Search NASA⌕ Search

SEARCH · Search NASA

Results for “BRAZING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

WETTING AND REACTIVE AIR BRAZING OF BSCF FOR OXYGEN SEPARATION DEVICES

Reactive air brazes Ag-CuO and Ag-V2O5 were evaluated for brazing Ba0.5Sr0.5Co0.8Fe0.2O(3-δ) (BSCF). BSCF has been determined in previous work to have the highest potential mixed ionic/electronic conducting (MIEC) ceramic material based on the design and oxygen flux requirements of an oxy-fuel plant such as an integrated gasification combined cycle (IGCC) used to facilitate high-efficiency carbon capture. Apparent contact angles were observed for Ag-CuO and Ag-V2O5 mixtures at 1000 °C for isothermal hold times of 0, 10, 30, and 60 minutes. Wetting apparent contact angles (θ<90°) were obtained for 1%, 2%, and 5% Ag-CuO and Ag-V2O5 mixtures, with the apparent contact angles between 74° and 78° for all compositions and furnace dwell times. Preliminary microstructural analysis indicates that two different interfacial reactions are occurring: Ag-CuO interfacial microstructures revealed the same dissolution of copper oxide into the BSCF matrix to form copper-cobalt-oxygen rich dissolution products along the BSCF grain boundaries and Ag-V2O5 interfacial microstructures revealed the infiltration and replacement of cobalt and iron with vanadium and silver filling pores in the BSCF microstructure. The Ag-V2O5 interfacial reaction product layer was measured to be significantly thinner than the Ag-CuO reaction product layer. Using a fully articulated four point flexural bend test fixture, the flexural fracture strength for BSCF was determined to be 95 ± 33 MPa. The fracture strength will be used to ascertain the success of the reactive air braze alloys. Based on these results, brazes were fabricated and mechanically tested to begin to optimize the brazing parameters for this system. Ag-2.5% CuO braze alloy with a 2.5 minute thermal cycle achieved a hermetic seal with a joint flexural strength of 34 ± 15 MPa and Ag-1% V2O5 with a 30 minute thermal cycle had a joint flexural strength of 20 ± 15 MPa.

Ag-CuO↗

Control of vacuum induction brazing system for sealing of instrumentation feed-through

The integrity of instrumentation cables is an important performance parameter in addition to the sealing performance in the brazing process. An accurate brazing control was developed for the brazing of the instrumentation feed-through in the vacuum induction brazing system in this paper. The experimental results show that the accurate brazing temperature control performance is achieved by the developed control scheme. Consequently, the sealing performances of the instrumentation feed-through and the integrities of the instrumentation cables were satisfied after brazing. (authors)

42 ENGINEERING↗

Wetting and Mechanical Performance of Zirconia Brazed with Silver/Copper Oxide and Silver/Vanadium Oxide Alloys

The wetting behavior and mechanical strength of silver/copper oxide and silver/vanadium oxide braze alloys were investigated for both magnesia-stabilized and yttria-stabilized (Mg-PSZ and Y-TZP) transformation toughened zirconia substrates. The temperatures investigated were 1000 to 1100°C, with oxide additions of 1 to 10 weight percent V2O5 or CuO, and hold times of 0.9 to 3.6 ks. Increasing either the isothermal hold temperature or time had a distinctly negative effect on the joint strength. The maximum strengths for both braze alloys were obtained for 5 wt. % oxide additions at 1050°C with a hold time of 0.9 ks. The Mg-PSZ/Ag-CuO system exhibited a average fracture strength of 255 MPa (45% of the reported monolithic strength), and the Y-TZP/Ag-CuO system had an average fracture strength of 540 MPa (30% of the reported monolithic strength). The fracture strengths were lower for the Ag-V2O5 braze alloys, with fracture strengths of approximately 180 MPa (30% of the monolithic strength) for Mg-PSZ versus approximately 160 MPa (10% of the monolithic strength) for Y-TZP. No interfacial products were observed in low magnification SEM analysis for the brazing alloys containing V2O5 additions, while there were interfacial products present for brazes prepared with CuO additions in the braze alloy.

