Search NASA⌕ Search

SEARCH · Search NASA

Results for “COERCIVE FORCE”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

Deposition of high permeability FeCoN films on mica substrates

In this study, sheet mica was explored as an alternative substrate for thin film deposition due to its unique layered structure and atomically flat surface. Static magnetic properties and microwave permeability of sputtered FeCoN films on mica with and without SiO{sub 2} under-layer were examined. In-plane isotropy and a large coercivity of 70 Oe were observed for the film directly deposited on mica substrate. With the insertion of 40 nm SiO{sub 2} under-layer between the film and mica substrate, well-defined in-plane anisotropy is formed due to the significant reduce in film residual stress, associated with a 3 Oe coercive force along easy axis. As a result, excellent microwave properties have been achieved and are comparable with the same film on Si substrate. Moreover, the permeability spectra are surprisingly stable from room temperature up to 390 K. Mica is proved as a promising substrate for magnetic films with high microwave performance, which is a great advantage for practical applications. Furthermore, our results provide an effective way to reduce the residual stress in sputtered films.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

The mechanism of magnetic properties improvement and microstructure refinement of Zr in Nd[subscript 2]Fe[subscript 14]B

In order to understand the role of Zr addition in Nd{sub 2}Fe{sub 14}B (2-14-1), a systematic study of Zr in Nd{sub 2}Fe{sub 14}B was done on a series of stoichiometric samples (Nd{sub 1-x}Zr{sub x}){sub 2}Fe{sub 14}B with 0 {le} x {le} 0.16. As-cast ingots formed significant amounts of Nd{sub 2}Fe{sub 17} starting at x = 0.06, while in the melt-spun ribbons, no Nd{sub 2}Fe{sub 17} was observed for the range studied. A monotonic decrease in lattice parameters for the 2-14-1 phase indicate Zr solubility in the melt-spun ribbons, but this is not observed in the ingots. Magnetic and thermal measurements on the ribbons showed that the saturated magnetization Ms (around 16 kG), the spin reorientation temperature (125 K), and the Curie temperature (583 K) do not depend on the Zr content, while the anisotropy field Ha slightly decreased as the Zr content increased. The energy product (BHmax) and the coercive force H{sub c} are highly dependent on the solidification and annealing process. Scanning electron microscopy and transmission electron microscopy on the as-melt spun alloys are consistent with x-ray diffraction showing Zr solubility in the 2-14-1 grains. After annealing, Zr diffuses to the grain boundaries to form Zr enriched compounds. Thus, while Zr may exhibit a metastable solubility in Nd{sub 2}Fe{sub 14}B, the enhanced magnetic behaviors observed in melt-spun ribbons are due to the refinement of the microstructure and enhanced grain-boundary pinning.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Effect of CeO{sub 2} buffer layer on the microstructure and magnetic properties of yttrium iron garnet film on Si substrate

Yttrium iron garnet films were grown by radio frequency magnetron sputtering on Si(111) substrate with and without CeO{sub 2} buffer layer, and influence of CeO{sub 2} buffer on the microstructure and magnetic behaviors of the films were investigated. As compared with the film without buffer, a larger saturation magnetizaton (M{sub s}), lower coercive force (H{sub c}), and higher remnant magnetization (M{sub r}) were obtained due to the introduction of CeO{sub 2} layer. The higher M{sub s} results from the denser structure and the smaller content of Fe{sup 2+} ions. The lower H{sub c} and higher M{sub r} can be explained by the small surface roughness and crystal grains size. The film on CeO{sub 2} buffer layer possess fine microstructure and its surface roughness is smaller than the unbuffered films, which provides an increased exchange between the crystal grains and an enhanced spontaneous magnetization effect, leading to the higher remnant magnetization.

