Assessment on Transport of Radioactive Species from Nuclear Facilities - 17079

It is generally recognized that radioactive nuclides are most hazardous fission products that could be released in the event of reactor accidents. The reactor coolant system of a pressurized water reactor (PWR) nuclear plant exhibits radioactivity from various sources. These radiation sources consist of the fission products from fuel element and activated products from corrosion products. The complex infrastructure of the processes does not allow detailed measurement of activity until after the reactor is shutdown. All of the components that require dismantling will be radioactive which was caused by neutron activation during operation, contamination by corrosion products, contamination by damaged by fuel rods and leaks by equipment. Due mainly to the various operation modes and their aging, there are the increasing needs to carry out repair works that are not sufficiently provided for by the original design. Many difficulties are involved in these tasks, namely, high radiation doses, cramped areas, hard to reach components, coupled with stringent quality conditions. The need to simulate the behavior of corrosion products in a nuclear power plant environment has attracted many researchers' attention. It has performed the in-depth reviews of the various theories and physics associated with the corrosion products transportation, the laboratory loop testing, and the field measurements in operating plants. Before we start the decommissioning of nuclear power plants, workers, the public and the environment shall be properly protected from radiation hazards. For this purpose, a safety assessment should be carried out relating to the potential hazards that may occur during the decommissioning. The radiological hazards involved in the decommissioning activities also should be identified, and be taken into account in the safety assessment. The radiation conditions of the primary circuit are determined by the activity of corrosion and fission products that have accumulated on the internal surfaces of the components. Therefore the estimation of contamination on the components is very important and, may be the first step in the reactor operation and decommissioning of components. The predominant radionuclide in the PWR primary coolant is Co-60, although Co-58 contributes significantly to radioactivity level at the early stage of a reactor operation. Since Co-60 is produced from the in-core Co-58, which is the source of cobalt in a reactor coolant system, many researchers have investigated its transmutation in the core, its transport around the system, and its subsequent deposition on surfaces. The major parameter influencing the behavior of radioactivity, such as Co-60 in the coolant, is the corrosion product oxides. The objective of this work is to analyze the corrosion product activity transported in the primary circuit by using a multi-region model. This model, which is incorporated with the mass and activity transport between the dissolved corrosion products in the coolant and the surface, describes the specific activity of corrosion products in coolant and on the surfaces according to the operation modes as well as decommissioning stage. In order to evaluate the analysis of the corrosion products in an integral type reactor, a multi-region mass balance model is applied. The specific activities of the various species on the surface of core and steam generator throughout the effective full power hours, 15,000 hours, are simulated for the various modes of operations. As a result, the specific activities of corrosion products from the surface of primary circuit were shown as very low compared to those of other commercial nuclear power plants. In this simulated reactor, a significant reduction of specific activities from the activated corrosion products is obtained due to the introduction of titanium alloy to the steam generator tube and the avoidance of boric acid induced corrosion. From this result we conclude that we are able to predict the level of radioactive nuclides generated by corrosion products in a primary circuit according to the various modes of operations by using multi-region model. In this point of view it is concluded that this multi-region model can be used as an engineering tool for analysis of the corrosion products within the primary coolant for the nuclear power plants. It is also considered that it is possible to extend to a calculation tool for estimating the radiological hazards involved in the decommissioning activities in terms of safety assessment. (authors)

07 ISOTOPE AND RADIATION SOURCES↗

Corrosion behavior in aluminum/galvanized steel resistance spot welds and self-piercing riveting joints in salt spray environment

