Search NASA⌕ Search

SEARCH · Search NASA

Results for “EPDM”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

Influence of biodiesel decomposition chemistry on elastomer compatibility

Here, the compatibility of biodiesel blends with five common elastomers (acrylonitrile rubber or NBR, fluorocarbon, neoprene, ethylene propylene diene monomer or EPDM, and silicone) was assessed using Hansen solubility parameters. A solubility analysis was performed over the full diesel blend range and the model used methyl hydroperoxide, acetaldehyde, and formic acid to represent the decomposition products of biodiesel. An empirical study was also conducted to determine the efficacy of the approach to predict the volume swell of elastomers. This study included the influence of biodiesel with acetaldehyde and formic acid. The solubility model showed good agreement with measured volumes for fluorocarbon, neoprene, EPDM, and silicone. However, solubility curves for NBR did not reflect the measured volume changes, and therefore the solubility parameters used for NBR in this study are not considered reliable. The results showed that formic acid caused higher swelling in NBR, fluorocarbon, neoprene, and silicone than did acetaldehyde. For EPDM, the measured volume decreased with both biodiesel concentration and the addition of formic acid.

09 BIOMASS FUELS↗

Evaluation of High Temperature Elastomers for Geothermal Wells

This report describes the extension of a performance screening study of elastomers for geothermal well applications. Elastomeric O-rings were subjected to compression while submerged in water at elevated temperatures and pressure to determine performance under more aggressive conditions. Following the experiment, the elastic moduli of the O-ring cross-sections were assessed for any changes which may affect O-ring function down-hole. All materials showed susceptibility to thermo-oxidative degradation at high temperatures and pressures. Type I FKM had the least amount of compression set of all materials tested at 150ºC while Kalrez FFKM O-rings had the least amount of edge hardening of all materials, regardless of aging temperature. Prior visual observation of materials aged in simulated environments revealed an unusual trend with EPDM and FEPM materials: the degradation and disintegration of these polymers in an oxidative thermal cycle environment, but the ability to maintain mechanical performance and shape during oxidative thermal cycling in the presence of steam. EPDM and FEPM were subjected to additional testing at SNL in order to better understand this aging anomaly. No abnormalities were observed in the chemical (oxidation rates, FTIR spectra, solvent uptake, gel content, and weight loss vs. temperature) or physical (modulus profiles) measurements that could explain the visually observed aging differences. SNL validated this observation through a secondary controlled aging test using only EPDM, where, once again, it was shown that thermo-oxidative conditions appear to cause more degradative damage (enhanced embrittlement) than did thermo-oxidative coupled with hydrolytic environments. From these data we conclude that water may favorably interfere with normal thermo-oxidative degradation processes via some type of inhibition pathway which has yet to be identified.

15 GEOTHERMAL ENERGY↗

Compatibility of polymers in super-critical carbon dioxide for power generation systems: High level findings for low temperatures and pressure conditions

Polymers such as PTFE (polytetrafluorethylene or Teflon), PEEK (polyetheretherketone), EPDM (ethylene propylene cliene monomer) rubber, Viton, EPR (ethylene propylene rubber), Nylon, Nitrile rubber, and perfluoroelastomers are commonly employed in super critical CO 2 (sCO2) energy conversion systems. O-rings and gaskets made from these polymers face stringent performance conditions such as elevated temperatures, high pressures, pollutants and corrosive humid environments. Critical knowledge gaps about polymer degradation from sCO2 exposure need to be addressed. To understand these effects, we have studied nine commonly used polymers subjected to elevated temperatures under isobaric conditions of sCO2 pressure. The polymers (PEEK, Nylon, PTFE, EPDM, Nitrile rubber, EPR, Neoprene, perfluoroelastomer FF 202 and Viton) were exposed for 1000 hours at 100°C to 25 MPa sCO2 pressure in an autoclave. In a second study, elastomers perfluoroelastomer (FF202) and EPDM were exposed to 25 MPa sCO2 for 1000 hours at 150°C. Samples were extracted for ex-situ characterization at t = 200 hours and then at the completion of the test at t=1000 hours. The polymer samples were examined for physical and chemical changes by Dynamic Mechanical and Thermal Analysis (DMTA), Fourier Transform Infrared (FTIR) spectroscopy, and compression set. Density and mass changes immediately after removal from test and 48 hours later, and optical microscopy techniques were also used. Microcomputer tomography (micro CI) data was generated on select specimens. Super-critical CO 2 effects have been identified as either physical or chemical effects. For each polymer, the dominance of one type of effect over the other was evaluated. Attempts were also made to qualitatively link sCO2 effects such as lowering or increase in glass transition temperatures, storage modulus changes, mass and compression set changes, chemical changes seen in FTIR analyses and blister and void formation seen post-exposure to polymer microstructure-related mechanisms such as plasticization of the polymer matrix, escape of volatiles from the polymer during depressurization, and filler and plasticizer effects on microstructure with rapid depressurization rates.

