Search NASA⌕ Search

SEARCH · Search NASA

Results for “Deformation mechanisms”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

Clarification of creep deformation mechanism in heat-affected zone of 9Cr steels with In Situ experiments

This work quantified nonuniform creep deformation across the heterogeneous heat-affected zone (HAZ) of Grade 91 steel with sophisticated experiments, including an electric-thermal finite element model–assisted Gleeble thermomechanical simulation and a high-temperature creep testing with in situ digital image correlation (DIC). High temperature creep properties of HAZ sub-zones were quantitatively measured by the DIC. Furthermore, by utilizing peak temperature, hardness, local creep strain, and underlying microstructures, creep deformation mechanisms in HAZ were further understood. DIC measurements reveal a creep-vulnerable zone (CVZ) exposed to a peak temperature of 932°C (close to A C3 ) in the intercritical HAZ experienced the fastest creep strength degradation instead of the soft zone with the lowest hardness prior to creep. The significantly reduced precipitation strengthening from misplacement of undissolved and coarsened M 23 C 6 carbides led to a faster recrystallization of tempered martensite in the CVZ. Weak untransformed tempered martensite (ferrite grains) stabilized by local Cr enrichment from dissolved M 23 C 6 also harmed the CVZ's creep resistance.

36 MATERIALS SCIENCE↗

Temperature Dependent Cyclic Deformation Mechanisms in Haynes 188 Superalloy

The cyclic deformation behavior of a wrought cobalt-base superalloy, Haynes 188, has been investigated over a range of temperatures between 25 and 1000 C under isothermal and in-phase thermomechanical fatigue (TMF) conditions. Constant mechanical strain rates (epsilon-dot) of 10(exp -3)/s and 10(exp -4)/s were examined with a fully reversed strain range of 0.8%. Particular attention was given to the effects of dynamic strain aging (DSA) on the stress-strain response and low cycle fatigue life. A correlation between cyclic deformation behavior and microstructural substructure was made through detailed transmission electron microscopy. Although DSA was found to occur over a wide temperature range between approximately 300 and 750 C the microstructural characteristics and the deformation mechanisms responsible for DSA varied considerably and were dependent upon temperature. In general, the operation of DSA processes led to a maximum of the cyclic stress amplitude at 650 C and was accompanied by pronounced planar slip, relatively high dislocation density, and the generation of stacking faults. DSA was evidenced through a combination of phenomena, including serrated yielding, an inverse dependence of the maximum cyclic hardening with epsilon-dot, and an instantaneous inverse epsilon-dot sensitivity verified by specialized epsilon-dot -change tests. The TMF cyclic hardening behavior of the alloy appeared to be dictated by the substructural changes occuring at the maximum temperature in the TMF cycle.

Rao, K. Bhanu Sankara↗

Dislocations: 75 years of Deformation Mechanisms

The selection of papers presented in this section reflect on themes to be explored at the "Dislocations: 75 years of Deformation Mechanisms" Symposium to be held at the Annual 2009 TMS meeting. The symposium was sponsored by the Mechanical Behavior of Materials Committee to give tribute to the evolution of a concept that has formed the basis of our mechanistic understanding of how crystalline solids plastically deform and how they fail.

Schneider, Judy↗

Deformation mechanisms of nanotwinned Al and binary Al alloys

The objective of this proposal is to investigate, at a fundamental level, the deformation mechanisms of nanotwinned (NT) Al alloys with high density twin boundaries (TBs) and stacking faults (SFs). Nanotwinned metals with low stacking fault energy (SFE), such as Cu and Ag, have shown outstanding strength and tensile ductility. Twin boundaries play a critical role to enhance the strength and work hardening ability of these metals and alloys, and thus lead to significant plasticity. Al alloys have ultra-high stacking fault energy, and thus are often considered to be nearly free from growth twins and SFs. However, our recent studies show that a significant number of nanotwins and 9R phase can be introduced in Al and certain Al alloys, and lead to high flow stresses.

