Search NASA⌕ Search

SEARCH · Search NASA

Results for “Coating cracking”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

The Characterization of the Selected Materials for Space Shuttle

The harsh conditions to which the Space Shuttles are exposed during flight required the development and use of many unique materials. These materials were specially designed to withstand extreme temperatures, in some cases over 1600 C, while other material must withstand the cryogenic conditions of -253 C, and others must operate while under extreme loads. All of these materials must not only operate in the harsh condition but they must be light weight as well. The Space Shuttle is composed of three major components when configured for launch, Figure 1; the Shuttle, solid rocket boosters, and external tank (ET). The different heat shields of the Shuttle make up the thermal protection system (TPS); this system consists of many different types of components designed to operate on various parts of the vehicle. The body of the Shuttle and ET are composed mainly of aluminum alloy and graphite epoxy. The TPS consists of reinforced carbon-carbon (RCC) used on the wing leading edges and nose cap areas while the upper forward fuselage areas, the entire underside of the Shuttle, the Orbiter maneuvering system, and reaction control system utilize blacc high temperature reusable surface insulation (HRSI) tiles, Figure 2. Other areas of the Orbiter are protected by fibrous refractory composite insulation (FRCI) tiles. Areas where the temperature stays below 649 C, such as the forward fuselage, mid-fuselage, aft fuselage, vertical tail, and upper wing, are protected by other material such as, white low temperature reusable surface insulation (LRSI) tiles, advanced flexible reusable surface insulation (AFRSI) blankets, and felt reusable surface insulation (FRSI) white blankets. The RCC is a pyrolized laminated carbon with the outer surface converted to silicon carbide to prevent oxidation. The FiRST tiles are made of a low-density, high purity silica 99.8-percent amorphous fiber insulation that is made rigid by ceramic bonding resulting in 90-percent void and 10-percent materials. The RCC and HRSI are used in areas where the temperature rises above 1260 T. The FRCI tiles are high strength tiles derived by adding alumina-bososilicate fiber to the pure silica tile slurry that welds the micron-sizes fibers of pure silica into a rigid structure during sintering. The FRCI is composed of 20-percent alumina-borosilicate fibers and 80-percent silica fibers, and provided improved strength, durability and resistance to coating cracking and weight reduction than HRSI.

Kim, Hae-Soo↗

Deep Impact Delta II Launch Vehicle Cracked Thick Film Coating on Electronic Packages Technical Consultation Report

The Deep Impact spacecraft was launched on a Boeing Delta II rocket from Cape Canaveral Air Force Station (CCAFS) on January 12, 2005. Prior to the launch, the Director of the Office of Safety and Mission Assurance (OS&MA) requested the NASA Engineering and Safety Center (NESC) lead a team to render an independent opinion on the rationale for flight and the risk code assignments for the hazard of cracked Thick Film Assemblies (TFAs) in the E-packages of the Delta II launch vehicle for the Deep Impact Mission. The results of the evaluation are contained in this report.

Cameron, Kenneth D.↗

Method for thermally spraying crack-free mullite coatings on ceramic-based substrates

A process for depositing a mullite coating on a silicon-based material, such as those used to form articles exposed to high temperatures and including the hostile thermal environment of a gas turbine engine. The process is generally to thermally spray a mullite powder to form a mullite layer on a substrate, in which the thermal spraying process is performed so that the mullite powder absorbs a sufficient low level of energy from the thermal source to prevent evaporation of silica from the mullite powder. Processing includes deposition parameter adjustments or annealing to maintain or reestablish phase equilibrium in the mullite layer, so that through-thickness cracks in the mullite layer are avoided.

Spitsberg, Irene T.↗

Method for thermally spraying crack-free mullite coatings on ceramic-based substrates

A process for depositing a mullite coating on a silicon-based material, such as those used to form articles exposed to high temperatures and including the hostile thermal environment of a gas turbine engine. The process is generally to thermally spray a mullite powder to form a mullite layer on a substrate, in which the thermal spraying process is performed so that the mullite powder absorbs a sufficient low level of energy from the thermal source to prevent evaporation of silica from the mullite powder. Processing includes deposition parameter adjustments or annealing to maintain or reestablish phase equilibrium in the mullite layer, so that through-thickness cracks in the mullite layer are avoided.