36 MATERIALS SCIENCE↗

Monitoring Degradation of Nuclear Cable Insulation Subjected To Sequential and Simultaneous Thermal and Radiation Aging

Predicting useful remaining life of cables in nuclear power plants is a topic of growing interest as plant continue to age. A typical electrical cable consists of polymeric materials, such as the cable jacket and insulation, which are susceptible to degradation due to exposure to both elevated temperatures and gamma irradiation over decades of service. In this work two insulation materials, crosslinked polyethylene (XLPE) and ethylene propylene diene (EPDM) elastomer, were characterized to quantify aging using total color difference and indenter modulus. Since the effects of thermal and gamma radiation are not additive but coupled, the effects of different aging scenarios including sequential and simultaneous aging were also evaluated. In the case of sequential aging, two aging scenarios were explored where the order in which thermal and gamma radiation received were altered. Total color difference of XLPE showed that sequentially aged insulation specimens, which received radiation first, degraded slightly more at maximum exposure than specimens which received thermal first. Similarly, in the case of EPDM, the extent of degradation evaluated using total color difference was found to be most severe in the case of sequentially aged insulation specimens which received radiation first. Indenter modulus was found to be insensitive to aging for XLPE but trended for EPDM. The largest variations were observed for the sequentially aged insulation specimens which received radiation first, similar to what was observed for total color difference.

Pallaka, Madhusudhan Reddy↗

Moisture ingress in commercial steel drums: Water content determination, diffusion modelling and predicted permeation rates

Commercial steel drums underpin the global economy, playing a pivotal role in the storage and transportation of critical materials. Transported and stored materials, such as food, chemical and nuclear waste, can be sensitive to ambient conditions, particularly moisture that can enhance negative effects such as corrosion and material degradation. Although international standards and regulations are in place for the qualification of steel drums, there are no current testing requirements, established limits or boundaries for the permeation of moisture into the drums during transportation or storage. This work aims to provide insights into the moisture ingress over time into properly sealed steel drums and provides estimated moisture ingress rates over time through extrapolation. Water vapour transmission rate (WVTR) measurements through the gasket material at 10–40°C were 0.11–2.1 g/m 2 /day resulting in a permeation activation energy of 30.2 kJ/mol. Water sorption measurements and Karl Fischer titration (KFT) on ethylene propylene diene monomer (EPDM) gasket material revealed a decrease in equilibrium moisture saturation with increasing temperature. KFT measurements also revealed the presence of moisture within the adhesive and drum wall after exposure to ambient conditions. KFT and Fourier transform infrared spectroscopy (FTIR) show that moisture will desorb from the EPDM and drum wall after exposure to desiccating conditions, although a minimal amount of moisture will remain present. When sealed to the manufacturer's recommendations, the steel drums are effective in minimizing moisture ingress. In conclusion, in sealed empty drums, moisture ingress rates for 19-L drums were 0.4–1.5 mg/day at 25°C 15% relative humidity (RH) and increased to 7.1–8.8 mg/day at 40°C 90% RH, and moisture ingress rates for 210-L drums were 2.5 and 3.5 mg/day at field deployment conditions of 15.5°C 51.5% RH and 23°C 40% RH, respectively.

