenite with the state of severely work-hardening or just completed dynamic recrystallization would hamper the nucleation and subsequent growth of lath martensite. Additionally, as for austenite with the state of work-hardening, the morphologies and width of laths changed little with the increasing of strain, whereas dislocations in the interior of laths dramatically increased. However, as for austenite with the state of dynamic recrystallization and subsequent growth, the width of laths obviously increased with the increasing of austenite grain size.

36 MATERIALS SCIENCE↗

Characteristic constitution model and microstructure of an Al-3.5Cu-1.5Li alloy subjected to thermal deformation

The constitution model and microstructure of 2A97 Al-Li alloy during thermal deformation were investigated. The thermal deformation behavior was dominated by the interaction between work hardening and dynamic softening. The constitution model was constructed to predict the rheology behavior, in which Zener-Holloman equation with a fifth-order polynomial was set to describe the effect of various strains on the material parameters. Processing maps displayed to exist two unstable domains in microstructure (one domain with the temperature range from 300 °C to 370 °C and the strain rate range from 10{sup 0.5} s{sup −1} to 10s{sup −1}, and the other with the temperature range from 380 °C to 500 °C and the strain rate range from 0 s{sup −1} to 10 s{sup −1}). Microstructural characteristics of dynamic recovery (DRV) and dynamic recrystallization (DRX) in the stable domain and local rheology in the unstable domain were observed, respectively. The dynamic precipitation (DPN) of T{sub 1} phases and the interaction between dislocations and Al{sub 20}Cu{sub 2}Mn{sub 3} and Al{sub 3}Zr phases were concluded by high resolution transmission electron microscopy (HRTEM), which was the first experimental evidence for the DPN in 2A97 Al-Li alloy. All these confirmed the occurrence of the continuous dynamic recrystallization during thermal deformation.

36 MATERIALS SCIENCE↗

Abnormal grain growth induced by grain boundary segregation of yttrium in grain-oriented Fe-3%Si steel

Highlights: • The abnormal grain growth in Fe-3%Si was induced without precipitates by alloying of yttrium. • Grains grew abnormally to sizes exceeding 10 mm after secondary recrystallization. • Observations by the Laue diffraction method confirmed that the abnormally grown grains had the Goss orientation. The possibility of abnormal grain growth in grain-oriented Fe-3%Si steel by grain boundary segregation was investigated. Yttrium was selected to inhibit normal grain growth because its segregation at grain boundaries would efficiently reduce the grain boundary energy of iron, decreasing the driving force for grain growth. After secondary recrystallization, abnormal grain growth was successfully achieved without any precipitates. Observations by the Laue diffraction method confirmed that the abnormally grown grains had the Goss orientation.

36 MATERIALS SCIENCE↗

Effect of pre-cold rolling on the evolution of microstructure, microtexture, and mechanical properties of the mushy state rolled in-situ Al-4.5Cu-5TiB2 composite

Highlights: • Microstructure-Microtexture evolution study of the mushy state rolled composite (MRC) and MRC with pre-cold rolling (PCMRC). • The Microstructure and microtexture were characterized using SEM, EBSD, and TEM. • Exactly opposite trends in micro-hardness variation across the thickness of MRC and PCMRC were discussed. • The PCMRC exhibited the best combination of hardness, strength, and ductility. • A proper microstructure-microtexture-property correlation was established with experimental evidence. The mushy state rolling has been found as a promising technique for near-net forming of the cast Al-4.5 wt% Cu-5 wt% TiB{sub 2} in-situ composite to obtain microstructural refinement and moderate mechanical properties. Cold rolling with 30% reduction in thickness was carried out before mushy state rolling, for achieving a relatively more homogeneous distribution of CuAl{sub 2}-TiB{sub 2} particles as well as an appropriate microstructure to enhance the mechanical properties. A comparative investigation on the microstructural and microtextural evolution, along with mechanical properties of both the mushy state rolled composite (MRC) and pre-cold rolled mushy-state rolled composite (PCMRC) was performed, and the microstructure-property correlation was established. The PCMRC exhibited the lowest homogenized lengthscale parameter (L{sub H} 29 μm) indicating the maximum uniformity of particle distribution, computed with the help of multi-scalar analysis of area fractions (MSAAF) technique. Electron back-scattered diffraction (EBSD) and transmission electron microscopy (TEM) studies revealed the presence of fine sub-grains within centrally located deformed Al grains due to dynamic recovery, as well as the particle stimulated nucleation of equiaxed fine Al grains by dynamic recrystallization or rapid solidification of liquid near edges for both the investigated composites. The PCMRC displayed a superior combination of hardness (96.82 ± 4.5 HV{sub 5kgf}), 40% higher ultimate tensile strength (301.4 ± 1.8 MPa), and 68% more uniform elongation (30.8% ± 0.5%), compared to the MRC. The improvement in mechanical properties is attributed to the uniform particle distribution and presence of both higher density of low angle boundaries and recrystallized grains adjacent to the particles, obtained from prior cold rolling.

36 MATERIALS SCIENCE↗