Search NASA⌕ Search

SEARCH · Search NASA

Results for “ALS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

Experimental study of the A(e,e'{pi}{sup +}) reaction on {sup 1}H, {sup 2}H, {sup 12}C, {sup 27}Al, {sup 63}Cu and {sup 197}Au.

Cross sections for the {sup 1}H(e,e'{pi}{sup +})n process on {sup 1}H, {sup 2}H, {sup 12}C, {sup 27}Al, {sup 63}Cu, and {sup 197}Au targets were measured at the Thomas Jefferson National Accelerator Facility (Jefferson Lab) to extract nuclear transparencies. Data were taken from Q{sup 2}=1.1-4.7 GeV{sup 2} for a fixed center-of-mass energy of W=2.14 GeV. The ratio of {sigma}{sub L} and {sigma}{sub T} was extracted from the measured cross sections for {sup 1}H, {sup 2}H, {sup 12}C, and {sup 63}Cu targets at Q{sup 2}=2.15 and 4.0 GeV{sup 2}, allowing for additional studies of the reaction mechanism. In this article, we present the experimental setup and the analysis of the data in detail, including systematic uncertainty studies. Differential cross sections and nuclear transparencies as a function of the pion momentum at different values of Q{sup 2} are presented. Our results are consistent with the predicted early onset of color transparency in mesons. Global features of the data are discussed and the data are compared with model calculations for the {sup 1}H(e,e'{pi}{sup +})n reaction from nuclear targets.

43 PARTICLE ACCELERATORS↗

Cross sections for monitor reactions {sup 27}Al((p, x){sup 24}Na, {sup 27}Al(p, x){sup 22}Na, and {sup 27}Al(p, x){sup 7}Be at proton energies in the range 0.04-2.6 GeV

The cross sections for the monitor reactions {sup 27}Al(p, x){sup 24}Na, {sup 27}Al(p, x){sup 22}Na, and {sup 27}Al(p, x){sup 7}Be at 12 proton energies, 2605, 1598, 1199, 799, 600, 400, 249, 147.6, 97.2, 66.0, 44.6, and 40.8 MeV, have been determined with 72 Multiplication-Sign 72-mm square and 10.5-mm-diameter round aluminum foils. The rates of the reactions of the production of {sup 24}Na, {sup 22}Na, and {sup 7}Be in the foils in each irradiation run have been determined by {gamma} spectrometry, whereas the number of protons transmitted through these foils has been determined using calibrated fast current transformers. The cross sections have been determined as the ratios of the corresponding reaction to the average proton fluence.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

Synthesis and structural characterization of the Zintl phases Na{sub 3}Ca{sub 3}TrPn{sub 4}, Na{sub 3}Sr{sub 3}TrPn{sub 4}, and Na{sub 3}Eu{sub 3}TrPn{sub 4} (Tr=Al, Ga, In; Pn=P, As, Sb)

15 new quaternary Zintl phases have been synthesized by solid-state reactions from the respective elements, and their structures have been determined by single-crystal X-ray diffraction. Na{sub 3}E{sub 3}TrPn{sub 4} (E=Ca, Sr, Eu; Tr=Al, Ga, In; Pn=P, As, Sb) crystallize in the hexagonal crystal system with the non-centrosymmetric space group P6{sub 3}mc (No. 186). The structure represents a variant of the K{sub 6}HgS{sub 4} structure type (Pearson index hP22) and features [TrPn{sub 4}]{sup 9–} tetrahedral units, surrounded by Na{sup +} and Ca{sup 2+}, Sr{sup 2+}, Eu{sup 2+} cations. The nominal formula rationalization [Na{sup +}]{sub 3}[E{sup 2+}]{sub 3}[TrPn{sub 4}]{sup 9–} follows the octet rule, suggesting closed-shell configurations for all atoms and intrinsic semiconducting behavior. However, structure refinements for several members hint at disorder and mixing of cations that potentially counteract the optimal valence electron count. - Graphical abstract: The hexagonal, non-centrosymmetric structure of Na{sub 3}E{sub 3}TrPn{sub 4} (E=Ca, Sr, Eu; Tr=Al, Ga, In; Pn=P, As, Sb) features [TrPn{sub 4}]{sup 9–} tetrahedral units, surrounded by Na{sup +} and Ca{sup 2+}, Sr{sup 2+}, Eu{sup 2+} cations. - Highlights: • 15 quaternary phosphides, arsenides, and antimonides are synthesized and structurally characterized. • The structure is a variant of the hexagonal K{sub 6}HgS{sub 4}-type, with distinctive pattern for the cations. • Occupational and/or positional disorder of yet unknown origin exists for some members of the series.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Microstructure and mechanical properties of a novel rapidly solidified, high-temperature Al-alloy