42 ENGINEERING↗

A diffusion–deformation model with damage for polymer undergoing rapid decompression failure

Green hydrogen is emerging as one of the most promising alternatives to replace fossil fuels. While hydrogen gas has a good energy density by weight, its poor energy density by volume requires it to be stored under high pressure for commercial use. The hydrogen infrastructure developed to handle this high pressure hydrogen contains multiple components made of polymers as sealing agents. Although polymers do not react chemically with hydrogen gas, they undergo a mechanical failure when high pressure hydrogen gas is suddenly depressurized. This phenomenon known as 'rapid decompression failure' occurs due to the diffusion of hydrogen through polymer and getting trapped inside pre-existing cavities or voids. Here, in this paper, a continuum mechanics-based coupled diffusion-deformation-damage model was developed to predict the hydrogen distribution, stress distribution, and damage propagation inside the polymer while it undergoes rapid decompression failure. The polymer was modeled as a hyperelastic material because it represents the nonlinear material response observed in uniaxial tensile tests perfectly. The effects of hydrogen diffusivity, pre-existing cavity size, cavity location, applied hydrogen pressure, and depressurization rate on damage initiation were studied. It was found that the coefficient of diffusion plays an important role in damage initiation and damage was mostly concentrated in the inside areas rather than near the surface. Experiments were conducted with EPDM polymer which agreed well with the predicted trends using the given model. The effect of adding carbon black and silica filler particles and plasticizer to the pure EPDM polymer was also studied. It was found that damage during RDF decreases with the addition of fillers, but increases with the addition of the plasticizer. Finally, the damage evolution in the presence of two cavities was also studied, and was found that the interaction of stress fields around the cavities alters the damage occurring during RDF.

36 MATERIALS SCIENCE↗

Degradation of different elastomeric polymers in simulated geothermal environments at 300°C

This study evaluates the degradation of six different elastomeric polymers used for O-rings: EPDM, FEPM, type I- and II-FKM, FFKM, and FSR, in five different simulated geothermal environments at 300 °C: 1) non-aerated steam/cooling cycles, 2) aerated steam/cooling cycles, 3) water-based drilling fluid, 4) CO 2 -rich geo-brine fluid, and, 5) heat–cool water quenching cycles. The factors assessed included the extent of oxidation, changes in thermal behavior, micro-defects, permeation of ionic species from the test environments into the O-rings, silicate-related scale-deposition, and changes in the O-rings' elastic modulus. The reliability of the O-rings to maintain their integrity depended on the elastomeric polymer composition and the exposure environment. FSR disintegrated while EPDM was oxidized only to some degree in all the environments, FKM withstood heat-water quenching but underwent chemical degradation, FEPM survived in all the environments with the exception of heat-water quenching where it underwent severe oxidation-induced degradation, and FFKM displayed outstanding compatibility with all the tested environments. This study discusses the degradation mechanisms of the polymers under the aforementioned conditions.

15 GEOTHERMAL ENERGY↗

Degradability Characterization of EPDM/IIR Blends by γ-irradiation

In this paper the modifications induced in butyl rubbers (pristine, chlorinated and brominated sorts) by γ-irradiation are investigated by swelling, chemiluminescence and FT-IR. The susceptibility of butyl rubbers for the generation of radicals orders their stabilities in the following sequence: IIR > IIR—Cl > IIR—Br. The incorporation of butyl rubbers into ethylene-propylene terpolymer matrix brings about increased densities of radicals initiating modifications in the oxidation state in respect with recombination, which are intensified as the processing dose increases. Based on the variation of carbonyl and hydroxyl indices the favorable route for the recycling EPDM based formulations would be suggested in this study. The chemiluminescence spectra proving the formation of peroxyl radicals at about 100 °C prove their availability as reclaiming solutions. IIR—Br is the recommendable butyl rubber for the recovery procedure by association with EPDM. The suitability of IIRs for recycling purposes is analyzed by the variation in their crosslink densities, free volumes and swelling degrees. The crosslinking behavior of stabilized EPDM/IIR blends that runs to the improvement of durability is depicted by Charlesby–Pinner representation, which involves the different simultaneous contribution of scission and crosslinking processes.