Sinnamon, Kathleen E.↗

Diffusion barriers in modified air brazes

A method for joining two ceramic parts, or a ceramic part and a metal part, and the joint formed thereby. The method provides two or more parts, a braze consisting of a mixture of copper oxide and silver, a diffusion barrier, and then heats the braze for a time and at a temperature sufficient to form the braze into a bond holding the two or more parts together. The diffusion barrier is an oxidizable metal that forms either a homogeneous component of the braze, a heterogeneous component of the braze, a separate layer bordering the braze, or combinations thereof. The oxidizable metal is selected from the group Al, Mg, Cr, Si, Ni, Co, Mn, Ti, Zr, Hf, Pt, Pd, Au, lanthanides, and combinations thereof.

36 MATERIALS SCIENCE↗

Diffusion barriers in modified air brazes

A method for joining two ceramic parts, or a ceramic part and a metal part, and the joint formed thereby. The method provides two or more parts, a braze consisting of a mixture of copper oxide and silver, a diffusion barrier, and then heats the braze for a time and at a temperature sufficient to form the braze into a bond holding the two or more parts together. The diffusion barrier is an oxidizable metal that forms either a homogeneous component of the braze, a heterogeneous component of the braze, a separate layer bordering the braze, or combinations thereof. The oxidizable metal is selected from the group Al, Mg, Cr, Si, Ni, Co, Mn, Ti, Zr, Hf, Pt, Pd, Au, lanthanides, and combinations thereof.

42 ENGINEERING↗

Titanium-deposition assisted brazing of SiC ceramics using inactive AgCu filler

Highlights: • Reliable joint of SiC ceramics was achieved via Titanium-deposition assisted brazing using inactive AgCu filler metal. • Microstructure characteristic of deposited-SiC brazed joint was investigated in detail. • Ti-deposition assisted brazing inhibited the formation of numerous intermetallic compounds. - Abstract: In this study, active titanium element film was designed to deposit on SiC ceramics directly to enhance the brazability of inactive AgCu brazing alloy on ceramics. The result showed the reliable joint was successfully obtained and the deposition of titanium film on SiC directly inhibited the formation of amounts of intermetallic compounds effectively in the brazing seam. Detailed interfacial microstructure of joint investigated by scanning electron microscope equipped with energy dispersive spectrum analysis and transmission electron microscope revealed that the interfacial reactions were based on deposited Ti film. The typical joint was SiC/TiCu + Ti{sub 2}Cu/TiC/Ti{sub 5}Si{sub 3} containing TiC particles/Ag(s,s) + Cu(s,s)/Ti{sub 5}Si{sub 3} containing TiC particles/TiC/TiCu + Ti{sub 2}Cu/SiC.

36 MATERIALS SCIENCE↗

Machining and brazing of accelerating RF cavity

BARC has developed 2856 MHz accelerating cavities for 6 MeV, 9 MeV and 10 MeV RF Linac. New vendors are developed for mass production of accelerating cavity for future projects. New vendors are developing for diamond turning machining, cleaning and brazing processes. Fabrication involved material testing, CNC diamond turning of cavity, cavity cleaning and brazing. Before and after brazing resonance frequency (RF) of cavity was checked with vector network analyser (VNA). A power feed test setup is also fabricated to test power feed cavity before brazing. This test setup will be used to find out assembly performance of power feed cavity and its coupler. This paper discusses about nano machining, cleaning and brazing processes of RF cavities. (author)

43 PARTICLE ACCELERATORS↗

Air Brazing: A New Method of Ceramic-Ceramic and Ceramic-Metal Joining

A new method of ceramic-ceramic and ceramic-metal joining has emerged over the past several years. Referred to as air brazing, the technique was originally designed and developed for use in fabricating high-temperature solid-state electrochemical devices such as planar SOFCs and oxygen and hydrogen concentrators. The primary advantage of air brazing is that a predominantly metallic joint can be formed directly in air without need of an inert cover gas or the use of surface reactive fluxes. The resulting bond is hermetic, offers excellent room temperature strength, and is inherently resistant to oxidation at high temperature. The key to developing a successful filler metal composition for air brazing is to identify a metal oxide wetting agent that is mutually soluble in a molten noble metal solvent. One particular oxide-metal combination that appears readily suited for this purpose is CuOx-Ag, a system originally of interest in the development of silver clad cuprate-based superconductors. Studies of the equilibrium phases studies in this system indicate that there are two invariant points in the pseudobinary CuOx-Ag phase diagram around which new braze compositions can be developed: 1) a monotectic reaction at 969±1°C, where CuO and a Ag-rich liquid L1 coexist with a second CuOx-rich liquid phase L2 at a composition of xAg/(xAg + xCu) = 0.10±0.03 Ag and 2) a eutectic reaction at 942±1°C, where CuO and Ag coexist with L1 at a composition of xAg/(xAg + xCu) = 0.99±0.005. Specifically, near-eutectic Ag-CuO filler metal compositions have shown good promise in joining electrochemically active ceramics such as yttria-stabilized zirconia, lanthanum strontium manganite, and barium strontium cobalt ferrite, as well as alumina and magnesia. More recently it has been found that various ternary additions can further improve the wetting characteristics of these filler metals, increase their potential operating temperatures, and/or increase the resulting strength of the joint strength. Here we review the basic concept of air brazing and illustrate filler metal selection and design using the Ag-CuO system as an example.