Here, this paper underlined the corrosion behavior of aluminum alloy/galvanized steel joints fabricated by resistance spot welding (RSW) and self-piercing riveting (SPR) exposed to different salt-spray cycles. It was found that the crevice generated by different joining methods has an important impact on corrosion behavior. Compared with the RSW joint, less corrosion happened on the coupled regions in SPR joints because of the higher local pH value resulted from the smaller crevice. The crevice, however, has less impact on the types of corrosion products. Galvanic corrosion happened in the coupled region for both RSW and SPR joints. The Pourbaix diagram explained the stable corrosion products of Al and Zn—Fe alloy, which are Al 2 O 3 , ZnO, and Fe 3 O 4 . Additional corrosion products observed from the experiment included α-Al(OH) 3 , Ca 4 Al 2 (CO 3 )(OH) 12 (H 2 O) 5 , Zn 5 (OH) 8 Cl 2 (H 2 O), Zn 5 (CO 3 ) 2 (OH) 6 , and Fe 2 (OH) 2 (CO 3 ), which can be understood by considering the metastable corrosion products, Pourbaix diagram, and possible chemical reactions.

36 MATERIALS SCIENCE↗

Corrosion of 907 Steel Influenced by Sulfate-Reducing Bacteria

The effect of sulfate-reducing bacteria (SRB) on the corrosion of 907 steel was investigated. Results demonstrated that the chemical composition of corrosion products, the corrosion rate, and corrosion type were altered due to the adherence of SRB and the subsequent formation of biofilm on the 907 steel surface. Different from the case in sterile medium that ferrous oxides predominated in the corrosion products, ferrous sulfide was an important component in SRB-containing medium. Meanwhile, corrosion of 907 steel was enhanced by SRB, and the corrosion rate was dependent on their metabolic activity, which increased, stabilized, and decreased in the exponential growth, death, and residual phases, respectively. Furthermore, the corrosion type was changed from uniform corrosion to localized corrosion with the introduction of SRB, and the development process was analyzed based on the current distribution map of wire beam electrodes. In sterile medium, the maximum current density decreased with the immersion time extended, and there were no significant anodic current peaks in the late period, while in SRB-containing medium, the ratio between cathodic areas and anodic areas was high in the exponential growth phase, and stable anodic sites formed gradually in death and residual phases, which facilitated the development of localized corrosion.

36 MATERIALS SCIENCE↗

Facile Separation of Sr-90, Fe-55, Nb-94, Ni-59,63 with Large Amount of Ca by Controlled pH Precipitation - 17190

it is important to manage low-and intermediate-level radioactive wastes from nuclear power plants due to a permanent disposal. According to the Nuclear Safety and Security Commission (NSSC), among all the regulatory radionuclides, a few radionuclides from the fission products and corrosion products such as Sr-90, Fe-55, Nb-94, Ni-59,63 which emit low-energy x-ray and beta radiation. Thus, it is necessary to separate beta-emitting nuclides individually. For that reason, KAERI has established analytical procedures which can separate Sr-90, Fe-55, Nb-94, Ni-59,63 from radioactive waste samples. However, when radioactive wastes contain large amount of Ca (above 300 mg), it is not easy to recover the target radionuclides because high concentration of Ca has a strong influence on the effective analyses. In order to combat this problem, there was an attempt to make the precipitate as CaF{sub 2} by using hydrofluoric acid. However, this way had a limitation; Fe-55, Nb-94 were precipitated as fluoride compounds as well as Ca. In this study, we have focused on developing a separation procedure stage by stage in the radioactive wastes with Sr-90, Fe-55, Nb-94, Ni-59,63 and large amount of Ca (1500 mg). The detailed steps are described below; (1) Separation of Fe-55, Nb-94, Ni-59,63 as metal hydroxide precipitates: low solubility product constant (Ksp) between pH 6 and pH 10. (2) Selective elimination of Ca-oxalate complex under strong acidic conditions. Consequently, all the metal sources were sequentially separated and quantitatively recovered by inductively coupled plasma atomic emission spectrometric (ICP-AES) analysis, the recovery is as follows; Sr-90 (3 mg): 89.47±5.48%, Fe-55 (20 mg): 99.80±3.19%, Nb-94 (20 mg): 97.45±2.42%, Ni-59,63 (2 mg): 83.59±15.31%, Ca (1500 mg): 85.32±6.38%, respectively. This methodology will help us separation of radioactive wastes efficiently if apply properly. (authors)