36 MATERIALS SCIENCE↗

Subdiffusive High-Pressure Hydrogen Gas Dynamics in Elastomers

We report elastomeric rubber materials serve a vital role as sealing materials in the hydrogen storage and transport infrastructure. With applications including O-rings and hose liners, these components are exposed to pressurized hydrogen at a range of temperatures, cycling rates, and pressure extremes. High-pressure exposure and subsequent rapid decompression often lead to cavitation and stress-induced damage of the elastomer due to localization of the hydrogen gas. Here, we use all-atom classical molecular dynamics simulations to assess the impact of compositional variations on gas diffusion within the commonly used elastomer ethylene–propylene–diene monomer (EPDM). With the aim to build a predictive understanding of precursors to cavitation and to motivate material formulations that are less sensitive to hydrogen-induced failure, we perform systematic simulations of gas dynamics in EPDM as a function of temperature, gas concentration, and cross-link density. Our simulations reveal anomalous, subdiffusive hydrogen motion at pressure and intermediate times. We identify two groups of gas with different mobilities: one group exhibiting high mobility and one group exhibiting low mobility due to their motion being impeded by the polymer. With decreasing temperatures, the low-mobility group shows increased gas localization, the necessary precursor for cavitation damage in these materials. At lower temperatures, increasing cross-link density led to greater hydrogen gas mobility and a lower fraction of caged hydrogen, indicating that increasing cross-link density may reduce precursors to cavitation. Finally, we use a two-state kinetic model to determine the energetics associated with transitions between these two mobility states.

36 MATERIALS SCIENCE↗

HYDROPHOBIC CHARACTERISTICS OF COMPOSITE INSULATORS IN SIMULATED INLAND ARID DESERT ENVIRONMENT

Presently along with traditional insulators i.e. glass and porcelain, etc., the polymeric insulators are also used world widely. These polymeric insulators are very sensitive to various environmental parameters e.g. UV radiations, heat, etc. The UV radiation level in the central region of Saudi Arabia is high as compared to the recommended IEC-61109 standard for the accelerated aging of the composite insulators. In this study, thermoplastic elastomer (TPE) and Ethylene Propylene Diene Monomer (EPDM) insulators were subjected to accelerated aging stress as per IEC standard as well as modified IEC standard simulating the inland arid desert's atmospheric conditions. The hydrophobic characteristics were studied by measuring the contact angle along the insulator surface before and after the accelerated aging of the samples. It was found that TPE loses its hydrophobic properties more as compared to EPDM insulator. This loss was proportional to the intensity of UV irradiation. The rate of recovery is also low for both the tested materials as compared to Silicone Rubber insulators.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Tritium Effects on Aromatic Carbon–Loaded Polymers

By incorporating carbon nanotubes (CNTs) and graphene nanomaterials with aromatic sp2 carbon structures, we have specifically tuned filled ethylene propylene diene monomer elastomer (EPDM) seal and gasket composite materials for radiation resistance. Our results show that CNTs and graphene have an increased ability to stabilize the EPDM matrix compared to standard carbon black (CB) as a radiation-resistant filler. Here, graphene outperforms both CNT and CB fillers when considering surface damage under conditions where beta exposure is an issue. Both graphene and CNT fillers offer significantly reduced changes in glass transition temperature under prolonged exposure to tritium compared to CB-filled standards, with a 2.5-fold and almost 5-fold reduction, respectively. Thus, CNT- and graphene-filled O-ring materials could be designed that would maintain acceptable seals significantly longer than currently used composites.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Miscibility Evaluation Of The Next Generation Solvent With Polymers Currently Used At DWPF, MCU, And Saltstone