Rapid solidification (RS) processing, as a production method, offers a variety of unique properties based on far-from-equilibrium microstructures obtained through rapid cooling rates. In this study, we seek to investigate the microstructures and properties of a novel Al-alloy specifically designed for high temperature mechanical stability. Synthesis of, AlFe{sub 11.4}Si{sub 1.8}V{sub 1.6}Mn{sub 0.9} (wt.%), was performed by two approaches: rotating cup atomization (“shot”) and melt spinning (“flake”). These methods were chosen because of their ability to produce alloys with tailored microstructures due to their inherent differences in cooling rate. The as-solidified precursor materials were microstructurally characterized with electron microscopy. The results show that the higher cooling rate flake material exhibited the formation of nanocrystalline regions as well additional phase morphologies not seen in the shot material. Secondary dendritic branching in the flake material was on the order of 0.1–0.25 μm whereas branching in the shot material was 0.5–1.0 μm. Consolidated and extruded material from both precursor materials was mechanically evaluated at both ambient and high (300 °C) temperature. The consolidated RS flake material is shown to exhibit higher strengths than the shot material. The ultimate tensile strength of the melt spun flake was reported as 544.2 MPa at room temperature and 298.0 MPa at 300 °C. These results forecast the ability to design alloys and processing approaches with unique non-equilibrium microstructures with robust mechanical properties at elevated temperatures. - Highlights: • A novel alloy, AlFe{sub 11.4}Si{sub 1.8}V{sub 1.6}Mn{sub 0.9} was fabricated by rapid solidification. • Room temperature yield strength exceeded 500 MPa. • Elevated temperature (300 °C) yield strength exceeded 275 MPa. • Forging, after extrusion of the alloy resulted in microstructural coarsening. • Decreased strength and ductility was identified as a result of forging.

36 MATERIALS SCIENCE↗

Influence of soluble oligomeric aluminum on precipitation in the Al-KOH-H2O system

The role of oligomeric aluminate (Al(OH)4-) species in the precipitation of aluminum phases such as gibbsite (a-Al(OH)3) from aqueous hydroxide solutions remains unclear and difficult to probe directly, despite its importance to developing accurate predictions of Al solubility in highly alkaline systems. Precipitation in this system entails a transition from predominantly tetrahedrally coordinated Al species in solution to octahedrally coordinated Al in gibbsite. Here we report a quantitative study of dissolved Al in the Al-KOH-H2O system using a combination of molecular spectroscopies. We established a relationship between changes in 27Al NMR chemical shifts and the relative intensity of Raman vibrational bands, indicative of variations in the ensemble speciation of Al in solution, and the formation of unique contact ion pair interactions with the aluminate dimer, Al2O(OH)62 . A strong correlation between the extent of Al oligomerization and the amount of solvated Al was demonstrated by systematically varying the KOH:Al molar ratio. The concentration of dissolved oligomeric Al in solution also directly impacted the particle size and morphology of gibbsite; high concentrations of dimeric Al2O(OH)62-, yielded smaller and more numerous anhedral to subhedral gibbsite particles, while low concentrations yielded fewer and larger euhedral gibbsite platelets. The collective observations suggest a key role of the Al2O(OH)62- dimer in promoting gibbsite precipitation from solution, where the potassium ion-paired dimer possibly catalyzes a more rapid transformation of Al coordination from tetrahedral in solution to octahedral in gibbsite.

