Search NASA⌕ Search

SEARCH · Search NASA

Results for “Directional solidification”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

Single Crystal Casting with Fluidized Carbon Bed Cooling: A Process Innovation for Quality Improvement and Cost Reduction

Superalloy gas turbine blades are being produced by investment casting and directional solidification. A new process, Fluidized Carbon Bed Cooling (FCBC), has been developed and is now being optimized in a prototype casting unit with 10 kg pouring weight. In early test runs with still rather simple mold cluster geometries, a reduction of the primary dendrite arm spacing of around 40 pct compared to the standard radiation cooling process (HRS) could be demonstrated. The improvement is mainly attributed to higher temperature gradients driving solidification, made possible by a functioning Dynamic Baffle. Compared to earlier development efforts in the literature, contamination of the melt and damage to the equipment are avoided using carbon-based fluidized bed materials and the so-called “counter pressure concept.”.

36 MATERIALS SCIENCE↗

Simultaneous Removal of Silicon and Iron-Rich Phases from Coarse Al-Si Alloys Using Manganese Under Electromagnetic Field

Coarse Al-Si alloy is produced from bauxite via carbon electro-thermal reduction method. Silicon and iron-rich phases are two main detrimental impurities in coarse Al-Si alloy, and they can be simultaneously removed by adding Mn under the electromagnetic field. We focus on the influence of different Mn additions, dropping rates, and current intensity on the simultaneous removal efficiency of Si and Fe. Experimental results show that as mole ratio of Mn/Fe reaches more than 0.8, the morphology of iron-rich phases together with silicon changed from harmful acicular-like to the contributing bulks, concentrated at the bottom of Al-Si alloy as intermetallic compounds. Furthermore, when Mn/Fe reaches 1.2 and a lower dropping rate (5 to 25 μm/s) is adopted, both Si and Fe contents in the Al-Si alloy decreased drastically after electromagnetic directional solidification process, reaching 11.42 and 0.4 pct, respectively, with a desirable Fe removal efficiency of 91 pct. Finally, the principle of simultaneously separating Si and removing iron-rich phases from Al-Si alloy is studied deeply.

36 MATERIALS SCIENCE↗

Processing, As-Cast Microstructure and Wear Characteristics of a Monotectic Al-Bi-Cu Alloy

Ternary Al-based monotectic alloys have a good combination of wear resistance and mechanical strength. While self-lubricating soft elements guarantee an adequate wear resistance, the modification with third elements can increase the ability to support load. In the present investigation, a collection of microstructures is generated through transient directional solidification of the Al-3.2wt.%Bi-3.0wt.%Cu alloy. Samples with different Bi spacing have been subjected to micro-adhesive wear ball tests. A relationship linking the wear volume, V, the microstructural spacing and the test time is proposed for Bi spacing higher than 16 μm, according to which V decreases with the decrease in Bi spacing. It is observed that wider and deeper grooves emerged on the surface of the samples related to more refined Bi and Al{sub 2}Cu phases, that is, associated with Bi spacing and Bi diameter lower than 16 and 2.4 μm, respectively. A reverse trend is noted for these finer microstructures, for which V increases with further decrease in Bi spacing. This can be caused by the detachment of the very fine and less cohesive Al{sub 2}Cu lamellas as the Al{sub 2}O{sub 3} oxide breaks up forming debris, with the presence of these lamellas as loose debris at the interface acting as third-body abrasives.

36 MATERIALS SCIENCE↗

Influence of oxygen on performance of multi-principal element alloy as braze filler for Ni-base alloys

In manufacturing of multi-principal element alloys (MPEAs), the casting process is often a primary point of oxygen introduction to the material system, which was demonstrated by the laboratory scale button arc-melting process. Oxygen introduction raises concerns for the mechanical performance of these alloys if employed as structural materials alone or in engineering applications, such as serving as filler materials to enable joining of similar or dissimilar alloy pairs that are conventionally considered difficult to join. In this work, oxide inclusions in an as-cast off-equiatomic MnFeCoNiCu MPEA and Ni-base alloy braze joints made with this MPEA were evaluated by synchrotron x-ray diffraction mapping and electron microscopy. MnO was found to be prevalent throughout the cast MPEA and was chemically reduced during brazing by trace Al from the base material, Ni-base Alloy 600. Incomplete reaction of the MnO with Al, and some alternative reaction with Cr, left a mixture of MnO, Al 2 O 3 , and Cr 2 O 3 in the as-brazed joint, with the oxides concentrated near the braze centerline due to directional solidification. Further, in the braze joints, the non-oxide constituent phases detected were an FCC matrix and particles of Cr 23 C 6 , Cr 7 C 3 , and TiN which are all native to Alloy 600. The evolution of oxides within the brazed joints at elevated service temperatures of 600-800°C was also evaluated. While MnO and Al 2 O 3 were stable during high-temperature service, Cr 2 O 3 particles grew to several hundred microns, with dissolved oxygen in the MPEA providing a significant source for oxide growth. Comparing tensile performance of the as-brazed condition with post-service conditions showed that the evolution of oxide particles contributed to an increase in strength and decrease in ductility of the brazed joints. Evaluating particle morphologies among fracture surfaces of individual specimens demonstrated that large Cr 2 O 3 particles and continuous cluster networks of Al 2 O 3 were the features most detrimental to total elongation. Hence, unmitigated evolution of oxygen-containing species during brazing and service conditions is detrimental to the ductility of the brazed joints, which highlights the importance of oxygen control in initial manufacturing of MPEAs for engineering applications.

