At least 55 records · Page 3

Effect of Quenching Process on Microstructures and Mechanical Properties of Fe-0.9Mn-0.5Cr-2.4Ni-0.5Mo-C Steel

To develop an appropriate quenching process to produce Fe-0.9Mn-0.5Cr-2.4Ni-0.5Mo-C steel, the microstructures and mechanical properties of this steel were investigated under the direct quenching and tempering (DQT) and the direct quenching, reheated quenching and tempering (DQQT) heat treatment processes. The microstructure of the DQQT specimen was basically tempered sorbite with spherical precipitates, while quite a bit of tempered martensite was in the DQT specimen with dispersive nanoscaled precipitates. The yield strengths of the DQT and DQQT specimens were 1154 and 955 MPa, respectively. The yield strength of the DQT specimen was higher than that of the DQQT specimen because of its finer grain size, higher density of dislocations and dispersed precipitates. The DQQT specimen had spherical precipitates, which hindered the propagation of the crack. Moreover, the high-angle grain boundaries in the DQQT specimen took a higher proportion. Therefore, the Charpy impact values of DQT and DQQT specimens at − 60 °C were 38 and 75 J, respectively. Consequently, the mechanical properties of the Fe-0.9Mn-0.5Cr-2.4Ni-0.5Mo-C steel, which met the standard of 1000 MPa grade steel plate for hydropower station, were acquired by the DQQT process.

36 MATERIALS SCIENCE↗

Friction and Wear Properties of CrSiCN/SiC Tribopairs in Water Lubrication

CrSiCN coatings (3.4 at.% Si) were prepared on 316L stainless steels using unbalanced magnetron sputtering. According to the analysis results of x-ray diffractometer and x-ray photoelectrons spectroscopy, silicon in CrSiCN coatings mainly presented in the amorphous forms of a-SiN, a-SiCN and a-SiC. The hardness and Young’s modulus of CrSiN coatings were 19.4 ± 0.6 and 306.1 ± 5.9 GPa, respectively. In addition, the ball-on-disk sliding tests of CrSiCN/SiC tribopairs were performed in distilled water at varying velocities (0.1-0.5 m/s) and loads (2-12 N). The friction coefficient of tribopairs presented a decreasing trend with respect to velocity at low applied loads (≤ 4 N). To be specific, the low friction coefficient of 0.05-0.14 accompanied with polished wear scar was obtained at high velocities and low loads. Finally, the wear mechanism map of CrSiCN/SiC tribopairs was proposed based on a combination of friction coefficient, wear scar morphology and wear rates of tribopairs.

36 MATERIALS SCIENCE↗

Sliding Wear Behavior of Spark-Plasma-Sintered Fe-Based Amorphous Alloy Coatings on Cu-Ni Alloy

This paper reports on the processing of Fe{sub 48}Cr{sub 15}Mo{sub 14}Y{sub 2}C{sub 15}B{sub 6} amorphous alloy coatings on Cu-10%Ni (wt.%) alloy using spark plasma sintering. The amorphous alloy coatings were sintered at temperatures ranging from 575 to 675 °C at a pressure of 50 MPa. The development of microstructure, phases, and wear properties with sintering temperature of the coatings is investigated. The sintered coatings were found to be near fully dense with hardness close to that of the sintered bulk amorphous alloy. X-ray analysis indicated increasing degree of devitrification of the amorphous coatings with increasing sintering temperature. The wear behavior of the coatings is significantly influenced by the sintering temperature with volume wear rate first decreasing in the temperature range of 575-650 °C and then increasing above 650 °C. The variation in wear behavior is explained based on relative stability of the protective surface layer and embrittlement of the surface with the sintering temperature.

36 MATERIALS SCIENCE↗

Microstructure and Wear Resistance of FeCrBSi Plasma-Sprayed Coating Remelted by Gas Tungsten Arc Welding Process

Herein, an FeCrBSi coating was fabricated via plasma spray on AISI1045 steel, and subsequently, a gas tungsten arc welding (GTA) process was employed to remelt the coating. The microstructure, microhardness, fracture toughness and surface roughness of the coating before and after remelting were investigated, as well as the wear resistance was tested by a UMT-3-type sliding wear apparatus. The results showed that, upon remelting, most defects in the as-sprayed coating were effectively eliminated, the surface roughness decreased by 43%, and the coating–substrate interface bonding changed from mechanical to metallurgical. The phase composition of the as-sprayed coating was primarily α-Fe and a small amount of hard Fe{sub 3}B phase, while the remelted coating consisted of α-Fe and (Fe,Cr){sub 23}C{sub 6} and a small quantity of CrB. In addition, remelting the coating was found to induce a 287.6% increase in the fracture toughness, a 33.4% increase in the average microhardness, and a 47.5% decrease in the wear volume, while the failure mechanism changed from abrasive wear to fatigue wear upon remelting. Therefore, GTA remelting of plasma-sprayed coating was found to be a feasible method to obtain a coating with good wear resistance.