The Office of Waste Processing, within the Office of Technology Innovation and Development, funded the development of an enhanced Caustic-Side Solvent Extraction (CSSX) solvent for deployment at the Savannah River Site for removal of cesium from High Level Waste. This effort lead to the development of the Next Generation Solvent (NGS) with Tris (3,7-dimethyl octyl) guanidine (TiDG). The first deployment target for the NGS solvent is within the Modular CSSX Unit (MCU). Deployment of a new chemical within an existing facility requires verification that the new chemical components are compatible with the installed equipment. In the instance of a new organic solvent, the primary focus is on compatibility of the solvent with organic polymers used in the affected facility. This report provides the calculated data from exposing these polymers to the Next Generation Solvent. An assessment of the dimensional stability of polymers known to be used or present in the MCU, Defense Waste Processing Facility (DWPF), and Saltstone facilities that will be exposed to the NGS showed that TiDG could selectively affect the elastomers and some thermoplastics to varying extents, but the typical use of these polymers in a confined geometry will likely prevent the NGS from impacting component performance. The polymers identified as of primary concern include Grafoil ® (flexible graphite), Tefzel ® , Isolast ® , ethylene-propylene-diene monomer (EPDM) rubber, nitrile-butadiene rubber (NBR), styrene-butadiene rubber (SBR), ultra high molecular weight polyethylene (UHMWPE), and fluorocarbon rubber (FKM). Certain polymers like NBR and EPDM were found to interact mildly with NGS but their calculated swelling and the confined geometry will impede interaction with NGS. In addition, it was found that Vellumoid (cellulose fibers-reinforced glycerin and protein) may leach protein and Polyvinyl Chloride (PVC) may leach plasticizer (such as Bis-Ethylhexyl-Phthalates) into the NGS solvent. Either case will not impact decontamination or immobilization operations at Savannah River Site (SRS). Some applications have zero tolerance for dimensional changes such as the operation of valves while other applications a finite dimensional change improves the function of the application such as seals and gaskets. Additional considerations are required before using the conclusions from this work to judge outcomes in field applications. Decane, a component of Isopar L that is most likely to interact with the polymers, mildly interacted with the elastomers and the propylene based polymers but their degree of swelling is at most 10% and the confined geometry that they are typically placed in indicate this is not significant. In addition, it was found that Vellumoid may leach protein into the NGS solvent. Since Vellumoid is used at the mixer in Saltstone where it sees minimum quantities of solvent, this leaching has no effect on the extraction process at MCU or the immobilization process at saltstone. No significant interaction is expected between MaxCalix and the polymers and elastomers used at MCU, DWPF, and Saltstone. Overall, minimal and insignificant interactions are expected on extraction and immobilization operations when MCU switches from CSSX to NGS solvent. It is expected that contacting NGS will not accelerate the aging rate of polymers and elastomers under radiation and heat. This is due to the minimal interaction between NGS and the polymers and the confined geometries for these polymers. SRNL recommends the use of the HSP method (for screening) and some testing to evaluate the impact of other organic such as alcohols, glycolate, and their byproducts on the polymers used throughout the site.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Collective Summary of sCO2 Materials Development (Supercritical Transformational Electric Power Generation (STEP) Level 2 Milestone Report) (Parts I - II)

Polymers such as PTFE (polytetrafluorethylene or Teflon), EPDM (ethylene propylene diene monomer) rubber, FKM fluoroelastomer (Viton), Nylon 11, Nitrile butadiene (NBR) rubber, hydrogenated nitrile rubber (HNBR) and perfluoroelastomers (FF_202) are commonly employed in super critical CO 2 (sCO2) energy conversion systems. O-rings and gaskets made from these polymers face stringent performance conditions such as elevated temperatures, high pressures, pollutants, and corrosive humid environments. In FY 2019, we conducted experiments at high temperatures (100°C and 120°C) under isobaric conditions (20 MPa). Findings showed that elevated temperatures accelerated degradation of polymers in sCO2, and that certain polymer microstructures are more susceptible to degradation over others. In FY 2020, the focus was to understand the effect of sCO2 on polymers at low (10 MPa) and high pressures (40 MPa) under isothermal conditions (100°C). It was clear that the same selectivity was observed in these experiments wherein certain polymeric functionalities showed more propensity to failure over others. Fast diffusion, supported by higher pressures and long exposure times (1000 hours) at the test temperature, caused increased damage in sCO2 environments to even the most robust polymers. We also looked at polymers under compression in sCO2 at 100°C and 20 MPa pressure to imitate actual sealing performance required of these materials in sCO2 systems. Compression worsened the physical damage that resulted from chemical attack of the polymers under these test conditions. In FY 2021, the effect of cycling temperature (from 50°C to 150°C to 50°C) for polymers under a steady sCO2 pressure of 20 MPa was studied. The aim was to understand the influence of cycling temperatures of sCO2 for typical polymers under isobaric (20 MPa) conditions. Thermoplastic polymers (Nylon, and PTFE) and elastomers (EPDM, Viton, Buna N, Neoprene, FF202, and HNBR) were subjected to 20 MPa sCO2 pressure for 50 cycles and 100 cycles in separate experiments. Samples were extracted for ex-situ characterization at 50 cycles and upon the completion of 100 cycles. Each cycle constituted of 175 minutes of cycling from 50°C to 150°C. The polymer samples were examined for physical and chemical changes by Dynamic Mechanical and Thermal Analysis (DMTA), Fourier Transform Infrared (FTIR) spectroscopy, and compression set. Density and mass changes immediately after removal from test were measured for degree of swell comparisons. Optical microscopy techniques and micro computer tomography (micro CT) images were collected on select specimens. Evaluations conducted showed that exposures to super-critical CO2 environments resulted in combinations of physical and/or chemical changes. For each polymer, the dominance of cycling temperatures under sCO2 pressures, were evaluated. Attempts were made to qualitatively link the permanent sCO2 effects to polymer micro- structure, free volume, backbone substitutions, presence of polar groups, and degree of crystallinity differences. This study has established that soft polymeric materials are conducive to failure in sCO2 through mechanisms of failure that are dependent on polymer microstructure and chemistry. Polar pendant groups, large atom substitutions on the backbone are some of the factors that are influential structural factors.