Spitsberg, Irene T.↗

Failure Mechanisms and Life Prediction of Thermal and Environmental Barrier Coatings under Thermal Gradients

Ceramic thermal and environmental barrier coatings (TEBCs) will play an increasingly important role in gas turbine engines because of their ability to further raise engine temperatures. However, the issue of coating durability is of major concern under high-heat-flux conditions. In particular, the accelerated coating delamination crack growth under the engine high heat-flux conditions is not well understood. In this paper, a laser heat flux technique is used to investigate the coating delamination crack propagation under realistic temperature-stress gradients and thermal cyclic conditions. The coating delamination mechanisms are investigated under various thermal loading conditions, and are correlated with coating dynamic fatigue, sintering and interfacial adhesion test results. A coating life prediction framework may be realized by examining the crack initiation and propagation driving forces for coating failure under high-heat-flux test conditions.

Zju, Dongming↗

Anodized aluminum coatings for thermal control. II - Environmental effects and cracking

The environmental effects of thermal cycling and humidity on coating cracking are examined. Experimental measurements of thermal deflection were used to calculate values for the thermal expansion coefficient and the in situ elastic modulus of an anodized aluminum. The thermal expansion coefficient is found to be approximately the same as for alumina in bulk form. The modulus in atmospheres with less than 100 ppm water is about 12,500 ksi. Two sets of experiments are used to study cracking directly during thermal excursions: one determines the minimum temperature (Tc) at which cracks first appear during a single heating cycle and the other involves rapid thermal cycling (RTC) between fixed T max and T min values. Fatigue models for describing initiation of the first crack and the development of multiple cracking are presented, which can be used as the basis for prediction of LEO cracking.

Mcclung, R. C.↗

Crack Driving Forces in a Multilayered Coating System for Ceramic Matrix Composite Substrates

The effects of the top coating thickness, modulus and shrinkage strains on the crack driving forces for a baseline multilayer Yttria-Stabilized-Zirconia/Mullite/Si thermal and environment barrier coating (TEBC) system for SiC/SiC ceramic matrix composite substrates are determined for gas turbine applications. The crack driving forces increase with increasing modulus, and a low modulus thermal barrier coating material (below 10 GPa) will have no cracking issues under the thermal gradient condition analyzed. Since top coating sintering increases the crack driving forces with time, highly sintering resistant coatings are desirable to maintain a low tensile modulus and maintain a low crack driving force with time. Finite element results demonstrated that an advanced TEBC system, such as ZrO2/HfO2, which possesses improved sintering resistance and high temperature stability, exhibited excellent durability. A multi-vertical cracked structure with fine columnar spacing is an ideal strain tolerant coating capable of reducing the crack driving forces to an acceptable level even with a high modulus of 50 GPa.

Ghosn, Louis J.↗

Nondestructive Evaluation (NDE) for Characterizing Oxidation Damage in Cracked Reinforced Carbon-Carbon

In this study, coated reinforced carbon-carbon (RCC) samples of similar structure and composition as that from the NASA space shuttle orbiter's thermal protection system were fabricated with slots in their coating simulating craze cracks. These specimens were used to study oxidation damage detection and characterization using nondestructive evaluation (NDE) methods. These specimens were heat treated in air at 1143 C and 1200 C to create cavities in the carbon substrate underneath the coating as oxygen reacted with the carbon and resulted in its consumption. The cavities varied in diameter from approximately 1 to 3mm. Single-sided NDE methods were used because they might be practical for on-wing inspection, while X-ray micro-computed tomography (CT) was used to measure cavity sizes in order to validate oxidation models under development for carbon-carbon materials. An RCC sample having a naturally cracked coating and subsequent oxidation damage was also studied with X-ray micro-CT. This effort is a follow-on study to one that characterized NDE methods for assessing oxidation damage in an RCC sample with drilled holes in the coating.

Roth, Don J.↗

High temperature constitutive and crack initiation modeling of coated single crystal superalloys

The purpose of this program is to develop life prediction models for anisotropic materials used in gas turbine airfoils. In the base portion of the program, two coated single crystal alloys are being tested. They are PWA 286 overlay coated and PWA 273 aluminide coated PWA 1480 and PWA 286 overlay coated Alloy 185. Viscoplastic constitutive models for these materials are also being developed to predict the cyclic stress-strain histories required for life prediction of the lab specimens and actual airfoil designs.