Dembowski, Mateusz↗

Assessment of phase constitution on the Al-rich region of rapidly solidified Al-Co-Fe-Cr alloys

The formation of quasicrystalline approximants in rapidly solidified Al-Co-Fe-Cr alloys was investigated. Alloys of atomic composition Al{sub 71}Co{sub 13}Fe{sub 8}Cr{sub 8}, Al{sub 77}Co{sub 11}Fe{sub 6}Cr{sub 6} and Al{sub 76}Co{sub 19}Fe{sub 4}Cr{sub 1} were produced using melt spinning and arc melting methods and their microstructural characterization was carried out by X-ray diffraction, scanning electron microscopy and transmission electron microscopy. Up to the present there is no consensus in the literature regarding the formation of quasicrystalline phase or quasicrystalline approximants in the Al{sub 71}Co{sub 13}Fe{sub 8}Cr{sub 8} alloy. This work presents, for the first time, a detailed structural characterization of selected alloys in the Al-Co-Fe-Cr system close to the atomic composition Al{sub 71}Co{sub 13}Fe{sub 8}Cr{sub 8}. The results indicated the samples to be composed, mostly, by two intermetallic phases, which are quaternary extensions of Al{sub 5}Co{sub 2} and Al{sub 13}Co{sub 4} and are quasicrystalline approximants. Although the Al{sub 5}Co{sub 2} phase has already been reported in the Al{sub 71}Co{sub 13}Fe{sub 8}Cr{sub 8} alloy, the presence of the monoclinic Al{sub 13}Co{sub 4} is now identified for the first time in the as cast state. In the binary Al-Co system a quasicrystalline phase is known to form in a rapidly solidified alloy with composition close to the monoclinic and orthorhombic Al{sub 13}Co{sub 4} phases. This binary quasicrystalline phase presents an average valence electron per atom (e/a) between 1.7 and 1.9; thus, in addition to the Al{sub 71}Co{sub 13}Fe{sub 8}Cr{sub 8} alloy, the compositions Al{sub 77}Co{sub 11}Fe{sub 6}Cr{sub 6} and Al{sub 76}Co{sub 19}Fe{sub 4}Cr{sub 1} were chosen to be within the region of formation of the quaternary extension of the Al{sub 13}Co{sub 4} phase and also within the (e/a) of 1.7 to 1.9. However, no quasicrystalline phase is present in any of the studied alloys. The Al-Co-Fe-Cr system, around the compositions studied, is composed of quaternary extensions of Al-Co intermetallic phases, which present solubility of Fe and Cr at Co atomic sites. - Highlights: •The Al rich region of the AlCoFeCr system is studied concerning phase formation on rapidly solidified alloys. •The alloys were composed mostly by quaternary extensions of Al-Co intermetallic phases. •Al{sub 5}Co{sub 2} and Al{sub 13}Co{sub 4} were the major phases observed in the alloys and are approximants of a quasicrystalline phase. •No quasicrystalline phase was observed in the Al{sub 71}Co{sub 13}Fe{sub 8}Cr{sub 8} composition.