air brazing↗

Evaluation of Contact Resistance and Fin Effectiveness of Enhanced, Brazed "Dogbone" Fin and Serpentine Tube Heat Exchangers for Air Conditioning and Heat Pump Applications

The energy consumption due to air conditioning is projected to increase by 1.3 and 4.5 times by 2050 compared to 2010 for members and non-members of the Organization of Economic Coordination and Development (OECD), respectively. Greenhouse Gas (GHG) emissions must be carefully managed to minimize their hazardous contribution to climate change. Air conditioners (AC) and heat pumps (HP) contribute with direct GHG emissions through systemic refrigerant leakage, which consequently degrades the system’s performance and therefore increases its indirect GHG emissions as well. To address this issue, the goals of new systems include minimizing leakage risk, using low global warming potential (GWP) refrigerants such as natural refrigerants, and increasing system efficiency. This paper presents part of the efforts in the development of a brazed “dogbone” fin to continuous serpentine tube heat exchanger (HX) for AC/HP applications. The main advantages of such technology are: 1) The potential to reduce 90% or more of the tube return-bends brazed joints compared to conventional tube-fin heat exchangers, thus minimizing leakage vulnerability, enabling the use of natural refrigerants like Propane and Ammonia that carry other concerning risks of flammability and toxicity ; and 2) The brazed fin to the tube joints should yield very low contact resistance. In order to quantify and estimate the impacts of contact resistance and fin effectiveness, a numerical-experimental study is investigated. The novel enhanced brazed “dog-bone” fin is compared to an equivalent pressure expanded fin. The results showed that the expanded fin has consistently greater effective heat transfer but greater contact resistance as well. Furthermore, the brazed fins have up to 20% lower pressure drop. The trade-off comparison shows that the thermal-hydraulic ratio between the two fins is equivalent for air velocities below 2m/s; for greater velocities, however, the expanded fin is favored since it has less fin efficiency penalty. For HVAC&R applications, the air velocities are typically low which makes the proposed technology competitive and a viable option in the pursuit of refrigerant leakage reduction.

30 DIRECT ENERGY CONVERSION↗

Microstructural development of diffusion-brazed austenitic stainless steel to magnesium alloy using a nickel interlayer

The differences in physical and metallurgical properties of stainless steels and magnesium alloys make them difficult to join using conventional fusion welding processes. Therefore, the diffusion brazing of 316L steel to magnesium alloy (AZ31) was performed using a double stage bonding process. To join these dissimilar alloys, the solid-state diffusion bonding of 316L steel to a Ni interlayer was carried out at 900 deg. C followed by diffusion brazing to AZ31 at 510 deg. C. Metallographic and compositional analyses show that a metallurgical bond was achieved with a shear strength of 54 MPa. However, during the diffusion brazing stage B{sub 2} intermetallic compounds form within the joint and these intermetallics are pushed ahead of the solid/liquid interface during isothermal solidification of the joint. These intermetallics had a detrimental effect on joint strengths when the joint was held at the diffusion brazing temperature for longer than 20 min.