36 MATERIALS SCIENCE↗

Dose Rate Effects on Degradation of Nuclear Power Plant Electrical Cable Insulation at a Common Dose

The intent of this report is to address an identified knowledge gap in relating accelerated aging of nuclear electrical cables to service aging: dose rate effects (DRE). Here, DRE refer to gamma radiation-induced polymer degradation being a function of dose rate in addition to total absorbed dose. The concern raised is that historical qualification conducted at higher dose rates to simulate service lifetime may underestimate insulation degradation that occurs at lower dose rates in service. In the work described herein, common nuclear cable insulation materials—cross-linked polyethylene (XLPE) and ethylene propylene diene elastomer (EPDM)—were subjected to accelerated aging at ambient temperature (26°C) at different gamma dose rates of 100, 200 and 1800 Gy/h for select exposure durations to achieve constant total doses of 170, 210 and 300 kGy to evaluate DRE. First, the cable insulation material types investigated are described. Then, the accelerated aging experimental process involving gamma irradiation applied to the insulation specimens at room temperature and different dose rates is discussed. Then, the experimental characterization techniques used to perform this work are elucidated. These include elongation at break (EAB), mass change, yellowness index (YI), carbonyl index (CI), density, indenter modulus (IM), and relaxation constant (t). Theory of polymer degradation is discussed, and characterization results and discussion are provided. Finally, concluding remarks are made. The findings from this work and cited prior work reveal that DRE are material dependent, even between similar material categories (e.g., XLPE). In the case of the EPDM studied, degradation of ductility was observed to be greater at higher dose rate for the same total dose, indicating accelerated gamma aging to be more conservative than extended aging. Thus, conclusions regarding the conservatism of historical qualification likely require additional consideration for specific materials and conditions in question. The results of this study support the contention that, due to inherent limitations and uncertainties associated with prediction of cable remaining useful life from accelerated aging experiments, trending of installed cable insulation health status will be more practical and useful for safe and efficient cable aging management repair and replace decisions than lifetime prediction from historical qualification. The combination of material robustness demonstrated by the qualification process and ongoing monitoring of cable health status combine to provide confidence in continued safe use of existing nuclear cables. Additional research into effective and efficient condition monitoring methods for non-destructive evaluation of installed cables is needed to support aging cable management, including material studies to inform interpretation of measured results.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

In Situ High Pressure Hydrogen Tribological Testing of Common Polymer Materials Used in the Hydrogen Delivery Infrastructure