36 MATERIALS SCIENCE↗

Investigation on Cracking Behavior and Development of a Fracture Model of Ti-47Al-2Nb-2Cr Alloy During Hot Deformation

When alloys are strained to a certain limit under the plastic deformation, ductile fracture occurs. Whether the required deformation can be put into effect before fracture appears has become a serious concern. A combination of compression tests, ductile fracture criteria as well as finite element simulation (FEM) were employed in this study to establish the fracture initiation prediction model of Ti-47Al-2Nb-2Cr alloy. To obtain the critical fracture strain, a technique was proposed to calculate the data for deformed cylindrical samples through isothermal compression tests in the temperature range between 1223 and 1423 K with strain rates ranging from 0.001 to 1 s{sup −1}. Five commonly used ductile fracture criteria were compared by FE simulation of compressing tests. It was found that the Brozzo criterion was found to be suitable and accordingly a failure criterion, considering temperature and strain ratio was established. Hot working parameters (critical fracture value and critical strain) in deformation could be obtained through the finite element simulation, revealing that this newly established failure criterion could accurately predict cracking initiation in compressing deformation of Ti-47Al-2Nb-2Cr alloy ingot.

36 MATERIALS SCIENCE↗

Electrochemical Corrosion Behavior of Plasma-Sprayed FeCrNiMoCBSi Amorphous/Nanocrystalline Coatings in Simulated Seawater Medium

A novel FeCrNiMoCBSi coating was fabricated on F22 marine steel by plasma spraying. The coating microstructure and composition were characterized by scanning electron microscope, transmission electron microscope, x-ray diffraction, differential scanning calorimetry, and x-ray photoelectron spectroscopy. The results showed that the coating consisted of amorphous and nanocrystalline phases. Additionally, the corrosion resistance in simulated seawater was evaluated by electrochemical corrosion methods. It was found that the coating exhibited an excellent resistance to pitting corrosion. For long-time immersion tests, the corrosion resistance was gradually decreased with the increasing through-porosity due to the permeation of the corrosive solution into the coating. The coating lost its efficacy through three stages, namely the protection stage, the permeation stage, and the failure stage.

36 MATERIALS SCIENCE↗

Crystal structures and polymorphism in compounds Bi{sub 6+x}T{sub 1-x}P{sub 2}O{sub 15+y}, T=first row transition metals and Pb

The compounds Bi{sub 6+x}T{sub 1-x}P{sub 2}O{sub 15+y}, T=Ti, Cr, Mn, Fe, Co, Ni, Cu, Zn and Pb display five polymorphic forms. Polymorph A is formed by the Ti, Mn, Fe and Ni phases. Polymorph B is exhibited by Co and Cu compounds. The Cr phase crystallizes as polymorphic form C and the Zn phase crystallizes as polymorph D. The Pb compound crystallizes in a new structure type designated as polymorph E. The transition metal crystal structures demonstrate a similar motive. OBi{sub 4} tetrahedra share edges to form two-dimensional Bi{sub 2}O{sub 2} layers that are spanned by PO{sub 4} tetrahedra and TO{sub 6-y} octahedra, pyramids and a trigonal bipyramid to form a three-dimensional network. Polymorph A crystallizes in space group C2; polymorph B is centrosymmetric with space group C2/c, the unit cell parameters differ and the unit cell volume is about double. Polymorph C crystallizes in space group P1-bar and polymorph D exhibits space group C2. Bi{sub 6.4}Pb{sub 0.6}P{sub 2}O{sub 15.2} can be considered as polymorph E, space group C2, with a new crystal structure but related stoichiometry. - Graphical abstract: View of Bi{sub 6.24}Cr{sub 0.09}P{sub 2}O{sub 14.4} perpendicular to [010].