36 MATERIALS SCIENCE↗

Multiscale Structural Characterization of a Smectic Liquid Crystalline Elastomer upon Mechanical Deformation Using Neutron Scattering

Liquid crystalline elastomers (LCEs) exhibit unique shape memory behavior due to the combination of liquid crystalline orientation and rubber elasticity. Multiscale structural characterization of these materials upon deformation is crucial to understanding their structure–property relationships. In this work, the structure evolution of an epoxy-based, main-chain LCE with deuterated flexible spacers upon uniaxial mechanical deformation is investigated at different length scales. Wide-angle and small-angle X-ray scattering (WAXS/SAXS) reveal the presence of smectic polymorphism and rotations of the smectic domains upon mechanical stretching, which is also confirmed by small-angle neutron scattering (SANS). Importantly, the selective deuteration enables an improved neutron scattering contrast between the smectic and amorphous domains. SANS patterns of the deformed, deuterated LCE exhibit strong scattering streaks that are not observed in SAXS or SANS of hydrogenated LCE, indicating the presence of highly aligned amorphous domains. The macroscopic orientation also results in the formation of structures in the micrometer scale revealed by the ultrasmall-angle neutron scattering (USANS) experiment.

36 MATERIALS SCIENCE↗

In situ high-energy X-ray study of deformation mechanisms in additively manufactured 316L stainless steel

A key structural material planned to be used in the core of the Transformational Challenge Reactor is the additively manufactured 316L stainless steel (AM 316L SS). While the deformation of conventionally-manufactured 316 SS have been extensively studied, the deformation mechanism of AM 316L SS is less known. Here the room-temperature tensile behavior of AM 316L SS was studied in situ using high-energy X-ray diffraction and X-ray tomography. Diffraction yielded the lattice strains and the dislocation densi-ties of the AM 316L SS, which were compared to those of a conventionally processed 316H SS. It was found that while the conventional 316H SS had three distinct deformation stages, namely stage II ather-mal hardening, stage III dynamic recovery, and stage IV, the AM 316L experienced only the stages III and IV after an initial transitional period. The plastic instability stresses (PIS), i.e. the true ultimate tensile strength, were nearly the same in both materials. The AM 316L had very low dislocation barrier strength throughout the plastic deformation, which, in combination with the invariant PIS, explained its high dis-location storage capability and the attractive combination of strength and ductility. Tomography revealed morphological changes of the built-in pores in the AM 316L during deformation and fracture, and it was concluded that large pores close to the surface might have significant roles in the necking stage.

316 stainless steel↗

Influence of stacking fault energy and hydrogen on deformation mechanisms in high Mn austenitic steels during in-situ tensile testing

High Mn austenitic steels are considered an economical alloy system for hydrogen storage and transport applications. This study used stacking fault energy (SFE) as a design parameter to achieve hydrogen embrittlement (HE)-resistant high Mn austenitic alloys. The role of hydrogen on the deformation mechanisms of low (29 mJ/m 2 ) and high SFE (49 mJ/m 2 ) alloys was evaluated through in-situ neutron diffraction during tensile loading. Hydrogen-precharging increased yield strength, partly due to hydrogen-induced lattice distortion (i.e., solute strengthening). Hydrogen accelerated the increase in defect density, including dislocations and stacking faults. The formation of planar deformation structures (twins and stacking faults), relative to dislocations, plays a critical role in promoting hydrogen-assisted fracture. The stacking fault frequency parameter obtained from neutron diffraction quantifies planar deformation tendencies, correlated with HE sensitivity. The higher SFE alloy exhibited greater resistance to HE, associated with the reduced propensity to form stacking faults and twins upon deformation in the hydrogen-precharged condition.

High Mn austenitic steel↗

Comparing the deformation mechanism in 316 L stainless steel fabricated by hybrid and additive manufacturing

This study rationalizes the relatively higher elongation with minimal strength drop of 316L stainless steel (316LSS) manufactured using the hybrid approach in comparison to a fully additive approach followed by machining. It was found that twinning was the dominant deformation mechanism in 316LSS produced by both additive and hybrid approaches. Additionally, the relatively lower fraction of twins in the as-fabricated state of hybrid approach compared to a fully additive approach resulted in delaying the onset of steady-state strain hardening rate to higher strain levels, thereby resulting in an overall increase in elongation to failure.