36 MATERIALS SCIENCE↗

Spectra of surface plasmon polariton enhanced electroluminescence from electroformed Al-Al{sub 2}O{sub 3}-Ag diodes

Narrow band-pass filters have been used to measure the spectral distribution of electroluminescent photons with energies between 1.8 eV and 3.0 eV from electroformed Al-Al{sub 2}O{sub 3}-Ag diodes with anodic Al{sub 2}O{sub 3} thicknesses between 12 nm and 18 nm. Electroforming of metal-insulator-metal (MIM) diodes is a non-destructive dielectric breakdown that results in a conducting channel in the insulator and changes the initial high resistance of the MIM diode to a low resistance state. It is a critical step in the development of resistive-switching memories that utilize MIM diodes as the active element. Electroforming of Al-Al{sub 2}O{sub 3}-Ag diodes in vacuum results in voltage-controlled negative resistance (VCNR) in the current-voltage (I-V) characteristics. Electroluminescence (EL) and electron emission into vacuum (EM) develop simultaneously with the current increase that results in VCNR in the I-V characteristics. EL is due to recombination of electrons injected at the Al-Al{sub 2}O{sub 3} interface with radiative defect centers in Al{sub 2}O{sub 3}. Measurements of EL photons between 1.8 eV and 3.0 eV using a wide band-pass filter showed that EL intensity is exponentially dependent on Al{sub 2}O{sub 3} thickness for Al-Al{sub 2}O{sub 3}-Ag diodes between 12 nm and 20 nm thick. Enhanced El intensity in the thinnest diodes is attributed to an increase in the spontaneous emission rate of recombination centers due to high electromagnetic fields generated in Al{sub 2}O{sub 3} when EL photons interact with electrons in Ag or Al to form surface plasmon polaritons at the Al{sub 2}O{sub 3}-Ag or Al{sub 2}O{sub 3}-Al interface. El intensity is a maximum at 2.0–2.2 eV for Al-Al{sub 2}O{sub 3}-Ag diodes with Al{sub 2}O{sub 3} thicknesses between 12 nm and 18 nm. EL in diodes with 12 nm or 14 nm of Al{sub 2}O{sub 3} is enhanced by factors of 8–10 over EL from a diode with 18 nm of Al{sub 2}O{sub 3}. The extent of EL enhancement in the thinnest diodes can vary significantly between samples. A narrow band of recombination centers was found in one Al-Al{sub 2}O{sub 3}-Ag diode with 12 nm of Al{sub 2}O{sub 3}; it had EL intensity 100 times greater at 2.15 eV than the diode with 18 nm of Al{sub 2}O{sub 3}. EL intensity for photons with energies greater than 2.6 eV is nearly the same for all diodes.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Formation Mechanism of Al{sub 2}O{sub 3}-Containing Inclusions in Al-Deoxidized Spring Steel

The source, characteristics, and mechanism of Al{sub 2}O{sub 3}-containing inclusions in Al-deoxidized spring steel were investigated using electron-probe X-ray microanalysis (EPMA). Spring samples were collected during vacuum degassing (VD) refining, in a tundish ladle, and after hot rolling, respectively. Based on primary inclusion components, seven types of inclusions were observed through the manufacturing process: Al{sub 2}O{sub 3}, Al{sub 2}O{sub 3}-SiO{sub 2}, Al{sub 2}O{sub 3}-CaO, Al{sub 2}O{sub 3}-MgO, Al{sub 2}O{sub 3}-MgO-CaO, Al{sub 2}O{sub 3}-SiO{sub 2}-MnO, and Al{sub 2}O{sub 3}-SiO{sub 2}-CaO. The Al{sub 2}O{sub 3} and Al{sub 2}O{sub 3}-SiO{sub 2} inclusions were mainly attributed to deoxidization products, less than 15 μm in diameter and with liquidus temperatures exceeding 1600 °C. For Al{sub 2}O{sub 3}-CaO inclusions, which were considered to be formed by the reduction of entrapped slag by Al dissolved in the steel, the Al{sub 2}O{sub 3}/CaO ratio obviously decreased with the increase of inclusion sizes. Most Al{sub 2}O{sub 3}-SiO{sub 2}-CaO inclusions were less than 15 μm in diameter, with their composition close to that of the refining slag and a liquidus temperature near 1500 °C. The Al{sub 2}O{sub 3}-MgO and Al{sub 2}O{sub 3}-SiO{sub 2}-MnO inclusions originated from inherent reactions between dissolved [Al], [Si], [Mn], [Mg], and [O] in the steel. Al{sub 2}O{sub 3}-MgO-CaO inclusions resulted from coalescence between Al{sub 2}O{sub 3}-MgO and Al{sub 2}O{sub 3}-CaO inclusions.