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Ti{sub 2}GaC, Ti{sub 4}GaC{sub 3} and Cr{sub 2}GaC-Synthesis, crystal growth and structure analysis of Ga-containing MAX-phases M{sub n+1}GaC{sub n} with M=Ti, Cr and n=1, 3

Single crystals of Ga-containing MAX-phases Ti{sub 2}GaC, Ti{sub 4}GaC{sub 3}, and Cr{sub 2}GaC were grown from a metallic melt generated by an excess of Ga. This technique allows the crystal growth at different temperatures to control the product distribution. Compounds developed were Ti{sub 2}GaC and TiC at 1500 deg. C, and Ti{sub 2}GaC and Ti{sub 4}GaC{sub 3} at 1300 deg. C. Crystal structures were refined from single crystal data. Ti{sub 2}GaC and Cr{sub 2}GaC were previously known, and belong to the Cr{sub 2}AlC type as well as the solid solutions V{sub 2}Ga{sub 1-x}Al{sub x}C and Cr{sub 2}Ga{sub 1-x}Al{sub x}C. Ti{sub 4}GaC{sub 3} is one of the few 413-phases (P6{sub 3}/mmc, a=3.0690(4) A, c=23.440(5) A) and the first Ga-containing representative. The crystal structures of MAX-phases are intergrowths of layers of an intermetallic MGa in a hexagonal stacking sequence with carbidic layers (MC){sub n} of the NaCl type. The thickness of the layer depends from the value of n. The results of the structure refinements also demonstrate that also the structural details follow this description. - Graphical abstract: Single crystals of Ga-containing MAX-Phases (TiC){sub n}(TiGa) (n=1, 3) were grown from a metallic melt including and characterised by X-ray diffraction. Ti{sub 4}GaC{sub 3} is one of the few 413-phase and the first containing Ga.

36 MATERIALS SCIENCE↗

Crystal structures and phase transitions of Sr{sub 2}CrSbO{sub 6}

Sr{sub 2}CrSbO{sub 6} was synthesized by the conventional solid-state reaction process. X-ray powder diffraction (XRPD) and neutron powder diffraction (NPD) has been used to reinvestigate the structure at room temperature and to study the phase transitions at high- and low-temperature. Rietveld analysis revealed that Sr{sub 2}CrSbO{sub 6} crystallizes at room temperature in a monoclinic system having a space group I2/m, with a=5.5574(1) A; b=5.5782(1) A; c=7.8506(2) A and beta=90.06(2), no P2{sub 1}/n space group as was previously reported. The high-temperature study (300-870 K) has shown that the compound presents the following temperature induced phase-transition sequence: I2/m-I4/m-Fm-3m. The low-temperature study (100-300 K) demonstrated that the room-temperature I2/m monoclinic symmetry seems to be stable down to 100 K. - Graphical abstract: The components of the GM{sup 3+} mode, responsible for the breaking of the symmetry to the I4/mmm tetragonal space group from the Fm-3m, observed experimentally at high. This mode involves the movements of all the oxygen atoms in the octahedra: those located in the (00z) positions move to the center (or out of) of the octahedra, as shown in (a); and the oxygen atoms located in the xy plane move outwards (inwards) along the diagonals of the basal plane of the octahedra (b). As the octahedra are corner sharing if one octahedra stretches the other one expands. (c) On the other hand, the mode GM{sup 4+} is responsible for the breaking of the symmetry down to the I4/m space group, and involves movements only of the oxygen atoms located in the xy plane (c): those displacements can be viewed as rotations (tilts) of the octahedra around the tetragonal axis.

36 MATERIALS SCIENCE↗

The binary tin-rich lanthanum stannides La{sub 2}Sn{sub 5} and La{sub 3}Sn{sub 7}-A structural and bond theoretical study