07 ISOTOPE AND RADIATION SOURCES↗

High temperature oxidation of corrosion resistant alloys from machine learning

Parabolic rate constants, k p , were collected from published reports and calculated from corrosion product data (sample mass gain or corrosion product thickness) and tabulated for 75 alloys exposed to temperatures between ~800 and 2000 K (~500–1700 °C; 900–3000°F). Data were collected for environments including lab air, ambient and supercritical carbon dioxide, supercritical water, and steam. Materials studied include low- and high-Cr ferritic and austenitic steels, nickel superalloys, and aluminide materials. A combination of Arrhenius analysis, simple linear regression, supervised and unsupervised machine learning methods were used to investigate the relations between composition and oxidation kinetics. The supervised machine learning techniques produced the lowest mean standard errors. The most significant elements controlling oxidation kinetics were Ni, Cr, Al, and Fe, with Mo and Co composition also found to be significant features. The activation energies produced from the machine learning analysis were in the correct distributions for the diffusion constants for the oxide scales expected to dominate in each class.

Materials Science↗

LABORATORY TESTING TO SIMULATE VAPOR SPACE CORROSION IN RADIOACTIVE WASTE STORAGE TANKS

Radioactive liquid waste has been stored in underground carbon steel tanks for nearly 70 years at the Hanford nuclear facility. Vapor space corrosion of the tank walls has emerged as an ongoing challenge to overcome in maintaining the structural integrity of these tanks. The interaction between corrosive and inhibitor species in condensates/supernates on the tank wall above the liquid level, and their interaction with vapor phase constituents as the liquid evaporates from the tank wall influences the formation of corrosion products and the corrosion of the carbon steel. An effort is underway to gain an understanding of the mechanism of vapor space corrosion. Localized corrosion, in the form of pitting, is of particular interest in the vapor space. CPP testing was utilized to determine the susceptibility of the steel in a simulated vapor space environment. The tests also investigated the impact of ammonia gas in the vapor space area on the corrosion of the steel. Vapor space coupon tests were also performed to investigate the evolution of the corrosion products during longer term exposures. These tests were also conducted at vapor space ammonia levels of 50 and 550 ppm NH{sub 3} (0.005, and 0.055 vol.%) in air. Ammonia was shown to mitigate vapor space corrosion.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Drying Wet Stored and Corroded Magnox Fuel for Interim Dry Storage - 20187

To investigate the feasibility of drying corroded Magnesium alloy clad nuclear fuel, the corrosion products of inactive and unirradiated Magnox simulant dry corrosion product and dried corroded Magnox sludge were characterised by X-ray diffraction and thermogravimetric analysis. XRD identified brucite in the dried corrosion product and both brucite and hydromagnesite in the sludge. TGA identified mass loss on dehydration of ∼9.1% up to 250 deg. C and 27.9% from dehydroxylation up to 440 deg. C, with total mass loss of 41.9% up to 800 deg. C for the dried corrosion product. The sludge TGA showed 8.3% mass loss up to 250 deg. C from dehydration, 7.5% up to 330 deg. C from dehydroxylation and 31.4% mass loss up to 47.2% for decarbonation, with total mass loss of 49.2% up to 800 deg. C. Water removal up to 1.8 g was performed by cold vacuum drying (40 deg. C-120 deg. C) on a ≅14.8 g (wet) corroded Magnox sample. The process was monitored by observing pressure, dew point, temperature and gas flow changes supported by measuring the sample mass loss as water is removed. From these tests, it was observed that the dried corroded Magnox displayed some hygroscopic capacity which has implications for water retention following vacuum drying and the length of exposure required to achieve the desired dryness. Whilst at higher temperatures the water was removed faster, the increased temperature also risks the fuel cladding undergoing unwanted chemical reactions with the residual water during the process. However, at lower temperatures the achievable levels of dryness were reduced. Therefore, from these observations this work has identified that there is a temperature balance that may be necessary to optimise the drying process with respect to allowing the greatest level of dryness whilst restricting unwanted chemical reactions. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

A closer look at corrosion of steel reinforcement bars in concrete using 3D neutron and X-ray computed tomography