36 MATERIALS SCIENCE↗

Correlative characterization of primary Al{sub 3}(Sc,Zr) phase in an Al–Zn–Mg based alloy

Three-dimensional electron backscatter diffraction, focused ion beam, transmission electron microscopy and energy filtered transmission electron microscopy were employed to investigate the structural information of primary Al{sub 3}(Sc,Zr) phase, i.e. size, shape, element distribution and orientation relationship with the α-Al matrix. It was found that (i) most primary Al{sub 3}(Sc,Zr) phases have a cubic three-dimensional morphology, with a size of about 6–10 μm, (ii) most primary Al{sub 3}(Sc,Zr) phases are located within the α-Al matrix, and exhibit a cube to cube orientation relationship with the α-Al matrix, and (iii) a layer by layer growth was observed within primary Al{sub 3}(Sc,Zr) phases. Al, Cu, Si and Fe are enriched in the α-Al matrix between the layers of cellular eutectic Al{sub 3}(Sc,Zr) phase, while Sc, Ti and Zr are enriched in small Al{sub 3}(Sc,Zr) phases. A peritectic reaction and subsequent eutectic reaction between Al{sub 3}Sc and Al was proposed to interpret the observed layer by layer growth. This paper demonstrates that the presence of impurities (Fe, Si, Cu, Ti) in the diffusion field surrounding the growing Al{sub 3}(Sc,Zr) particle enhances the heterogeneous nucleation of Al{sub 3}(Sc,Zr) phases. - Highlights: • Most fine cubic primary Al{sub 3}(Sc,Zr) phases were observed within the α-Al matrix. • A layer by layer growth within primary Al{sub 3}(Sc,Zr) phase was observed. • A peritectic and subsequent eutectic reaction between Al{sub 3}Sc and Al was proposed. • Impurities in diffusion fields enhance heterogeneous nucleation of Al{sub 3}(Sc,Zr)

36 MATERIALS SCIENCE↗

Crystal-chemistry of mullite-type aluminoborates Al{sub 18}B{sub 4}O{sub 33} and Al{sub 5}BO{sub 9}: A stoichiometry puzzle

Orthorhombic Al{sub 2}O{sub 3}-rich aluminoborate is an important ceramic material for which two slightly different compositions have been assumed: Al{sub 5}BO{sub 9} (5Al{sub 2}O{sub 3}:B{sub 2}O{sub 3}) and Al{sub 18}B{sub 4}O{sub 33} (9Al{sub 2}O{sub 3}:2B{sub 2}O{sub 3}). The formula Al{sub 18}B{sub 4}O{sub 33} (=Al{sub 4.91}B{sub 1.09}O{sub 9}) was derived from results of chemical analyses when crystal structure data were not yet available. Subsequent structural investigations indicated Al{sub 5}BO{sub 9} composition. Nevertheless, Al{sub 18}B{sub 4}O{sub 33} was still accepted as the correct stoichiometry assuming that additional B replaces 9% Al. Powder samples of both compositions and ones with excess boron were prepared by solid state reactions between {alpha}-Al{sub 2}O{sub 3} and B{sub 2}O{sub 3}/H{sub 3}BO{sub 3} at temperatures above 1100 {sup o}C and single-crystals were grown from flux at 1100 and 1550 {sup o}C. Products were investigated by single-crystal and powder XRD, {sup 11}B and {sup 27}Al solid-state MAS-NMR, Raman and FTIR spectroscopy as well as Laser-ablation ICP-MS. No indication of the predicted 9% B{yields}Al substitution was found. LA ICP-MS indicated 12.36(27) wt% B{sub 2}O{sub 3} corresponding to Al{sub 4.97}B{sub 1.03}O{sub 9}. Hence, the suggested Al{sub 18}B{sub 4}O{sub 33} stoichiometry can be excluded for all synthesized samples. A very low amount of Al vacancies at a five-fold coordinated site are likely, charge balanced by an additional nearby three-fold coordinated B site. All evidences indicate that the title compound should be reported as Al{sub 5-x}B{sub 1+x}O{sub 9} with x<0.038(6), which is close to Al{sub 5}BO{sub 9}. -- Graphical abstract: A chemical composition of Al{sub 18}B{sub 4}O{sub 33}=Al{sub 4.91}B{sub 1.09}O{sub 9}=9Al{sub 2}O{sub 3}:2B{sub 2}O{sub 3} has been assumed for mullite-type aluminoborate with Al{sub 5}BO{sub 9} structure. However, samples prepared by different routes showed compositions close to 5Al{sub 2}O{sub 3}:B{sub 2}O{sub 3}. Display Omitted