The three tin-rich lanthanum stannides LaSn{sub 3}, La{sub 2}Sn{sub 5} and La{sub 3}Sn{sub 7}, which were known only from indexed powder diagrams, have been synthesized from melts of the elements by slow cooling of sealed sample tubes or arc melting and quenching. Their crystal structures were refined from X-ray powder diffractometer data using the Rietveld method. LaSn{sub 3} (cubic, space group Pm3-bar m, a=477.77(1) pm, Z=1, R{sub F}{sup 2}=0.044) crystallizes with the common Cu{sub 3}Au structure type, which can be described either as an ordered close packing or as a network of [Sn{sub 6}] octahedra (closo clusters) connected via common vertices. The structures of La{sub 2}Sn{sub 5} (Ce{sub 2}Sn{sub 5} structure type, orthorhombic, space group Cmmm, a=463.85(3), b=3581.3(3), c=469.83(4) pm, Z=4, R{sub F}{sup 2}=0.075) and La{sub 3}Sn{sub 7} (Gd{sub 3}Sn{sub 7} structure type, orthorhombic, space group Cmmm, a=457.83(4), b=2628.40(2), c=467.99(4) pm, Z=2, R{sub F}{sup 2}=0.068), which retain some similarities to ordered close packings as well, show 2D blocks of corner-sharing [Sn{sub 6}] octahedra terminated by [Sn{sub 5}] square pyramids (nido clusters). In between these layers, isolated Sn zigzag chains similar to those observed in LaSn (CrB structure type) are interspersed. A simple v.e. count after Zintl and Wade/Jemmis for the polyanionic Sn building blocks resulting from these structure descriptions fits the observed v.e. numbers of the three compounds almost exactly. It is also possible to explain the minima of the tDOS close to E{sub F}, which have been calculated within the framework of the FP-LAPW DFT approach. However, the simple assumption of an exclusively Sn-p bonded polyanion would neglect the large Sn-La bonding contributions and the reduced amount of electron transfer from La to Sn when compared to related alkaline earth stannides. - Graphical Abstract: La{sub 2}Sn{sub 5} and La{sub 3}Sn{sub 7}, stacking variants of LaSn{sub 3} (Cu{sub 3}Au type, closo clusters) and LaSn (CrB type, zig-zag chains) Highlights: > Preparation of binary La stannides LaSn{sub 3}, La{sub 2}Sn{sub 5} and La{sub 3}Sn{sub 7}. > La{sub 2}Sn{sub 5} and La{sub 3}Sn{sub 7} do not appear in published phase diagrams. > Full pattern Rietveld refinements of the crystal structures of all compounds. > Revised description of the structure types emphasizes polyanionic Sn framework. > Structural motifs rationalized through DFT calculations and Zintl and Wade rules.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

A mixture of massive and feathery microstructures of Ti48Al2Cr2Nb alloy by high undercooled solidification

A mixture of massive and feathery microstructures was observed in Ti48Al2Cr2Nb alloy subjected to the undercooled solidification rather than the heat treatments in most cases. Double recalescence events and primary β solidification confirmed that massive γ phase did not directly nucleate from the undercooled melt but formed during the solid-state transformations. It is believed that small white areas (aluminium-poor) along lamellar grain boundaries may be closely related to the formation of massive γ phase and feathery γ phase. High dislocation density and stacking faults were detected in massive γ phase by transmission electron microscopy. The high energy of defects and undercooling in the solid state phase transformation can provide sufficiently high driving force for the nucleation of massive γ phase. - Graphical abstract: Display Omitted - Highlights: • A mixture of massive and feathery microstructures was observed. • Massive γ formed during the solid-state transformations. • Defects and undercooling provide driving force for the nucleation of massive γ.

36 MATERIALS SCIENCE↗

Widmannstätten laths in Ti48Al2Cr2Nb alloy by undercooled solidification

Widmannstätten laths in Ti48Al2Cr2Nb alloy were obtained by containerless electromagnetic levitation during undercooled solidification rather than heat treatments in most cases. The nucleation of γ{sub Widmannstätten} is confirmed by the thermal history of the second recalescence behaviour. High dislocation density, stacking faults and dislocation slip are observed by transmission electron microscopy. By quantitative analysis of the transformation energy, the driving force for γ{sub Widmannstätten} in the solid state phase transformation is calculated, compared with that of heat treatments. Meanwhile, the proper undercoolings (ΔT = 257–300 K), post-solidification cooling rates (11.1–29.1 K/s), the fine lamellar colony sizes (306–467 μm) and proper undercoolings in the solid state phase transformation are in favour of promoting the formation of Widmannstätten laths at moderate undercoolings. - Graphical abstract: Display Omitted - Highlights: • Widmannstätten laths were observed in undercooled TiAl alloy. • The influencing factors were discussed in undercooled TiAl alloy. • An analysis of the nucleation of γ{sub Widmannstätten} is carried out.

