Search NASA⌕ Search

SEARCH · Search NASA

Results for “CORROSIVE EFFECTS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

Surface effects of corrosive media on hardness, friction, and wear of materials

Hardness, friction, and wear experiments were conducted with magnesium oxide exposed to various corrosive media and also with elemental iron and nickel exposed to water and NaOH. Chlorides such as MgCl2 and sodium containing films were formed on cleaved magnesium oxide surfaces. The MgCl2 films softened the magnesium oxide surfaces and caused high friction and great deformation. Hardness was strongly influenced by the pH value of the HCl-containing solution. The lower the pH, the lower the microhardness. Neither the pH value of nor the immersion time in NaOH containing, NaCl containing, and HNO3 containing solutions influenced the microhardness of magnesium oxide. NaOH formed a protective and low friction film on iron surfaces. The coefficient of friction and the wear for iron were low at concentrations of NaOH higher than 0.01 N. An increase in NaOH concentration resulted in a decrease in the concentration of ferric oxide on the iron surface. It took less NaOH to form a protective, low friction film on nickel than on iron.

Miyoshi, K.↗

Strength and fracture of glass in the lunar environment

Due to the lack of water on the moon, the effects of hydrolytic depolymerization - stress corrosion cracking - will be nonexistent in glasses produced and used on the moon. This would seem to make lunar glass very attractive for use in a wide variety of space engineering applications. We have applied the equation that describes stress corrosion cracking to lunar glass to show that, indeed, decreasing water vapor pressure results in an increase in strength. Experimental results on simulated lunar glass confirm this. The stress corrosion equation predicts an extremely high strength for glasses produced on the moon. This equation, however, cannot be applied to glasses under anhydrous conditions. In an environment completely devoid of water, the strength of glass will be determined by the fracture of the glass at the tip of a flaw, without the corrosive effects of water. Under this condition, in accordance with fracture theory, the strength of the glass will primarily be a function of the flaw size. Our experimental results show that the presence of surface flaws is more detrimental to the strength of simulated lunar glass than the effect of hydrolytic depolymerization.

Allen, Daniel D.↗

Real-Time Electrochemical Measurements Of Carbon Steel In Ground Water With Sulfate Reducing Bacteria Enrichment - 15604

A new laboratory system for studying the microbiological corrosion of decommissioning waste was designed and developed during this project. The material in this part of the laboratory studies was carbon steel (AISI/SAE 1005/UNS G10050). In order to estimate the corrosive effects of microbial activity both biotic and abiotic (containing the biocides methyl-isothiazolinone and glutaraldehyde) mesocosms were prepared. To enhance the effects of sulfate reducing bacteria an enrichment of these bacteria isolated from the native drill hole water from the repository site was inoculated in to the biotic mesocosms. Microbiological corrosion was studied using new electrochemical technologies, such as multi-electrode arrays sensors, and molecular biology methods in the laboratory. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Effect of H2S on performance of Pd4Pt alloy membranes

The effect of H2S on the performance of a hydrogen separation membrane with the composition Pd4Pt was evaluated at 350, 400 and 450°C. Exposure to hydrogen containing 1000 ppm H2S and 10%He resulted in two performance trends. At 350°C, a continuous decline in flux was observed which was attributed to the growth of sulphide corrosion on the membrane surface linked to surface contamination by stainless steel derived particles. At 400 and 450°C, the H2 flux decreased sharply followed by a slow recovery. This trend was attributed to Pt enrichment of the surface resulting from extraction of Pd through the formation of Pd4Pt. Also at 400 and 450°C, stainless steel based particle contamination was found to modify and/or enhance the corrosive effects of the H2S containing test gas. The implications of the metallic and/or metal sulphide surface contaminant effects are significant in that these contaminants could result in severe performance degradation and ultimately even mechanical failure.