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Aluminium distribution in ZSM-5 revisited: The role of Al-Al interactions

We present a theoretical study of the distribution of Al atoms in zeolite ZSM-5 with Si/Al=47, where we focus on the role of Al-Al interactions rather than on the energetics of Al/Si substitutions at individual sites. Using interatomic potential methods, we evaluate the energies of the full set of symmetrically independent configurations of Al siting in a Si{sub 94}Al{sub 2}O{sub 192} cell. The equilibrium Al distribution is determined by the interplay of two factors: the energetics of the Al/Si substitution at an individual site, which tends to populate particular T sites (e.g., the T14 site), and the Al-Al interaction, which at this Si/Al maximises Al-Al distances in general agreement with Dempsey's rule. However, it is found that the interaction energy changes approximately as the inverse of the square of the distance between the two Al atoms, rather than the inverse of the distance expected if this were merely charge repulsion. Moreover, we find that the anisotropic nature of the framework density plays an important role in determining the magnitude of the interactions, which are not simply dependent on Al-Al distances. - Graphical abstract: Role of Al-Al interactions in high silica ZSM-5 is shown to be anisotropic in nature and not dependent solely on Coulombic interactions. Highlights: Black-Right-Pointing-Pointer Si-Al distribution in ZSM-5 is revisited, stressing the role of the Al-Al interaction. Black-Right-Pointing-Pointer Coulomb interactions are not the key factors controlling the Al siting. Black-Right-Pointing-Pointer Anisotropy of the framework is identified as a source of departure from Dempsey's rule.

36 MATERIALS SCIENCE↗

Structure of oxides prepared by decomposition of layered double Mg–Al and Ni–Al hydroxides

Abstracts: Thermal decomposition of Mg–Al and Ni–Al layered double hydroxides LDH at temperatures lower than 800 °C leads to the formation of oxides with different structures. Mg–Al oxide has a very defective structure and consists of octahedral layers as in periclase MgO and mixed octahedral–tetrahedral layers as in spinel MgAl{sub 2}O{sub 4}. Mixed Ni–Al oxide has a sandwich-like structure, consisting of a core with Al-doped NiO-like structure and some surface layers with spinel NiAl{sub 2}O{sub 4} structure epitaxial connected with the core. Suggested models were verified by simulation of X-ray diffraction patterns using DIFFaX code, as well as HRTEM, IR-, UV-spectroscopies, and XPS. - Graphical abstract: In the Mg–Al layered double hydroxide Al{sup 3+} ions migrate into interlayers during decomposition. The Mg–Al oxide represents sequence of octahedral and octahedral–tetrahedral spinel layers with vacancies. The Ni–Al oxide has a sandwich-like structure with NiO-like core and surface spinel layers as a result of migration of Al{sup 3+} ions on the surface. The models explain the presence and absence of “memory effect” for the Mg–Al and Ni–Al oxides, respectively. - Highlights: • We study products of Mg(Ni)–Al LDH decomposition by calcination at 500(400)–800 °C. • In Mg–Al/Ni–Al LDH Al ions migrate into interlayers/on the surface during decomposition. • Mg–Al oxide represents sequence of periclase- and spinel-like layers with vacancies. • Ni–Al oxide has a sandwich-like structure with NiO-like core and surface spinel layers. • The models explain the presence/absence of “memory effect” for Mg–Al/Ni–Al oxides.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Structural and compositional evolution of Al{sub 3}(Zr,Y) precipitates in Al-Zr-Y alloy