Corrosion of reinforcing bars constitutes the largest threat to the durability of concrete structures. Thus, several studies have investigated the nature of the corrosion products, most using post-mortem analyses. However, corrosion products evolve when in contact with oxygen, hindering result interpretation. This work presents instead a state-of-the-art, non-destructive 3D method for the assessment of corrosion of embedded reinforcements. Multimodal neutron and X-ray tomography was used to observe, non-destructively, the characteristics of the corrosion products in two concrete samples, with the aim of investigating possible benefits of the use of this technique for reinforced concrete structures. One sample was naturally corroded, extracted from an 81-year-old bridge, the other was corroded via the galvanostatic method, resulting in corrosion-induced cracks. Quantitative and qualitative data was acquired, including the iron-to-rust volumetric ratio in macroscopic interfacial voids and the thickness of the corrosion layer at the steel concrete interface. The iron-to-rust volumetric ratio corresponded to large, soluble, corrosion products, forming in environments with low availability of oxygen for both samples.

36 MATERIALS SCIENCE↗

Monitoring reinforcement corrosion and corrosion-induced cracking by X-ray microcomputed tomography method

X-ray microcomputed tomography (X-ray μCT) method is proposed to trace steel corrosion and corrosion-induced cracking in cement paste. Experimental results show it can track the time-dependent development of steel corrosion and corrosion products, as well as the subsequent initiation and propagation of corrosion-induced cracks. Furthermore, the information of corrosion pits, corrosion products, and corrosion-induced cracks can be clearly obtained from the whole specimen by this novel method. Additionally, SEM/EDS results agree closely with image analyses by X-ray μCT. This method provides a new angle to investigate the reinforcement corrosion process and can help to improve the numerical analysis of corrosion-induced damage in reinforced concrete structures. - Highlights: • Reinforcement corrosion and corrosion-induced cracking is traced by X-ray μCT method. • The development of corrosion products can be determined as a function of time and space. • Subsequent initiation and propagation of corrosion-induced cracks can be monitored. • The time-dependent corrosion process can be quantitative analyzed by X-ray μCT measurement.

36 MATERIALS SCIENCE↗

Corrosion of 304 stainless steel in static liquid lithium under high vacuum

To study the compatibility especially the corrosion characteristic of structural material stainless steel (SS) with liquid lithium (Li) is an important factor for the simultaneous application of liquid Li and SS as a blanket material or potential plasma facing material (PFM) in future fusion devices. Here, the corrosion behaviors of 304SS exposed to liquid Li at 700 K for 1320 hr under high vacuum were investigated. After exposure to liquid Li, 304SS produces non-uniform corrosion which includes corrosion products and grain boundary corrosion. Compared with the corrosion behaviors at 600 K and 640 K, temperature plays an important role in the corrosion behaviors of 304SS in static liquid Li. The weight loss, corrosion depth and corrosion products of 304SS specimens increase with the corrosion temperature. In general, the compatibility between 304SS and static liquid Li is relatively good under the experimental conditions. And besides, it is unexpectedly found that the compatibility of copper with Li is not good.

304SS↗

CRUD Source Term Assessment and Development for VERA

In pressurized water reactors, corrosion of primary loop materials is an ongoing process, as primary loop components (steam generator, hot leg, cold leg, and core) are constantly exposed to the coolant. As a result of this corrosion, primary loop materials are released into the coolant in the form of aqueous metal ions and particulate oxides. These corrosion products are the source of materials that form crud deposits on fuel rod clad surfaces. The mass of corrosion products available to create crud will limit the rate and extent of crud buildup that occurs. This is commonly referred to as the crud “source term”. The major contribution to the source term mass comes from the steam generator, due to the large surface area exposed to the coolant. Steam generators are not identical; the wetted area exposed to the coolant and the alloy used in the steam generator tubes vary. Different alloys corrode at different rates; Inconel 690 corrodes at approximately one-third of the rate of corrosion of Inconel 600. The mass of corrosion products released from the steam generator also varies by the area exposed to the coolant. The release of these corrosion products depends on the local environmental factors within the primary loop, including temperature, pH, local fluid conditions, electrochemical potential, and thermodynamic solubilities of the species present within this system. As such, each PWR will have a different crud source term based on these plant-specific parameters. In order to accurately model and predict crud growth and issues that arise from the presence of crud (CIPS, CILC), the source of these corrosion product materials must be accurately modeled in a system mass balance. These models should be mechanistic, representative of the underlying physics phenomena, and account for the effects of the plant-specific design and operating parameters, including the alloys used, local temperatures, and fluid flow conditions.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Analysis of failed and nickel-coated 3093 beam clamp components at the East Tennessee Technology Park (ETTP).