36 MATERIALS SCIENCE↗

Influence of Mn addition on the microstructure and mechanical properties of a directionally solidified γ-TiAl alloy

Highlights: • Mn addition can significantly improve the yield strength of TiAl alloy. • Introduction of Mn facilitates the operation of twinning-controlled deformation. • Twin-dislocation interactions cause a continuous increase in work hardening rate. - Abstract: TiAl alloys with nominal compositions of Ti-47Al-2Nb-2Cr-(0, 1, 3, 5)Mn were prepared via electromagnetic cold crucible directional solidification (ECCDS), and the influence of Mn addition on the microstructure and mechanical properties of the alloys was investigated. The experimental results showed that the Mn atoms were dissolved within the TiAl alloy, and no Mn compounds were formed. Based on the X-ray diffraction (XRD) analysis results, the peak angle of the Mn-containing sample shifted to a higher value, indicating lattice shrinkage. The Mn addition also increased the volume fraction of the B2 phase. The yield strength of the TiAl alloy monotonically increased as the content of the substitutional-solute Mn atoms increased. The ultimate strengths of the TiAl alloys containing 1 at.%, 3 at.%, and 5 at.% Mn consequently decreased because micro-cracks were preferentially formed in the B2 phase during room-temperature deformation. The introduction of substitutional-solute Mn atoms could result in a reduction of the stacking-fault energy of the γ phase, and facilitate the operation of twinning-controlled plastic-deformation during the intermediate stage of the plastic deformation process. The interaction between the deformation twins and movable dislocations led to a continuous increase in the work-hardening rate.

36 MATERIALS SCIENCE↗

Interfacial morphology evolution in directionally solidified FeCrAl alloys

Highlights: • The variations of cellular/dendritic spacing with different Al contents and velocities were studied by experiments. • The experimental data were compared with the Hunt-Lu model. • The effect of Al content on the interfacial morphology evolution was discussed for the directional solidified FeCrAl alloys. - Abstract: Interfacial morphology evolution in FeCrAl alloys with varying Al content has been investigated by conducting a series of directional solidification experiments. A comparison between the experimental data and the Hunt-Lu model confirms that cellular spacing widens while dendritic spacing narrows as Al content of the alloy increases. The ratio of upper and lower limit cellular/dendritic spacing λ{sub max}/λ{sub min} is only weakly dependent on growth velocity and Al content. Under the experimental conditions in the present study, cell to dendrite transition (CDT) occurs at a growth velocity between 25 μm/s and 50 μm/s, and dendrite to cell transition (DCT) is observed at a growth velocity less than 100 μm/s. Critical spacing of CDT λ{sub cd} and local solidification time (LST) t{sub f} are used to discuss the influence of Al content on CDT and DCT respectively. The transition between non-planar and planar interface of the alloy is investigated based on the interface stabilization theory of Mullins and Sekerka.

36 MATERIALS SCIENCE↗

Effects of composition and growth parameters on phase formation in multicomponent aluminum garnet crystals

The effects of com­position on the phase formation of multicom­ponent garnet crystals grown via directional solidification by the micro-pulling-down method are studied. A relatively wide range of rare-earth (RE) average ionic radii (AIR) is explored by formulating ten com­positions from the system (Lu,Y,Ho,Dy,Tb,Gd) 3 Al 5 O 12 . Crystals were grown at either 0.05 or 0.20 mm min -1 . The hypothesis is that multicom­ponent com­pounds with large AIR will form secondary phases as the single-RE aluminum garnets formed by larger Tb 3+ or Gd 3+ ; this will result in crystals of poor optical quality. Crystals with large AIR have a central opaque region in optical microscopy images, which is responsible for their reduced transparency com­pared to crystals with small AIR. Slow pulling rates suppress the formation of the opaque region in crystals with inter­mediate AIR. Powder and single-crystal X-ray diffraction and electron probe microanalysis results indicate that the opaque region is a perovskite phase. Scanning electron microscopy and energy dispersive spectroscopy measurements reveal eutectic inclusions at the outer surface of the crystals. Finally, the concentration of the eutectic inclusions increases with increasing AIR.