36 MATERIALS SCIENCE↗

Delayed demagnetization jumps in (NdDy)(FeCo)B magnets in a steady-state magnetic field

Spontaneous demagnetization jumps are observed in sintered magnets (Nd{sub 0.6}Dy{sub 0.4}){sub 16}(Fe{sub 0.77}Co{sub 0.23}){sub 78}B{sub 6} in a constant magnetic field after a sharp decrease in an external magnetic field from the value corresponding to the saturation to a value close to the coercive force. It is shown that the number of the magnetization jumps is proportional to their amplitudes. A low value of the autocorrelation coefficient between the jump amplitude and the time of its appearance (R < 0.1) demonstrate the stochasticity of the jumps. It is found that the spectral jump density is independent of the frequency, i.e., a white magnetic noise is observed. The distribution of the magnetic field gradient has been obtained near the sample surface that makes it possible to distinguish domains and the grain magnetization in the dependence on the direction of the texturing of the sintered magnet.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Magnetic properties of Fe{sub 7}Co{sub 3} films with gas cluster ion beam irradiations

Gas cluster ion beam (GCIB) irradiation was performed on Fe{sub 7}Co{sub 3} films to examine the magnetic properties. After Ar ion beam etching, the coercive force (H{sub c}) increased from the initial value; this may have been caused by irradiation damage from high-energy Ar ions. H{sub c} decreased after Ar-GCIB irradiation (acceleration voltage (V{sub a}): 20 kV, ion fluence (F): 1 Multiplication-Sign 10{sup 15} ions/cm{sup 2}). Since GCIB is an equivalent low-energy (several eV/atom) ion beam, it shows a damage-recovery effect. When the ionization electron voltage (V{sub e}) was reduced from 200 to 60 V, H{sub c} was observed to further decrease. Since the fraction of multiply charged Ar-GCIB decreased with decreasing V{sub e}, severe damage of Fe{sub 7}Co{sub 3} films can be minimized by employing low V{sub e}.

36 MATERIALS SCIENCE↗

Highly spin-polarized current in Co-substituted Fe{sub 3}O{sub 4} epitaxial thin films at room temperature

Epitaxial thin films of cobalt ferrite Co{sub x}Fe{sub 3−x}O{sub 4} (x = 0.0, 0.5, and 1.0) were fabricated on α-Al{sub 2}O{sub 3} (001) substrates using pulsed laser deposition. It was found that the coercive force of the cobalt ferrite films could be tuned by changing the Co content. The films prepared under low oxygen pressure (1.0 × 10{sup −6 }Pa) showed semiconducting behavior even for x = 1.0. X-ray photoelectron spectroscopy revealed that the Co ions were 2{sup +} for all compositions. On the other hand, it was found that the Fe ions were in the Fe{sup 2+}/Fe{sup 3+} valence state, which may cause small-polaron hopping among the Fe-3d electrons in the films. An anomalous Hall effect was observed in the Co{sub 0.5}Fe{sub 2.5}O{sub 4} film even at 300 K, suggesting that carriers in the films were highly spin-polarized at room temperature.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Magnetic and absorbing properties of M-type substituted hexaferrites BaFe{sub 12–x}Ga{sub x}O{sub 19} (0.1 < x < 1.2)

X-ray powder diffraction is used to determine the unit cell parameters and to refine the crystal structure of the solid solutions of M-type hexagonal barium ferrite BaFe{sub 12–x}Ga{sub x}O{sub 19} (x = 0.1–1.2) with isostructural diamagnetic cation Ga{sup 3+} substitution at T = 300 K. As the level of substitution increases, the unit cell parameters are shown to decrease monotonically. The temperature (300 K ≤ T ≤ 750 K, H = 8.6 kOe) and field (T = 300 K,–20 kOe ≤ H ≤ 20 kOe) dependences of the saturation magnetization of these solid solutions are studied with a vibrating-sample magnetometer. The concentration dependences of the Curie temperature T{sub C}, the specific spontaneous magnetization, and the coercive force are plotted. The magnetic parameters are found to decrease with increasing substitution. The microwave properties of the solid solutions are analyzed in an external magnetic field (0 ≤ H ≤ 4 kOe). As the cation Ga{sup 3+} concentration increases from x = 0.1 to 0.6, the natural ferromagnetic resonance (NFMR) frequency decreases; as the concentration increases further to x = 1.2, this frequency again increases. As the cation Ga{sup 3+} concentration increases, the NFMR line width increases, which indicates a widening of the frequency range where electromagnetic radiation is intensely absorbed. Here, the resonance curve peak amplitude changes insignificantly. The shift of the NFMR frequency in an applied magnetic field is more pronounced for samples with low cation Ga{sup 3+} concentrations. The role of diamagnetic substitution is revealed, and the prospects and advantages of Ga-substituted beryllium hexaferrite as the material absorbing high-frequency electromagnetic radiation are demonstrated.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Magnetic properties of Fe-rich Fe-V alloy films