The U.S. Department of Energy and its contractor, Bechtel Jacobs Company (BJC), are undertaking a major effort to clean up the former gaseous diffusion facility (K-25) located in Oak Ridge, TN. The decontamination and decommissioning activities require systematic removal of contaminated equipment and machinery followed by demolition of the buildings. As part of the cleanup activities, a beam clamp, used for horizontal life lines (HLLs) for fall protection, was discovered to be fractured during routine inspection. The beam clamp (yoke and D-ring) was a component in the HLL system purchased from Reliance Industries LLC. Specifically, the U-shaped stainless steel yoke of the beam clamp failed in a brittle mode at under less than 10% of the rated design capacity of 14,500 lb. The beam clamp had been in service for approximately 16 months. Bechtel Jacobs approached Argonne National Laboratory to assist in identifying the root cause of the failure of the beam clamp. The objectives of this study were to (1) review the prior reports and documents on the subject, (2) understand the possible failure mechanism(s) that resulted in the failed beam clamp components, (3) recommend approaches to mitigate the failure mechanism(s), and (4) evaluate the modified beam clamp assemblies. Energy dispersive x-ray analysis and chemical analysis of the corrosion products on the failed yoke and white residue on an in-service yoke indicated the presence of zinc, sulfur, and calcium. Analysis of rainwater in the complex, as conducted by BJC, indicated the presence of sulfur and calcium. It was concluded that, as a result of galvanic corrosion, zinc from the galvanized components of the beam clamp assembly (D-ring) migrated to the corroded region in the presence of the rainwater. Under mechanical stress, the corrosion process would have accelerated, resulting in the catastrophic failure of the yoke. As suggested by Bechtel Jacobs personnel, hydrogen embrittlement as a consequence of corrosion was also explored as a failure mechanism. Corroded and failed yoke samples had hydrogen concentrations of 20-60 ppm. However, the hydrogen content reduced to 4-11 ppm (similar to baseline as-received yoke samples) when the corrosion products were polished off. The hydrogen content in the scraped off corrosion product powders was >7000 ppm. These results indicate that hydrogen is primarily present in the corrosion products and not in the underlying steel. Rockwell hardness values on the corroded yoke and D-rings were R{sub c} {approx} 41-46. It was recommended to the beam clamp manufacturer that the beam clamp components be annealed to reduce the hardness values so that they are less susceptible to brittle failure. Upon annealing, hardness values of the beam clamp components reduced to R{sub c} {approx} 25. Several strategies were recommended and put in place to mitigate failure of the beam clamp components: (a) maintain hardness levels of both yokes and D-rings at R{sub c} < 35, (b) coat the yoke and D-rings with a dual coating of nickel (with 10% phosphorus) to delay corrosion and aluminum to prevent galvanic corrosion since it is more anodic to zinc, and (c) optimize coating thicknesses for nickel and aluminum while maintaining the physical integrity of the coatings. Evaluation of the Al- and Ni-coated yoke and D-ring specimens indicated they appear to have met the recommendations. Average hardness values of the dual-coated yokes were R{sub c} {approx} 25-35. Hardness values of dual-coated D-ring were R{sub c} {approx} 32. Measured average coating thicknesses for the aluminum and nickel coatings for yoke samples were 22 {micro}m (0.9 mils) and 80 {micro}m (3 mils), respectively. The D-rings also showed similar coating thicknesses. Microscopic examination showed that the aluminum coating was well bonded to the underlying nickel coating. Some observed damage was believed to be an artifact of the cutting-and-polishing steps during sample preparation for microscopy.