Meyer, Thomas G.↗

Surface Cracking and Interface Reaction Associated Delamination Failure of Thermal and Environmental Barrier Coatings

In this paper, surface cracking and interface reactions of a BSAS coating and a multi-layer ZTO2-8wt%Y2O3 and mullite/BSAS/Si thermal and environmental barrier coating system on SiC/SiC ceramic matrix composites were characterized after long-term combined laser thermal gradient and furnace cyclic tests in a water vapor containing environment. The surface cracking was analyzed based on the coating thermal gradient sintering behavior and thermal expansion mismatch stress characteristics under the thermal cyclic conditions. The interface reactions, which were largely enhanced by the coating surface cracking in the water vapor environment, were investigated in detail, and the reaction phases were identified for the coating system after the long- term exposure. The accelerated coating delamination failure was attributed to the increased delamination driving force under the thermal gradient cyclic loading and the reduced interface adhesion due to the detrimental interface reactions.

Zhu, Dongming↗

Surface Cracking and Interface Reaction Associated Delamination Failure of Thermal and Environmental Barrier Coatings

In this paper, surface cracking and interface reactions of a BSAS coating and a multi-layer ZrO2-8wt%Y2O3 and mullite/BSAS/Si thermal and environmental barrier coating system on SiC/SiC ceramic matrix composites were characterized after long-term combined laser thermal gradient and furnace cyclic tests in a water vapor containing environment. The surface cracking was analyzed based on the coating thermal gradient sintering behavior and thermal expansion mismatch stress characteristics under the thermal cyclic conditions. The interface reactions, which were largely enhanced by the coating surface cracking in the water vapor environment, were investigated in detail, and the reaction phases were identified for the coating system after the long-term exposure. The accelerated coating delamination failure was attributed to the increased delamination driving force under the thermal gradient cyclic loading and the reduced interface adhesion due to the detrimental interface reactions.

Zhu, Dong-Ming↗

NDE for Characterizing Oxidation Damage in Reinforced Carbon-Carbon

In this study, coated reinforced carbon-carbon (RCC) samples of similar structure and composition as that from the NASA space shuttle orbiter s thermal protection system were fabricated with slots in their coating simulating craze cracks. These specimens were used to study oxidation damage detection and characterization using NDE methods. These specimens were heat treated in air at 1143 and 1200 C to create cavities in the carbon substrate underneath the coating as oxygen reacted with the carbon and resulted in its consumption. The cavities varied in diameter from approximately 1 to 3 mm. Single-sided NDE methods were used since they might be practical for on-wing inspection, while x-ray micro-computed tomography (CT) was used to measure cavity sizes in order to validate oxidation models under development for carbon-carbon materials. An RCC sample having a naturally-cracked coating and subsequent oxidation damage was also studied with x-ray micro-CT. This effort is a follow-on study to one that characterized NDE methods for assessing oxidation damage in an RCC sample with drilled holes in the coating. The results of that study are briefly reviewed in this article as well. Additionally, a short discussion on the future role of simulation to aid in these studies is provided.

Roth, Don J.↗

Nondestructive Evaluation (NDE) for Characterizing Oxidation Damage in Cracked Reinforced Carbon-Carbon (RCC)

In this study, coated reinforced carbon-carbon (RCC) samples of similar structure and composition as that from the NASA space shuttle orbiter's thermal protection system were fabricated with slots in their coating simulating craze cracks. These specimens were used to study oxidation damage detection and characterization using nondestructive evaluation (NDE) methods. These specimens were heat treated in air at 1143 and 1200 C to create cavities in the carbon substrate underneath the coating as oxygen reacted with the carbon and resulted in its consumption. The cavities varied in diameter from approximately 1 to 3 mm. Single-sided NDE methods were used since they might be practical for on-wing inspection, while x-ray micro-computed tomography (CT) was used to measure cavity sizes in order to validate oxidation models under development for carbon-carbon materials. An RCC sample having a naturally-cracked coating and subsequent oxidation damage was also studied with x-ray micro-CT. This effort is a follow-on study to one that characterized NDE methods for assessing oxidation damage in an RCC sample with drilled holes in the coating.