36 MATERIALS SCIENCE↗

NASA's Corrosion Technology Laboratory at the Kennedy Space Center: Anticipating, Managing, and Preventing Corrosion

Corrosion is the degradation of a material that results from its interaction with the environment. The marine environment at NASAs Kennedy Space Center (KSC) has been documented by ASM International (formerly American Society for Metals) as the most corrosive in the United States. With the introduction of the Space Shuttle in 1981, the already highly corrosive conditions at the launch pads were rendered even more severe by the 70 tons of highly corrosive hydrochloric acid that were generated by the solid rocket boosters. Numerous failures at the launch pads are caused by corrosion.The structural integrity of ground infrastructure and flight hardware is critical to the success, safety, cost, and sustainability of space missions. As a result of fifty years of experience with launch and ground operations in a natural marine environment that is highly corrosive, NASAs Corrosion Technology Laboratory at KSC is a major source of corrosion control expertise in the launch and other environments. Throughout its history, the Laboratory has evolved from what started as an atmospheric exposure facility near NASAs launch pads into a world-wide recognized capability that provides technical innovations and engineering services in all areas of corrosion for NASA and external customers.This presentation will provide a historical overview of the role of NASAs Corrosion Technology in anticipating, managing, and preventing corrosion. One important challenge in managing and preventing corrosion involves the detrimental impact on humans and the environment of what have been very effective corrosion control strategies. This challenge has motivated the development of new corrosion control technologies that are more effective and environmentally friendly. Strategies for improved corrosion protection and durability can have a huge impact on the economic sustainability of human spaceflight operations.

Corrosion↗

NASA's Corrosion Technology Laboratory at the Kennedy Space Center: Anticipating, Managing, and Preventing Corrosion

The marine environment at NASAs Kennedy Space Center (KSC) has been documented by ASM International (formerly American Society for Metals) as the most corrosive in North America. With the introduction of the Space Shuttle in 1981, the already highly corrosive conditions at the launch pads were rendered even more severe by the highly corrosive hydrochloric acid (HCl) generated by the solid rocket boosters (SRBs). Numerous failures at the launch pads are caused by corrosion. The structural integrity of ground infrastructure and flight hardware is critical to the success, safety, cost, and sustainability of space missions. NASA has over fifty years of experience dealing with unexpected failures caused by corrosion and has developed expertise in corrosion control in the launch and other environments. The Corrosion Technology Laboratory at KSC evolved, from what started as an atmospheric exposure test site near NASAs launch pads, into a capability that provides technical innovations and engineering services in all areas of corrosion for NASA, external partners, and customers.This paper provides a chronological overview of NASAs role in anticipating, managing, and preventing corrosion in highly corrosive environments. One important challenge in managing and preventing corrosion involves the detrimental impact on humans and the environment of what have been very effective corrosion control strategies. This challenge has motivated the development of new corrosion control technologies that are more effective and environmentally friendly. Strategies for improved corrosion protection and durability can have a huge impact on the economic sustainability of human spaceflight operations.

Corrosion Control↗

Synthesis and Characterization of Zeolites for Anti-corrosion Application: The Effect of Precursor and Hydrothermal Treatment

Four different hydrothermal processes were used to synthesize NaX zeolites. The effect of the precursor, hydrothermal time and temperature on the zeolite structure was investigated in this research. The results of XRD and FESEM/EDX analysis indicated the key role of aluminum sources in the amorphous content and the structure of zeolite from non-zeolite sodium aluminum silicate hydrate to favorable NaX-faujasite. Moreover, the irregular shape of agglomerated hydrogel was changed from micro- to nano-zeolite structure via the hydrothermal process of different aluminum sources. It was found that the nano-zeolites could be formed by sodium aluminate source. In addition, the synthesized zeolite particles were examined as corrosion inhibitor reservoir, considering the effect of Si/Al ratio, particle size, and amorphous content. It was shown that there is a direct relation between crystallization and ion exchange capacity. Through monitoring the behavior of bare mild steel in sodium chloride solution containing zinc cations released from the zeolite particles, it was found that the nano-zeolite particles with low Si/Al ratio can offer the most effective corrosion inhibition.

36 MATERIALS SCIENCE↗

Corrosion of Candidate Materials in Molten FLiBe Salt for Fluoride-Salt-Cooled High-Temperature Reactor (FHR)