08 HYDROGEN↗

In Situ Spectroscopic Monitoring of MSR Molten Salt and Off-Gas Systems

A significant challenge that must be overcome before commercialization of molten salt reactors is tracking special nuclear material (SNM) through the reactor and subsystems such as fuel chemical processing and off-gas systems. In recent years, several approaches have been explored to track SNM, fission products, and corrosion products in these different subsystems. One such approach is to employ laser and optical spectroscopy to measure the atomic and molecular signals of MSR salts. The advantages of these approaches are that they typically are non-intrusive and offer the capability of process monitoring while still providing low uncertainties. At the Idaho National Laboratory, spectroscopy approaches such as laser-induced breakdown spectroscopy (LIBS) and ultraviolet-visible (UV-Vis) spectroscopy have been utilized to investigate molten salts in an aerosol (LiCl, KCl, RbCl2, NdCl3, and PrCl3) and vapor phases (MgCl5, NdCl5, and ZrCl4) with success. Testing to date has yielded qualitative information on all the above species and quantitative data and analytical figures of merit for species in the vapor phases. These findings, including results from ongoing testing, as well as the experimental conditions and potential applications will be presented.

98 - NUCLEAR DISARMAMENT, SAFEGUARDS, AND PHYSICAL↗

Identifying the speciation of salt-based actinides in the presence of contaminants [Slides]

Molten salt reactors (MSR) present advantages over light water reactors, such as higher safety and energy efficiency, convenient waste processing, and the ability to use more abundant thorium instead of uranium as the fuel source. However, due to the high temperatures associated with these reactors the reactor container corrosion product can have a high influence on the molten salt system, and they are considered as a part of the fuel salt system. It is essential to have a comprehensive understanding of the chemical reactions that are occurring in the molten salt in the presence of contaminants such as nickel, manganese, chromium chlorides and oxides. Because they can change the local structure of these salts and the local structures of these salts govern the thermophysical properties of the molten salts, which would determine the safety and operational parameters of the reactor. This study is focused on identifying f-element materials speciation resulting from reaction with corrosion/degradation products in a molten salt environment to understand the flow of MSR. In this work, f-element chlorides are mixed with alkali and alkali earth metals and corrosion products such as transition metal chlorides are introduced systematically, inside a glovebox. Then these are heated to around 700 ? and slowly cooled to room temperature. Afterwards, these are analyzed using different characterization techniques such as powder X-ray diffraction, UV-vis and Raman spectroscopy and solid-state NMR. The initial work was conducted with lanthanide chlorides as a surrogate for actinides and the acquired data strongly indicates that in the presence of corrosion products new phase formation/ change in coordination environments occurs. This work has been presented at multiple conference presentations. The proposed work would allow to extend this work to actinides (depleted uranium and thorium) and this would assist to identify the speciation of actinide chloride in the presence of corrosion products. Also, this work would open an opportunity to compare the coordination behavior of lanthanides with the actinides.

37 - INORGANIC, ORGANIC, PHYSICAL AND ANALYTICAL C↗

Rust transformation/rust compatible primers

Proper surface preparation has been the key to obtain good performance by a surface coating. The major obstacle in preparing a corroded or rusted surface is the complete removal of the contaminants and the corrosion products. Sandblasting has been traditionally used to remove the corrosion products before painting. However, sandblasting can be expensive, may be prohibited by local health regulations and is not applicable in every situation. To get around these obstacles, Industry developed rust converters/rust transformers and rust compatible primers (high solids epoxies). The potential use of these products for military equipment led personnel of the Belvoir Research, Development and Engineering Center (BRDEC) to evaluate the commercially available rust transformers and rust compatible primers. Prior laboratory experience with commercially available rust converters, as well as field studies in Hawaii and Puerto Rico, revealed poor performance, several inherent limitations, and lack of reliability. It was obvious from our studies that the performance of rust converting products was more dependent on the amount and type of rust present, as well as the degree of permeability of the coating, than on the product's ability to form an organometallic complex with the rust. Based on these results, it was decided that the Military should develop their own rust converter formulation and specification. The compound described in the specification is for use on a rusted surface before the application of an organic coating (bituminous compounds, primer or topcoat). These coatings should end the need for sandblasting or the removing of the adherent corrosion products. They also will prepare the surface for the application of the organic coating. Several commercially available rust compatible primers (RCP) were also tested using corroded surfaces. All of the evaluated RCP failed our laboratory tests for primers.