Roth, Don J.↗

Environmental Barrier Coating Fracture, Fatigue and High-Heat-Flux Durability Modeling and Stochastic Progressive Damage Simulation

Advanced environmental barrier coatings will play an increasingly important role in future gas turbine engines because of their ability to protect emerging light-weight SiC/SiC ceramic matrix composite (CMC) engine components, further raising engine operating temperatures and performance. Because the environmental barrier coating systems are critical to the performance, reliability and durability of these hot-section ceramic engine components, a prime-reliant coating system along with established life design methodology are required for the hot-section ceramic component insertion into engine service. In this paper, we have first summarized some observations of high temperature, high-heat-flux environmental degradation and failure mechanisms of environmental barrier coating systems in laboratory simulated engine environment tests. In particular, the coating surface cracking morphologies and associated subsequent delamination mechanisms under the engine level high-heat-flux, combustion steam, and mechanical creep and fatigue loading conditions will be discussed. The EBC compostion and archtechture improvements based on advanced high heat flux environmental testing, and the modeling advances based on the integrated Finite Element Analysis Micromechanics Analysis Code/Ceramics Analysis and Reliability Evaluation of Structures (FEAMAC/CARES) program will also be highlighted. The stochastic progressive damage simulation successfully predicts mud flat damage pattern in EBCs on coated 3-D specimens, and a 2-D model of through-the-thickness cross-section. A 2-parameter Weibull distribution was assumed in characterizing the coating layer stochastic strength response and the formation of damage was therefore modeled. The damage initiation and coalescence into progressively smaller mudflat crack cells was demonstrated. A coating life prediction framework may be realized by examining the surface crack initiation and delamination propagation in conjunction with environmental degradation under high-heat-flux and environment load test conditions.

Mechanical creep and fatigue loading condition↗

Thermophysical and Thermomechanical Properties of Thermal Barrier Coating Systems

Thermal barrier coatings have been developed for advanced gas turbine and diesel engine applications to improve engine reliability and fuel efficiency. However, the issue of coating durability under high temperature cyclic conditions is still of major concern. The coating failure is closely related to thermal stresses and oxidation in the coating systems. Coating shrinkage cracking resulting from ceramic sintering and creep at high temperatures can further accelerate the coating failure process. The purpose of this paper is to address critical issues such as ceramic sintering and creep, thermal fatigue and their relevance to coating life prediction. Novel test approaches have been established to obtain critical thermophysical and thermomechanical properties of the coating systems under near-realistic temperature and stress gradients encountered in advanced engine systems. Emphasis is placed on the dynamic changes of the coating thermal conductivity and elastic modulus, fatigue and creep interactions, and resulting failure mechanisms during the simulated engine tests. Detailed experimental and modeling results describing processes occurring in the thermal barrier coating systems provide a framework for developing strategies to manage ceramic coating architecture, microstructure and properties.

Zhu, Dongming↗

Research on High Temperature Ceramic Insulation for Electrical Conductors

Three methods for applying ceramic coatings to wires were examined in depth and a fourth (chemical vapor deposition) was studied briefly. CVD coatings were not reported in the thesis because it was realized early in the study that the deposition rate of the coatings was too slow to be used in a commercial process. Of the methods reported in the thesis, slurry coating was the most promising. This method consists of slowly drawing a platinum wire through a thixotropic slurry of alumina in a vehicle composed of polyvinyl butyral, methyl ethyl ketone, and toluene. The coatings produced by this method were continuous and free of cracks after sintering. The sintered coatings crack when the wire is bent around sharp corners, but most of the coating remains in place and still provides electrical insulation between the wire and any metallic structure to which the wire may be attached. The coating thickness was 0.61 mm (16 micrometers). The electrical resistivity of the intact coating was 340 M-Ohm-cm at 800 C and 23 M-Ohm-cm at 1050 C. Therefore, these coatings more than meet the electrical requirements for use in turbine engines. Although adherence of the coating to the wire was generally excellent, a problem was noted in localized areas where the coating flaked off. Further work will be needed to obtain good coating adherence along the entire length of the wire. The next most promising coatings were made by electrophoretic deposition (EPD) of Al2O3 onto platinum wires, using mixtures of ethanol and acetone as the suspending liquid. These EPD coatings were made only on short lengths of wire because the coating is too fragile to allow spooling of the wire. The worst coatings were those made by electrophoretic deposition from aqueous suspensions. Continuous slurry coating of wire was achieved, but due to lack of suitable equipment, the wire had to be cut into short lengths for sintering.

Kreidler, Eric R.↗