Molten fluoride salts have attracted considerable attention because of their desirable thermophysical properties that lead to superior heat transfer. Recently, fluoride salts are being considered as coolants in the fluoride salt-cooled high temperature reactors (FHRs). The successes of the molten salt reactor experiment (MSRE) program in 1950's-70's at Oak Ridge National Laboratory (ORNL) has also driven the pursuit of molten salt nuclear reactor as one of the lead next generation nuclear reactor concepts. Unlike MSRE where the uranium fuel was dissolved in the molten fluoride salt, the FHR concept is expected to use molten salt (2LiF-BeF{sub 2}, FLiBe) only as coolant in conjunction with solid TRISO fuel particles immersed in the molten salt. One of the important challenges in FHR development is corrosion of structural materials in high-temperature molten 2LiF-BeF{sub 2} (FLiBe) salt. Currently, 316 stainless steel (nominal composition: Fe-12Ni-17Cr-2.5Mo-1Si-2Mn-0.03C) and Hastelloy N (nominal composition: Ni-7Cr-16Mo-5Fe-1Si-0.8Mn) are deemed as promising candidate alloys for the construction of some of the structural components of FHR. 316 stainless steel is ASME code certified for high temperatures (up to 760 deg. C) applications. Hastelloy N has been shown to have outstanding corrosion resistance in molten FLiBe but present code certification data limit the use of this alloy to only about 704 deg. C. Modifications of Hastelloy N with higher creep strength are presently being developed at ORNL. Other materials such graphite, SiC/SiCf and C/Cf composites, are also considered for structural applications in the FHR. The presence of these multiple materials in a molten FLiBe salt medium can further exacerbate and complicate corrosion effects. Therefore, it is necessary to understand the corrosion behavior of these materials in molten FLiBe salt. The corrosion behavior of Hastelloy N, 316 stainless steel, and CVD SiC and two types of SiC-SiC{sub f} composites have been tested in molten FLiBe salt at 700 deg. C. When tested in metal-lined crucibles both Hastelloy N and 316 stainless steel showed very good corrosion resistance. Samples tested in graphite crucibles showed greater propensity for corrosion and carburization was observed in the near surface regions of the alloys. CVD SiC showed outstanding corrosion resistance. However, the two SiC-SiC{sub f} composites exhibited corrosion attack implying that the manufacturing process may play a role in the corrosion of these composites. (authors)

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Mechanical Properties and Corrosion Behavior of AA5754-AA6061 Dissimilar Aluminum Alloys Welded by Cold Metal Transfer

The trend of using lightweight materials in the automotive industry brings along the necessity of dissimilar welding of aluminum alloys such as AA5754 and AA6061. Hybrid structures in automobiles are subjected not only to mechanical forces but also corrosive effects of the environment. In this study, cold metal transfer welding, which is suitable for welding thin sheets and dissimilar materials, was applied to join AA5754 to AA6061. It was aimed to investigate the effect of weld heat input on mechanical properties and corrosion rate measured by the Tafel extrapolation method in 3.5 wt.% NaCl solution at room temperature. The tensile strength of AA5754-AA6061 joints tended to reduce with increasing heat input. Corrosion test results showed that the increased heat input decreased the corrosion resistance and caused intergranular corrosion besides pitting corrosion.

36 MATERIALS SCIENCE↗

Laser Confocal Microscopy Uncertainty Quantification Study

At Los Alamos National Laboratory (LANL), the Storage Safety and Engineering (SSE) team completes annual surveillance on a subset of in-use interim nuclear material storage containers in fulfilment of requirements outlined in DOE Manual M 441.1-1. The containers are selected through several methods, such as subject matter expert judgement, random selection, and trending items. Following these selections, the SSE team has the capacity to complete surveillance on 15-20 containers each fiscal year, composed of a combination of SAVY-4000 and Hagan storage containers. Through previous work, the stainless-steel components of the containers have been identified as life limiting components, with an emphasis on the thin-walled bodies. The team is focused on understanding the extent of general and pitting corrosion, due to observations of extensive corrosion from stored contents and bag-out-bag degradation. Quantifying corrosion effects on the thin-walled stainless steel container bodies, and understanding potential impacts to the respective design release rates and design qualification release rates is paramount to the team. To date, destructive examination (DE) has proven to be the most insightful method for developing an understanding on the extent of corrosion on used containers. To standardize this process, the SSE team developed a destructive examination guide for analyzing stainless steel components of the containers. Corroded containers of interest are identified during surveillance activities and set aside for sectioning and characterization. Following sectioning, a major step in the DE workflow is the utilization of laser confocal microscopy for scanning corroded samples of interest and extracting data on pits, such as count, depth, and equivalent diameter. Adhering to the techniques outlined in the DE guide, analysis has been completed on two Hagans and one SAVY-4000 container, with the maximum pit depth recorded as 139.1 ± 22.82 μm on a 17.5 year old Hagan. The findings from the completed destructive examinations will be utilized to support lifetime extension efforts of the SAVY-4000 as the team can better estimate corrosion rates and effects over time based on stored contents and age. Due to the implications of observing extreme pit depths that approach the nominal container body thickness of .0299 inches (0.759 mm) or minimum container thickness of 0.236” (0.6 mm), high confidence in the LCM measurements is desired. Through testing outlined in, it was concluded that the total error ascribed to the 20x objective when conducting large image mapping on the Keyence VK-X3050 laser confocal microscope (LCM) relative to a 50x objective (reference) is 16.4% (± 8.73%). For shallow features on the order of pristine SAVY surface defects (i.e. 5 μm), this uncertainty is appropriate. However, this conservative estimate of total error poses a fundamental concern for pit depths that approach the thickness of the measured samples. That is, with the measurement uncertainty currently employed on all measurements, the LCM would be unable to resolve if a pit with a depth of 515 μm is through wall. Standard step height samples were procured and used in the present study to assess the resolution and repeatability of height measurements. Understanding the resolution and repeatability of height measurements was the first focus of the team as it relates directly to pit depth, which is of primary concern. Calibration gratings were procured to evaluate the resolution and repeatability of measurements in the X and Y axes of the LCM stage. The results of the depth uncertainty study were conducted first and presented in the subsequent sections. The planar uncertainty study is appended to the depth study with conclusions from both summarized at the end of the report.