36 MATERIALS SCIENCE↗

Determination of the volume fraction of precipitates in a nitrided Fe-0.354 wt% C-2.93 wt% Cr model alloy by anomalous small angle X-ray scattering

Highlights: • Anomalous small-angle X-ray scattering (ASAXS) is used to study nitriding of Fe-Cr-C steels. • ASAXS gives access to chemical information of nanoscaled nitrides. • The volume fraction of nitrides is determined along the diffusion layer. - Abstract: Anomalous small angle scattering (ASAXS) is a powerful non-destructive technique that can provide characteristic features of nanoscale precipitates such as the volume fraction, and chemical composition. In this paper, the technique is used for the first time to explore nanoscale MN nitrides (M = Cr,Fe) after nitriding of a model iron alloy (Fe-0.354 wt% C-2.93 wt% Cr).

36 MATERIALS SCIENCE↗

Mechanical properties, deformation behavior and microstructure evolution of Ti-43Al-6Nb-1Mo-1Cr alloys

Highlights: • The alloys exhibit excellent high-temperature tensile properties. • Activation energy of deformation (Q) and n are 571 KJ/mol and 2.765, respectively. • The hot processing maps of strain 0.5 and 0.6 are displayed. • Phase transformations and microstructure evolution are explained in different conditions. • Three types of deformation mechanisms are exhibited at different temperature. - Abstract: The high-temperature properties, microstructure evolution and deformation behavior of a novel Ti-43Al-6Nb-1Mo-1Cr(at.%) alloy were studied in this paper. The ultimate tensile strength (UTS) and elongation (δ) were tested at 800, 850, and 900 °C, in which the excellent strength 551 MPa, 510 MPa, and 382 MPa, and elongation 2.9%, 12.7%, and 16.8% were exhibited, respectively. Isothermal compression tests were carried out in the temperature range of 1100–1250 °C and strain rate range of 0.001–1.0 s{sup − 1}. Based on dynamic materials model (DMM) and phase diagram, dynamic recrystallization mechanism and phase transformation during thermal deformation were clarified and the hot processing maps were calculated. The experimental results show that the values of stress exponent (n) and the apparent deformation activation energy (Q) of Ti-43Al-6Nb-1Mo-1Cr(at.%) were calculated to be 2.77 and 571 KJ/mol. Meanwhile, three various types of microstructure evolution in different deformation conditions were discussed and concluded.

36 MATERIALS SCIENCE↗

Characterization of the microstructures and the shape memory properties of the Fe-Mn-Si-Cr-Ni-C shape memory alloy after severe plastic deformation by differential speed rolling and subsequent annealing

Highlights: • The Fe-SMA was subjected to severe plastic deformation and then annealed. • Recovery strain increased with increasing grain size. • An optimum grain size existed for the largest recovery stress. • Grain reduction is useful for having a high recovery stress. - Abstract: The Fe-13.51Mn-4.82Si-8.32Cr-3.49Ni-0.15C shape memory alloy was subjected to severe plastic deformation by high-ratio differential speed rolling and subsequent annealing (between 873 and 1373 K) to find the factors that affect recovery stress and recovery strain. As the annealing temperature increased (i. e., as grain size increased), the recovery strain increased. This was attributed to decrease in the density of grain boundaries and the density of twins with increasing grain size. The recovery stress, however, showed a different behavior. It increased with annealing temperature up to 973 K, at which an ultrafine grain size near 1.6 μm was obtained, and then decreased with further increase in the temperature. The difference between the recovery strain and the plastic strain induced by recovery stress under constrained displacement during cooling was proposed to determine the amount of recovery stress. There was an optimum grain size for the largest difference between the recovery strain and the plastic strain. The current study shows that grain-size reduction is not good for having a high recovery strain but it is beneficial for having a high recovery stress in the Fe-Mn-Si shape memory alloys.