36 MATERIALS SCIENCE↗

Manufacturing of Advanced Alnico Magnets for Energy Efficient Traction Drive Motors CRADA Final Report

The primary theme of this Technology Commercialization Fund (TCF) project was refining the pre-alloyed powder processing approach (with alnico 8, modified for higher coercivity) of that came out of the previous Development of Radically Enhanced alnico Magnets (DREaM) project to permit full size net-shape alnico magnets to be produced in a reproducible manner that could allow testing in an advanced Permanent Magnet (PM) drive motor. Previously, a lack of sufficient coercivity in alnico magnets limits their energy product and their application in automotive traction drive motors, despite their high temperature stability. Use of enhanced sintered alnico magnets, instead of rare earth (RE) magnets or larger cast alnico magnets, could lower costs and decrease cooling needs of these motors. Conventional production of the best (aligned) alnico magnets (alnico 9) involves costly directional solidification (DS) and achieves good alignment, but modest energy product (10 MGOe), because of low coercivity. Other limitations of cast alnico 9 magnets are poor mechanical properties and difficulty in scaling special casting molds to mass production. In spite of these problems with alnico 9, a commercial electric motor company, UQM, developed a fully capable traction drive motor that met many 2022 DOE-VTO performance targets, except full speed operation, due to brittle mechanical behavior. While UQM demonstrated an advanced drive motor that used alnico 9, they also encouraged the development of improved alnico, especially for greater coercivity (seeking 2X) and improved mechanical properties. While commercial sintered alnico magnets are less brittle and have improved coercivity, they have an inferior energy product due to their non-aligned, fine-grained microstructure. Thus, full development and up-scaling of well-aligned alnico magnets with a further increase in coercivity and good mechanical properties by a low cost powder processing route became the theme of this TCF project. The processing route for this project involved high-pressure gas atomization, at Ames and Carpenter, of modified alnico 8 compositions, compression molding of the resulting pre-alloyed powders into bulk samples, de-binding and sintering the samples to full density, and a final magneto-thermal treatment of the resulting bulk magnets, at Ames and Arnold Magnetic Technologies, to produce aligned magnets, which were intended for motor testing at UQM and Ford.

42 ENGINEERING↗

Fundamentals of Scalable Nanoparticle Assembly in Engineering Polymres

Systematically improving the properties of polymer nanocomposites is contingent on effectively controlling nanoparticle (NP) dispersion; further, it is necessary to attain this at scale if these methods are to impact practical applications. While most past work has focused on amorphous polymers, ≈ 70% of all polymers sold annually are semicrystalline. Inspired by this apparent disconnect, our work in the current DOE funded grant and this renewal proposal employs a novel handle, polymer crystallization, to organize NPs into the various amorphous zones of the lamellar semicrystalline morphology (interlamellar, interfibrillar and interspherulitic domains) of stereoregular polymers. We hypothesize that the isothermal crystallization rate of a polymer host, G, and NP diffusivity, are the two relevant control parameters in this context. In the case where the NPs are miscible in the melt, they remain spatially well-dispersed when the polymer is crystallized at a rate that is fast relative to NP diffusion. In contrast, monolayer-thick NP sheets with intersheet spacing of ~10-100nm form in slowly crystallized samples. This sheet stacking is remarkably similar to that seen in natural materials, e.g., Nacre. There is also ordering of the NPs at the larger interfibrillar scale. Importantly, the relative fraction of engulfed, interlamellar and interfibrillar NPs is determined by G. Further, the modulus of these materials can increase by a factor of 2-3 due to the organization state of the NPs, while leaving fracture toughness unaffected. We have established the broad applicability of this approach in two polymers, polyethylene (PE) and polyethyleneoxide (PEO). To achieve this goal we developed a method for grafting long PE chains from NPs with controlled graft density and molecular weight, giving us the ability to tailor their dispersion in the PE melt prior to crystallization. In this renewal proposal, we will develop the fundamental, quantitative understanding that will allow us to independently tailor polymer crystallization rate, NP diffusivity and NP agglomeration state in semicrystalline polymers so as to facilely control NP ordering and hence properties. A program that tightly integrates experiment and theory is proposed, and a key outcome of this research will be a three-dimensional design map for different regimes of NP organization (and hence properties) that can be achieved by polymer crystallization. A second independent outcome is the role of directional solidification and how it competes with the rates of polymer crystallization and NP mobility to affect the organization of the NP.