36 MATERIALS SCIENCE↗

Environmentally Friendly Zr-Based Conversion Nanocoatings for Corrosion Inhibition of Metal Surfaces Evaluated by Multimodal X-ray Analysis

Chemical conversion coating as an effective corrosion inhibition has wide range of applications in industries and is of great expectation to be environmentally friendly and cost-effective. Zirconium-based (Zr-based) conversion coating using hexafluorozirconic acid with copper (Cu) additive on low carbon steel which improves anticorrosion and adhesion properties was studied using synchrotron X-ray and electron-based techniques. To understand the elemental evolution during coating formation process, in situ synchrotron X-ray fluorescence (XRF) microscopy has been applied to observe Zr, Cu, iron (Fe), and zinc (Zn) concentration evolution. By quantifying the density, average size, and size distribution of the cluster as a function of time and temperature, the growth mechanism of the coating can be concluded as a reaction-controlled mechanism. X-ray absorption near edge structure and X-ray photoelectron spectroscopy (XPS) were used to characterize the composition of the Cu-rich clusters embedded in the coating which was determined to be mainly Cu 2 O, Cu, and CuF 2 ; the cluster composition varies from the surface to the internal region as determined by the depth-profiling of XPS. Our study shed light on the chemical and morphological evolution in environmentally friendly surface conversation coating and demonstrated new methodology in studying the coating formation via in situ synchrotron XRF.

36 MATERIALS SCIENCE↗

A Semi-Empirical Two Step Carbon Corrosion Reaction Model in PEM Fuel Cells

The cathode CL of a polymer electrolyte membrane fuel cell (PEMFC) was exposed to high potentials, 1.0 to 1.4 V versus a reversible hydrogen electrode (RHE), that are typically encountered during start up/shut down operation. While both platinum dissolution and carbon corrosion occurred, the carbon corrosion effects were isolated and modeled. The presented model separates the carbon corrosion process into two reaction steps; (1) oxidation of the carbon surface to carbon-oxygen groups, and (2) further corrosion of the oxidized surface to carbon dioxide/monoxide. To oxidize and corrode the cathode catalyst carbon support, the CL was subjected to an accelerated stress test cycled the potential from 0.6 VRHE to an upper potential limit (UPL) ranging from 0.9 to 1.4 VRHE at varying dwell times. The reaction rate constants and specific capacitances of carbon and platinum were fitted by evaluating the double layer capacitance (Cdl) trends. Carbon surface oxidation increased the Cdl due to increased specific capacitance for carbon surfaces with carbon-oxygen groups, while the second corrosion reaction decreased the Cdl due to loss of the overall carbon surface area. The first oxidation step differed between carbon types, while both reaction rate constants were found to have a dependency on UPL, temperature, and gas relative humidity.