36 MATERIALS SCIENCE↗

The impact of alkali‐ion intercalation on redox chemistry and mechanical deformations: Case study on intercalation of Li, Na, and K ions into FePO 4 cathode

Abstract Batteries made of charge carriers from Earth‐crust abundant materials (e.g., Na, K, and Mg) have received extensive attention as an alternative to Li‐ion batteries for grid storage. However, a lack of understanding of the behavior of these larger ions in the electrode materials hinders the development of electrode structures suitable for these large ions. In this study, we investigate the impact of alkali ions (Li, Na, and K) on the redox chemistry and mechanical deformations of iron phosphate composite cathodes by using electrochemical techniques and in situ digital image correlation. Na‐ion and Li‐ion intercalation demonstrate a nearly linear correlation between electrochemical strains and the state of charge and discharge. The strain development shows nonlinear dependance on the state of charge and discharge for K ions. Strain rate calculations show that K ion intercalation results in a progressive increase in the strain rate for all cycles. Li and Na intercalation induce nearly constant strain rates with the exception of the first discharge cycle of Na intercalation. When the same amount of ions are inserted into the electrode, the electrode shows the lowest strain generation upon Li intercalation compared to larger alkali ions. Na and K ions induce similar volumetric changes in the electrode when the state of charge and discharge is around 30%. Although the electrode experiences larger absolute strain generation at the end of the discharge cycles upon Na intercalation, strain rates were found to be greater for K ions. Potential‐dependent behaviors also demonstrate more sluggish redox reactions during K intercalation, compared to Li and Na. Our quantitative analysis suggests that the strain rate, rather than the absolute value of strain, is the critical factor in amorphization of the crystalline electrode.

25 ENERGY STORAGE↗

Geometrically Necessary Dislocation Analysis of Deformation Mechanism for Magnesium under Fatigue Loading at 0 °C

This study focused on the analysis of geometrically necessary dislocation (GND) densities for five selected fine-grained magnesium samples. Among the samples, three were tested under different fatigue-loading conditions at 0 °C, one experienced quasi-static tensile loading at 0 °C, and one represented the as-rolled state. The fatigue-tested samples were chosen according to the relationship between the maximum loading stress of a test and the material’s yield strength. This study provides new insights on the deformation mechanism of fine-grained magnesium at 0 °C. It is observed that the average GND densities were increased by 95~111% for the tested samples when compared with the as-rolled sample. It is especially interesting that there is a significant increase in the average GND density for the sample that experienced the fatigue loading with a low-maximum applied stress, and the maximum applied stress was lower than the material’s yield strength. This observation implies that the grain boundary mediated the dislocation-emission mechanism.

Li, Qizhen↗

New Deformation Mechanisms in Nanocrystalline Nano-porous Small Scale Metals as Defined by Kinetically-driven Microstructures

This report describes recent advances in the design and fabrication of nanostructured metallic pillars with hierarchical microstructures using a novel nanoscale additive manufacturing approach. Through a hydrogel-infusion-based two-photon lithography (TPL) method, we successfully fabricated 3D nickel nanopillars exhibiting both nanocrystalline and nanoporous features. The resulting “bamboo-like” internal architecture comprises 30–50 nm grains and voids with similarly scaled pores. These geometrically tunable pillars, with diameters ranging from ~130 to 550 nm, serve as an ideal platform for probing deformation mechanisms in structurally heterogeneous metals at the nanoscale.

36 MATERIALS SCIENCE↗

Understanding the deformation mechanisms in Ni-based superalloys with using crystal plasticity finite element method

Nl-based superalloy is considered as a good candidate due to its excellent resistance to elevated temperature deformation for long term period application. Understanding the deformation and failure mechanisms of Ni-Based superalloys is very helpful for providing design guidelines for processing Ni-based superalloys. Experimental characterization indicates that the deformation mechanisms of Ni based superalloy is strongly microstructure dependent. Besides, damage transform from the void nucleation to the macro cracks by voids growth leading to the failure of the Ni-based superalloys are also showing strong microstructure sensitivity. Therefore, this work focuses on the prediction and comprehension of the deformation and void growth behavior in Ni based superalloy at different working conditions via crystal plasticity finite element modeling and simulation. Physically based crystal plasticity frameworks were developed for newly Ni- based superalloy Haynes 282. It was found that dislocation shearing through the precipitates were acting as the main contributor to the strength of Haynes 282 at room temperature and 815°C. Our analysis of the creeping behavior of Haynes 282 exhibited that resistance of general climb replaced by the resistance induced by the deposited climb dislocation density. In addition, in the study of void growth behavior, our simulation results demonstrated that as the main loading axis perpendicular to the grain boundary (GB), voids grow more slowly on tilt GBs in bicrystals than those in single and bicrystals with twist GBs. And tilt GBs would promote the void grow into irregular shape.

