Search NASA⌕ Search

SEARCH · Search NASA

Results for “CIRFT”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

41 records · Page 3

Sister Rod Destructive Examinations (FY22) Appendix F: Cyclic Integrated Reversible-Bending Fatigue Tests

This report documents work performed under the Spent Fuel and Waste Disposition’s Spent Fuel and Waste Science and Technology program for the US Department of Energy (DOE) Office of Nuclear Energy (NE). This work was performed to fulfill Level 3 Milestone M3SF-22OR010201046, “Draft FY2022 ORNL Report on High Burnup Sibling Pin Testing Results,” within work package SF-22OR01020104 and is an update to the work reported in M2SF-22OR010201047, M2SF-21OR010201032, M2SF-19ORO010201026 and M2SF-19OR010201028. As a part of DOE NE High Burnup Spent Fuel Data Project, Oak Ridge National Laboratory (ORNL) is performing destructive examinations (DEs) of high burnup (HBU) (>45 GWd/MTU) spent nuclear fuel (SNF) rods from the North Anna Nuclear Power Station operated by Dominion Energy. The SNF rods, called sister rods or sibling rods, are all HBU and include four different kinds of fuel rod cladding: standard Zircaloy-4 (Zirc-4), low-tin (LT) Zirc-4, ZIRLO, and M5. The DEs are being conducted to obtain a baseline of the HBU rods’ condition before dry storage and are focused on understanding overall SNF rod strength and durability. Composite fuel and defueled cladding will be tested to derive material properties. Although the data generated can be used for multiple purposes, one primary goal for obtaining the post-irradiation examination data and the associated measured mechanical properties is to support SNF dry storage licensing and relicensing activities by (1) addressing identified knowledge gaps and (2) enhancing the technical basis for post-storage transportation, handling, and subsequent disposition. This appendix documents the status of the ORNL Phase 1 DE activities related to tests of the sister rods using the Cyclic Integrated Reversible-Bending Fatigue Tester (CIRFT) in Phase 1 of the sister rod test program.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Sister Rod Destructive Examinations (FY22) Appendix J: Leaching of High Burnup Used Nuclear Fuel in Deionized Water

The leaching experiment aims to understand the trends in the radiolysis-enhanced dissolution of HBU SNF when exposed to water (e.g., in-reactor or in-pool cladding failures). Specimens from a baseline M5-clad rod and a heat-treated M5 rod were cut from the fractured CIRFT specimens and placed in 100 mL deionized water for a period of 128 days. Both radial and axial sections were cut to provide different surface areas of fuel in contact with the leachate. During the four-month exposure period, aliquot samples of the leachate were analyzed using gamma spectroscopy and inductively coupled plasma - mass spectrometry (ICP-MS). The analysis quantified the amount of fuel leached into the solutions and provided individual isotopic release fractions (of 30+ isotopes) which were compared as a function of time and surface area of the fuel exposed.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Fatigue Testing and Characterization of Pre-hydrided Zircaloy-4 Cladding Tubes

The solubility of hydrogen in Zircaloy-4 (Zry-4) at the cladding operating temperature is near 100 wt. ppm. Above this solubility limit, excess hydrogen precipitates as δ-hydride platelets in the cladding material. Because of the effect of the thermal gradient across the cladding thickness on the migration and precipitation of hydrogen, hydride rims are often observed at the cladding outer surface; under excessive corrosion conditions hydride blisters are possible. It is well known that the fatigue of metal alloys, especially high cycle fatigue, is sensitive to the status of surface including the microstructure, roughness, and residual stress. Thus, the question considered herein, is whether excessive hydrogen pickup modifies the microstructure such that it has a degradation effect on the fatigue performance of cladding during operation. This report describes the evaluation of fatigue performance of a pre-hydrided Zry-4 cladding. A commercial Zry-4 was polished and pre-hydrided to 800 ppm and 1300 ppm H contents. The fatigue testing was conducted under strain control at 5 Hz with fully-reversed bending by using a cyclic integrated reversible bending fatigue tester (CIRFT). Six specimens with 1300 ppm and one specimen with 800 ppm were tested. Significant variation in test results were observed. While two of the 1300 ppm specimens failed with less than 1 ×10 5 cycles (at 0.32% and 0.41%), the four other samples did not fail over the strain amplitude range of 0.25% to 0.38%. Interestingly, the fracture initiation site of the failed samples was on the outside diameter (OD) surface rather than on the inside diameter (ID) surface as is typical for the as-polished cladding. This suggested a degrading effect of the hydriding process. Subsequently, three of the unfailed specimens were then further tested at ~0.43% to observe where failure initiation occurred. Significant variation was also observed in these three specimens. One specimen failed at ~9000 cycles while the two others failed at 43000 and 1.06 ×10 5 cycles. The performance here correlated to the location of failure initiation; failure initiated on the OD in the sample that failed after 9000 cycles while it initiated on the ID in the sample that failed after 43000 and 1.06 ×10 5 cycles. Flat features at the OD initiation sites suggest a brittle hydride feature on the surface of those samples was the cause of the degradation in fatigue performance, though the overall hydrogen levels in all samples was similar. A summary of all the observations is provided below: • The un-failed specimens with 1300 ppm H were cycled to failure with a higher amplitude near 0.43%. In addition, the fatigue-treated specimen tended to have a longer fatigue at the same induced amplitude. • Fractography revealed a mixed failure mode for the pre-hydrided specimen. Particularly, the specimen with fracture initiation site (FIS) located on the outer diameter surface of tube tended to have a shorter fatigue life than that of FIS on the inner diameter surface. • Etched cross section was shown to have hydride platelets aligned with tube longitudinal axis as expected, and the density of hydrides is at the similar level as in literature data. Meanwhile, a LECO procedure was applied for hydrogen concentration measurement, which showed the measured hydrogen contents are close to the nominal value. • With the polished cladding tube as baseline, O’Donnell-Lager (O-L) analysis showed that a decrease of about 50% in reduction-of-area (RA) would be needed for the O-L fitting to the fatigue data of 1300 ppm cladding. The suggestion for the next steps is provided.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Sister Rod Destructive Examinations (FY23): Appendix J: Leaching of High Burnup Used Nuclear Fuel in Deionized Water