36 MATERIALS SCIENCE↗

Effect of processing parameters on the formation of C{sub f}/LAS composites/Ag−Cu−Ti/TC4 brazed joint

C{sub f}/LAS composites were successfully jointed to TC4 alloy with Ag−Cu−Ti filler by vacuum brazing. The interfacial microstructure of TC4/C{sub f}/LAS composites joints was characterized by employing scanning electron microscope (SEM), energy dispersive spectrometer (EDS), X-diffraction (XRD) and transmission electron microscopy (TEM). The determination of the thin interfacial reaction layer (TiSi{sub 2} + TiC layer) was realized by TEM. The effect of holding time on the interfacial microstructure and shear strength were investigated. With the increasing holding time, the thickness of diffusion layer, Ti{sub 3}Cu{sub 4} layer, and TiSi{sub 2} + TiC layer increased obviously, on the contrary, that of Ti−Cu intermetallic compound layers decreased gradually. Besides, blocky Ti{sub 3}Cu{sub 4} phase was coarsened when the joint was brazed at 890 °C for 20 min, which deteriorated the mechanical properties of the joint dramatically. The interfacial evolution of TC4/C{sub f}/LAS composites joint and the formation of TiSi{sub 2}, TiC, Ti{sub 3}Cu{sub 4}, TiCu and Ti{sub 2}Cu phases were expounded. The maximum shear strength of 26.4 MPa was obtained when brazed at 890 °C for 10 min. - Highlights: •The thin interface reaction layer was determined to be TiSi{sub 2} + TiC layer by TEM. •Holding time had influence on the interfacial microstructure and joint properties. •Microstructural evolution mechanism and reactions of brazed joints were expounded.

36 MATERIALS SCIENCE↗

Effect of Cu Interlayer on the Microstructure and Strength for Brazing of Tungsten/316L Steel

Brazing is an effective technique for joining tungsten and steel. However, the high residual stresses are produced due to the different coefficients of thermal expansions between tungsten and steel. Compared with the direct brazing with BNi-2 foil filler, BNi-2/Cu/ BNi-2 multiple interlayer was used as filler to minimize the residual stresses between tungsten and 316L steel. The brazing experiments were conducted at 1050 °C for 25 min using Cu foils with different thickness. The results show that tungsten and 316L steel have been successfully joined by brazing. The intermetallic compound of NiW formed at the W/BNi-2 interface, which was detrimental to the strength of the joint. The microhardness of different diffusion zones is higher than that of the substrates owing to the formation of intermetallic compound and solid solution. All specimens of shear testing fractured at the W/BNi-2 interface close to W substrate, and the average strength of joints was 197, 275 and 268 MPa with multiple interlayer thickness of 0.2 , 0.1 and 0.05 mm copper foil, respectively, while the average strength of joints was 143 MPa with BNi-2 foil filler. The significant increase in the joint shear strength can be ascribed to the Cu foil in the multiple interlayer because of with excellent plasticity and toughness.

36 MATERIALS SCIENCE↗

Predictive dynamic wetting, fluid–structure interaction simulations for braze run-out

Brazing and soldering are metallurgical joining techniques that use a wetting molten metal to create a joint between two faying surfaces. Here, the quality of the brazing process depends strongly on the wetting properties of the molten filler metal, namely the surface tension and contact angle, and the resulting joint can be susceptible to various defects, such as run-out and underfill, if the material properties or joining conditions are not suitable. In this work, we implement a finite element simulation to predict the formation of such defects in braze processes. This model incorporates both fluid–structure interaction through an arbitrary Eulerian–Lagrangian technique and free surface wetting through conformal decomposition finite element modeling. Upon validating our numerical simulations against experimental run-out studies on a silver-Kovar system, we then use the model to predict run-out and underfill in systems with variable surface tension, contact angles, and applied pressure. Finally, we consider variable joint/surface geometries and show how different geometrical configurations can help to mitigate run-out. This work aims to understand how brazing defects arise and validate a coupled wetting and fluid–structure interaction simulation that can be used for other industrial problems.

36 MATERIALS SCIENCE↗

Microstructure and mechanical properties development of micro channel tubes in extrusion, rolling and brazing

Highlights: • Rolling and brazing greatly affect the properties of micro-channel tubes (MCTs). • The properties of MCTs are investigated by the evolution of the microstructure. • Strength is decreased by 47% at 5%-rolling reduction ratio and 3-minute brazing. • Ductile fracture mode is observed by OM at failure of MCTs under inner pressure. - Abstract: In addition to extrusion, the post-processing of rolling and brazing has significant effect on the mechanical properties of multi-port tubes. The aluminum micro channel tubes, especially the seam welding zone in the internal webs, are investigated in terms of mechanical tests, microstructure characterization, and finite element analysis. The effect of the post-process of rolling are quantified by varying amount of rolling reduction ratios. Tensile strength and pressure bearing capacity are determined by tensile tests and burst pressure tests, respectively. The evolution of the microstructure within the seam wielding zone is characterized by Electron backscattered diffraction (EBSD) and optical microscopy (OM). The fracture profile observed by OM indicates ductile fracture mode. The pressure bearing capacity is reduced by ~47% at 5% reduction ratio of rolling followed by 3-minute brazing, where largest grains are obtained due to abnormal grain growth.