Polycrystalline Fe{sub 100-x}V{sub x} with x=0 to 14 at.% V films on a glass substrate were made by the dc magnetron sputtering method. The deposition temperature was 250 deg. C. The magnetic properties, i.e., saturation magnetization 4piM{sub s}, bulk-pinning field for a domain wall H{sub cw}, coercive force H{sub c}, initial permeability mu{sub i}, maximum permeability mu{sub m}, saturation magnetostriction lambda{sub s}, and electrical property, such as the electrical resistivity rho of the Fe-V films, were measured. We find that 4piM{sub s} is a decreasing function of x, H{sub c}, and/or H{sub cw} has a minimum at xapprox =x{sub 0}=8 at. % V, mu{sub i}, mu{sub m}, and/or mu{sub c} has a maximum at x=x{sub 0}, lambda{sub s}approx =0 at x=x{sub 0}, and rho is an increasing function of x. These new magnetic results are consistent with earlier magnetostriction measurements [Jen and Chen, J. Magn. Magn. Mater. 204, 165 (1999)] and theoretical calculations [Ostanin, Staunton, and Razee, Phys. Rev. B 69, 064425 (2004)]. Moreover, all the magnetic features in the x dependence of H{sub c}, H{sub cw}, mu{sub i}, mu{sub m}, mu{sub c}, and lambda{sub s}, respectively, can be explained within the framework of the bulk-pinning (or surface-pinning) and the end-pinning (or nucleation) models. Briefly, the pinning model analysis of the magnetic hysteresis data confirms the inference that near zero lambda{sub s} implies maximal permeabilities and smallest H{sub c} and H{sub cw}. Among all the Fe-V films, the Fe{sub 92}V{sub 8} film has the optimal magnetic and electrical properties for application.

36 MATERIALS SCIENCE↗

Synthesis and Characterization of FeCo Nanowires with High Coercivity

Ferromagnetic FeCo nanocrystals with high coercivity have been synthesized using a reductive decomposition method. The sizes and shapes of the nanocrystals were found to be dependent on reaction parameters such as the surfactant ratio, the precursor concentration and the heating rate. Synthesized nanocrystals have a body-centered cubic crystal structure for both particles and nanowires and the (110) crystalline direction is along the long axis of the nanowires. The coercivity and magnetization of the FeCo nanocrystals are found to be dependent on morphology. Nanowires of Fe 60 Co 40 with saturation magnetization of 92 emu g -1 and coercive force of 1.2 kOe have been obtained in this study.

36 MATERIALS SCIENCE↗

Magnetic single-enzyme nanoparticles with high activity and stability

Magnetic single-enzyme nanoparticles (SENs) encapsulated within a composite inorganic/organic polymer network were fabricated via the surface modification and in situ aqueous polymerization of separate enzyme molecule. The resultant nanoparticles were characterized by transmission electron microscope (TEM), Fourier transform infrared (FTIR) spectrometer and X-ray diffraction (XRD). These particles are almost spherical in shape and have a unique size of about 50 nm in diameter. Electrical and magnetic measurements reveal that the magnetic SENs have a conductivity of 2.7 x 10{sup -3} S cm{sup -1}, and are superparamagnetic with a saturation magnetization of 14.5 emu g{sup -1} and a coercive force of 60 Oe. Compared with free enzyme, encapsulated enzyme exhibits a strong tolerance to the variation of solution pH, high temperature, organic solvent and long-term storage, thus showing significantly enhanced enzyme performance and stability.

60 APPLIED LIFE SCIENCES↗

Hard magnetic properties observed in bulk Mn 1–x Ga x

Here, Mn-Ga binary alloys have shown promising magnetic properties, even though these alloys contain no rare-earth metals. Both theoretical predictions and experimental work showed that nanoscaled Mn-Ga samples, such as thin films could have remarkable magnetic properties. Although the prediction provides a useful guideline and thin films supply us with materials in some application, bulk materials are required for majority of the applications that require a strong magnetic field. We have made bulk Mn 1-x Ga x alloys by mechanically milling and heat treatments. In this paper, we report annealed Mn 1-x Ga x bulk composites that exhibit coercivity up to 18.8 kOe.