Structural and compositional evolution of Al{sub 3}(Zr,Y) precipitates in aged Al-Zr-Y alloy was investigated through atom probe tomography (APT) and transmission electron microscope (TEM) analysis and first principles calculations. The results show that short-bar-shaped D0{sub 19}-Al{sub 3}Y with some Zr atoms dissolved in precipitated at the very beginning of decomposition and worked as heterogeneous nuclei for L1{sub 2}-Al{sub 3}Zr with spherical morphology after being aged at 400 °C for 2 h. Quasi-static coarsening happened as the aging treatment lasted from 2 h to 200 h. However, distribution of Zr and Y atoms in Al{sub 3}(Zr,Y) is nearly uniform and Al{sub 3}(Zr,Y) do not have the typical “Al{sub 3}RE core-Al{sub 3}Zr shell” structure which observed in other RE containing Al-Zr-RE alloys with L1{sub 2}-Al{sub 3}RE as nuclei. First principles calculations revealed that binding energy between Y and Zr is strong during the growth of Al{sub 3}(Zr,Y), which led to the co-precipitation of Y and Zr atoms and attribute to the evolution of Al{sub 3}(Zr,Y). - Highlights: •Al{sub 3}Y precipitated firstly and then became nuclei for Al{sub 3}Zr during aging of Al-Zr-Y. •Al{sub 3}(Zr,Y) precipitates do not have the typical “Al{sub 3}Y core-Al{sub 3}Zr shell” structure. •Strong binding between Y and Zr led to the co-precipitation of Y and Zr atoms.

36 MATERIALS SCIENCE↗

First-principles investigation of thermodynamic, elastic and electronic properties of Al{sub 3}V and Al{sub 3}Nb intermetallics under pressures

The thermodynamic, elastic, and electronic properties of D0{sub 22}-type Al{sub 3}V and Al{sub 3}Nb intermetallics were studied using the first-principle method. The results showed the pressure has profound effects on the structural, mechanical and electronic properties in both Al{sub 3}V and Al{sub 3}Nb. Thermodynamically, the formation enthalpies for Al{sub 3}V and Al{sub 3}Nb were derived, which agreed well with available experimental and theoretical values. Comparably, Al{sub 3}Nb was a more stable phase with the more negative H{sub f} than Al{sub 3}V. Mechanically, the calculated elastic constants showed linearly increasing tendencies, and satisfied the Born's criteria from 0–20 GPa, indicating the mechanically stability of Al{sub 3}V and Al{sub 3}Nb under this pressure range. Further, the mechanical parameters (i.e., bulk modulus (B), shear modulus (G), and Young's modulus (E)) were derived using the Voigt-Reuss-Hill (VRH) method, and in good agreement with available experimental results at the ground state. All these parameters presented the linearly increasing dependences on the external pressure. The B/G ratios and Poisson's ratio indicated that the Al{sub 3}V and Al{sub 3}Nb crystals should exhibit brittle behavior at 0–20 GPa. Additionally, the bulk modulus can be obtained through fitting the Birch-Murnaghan equation (B{sub 0}), computing by VRH method (B{sub H}), and deriving from the elastic theory (B{sub relax}) in both intermetallics. The uniformity of these calculated bulk moduli in each compound exhibited the excellent reliability and self-consistency. In addition, Debye temperature was estimated from the average sound velocity. The Debye temperature showed an increasing dependence on the pressures. Finally, through density of states analysis, Al{sub 3}V and Al{sub 3}Nb were suggested to possess naturally metallic behavior. Under pressures, it was noted that the shapes of peaks and pseudogaps exhibited relative few changes, suggesting Al{sub 3}V and Al{sub 3}Nb has kept structurally stable up to 20 GPa. At zero pressure, Al{sub 3}Nb was considered as a more structurally stable phase with the more number of bonding electrons per atom than Al{sub 3}V. This conclusion was in consistent with the one drawn from the thermodynamic analysis.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