36 MATERIALS SCIENCE↗

Fatigue Behavior and Deformation Mechanisms in Inconel 718 Superalloy Investigated

The nickel-base superalloy Inconel 718 (IN 718) is used as a structural material for a variety of components in the space shuttle main engine (SSME) and accounts for more than half of the total weight of this engine. IN 718 is the bill-of-material for the pressure vessels of nickel-hydrogen batteries for the space station. In the case of the space shuttle main engine, structural components are typically subjected to startup and shutdown load transients and occasional overloads in addition to high-frequency vibratory loads from routine operation. The nickel-hydrogen battery cells are prooftested before service and are subjected to fluctuating pressure loads during operation. In both of these applications, the structural material is subjected to a monotonic load initially, which is subsequently followed by fatigue. To assess the life of these structural components, it is necessary to determine the influence of a prior monotonic load on the subsequent fatigue life of the superalloy. An insight into the underlying deformation and damage mechanisms is also required to properly account for the interaction between the prior monotonic load and the subsequent fatigue loading. An experimental investigation was conducted to establish the effect of prior monotonic straining on the subsequent fatigue behavior of wrought, double-aged, IN 718 at room temperature. First, monotonic strain tests and fully-reversed, strain-controlled fatigue tests were conducted on uniform-gage-section IN 718 specimens. Next, fully reversed fatigue tests were conducted under strain control on specimens that were monotonically strained in tension. Results from this investigation indicated that prior monotonic straining reduced the fatigue resistance of the superalloy particularly at the lowest strain range. Some of the tested specimens were sectioned and examined by transmission electron microscopy to reveal typical microstructures as well as the active deformation and damage mechanisms under each of the loading conditions. In monotonically strained specimens, deformation during the subsequent fatigue loading was mainly confined to the deformation bands initiated during the prior monotonic straining. This can cause dislocations to move more readily along the previously activated deformation bands and to pile up near grain boundaries, eventually making the grain boundaries susceptible to fatigue crack initiation. The mechanisms inferred from the microstructural investigation were extremely valuable in interpreting the influence of prior monotonic straining on the subsequent fatigue life of Inconel 718 superalloy.

Source record↗

Virtual texture analysis to investigate the deformation mechanisms in metal microstructures at the atomic scale

Understanding the deformation behavior of metallic materials at high strain rates requires the characterization of plasticity contributors such as twins, phase transformed regions, and dislocations. However, predicting the contributions from phase transformation and twinning relies on a complete understanding of the selection of variants for various loading orientations and the evolution of their volume fractions. This manuscript presents a new virtual texture (VirTex) analysis approach to characterize phase transformation and twinning variants in deformed microstructures generated using molecular dynamics (MD) simulations. Furthermore, the VirTex method involves the construction of a rotation matrix to calculate the angle/axis pairs and misorientation angles for each atom in the microstructure. Any changes in the orientation angle from angle/axis pairs and/or structure types are analyzed to determine the nucleation and evolution of variants in the microstructure. The study uses shock deformed single-crystal Fe, Ta, and Cu to analyze the variant selections for phase transformation or twinning or both in BCC and FCC systems. In addition, the VirTex analysis is able to characterize the phase transformation and twinning variants in nanocrystalline Fe and Ta microstructures. Besides characterizing variants, orientation mapping also provides an accelerated and on-the-fly approach for quantifying twin fractions in MD microstructures.

36 MATERIALS SCIENCE↗

Plastic deformation mechanisms in polyimide resins and their semi-interpenetrating networks

High-performance thermoset resins and composites are critical to the future growth of space, aircraft, and defense industries in the USA. However, the processing-structure-property relationships in these materials remain poorly understood. In the present ASEE/NASA Summer Research Program, the plastic deformation modes and toughening mechanisms in single-phase and multiphase thermoset resins were investigated. Both thermoplastic and thermoset polyimide resins and their interpenetrating networks (IPNs and semi-IPNs) were included. The fundamental tendency to undergo strain localization (crazing and shear banding) as opposed to a more diffuse (or homogeneous) deformation in these polymers were evaluated. Other possible toughening mechanisms in multiphase thermoset resins were also examined. The topological features of network chain configuration/conformation and the multiplicity of phase morphology in INPs and semi-IPNs provide unprecedented opportunities for studying the toughening mechanisms in multiphase thermoset polymers and their fiber composites.

Jang, Bor Z.↗