36 MATERIALS SCIENCE↗

Unexpected Magnetic Domain Behavior in LTP-MnBi

Low-temperature-phase MnBi (LTP-MnBi) has attracted much interest as a potential rare-earth-free permanent magnet material because of its high uniaxial magnetocrystalline anisotropy at room temperature, K approximate to 10(7) ergs/cc, and the unusual increase of anisotropy with increasing temperature, with an accompanying increasing coercive force (H-C) with temperature. However, due to the complex Mn-Bi phase diagram, bulk samples of LTP-MnBi with the optimum saturation moment, similar to 75-76 emu/g have been achieved only with zone-refined single crystals. We have prepared polycrystalline samples of LTP-MnBi by induction melting and annealing at 300 degrees C. The moment in 70 kOe is 73.5 emu/g, but H-C is only 50 Oe. This is quite surprising-the high saturation moment indicates the dominating presence of LTP-MnBi. Therefore, an H-C c of some significant fraction of 2K/M-S approximate to 30 kOe would seem reasonable in this polycrystalline sample. By examining "Bitter" patterns, we show that the sample is composed of similar to 50 - 100 mu m crystallites. The randomly oriented crystallites exhibit the variety of magnetic domain structures and orientations expected from the hexagonal-structured MnBi with its strong uniaxial anisotropy. Clearly, the reversal of magnetization in the sample proceeds by the low-field nucleation of reversed magnetization in each crystallite, rather than by a wall-pinning mechanism. When the annealed sample was milled into fine particles, H-C increased by several orders of magnitude, as expected.

Nguyen, PK↗

Low frequency creep in CoNiFe films

The results of an investigation of domain wall motion excited by slow rise-time, bipolar, hard-axis pulses in vacuum deposited CoNiFe films 1500A to 2000A thick are presented. The results are consistent with those of comparable NiFe films in spite of large differences in film properties. The present low frequency creep data together with previously published results in this and other laboratories can be accounted for by a model which requires that the wall structure change usually associated with low frequency creep be predominately a gyromagnetic process. The correctness of this model is reinforced by the observation that the wall coercive force, the planar wall mobility, and the occurrence of an abrupt wall structure change are the only properties closely correlated to the creep displacement characteristics of a planar wall in low dispersion films.

Bartran, D. S.↗

Design and material selection for inverter transformer cores

Report is announced which studied magnetic properties of candidate materials for use in spacecraft transformers, static inverters, converters, and transformer-rectifier power supplies. Included are material characteristics for available alloy compositions in tabular form, including: trade names, saturated flux density, dc coercive force, loop squareness, material density, and watts per pound at 3 KHz.

Mclyman, W. T.↗

A preliminary report on the magnetic measurements of samples 72275 and 72255

The direction and magnitude of natural remanent magnetization of five approximately 3-g subsamples of 72275 and 72255 and the high field saturation magnetization, coercive force, and isothermal remanent magnetization of 100-mg chip from each of these samples, were studied. Given an understanding of the magnetization processes, group 1 experiments provide information about the absolute direction of the ancient magnetizing field and a qualitative estimate of its size (paleointensity). The group 2 experiments yield a quantitative estimate of the iron content and a qualitative ideal of the grain sizes.

Banerjee, S. K.↗

Remanent magnetization and structural effects due to shock in natural and man-made iron-nickel alloys

Explosive shock or meteorite impact are significant remagnetization processes. The mechanisms of remagnetization associated with the dynamic processes depend on the peak shock pressure, the nature of the shocked materials, and the behavior of the shock in the material. Magnetic measurements can be used to classify products formed during a shock process, and magnetic measurements can be used to investigate the process itself because of the special characteristics of the remanent magnetization vectors. The magnetic coercive force increases more rapidly in quenched and annealed iron-nickel alloys as nickel is added than it does in the alloys which have been shocked.

Wasilewski, P. J.↗

Coercivity maxima at low temperatures

Recent measurements have shown that the magnetic coercive forces of some Apollo lunar samples show an unexpected decrease with decreasing temperature at cryogenic temperatures. This behavior can be explained quantitatively in terms of a model which considers additive contributions from a soft, reversible magnetic phase and from a harder, hysteretic magnetic phase.

Schwerer, F. C.↗