First-principles analysis of the Al-rich corner of Al-Li-Cu phase diagram

The phase diagram of Al-Li-Cu system in the Al-rich region was determined by means of first-principles calculations and statistical mechanics. The mixing enthalpies of many configurations for different lattices in the whole Al-Li-Cu system were determined by density functional theory simulations to find the stable phases in the convex hull. They were fitted with a cluster expansion to calculate the free energy of the configurations with different compositions as a function of temperature in the Al-rich region (Al content > 40 at.%) by means of Monte Carlo simulations. It was found that the ground state phases in the Al-rich part of the Al-Li-Cu phase diagram were α-Al, θ' (Al 2 Cu), $δ$' (Al 3 Li), $δ$ (AlLi) and T 1 (Al 6 Cu 4 Li 3 ), while θ'' (Al 3 Cu), T 1' (Al 2 CuLi) and Al 3 Cu 2 Li were found on the lowest mixing enthalpy surfaces of their lattices and were metastable. α-Al, $δ$ and T 1 are stable phases in the whole temperature range while $δ$' becomes metastable at very low temperature and θ (Al 2 Cu) replaces θ' as the stable phase at approximately 550 K due to the vibrational entropic contribution. In addition, the phase diagram in the Al-rich region was built and it was shown in isothermal sections from 100 to 900 K. They were in good agreement with the limited experimental data in the literature and provided new information regarding the stability, solubility and stoichiometry of the different phases. This information is important to understand the precipitation mechanisms during high temperature aging.

36 MATERIALS SCIENCE↗

On the high-temperature stability of the Al 8 Cu 3 Ce intermetallic in an additively manufactured Al-Cu-Ce-Zr alloy

High-temperature resistant eutectic Al alloys are crucial materials for lightweight and energy efficient design in the automotive and aviation industries. Additive manufacturing offers a pathway to refine eutectic microstructures and develop novel alloys with superior high-temperature strength. High-volume fraction intermetallic Al-Cu-Ce alloys have been developed to deliver high-temperature strength in combination with reduced hot-tearing susceptibility. Zr is added to provide additional strengthening via nanoscale Al 3 Zr precipitation, and to stabilize and avoid coarsening of the Al 8 Cu 3 Ce phase. However, the detailed interaction between Zr and Al 8 Cu 3 Ce remains unexplored. In this work, we show with synchrotron X-ray diffraction that laser powder bed fusion fabricated Al-Cu-Ce and Al-Cu-Ce-Zr alloys contain predominantly the Al 8 Cu 3 Ce intermetallic in the as-fabricated condition. Heat treatment of the Al-Cu-Ce alloy results in the Al 8 Cu 3 Ce → Al 8 Cu 4 Ce phase transformation. In the Al-Cu-Ce-Zr alloy, minor fractions of (Al,Cu,Si) 4 Ce and Al 2 Cu-θ are found in the as-fabricated condition, while Al 8 Cu 3 Ce remains stable during heat treatment. Atom probe microscopy quantifies intermetallic stoichiometries and reveals how Zr is enriched at the Al-matrix/Al 8 Cu 3 Ce interface acting as a diffusion barrier against solute exchange. Calibrated thermodynamic modeling underpins this as a kinetic effect. Here, a qualitative microstructural model summarizes, how Zr stabilizes Al 8 Cu 3 Ce against phase transformations and coarsening.

36 MATERIALS SCIENCE↗