36 MATERIALS SCIENCE↗

Brazed Carbon Nanotube Arrays: Decoupling Thermal Conductance and Mechanical Rigidity

Bonding two solids at their interface is the most effective way to achieve a mechanically robust and thermally conducting interface. However, for high‐temperature applications, bonded interfaces between dissimilar materials experience high thermomechanical stress that degrades their performance in terms of cyclic stability (under thermal load) and lifetime. The present study shows that integrating a carbon nanotube (CNT) array as a stress‐relief element to a traditional braze joint mitigates the adverse effects of thermomechanical stress while preserving mechanical robustness and excellent heat transfer characteristic at the interface. A substantial reduction in total thermal interface resistance is achieved (from 41 mm 2 K W −1 for bare CNT array to less than 3 mm 2 K W −1 for a CNT array integrated with braze alloy). A brazed metal/insulator interface (between Cu and quartz) with a CNT array between them exhibits low thermal interface resistance even after extreme thermal cycling whereas the same interface delaminates readily when brazed without a CNT array. The reported technique provides a promising route for substantially improving the problematic high‐temperature interface, a major hindrance in achieving stable and efficient operation for systems such as thermoelectric generators that operate at elevated temperatures (above 400 °C).

Hao, Menglong↗

Triaxial Constraint and Tensile Strength Enhancement in Brazed Joints

A brazed joint consists of a low-melting point and thin interlayer sandwiched between the high-melting-point base materials, in which the interlayer strength is typically lower than that of the base material. When this butt-joined composite is loaded uniaxially in the direction perpendicular to the plane of the brazing layer, the tensile strength is found to be much higher than that of the braze. This seems to violate the iso-stress condition in such a butt-joint serial configuration. Furthermore, the stress triaxiality has been usually ascribed, but without a quantitative rationalization, as being responsible for this tensile strength enhancement. Here a complete finite element simulation has been conducted to study the dependence of triaxiality and strength enhancement on geometric and material parameters. Two asymptotic limit solutions (based on Bridgman and Xia–Shih solutions, respectively) have been identified to understand the simulation results. The critical role of void evolution has been revealed when making a quantitative comparison to available experiments. In addition, ductility of the brazed joint, which has not been fully addressed in literature, is investigated by the Gurson–Tvergaard–Needleman model.

36 MATERIALS SCIENCE↗

Interface Reactions Responsible for Run-out in Active Brazing: Part 2

This Part 2 study examined the microstructural characteristics of braze joints made between two KOVar TM base materials using the filler metals, Ag-xAl, having x = 0, 2, 5, and 10 wt.% Al additions. Brazing processes had temperatures of 965°C (1769°F) and 995°C and brazing times of 5 and 20 min. All brazing was performed under high vacuum.

36 MATERIALS SCIENCE↗

The Effect of Mo Particles Addition in Ag-Cu-Ti Filler Alloy on Ti(C,N)-Based Cermet/45 Steel-Brazed Joints

Reliable brazing of Ti(C,N)-based cermet and 45 steel was successfully achieved by using the Mo-particle-reinforced Ag-Cu-Ti composite filler. The effects of Mo content on the interfacial microstructure and mechanical properties of Ti(C,N)-based cermet/45 steel joints were analyzed. The results showed that the joint microstructure was primarily composed of Ni{sub 3}Ti+Cu{sub 3}Ti{sub 2}, Ag(s,s)+Cu(s.s), CuTi+Mo, Ti-based solid solution, and FeTi+Fe{sub 2}Ti. With the increase in Mo content in filler, the thickness of the Ni{sub 3}Ti+Cu{sub 3}Ti{sub 2} layer adjacent to the Ti(C,N)-based cermet decreases, while more blocky Ti-Cu intermetallic were observed in the brazing seam. The shear strength of the joint could be significantly improved by adding suitable amounts of Mo into the Ag-Cu-Ti filler, and the peak value of 263 MPa was achieved when the alloys were brazed with Ag-Cu-Ti+8wt.%Mo composite filler at 920 °C for 20 min.

36 MATERIALS SCIENCE↗