The leaching experiment aims to understand the trends in the radiolysis-enhanced dissolution of HBU SNF when exposed to water (e.g., in-reactor or in-pool cladding failures). Specimens from a baseline M5-clad rod and a heat-treated M5 rod were cut from the fractured CIRFT specimens and placed in 100 mL deionized water for a period of 128 days. Both radial and axial sections were cut to provide different surface areas of fuel in contact with the leachate. During the four-month exposure period, aliquot samples of the leachate were analyzed using gamma spectroscopy and inductively coupled plasma - mass spectrometry (ICP-MS). The analysis quantified the amount of fuel leached into the solutions and provided individual isotopic release fractions (of 30+ isotopes) which were compared as a function of time and surface area of the fuel exposed. Consistent with existing literature, the leaching followed a trend in which isotopes of certain elements such as Cs and Mo were among the first species in the matrix to dissolve, and with the highest release rates. This was followed by a gradual matrix dissolution consisting of uranium and other actinides and a slower-than-matrix release from some isotopes, including Ru and Rh. It was also observed that the circumferential samples having less exposed fuel surface area (to begin with) leached more than the axial samples for a majority of the isotopes during the timespan of the study. Previous experiments were conducted by decladding or exposing the pellet-clad surface completely, but the samples used in this study retained the cladding. One possible explanation for the higher leaching rate of the circumferential samples is that the pellet-clad interface, which has a greater density of grain boundaries and defects, may be the most vulnerable area to leaching of fuel in the presence of water.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Fatigue Test Result for High Burnup Pressurized Water Reactor Rods

The High Burnup Spent Fuel Data Project, sponsored by DOE-NE, is focused on understanding the effects of long-term storage and transportation on high burnup (HBU) (>45 gigawatt days per metric ton uranium) light water reactor fuel. The experiment includes 32 HBU spent nuclear fuel (SNF) assemblies that will be stored in a typical Independent Spent Fuel Storage Installation (ISFSI) and 25 sister rods - nine SNF rods that were removed from the fuel assemblies prior to insertion to the ISFSI and 16 SNF rods removed from similar HBU assemblies. The sister rods provide a baseline of the condition of the HBU rods prior to loading, drying, and long-term dry storage. Destructive examinations of the sister rods are focused on understanding overall SNF rod strength and durability. Both composite fuel and empty cladding will be tested to derive material properties. While the data generated can be used for multiple purposes, a primary goal of the sister rod PIE data and associated measured mechanical properties is to support existing fuel storage licensing and relicensing activities by addressing identified knowledge gaps, and enhance the technical basis for post-storage transportation, handling, and consolidation activities. Fatigue tests of HBU M5-clad, ZIRLO-clad, Zircaloy-4, and low tin Zircaloy-4 segments have been completed using ORNL’s Cyclic Integral Reversible Fatigue Tester (CIRFT). This is the first time ZIRLO-clad rods have been tested. Some of the segments were heat-treated to understand the effects of thermal transients such as those encountered during dry storage vacuum drying on the fatigue lifetime. This paper presents results of the fatigue tests obtained to date and discusses planned future tests.

Montgomery, Rose↗