36 MATERIALS SCIENCE↗

Processing of Alnico Magnets by Additive Manufacturing

Permanent magnets without rare earth (RE) elements, such as alnico, will improve supply stability and potentially decrease permanent magnet cost, especially for traction drive motors and other increased temperature applications. Commercial alnico magnets with the highest energy product are produced by directional solidification (DS) to achieve a < 001 > columnar grain orientation followed by significant final machining, adding to the high cost. Additive manufacturing (AM) is an effective method to process near net-shape parts with minimal final machining of complex geometries. AM also, has potential for texture/grain orientation control and compositionally graded structures. This report describes fabrication of alnico magnets by AM using both laser engineered net shaping (LENS)/directed energy deposition (DED) and electron beam melting powder bed fusion (EBM/PBF). High pressure gas atomized (HPGA) pre-alloyed alnico powders, with high purity and sphericity, were built into cylindrical and rectangular samples, followed by magnetic annealing (MA) and a full heat treatment (FHT). The magnetic properties of these AM processed specimens were different from their cast and sintered counterparts of the same composition and show a great sensitivity to heat treatment. The AM process parameters used in this developmental study did not yet result in any preferred texture within the alnico AM builds. These findings demonstrate feasibility for near net-shape processing of alnico permanent magnets for use in next generation traction drive motors and other applications requiring increased operating temperatures and/or complex engineered part geometries, especially with further AM process development for texture control.

36 MATERIALS SCIENCE↗

Rationalization of solidification mechanism of Nd–Fe–B magnets during laser directed-energy deposition [Rationalization of solidification mechanism of neodymium-iron-boron magnets obtained after laser directed-energy deposition process]

Here, near-net fabrication techniques are highly beneficial to minimize rare earth metal usage to fabricate dense fully functional magnets. In this study, feasibility of using the directed-energy deposition technique for fabrication of magnets is evaluated. The results show that despite the ability to fabricate highly reactive materials in the laser deposition process, the magnetic coercivity and remanence of the hard magnets is significantly reduced. X-ray powder diffraction in conjunction with electron microscopy showed that the material experienced a primary Nd 2 Fe 17 B x solidification. Consequently, the absence of the hard magnetic phase resulted in deterioration of the build properties.

36 MATERIALS SCIENCE↗

Prediction of Cooling Curves for Controlled Unidirectional Solidification Under the Influence of Shrinkage: A Semi-analytical Approach

Quality of casting products can be significantly improved by controlling the crystal growth rate. Both dendritic and equiaxed grain structures depend strongly on crystal growth rate along the crystallographic direction. Uncontrolled solidification processes may lead to the formation of porous and columnar material with an extremely non-homogeneous composition distribution. These undesirable micro-structures can be avoided by adopting an optimal cooling rate (K/s) during the crystal growth. The present work focuses on determining suitable cooling curves to obtain desired unidirectional crystal growth rates, by implementing a semi-analytical model. Here, we defined cooling curve as the time history of temperature evolution at the cold boundary. The proposed semi-analytical heat transfer model is diffusion driven and accounts for shrinkage effect during solidification. The proposed model is found capable of predicting cooling curves for prescribed interface velocities. The model is self-sufficient in validating itself by means of solving inverse and forward problems. The cooling curve prediction by the model is validated by using it as the transient boundary condition for an existing enthalpy updating scheme-based numerical model. The proposed model is also applied to empirical data reported in literature, to validate the model against experimental results. All the validations showcased excellent fit. The proposed model will facilitate controlled unidirectional crystal growth rate by providing cooling rate (K/s) as an input for the experiments involving directional solidification.