Emeric, Dario A.↗

LDRD poster - Identifying the speciation of salt-based actinides in the presence of contaminants

Molten salt reactors (MSRs) are among the most promising Generation IV nuclear reactors. The salts used in these reactors exhibit a high affinity for moisture and oxygen, and heating does not eliminate the oxides that are formed. Additionally, due to the high operating temperatures, reactor parts experience pronounced corrosion, and the resulting corrosion products integrate into the fuel salt system. It is hypothesized that the speciation of f-elements in molten salts would change in the presence of oxides and corrosion products. These changes in local structure can alter the rheological properties, which are critical to the operational and safety parameters of the reactors. Therefore, an in-depth understanding of how corrosion products influence lanthanide/actinide speciation is crucial. To test this hypothesis, lanthanides (as surrogates for actinides) and actinide chlorides were mixed with oxides (such as nickel oxide and lithium oxide) and/or corrosion products (e.g., nickel chloride) and reacted in molten salts. The resulting phases were analyzed using techniques such as powder X-ray diffraction, Raman spectroscopy, UV-Visible spectroscopy, and nuclear magnetic resonance spectroscopy. In the presence of oxides, due to the high oxophilicity of f-elements, these elements capture oxygen from the oxides, forming lanthanide/actinide oxide or oxychloride phases. Specifically, with cerium chloride, the introduction of lithium oxide to the formation of various final products depending on the oxide concentration. At lower oxide concentrations, cerium oxychloride (CeOCl) in the +3 oxidation state was observed, while an increase in the oxide concentration led to the formation of cerium dioxide (CeO2), where cerium is in the +4 oxidation state. In contrast, with nickel oxide, CeOCl formation was consistently observed, regardless of the oxide concentration. This project successfully determined that the speciation of f-elements change in the presence of oxides and different oxides in molten salts result in different final products. When the influence of nickel chloride was examined, changes in f-element speciation were not observed. However, it reacted with lithium chloride to generate a lithium-nickel-chloride (Li6NiCl8) phase, which was also observed when nickel oxide was reacted. Computational models were developed to simulate the phases anticipated under experimental conditions.

37 - INORGANIC, ORGANIC, PHYSICAL AND ANALYTICAL C↗

Effect of chloride content of molten nitrate salt on corrosion of A516 carbon steel.

The corrosion behavior of A516 carbon steel was evaluated to determine the effect of the dissolved chloride content in molten binary Solar Salt. Corrosion tests were conducted in a molten salt consisting of a 60-40 weight ratio of NaNO{sub 3} and KNO{sub 3} at 400{sup o}C and 450{sup o}C for up to 800 hours. Chloride concentrations of 0, 0.5 and 1.0 wt.% were investigated to determine the effect on corrosion of this impurity, which can be present in comparable amounts in commercial grades of the constituent salts. Corrosion rates were determined by descaled weight losses, corrosion morphology was examined by metallographic sectioning, and the types of corrosion products were determined by x-ray diffraction. Corrosion proceeded by uniform surface scaling and no pitting or intergranular corrosion was observed. Corrosion rates increased significantly as the concentration of dissolved chloride in the molten salt increased. The adherence of surface scales, and thus their protective properties, was degraded by dissolved chloride, fostering more rapid corrosion. Magnetite was the only corrosion product formed on the carbon steel specimens, regardless of chloride content or temperature.

36 MATERIALS SCIENCE↗