08 HYDROGEN↗

Effect of Control Mode and Test Rate on the Measured Fracture Toughness of Advanced Ceramics

The effects of control mode and test rate on the measured fracture toughness of ceramics were evaluated by using chevron-notched flexure specimens in accordance with ASTM C1421. The use of stroke control gave consistent results with about 2% (statistically insignificant) variation in measured fracture toughness for a very wide range of rates (0.005 to 0.5 mm/min). Use of strain or crack mouth opening displacement (CMOD) control gave approx. 5% (statistically significant) variation over a very wide range of rates (1 to 80 μm/m/s), with the measurements being a function of rate. However, the rate effect was eliminated by use of dry nitrogen, implying a stress corrosion effect rather than a stability effect. With the use of a nitrogen environment during strain controlled tests, fracture toughness values were within about 1% over a wide range of rates (1 to 80 micons/m/s). CMOD or strain control did allow stable crack extension well past maximum force, and thus is preferred for energy calculations. The effort is being used to confirm recommendations in ASTM Test Method C1421 on fracture toughness measurement.

silicon nitride↗

Effect of Control Mode and Load Rate on Fracture Toughness of Brittle Ceramics

The effects of control mode and rate on the fracture toughness of ceramics were measured by using chevron-notched flexure specimen in accordance with ASTM C1421. The use of stroke control gave consistent results with about 2% variation in measured fracture toughness for a very wide range of rates (0.005 to 0.5 mm/min). Use of strain or CMOD control gave an approximately 5% variation over a very wide range of rates, with the measurements being a function of rate. However, the effect was eliminated by use of dry nitrogen, implying a stress corrosion effect rather than a stability effect. With the use of nitrogen for strain control, fracture toughness values were within about 1% over a wide range of rates (1 to 80 micro-epsilon/sec.). CMOD or strain control did allow stable crack extension well past maximum load, and thus is preferred for energy calculations. The effort is being used to confirm recommendations in ASTM International standard C1421 on fracture toughness measurement.

control mode↗

Effect of Control Mode and Test Rate on Fracture Toughness of Advanced Ceramics

The effects of control mode and rate on the fracture toughness of ceramics were measured by using chevron-notched flexure specimen in accordance with ASTM C1421. The use of stroke control gave consistent results with about 2% variation in measured fracture toughness for a very wide range of rates (0.005 to 0.5 mm/min). Use of strain or CMOD control gave ~5% variation over a very wide range of rates, with the measurements being a function of rate. However, the effect was eliminated by use of dry nitrogen, implying a stress corrosion effect rather than a stability effect. With the use of nitrogen for strain control, fracture toughness values were within about 1% over a wide range of rates (1 to 80 /s). CMOD or strain control did allow stable crack extension well past maximum load, and thus is preferred for energy calculations. The effort is being used to confirm recommendations in ASTM International standard C1421 on fracture toughness measurement.

fracture toughness↗

Evaluation of Aluminum-Boron Carbide Neutron Absorbing Materials for Interim Storage of Used Nuclear Fuel

The objective of this work was to understand the corrosion behavior of Boral® and Bortec® neutron absorbers over long-term deployment in a used nuclear fuel dry cask storage environment. Corrosion effects were accelerated by flowing humidified argon through an autoclave at temperatures up to 570°C. Test results show little corrosion of the aluminum matrix but that boron is leaching out of the samples. Initial tests performed at 400 and 570°C were hampered by reduced flow caused by the rapid build-up of solid deposits in the outlet lines. Analysis of the deposits by XRD shows that the deposits are comprised of boron trioxide and sassolite (H 3 BO 3 ). The collection of boron- containing compounds in the outlet lines indicated that boron was being released from the samples. Observation of the exposed samples using SEM and optical microscopy show the growth of new phases in the samples. These phases were most prominent in Bortec® samples exposed at 570°C. Samples of Boral® exposed at 570°C showed minimal new phase formation but showed nearly the complete loss of boron carbide particles. Boron carbide loss was also significant in Boral samples at 400°C. However, at 400°C phases similar to those found in Bortec® were observed. The rapid loss of the boron carbide particles in the Boral® is suspected to inhibit the formation of the new secondary phases. However, Material samples in an actual dry cask environment would be exposed to temperatures closer to 300°C and less water than the lowest test. The results from this study conclude that at the temperature and humidity levels present in a dry cask environment, corrosion and boron leaching will have no effect on the performance of Boral® and Bortec® to maintain criticality control.