36 MATERIALS SCIENCE↗

Influence of Electropulsing Treatment on the Initial Solidification of Molten Steel During Continuous Casting

An electropulsing-assisted mold simulator (EPMS) technique was developed to investigate the effect of pulsed electric current on the initial solidification behavior of molten steel during the process of continuous casting. The results indicated that the variation of mold hot surface temperatures in the meniscus area decreased from 375.8 K to 394 K for the case without electropulsing treatment (EPT) to 363.5 K to 377.3 K for the one with EPT. The mold surface heat fluxes fluctuated around the baseline of 0.83 and 2.42 MW/m{sup 2} in the cases with and without EPT, respectively, which indicated that a higher thermal resistance between the initial shell and copper mold was introduced by employing the EPT. The crystal fraction of slag films increased from 69.8 to 77.9 pct, whereas the grain size of mold flux film decreased, when compared the case of EPT treatment with the benchmark one, which suggested that the pulsed electric current promotes the movement of molten clusters and particles, leading to the enhancement of mold flux crystallization and the improvement of thermal resistance. Moreover, the solidification structure of steel along the direction of solidification (from the mold to melt) includes a fine chilled grain layer close to the mold, a columnar dendrite layer in the middle, and equiaxed grains next to the melt core, in which a compacted microstructure with smaller secondary dendrite arm spacing was observed in the case of the EPT. The results demonstrate that the EPT could refine the as-cast solidification microstructure.

36 MATERIALS SCIENCE↗

A lightweight Fe–Mn–Al–C austenitic steel with ultra-high strength and ductility fabricated via laser powder bed fusion

Lightweight Fe–Mn–Al–C steels have become a topic of significant interest for the defense and automotive industries. These alloys can maintain high strength and ductility while also reducing weight in structural applications. Conventionally processed Fe–Mn–Al–C austenitic steels with high Al content (~9 wt%) demonstrate greater than 1.5 GPa strength with 35% elongation. Several recent studies have demonstrated success in fabricating steel parts using laser powder bed fusion (L-PBF) additive manufacturing (AM), which can generate near-net-shape components with complex geometries and is capable of local microstructural control. However, studies on L-PBF processing of Fe–Mn–Al–C alloys have focused on low Al content (<5 wt%) compositional regimes representing alloys that undergo transformation-induced plasticity (TRIP) and twinning-induced plasticity (TWIP). Here, in this study, we present the effects of L-PBF processing on the microstructure and mechanical properties of an Fe–30Mn–9Al–1Si-0.5Mo-0.9C austenitic steel. A process optimization framework is employed to determine an ideal L-PBF processing space that will result in >99% density parts. Implementing this framework resulted in near-fully dense specimens fabricated over a broad range of process parameters. Additionally, two bi-directional scan rotation strategies (90° and 67°) were applied to understand their effects on texture and anisotropy in this material. As-printed specimens displayed considerable work-hardening characteristics with average strengths of up to 1.3 GPa and 36% elongation in the build direction. However, solidification microcracks oriented in the build direction resulted in anisotropy in tensile strength and ductility resulting in average strengths of 1.1 GPa and 20% elongation perpendicular to the build direction. The successful L-PBF fabrication of Fe–30Mn–9Al–1Si-0.5Mo-0.9C presented here is expected to open new avenues for weight reduction in structural applications with a high degree of control over part topology.

36 MATERIALS SCIENCE↗

Controlling solute channel formation using magnetic fields

Solute channel formation introduces compositional and microstructural variations in a range of processes, from metallic alloy solidification, to salt fingers in ocean and water reservoir flows. Applying an external magnetic field interacts with thermoelectric currents at solid/liquid interfaces generating additional flow fields. This thermoelectric (TE) magnetohydrodynamic (TEMHD) effect can impact on solute channel formation, via a mechanism recently drawing increasing attention. To investigate this phenomenon, we combined in situ synchrotron X-ray imaging and Parallel-Cellular-Automata-Lattice-Boltzmann based numerical simulations to study the characteristics of flow and solute transport under TEMHD. Observations suggest the macroscopic TEMHD flow appearing ahead of the solidification front, coupled with the microscopic TEMHD flow arising within the mushy zone are the primary mechanisms controlling plume migration and channel bias. Two TE regimes were revealed, each with distinctive mechanisms that dominate the flow. Further, we show that grain orientation modifies solute flow through anisotropic permeability. These insights led to a proposed strategy for producing solute channel-free solidification using a time-modulated magnetic field.

36 MATERIALS SCIENCE↗

Anomalous Annealing Response of Directed Energy Deposited Type 304L Austenitic Stainless Steel

Directed energy deposited (DED) and forged austenitic stainless steels possess dissimilar microstructures but can exhibit similar mechanical properties. In this study, annealing was used to evolve the microstructure of both conventional wrought and DED type 304L austenitic stainless steels, and significant differences were observed. In particular, the density of geometrically necessary dislocations and hardness were used to probe the evolution of the microstructure and properties. Forged type 304L exhibited the expected decrease in measured dislocation density and hardness as a function of annealing temperature. Here, the more complex microstructure–property relationship observed in the DED type 304L material is attributed to compositional heterogeneities in the solidification microstructure.

36 MATERIALS SCIENCE↗