36 MATERIALS SCIENCE↗

Influence of Mn addition on the microstructure and mechanical properties of a directionally solidified γ-TiAl alloy

Highlights: • Mn addition can significantly improve the yield strength of TiAl alloy. • Introduction of Mn facilitates the operation of twinning-controlled deformation. • Twin-dislocation interactions cause a continuous increase in work hardening rate. - Abstract: TiAl alloys with nominal compositions of Ti-47Al-2Nb-2Cr-(0, 1, 3, 5)Mn were prepared via electromagnetic cold crucible directional solidification (ECCDS), and the influence of Mn addition on the microstructure and mechanical properties of the alloys was investigated. The experimental results showed that the Mn atoms were dissolved within the TiAl alloy, and no Mn compounds were formed. Based on the X-ray diffraction (XRD) analysis results, the peak angle of the Mn-containing sample shifted to a higher value, indicating lattice shrinkage. The Mn addition also increased the volume fraction of the B2 phase. The yield strength of the TiAl alloy monotonically increased as the content of the substitutional-solute Mn atoms increased. The ultimate strengths of the TiAl alloys containing 1 at.%, 3 at.%, and 5 at.% Mn consequently decreased because micro-cracks were preferentially formed in the B2 phase during room-temperature deformation. The introduction of substitutional-solute Mn atoms could result in a reduction of the stacking-fault energy of the γ phase, and facilitate the operation of twinning-controlled plastic-deformation during the intermediate stage of the plastic deformation process. The interaction between the deformation twins and movable dislocations led to a continuous increase in the work-hardening rate.

36 MATERIALS SCIENCE↗

Modification of microstructure and properties of Ti-47Al-2Cr-4Nb-0.3W alloys fabricated by SPS with trace multilayer graphene addition

Highlights: • The TiAl alloys with different content addition of multilayer graphene were fabricated. • When the graphene content is 0.8 at.%, the mean grain size decreases to 8.2 μm. • The bending and fracture strength increase to 1000 MPa and 2347 MPa, respectively. • The friction coefficient decreased from 0.6 to 0.4, with a decrease by 1/3. - Abstract: In this paper, Ti-47Al-2Cr-4Nb-0.3W alloys with trace multilayer graphene addition were fabricated by spark plasma sintering to enhance both mechanical properties and tribological property simultaneously. With the addition of multilayer graphene, bending strength, compressive strength and tribological property of TiAl alloys are all improved. When graphene content increases from zero to 0.8 at.%, the mean grain size decreases from 14.8 ± 1.4 μm to 8.2 ± 0.8 μm. The bending strength reaches almost 1000 MPa and the fracture strength increases to 2347 ± 12 MPa, an increase of 15% compared with TiAl alloy. The friction coefficient also decreases from about 0.6 to 0.4, a decrease by 1/3 compared with TiAl alloy. The reasons for the improved mechanical properties and tribological property are the in-situ reaction plate-shape Ti{sub 2}AlC phase, fine needle-like Ti{sub 3}AlC phase as well as fine and homogeneous microstructure. The wear mechanism changes from abrasive wear to abrasive wear plus adhesive wear with the increased graphene content.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Microstructural evolution of ω assisted α precipitates in β-CEZ alloy during ageing process

Highlights: • Ultrafine Athermal ω precipitates were formed in β-CEZ alloy by quenching from above the β transus temperature. • In the ageing process, these ω precipitates coarsen, accompanied by the form of needle-like α phase. • ω precipitates were formed by {111}β planes shift 0.5d222 along the direction. • The superfine α particles are formed in close proximity of the ω/β interface. - Abstract: The microstructural evolution in β-CEZ (Ti-5Al-2Sn-4Zr-4Mo-2Cr-1Fe wt%) alloy, after quenching and ageing, has been investigated by combining results from orientation imaging microscopy, transmission electron microscopy, high-resolution TEM (HRTEM). Ultrafine Athermal ω precipitates (about 1 nm) are formed in this alloy by quenching from above the β transus temperature. In the ageing process, these ω precipitates coarsen, accompanied by the form of needle-like α phase. The scale of ω assisted α increased from 5 to 10 nm in width and about 50 nm in length to 10 nm in width and 100–300 nm in length while extending ageing time from 2 h to 5 h at 350 °C. However, when going on extending the ageing time from 5 h to 20 h at 350 °C, the scale of α didn't grow dramatically but the density of α increased clearly. When increasing the ageing temperature from 350 °C to 450 °C, the scale of ω assisted α grow dramatically. Furthermore, the structural relationship of ω and α is observed by HRTEM images. It can be found that ω precipitates were formed by {111}β planes shift 0.5d222 along the <111> direction, and the superfine α particles are formed in close proximity of the ω/β interface.

36 MATERIALS SCIENCE↗