High pressure hydrogen gas is known to adversely affect metallic components of compressors, valves, hoses, and actuators. However, relatively little is known about the effects of high pressure hydrogen on the polymer sealing and barrier materials also found within these components. More study is required in order to determine the compatibility of common polymer materials found in the components of the hydrogen fuel delivery infrastructure with high pressure hydrogen. As a result, it is important to consider the changes in physical properties such as friction and wear in situ while the polymer is exposed to high pressure hydrogen. In this protocol, we present a method for testing the friction and wear properties of ethylene propylene diene monomer (EPDM) elastomer samples in a 28 MPa high pressure hydrogen environment using a custom-built in situ pin-on-flat linear reciprocating tribometer. Representative results from this testing are presented which indicate that the coefficient of friction between the EPDM sample coupon and steel counter surface is increased in high pressure hydrogen as compared to the coefficient of friction similarly measured in ambient air.

hydrogen↗

Compatibility of Elastomers with Polyoxymethylene Dimethyl Ethers and Blends with Diesel

Polyoxymethylene dimethyl ethers (PODEs) have shown promise as candidates for diesel fuel blendstocks due to their low sooting tendency, high cetane number, and diesel-comparable boiling point range. However, there is a lack of literature regarding compatibility of PODEs with common automotive elastomers, which would be a prerequisite to their adoption into the marketplace. To address this need, an exposure study and complementary solubility analysis were undertaken. A commercially available blend of PODEs with polymerization degree ranging from 3 to 6 was blended with diesel certification fuel at 0, 33, 50, 67, at 100% by mass. Elastomer coupons were exposed to the various blends for a period of 4 weeks and evaluated for volume swell. The elastomer materials included multiple fluoroelastomers (Viton and fluorosilicone) and acrylonitrile butadiene rubbers (NBR), as well as neoprene, polyurethane, epichlorohydrin (ECO), PVC-nitrile blend (OZO), ethylene propylene diene monomer (EPDM), styrene-butadiene rubber (SBR), and silicone. The exposure results indicated overall poor compatibility for PODE, with every elastomer except for fluorosilicone exhibiting greater than 30% volume swell at the 33% blend level. The general trend across the elastomers was either a consistent increase in volume swell with PODE concentration, or maximum in volume swell at an intermediate blend fraction. One notable exception is EPDM, which is not generally compatible with diesel fuel and which exhibited a reduction in volume swell with increasing PODE concentration. The same elastomers and PODE/diesel blends were evaluated using Hansen solubility parameter analysis, which predicted similar trends to the exposure study with the exception of ECO. From these results, we conclude that adoption of PODEs as a diesel fuel blendstock will require either the development of specialized elastomers, or that the blend fraction be kept to a low level to maintain compatibility with existing elastomers.

42 ENGINEERING↗

ODC-Free Solvent Implementation Issues for Vulcanized Rubber and Bond Systems

Thiokol Propulsion has worked extensively to replace 1,1,1-trichloroethane (TCA) with ozone depleting chemicals (ODC)-free solvents for use in the manufacture of the Reusable Solid Rocket Motor (RSRM) for the Space Shuttle Program. As Thiokol has transitioned from sub-scale to full-scale testing and implementation of these new solvents, issues have been discovered which have required special attention. The original intent of Thiokol's solvent replacement strategy was to replace TCA with a single drop-in solvent for all equivalent applications. We have learned that a single candidate does not exist for replacing TCA. Solvent incompatibility with process materials has caused us to seek for niche solvents and/or processing changes that provide an ODC-free solution for special applications. This paper addresses some of the solvent incompatibilities, which have lead to processes changes and possible niche solvent usage. These incompatibilities were discovered during full-scale testing of ODC-free solvents and relate to vulcanized rubber and bond systems in the RSRM. Specifically, the following items are presented: (1) Cure effects of d-limonene based solvents on Silica Filled Ethylene Propylene Diene Monomer (SF-EPDM) rubber. During full-scale test operations, Thiokol discovered that d-limonene (terpene) based solvents inhibit the cure of EPDM rubber. Subsequent testing showed the same issue with Nitrile Butadiene Rubber (NBR). Also discussed are efforts to minimize uncured rubber exposure to solvents; and (2) Cured bond system sensitivity to ODC-free solvents. During full scale testing it was discovered that a natural rubber to steel vulcanized bond could degrade after prolonged exposure to ODC-free solvents. Follow on testing showed that low vapor pressure and residence time seemed to be most likely cause for failure.

Hodgson, James R.↗

Bright is the New Black - Multi-Year Performance of Generic High-Albedo Roofs in an Urban Climate

High-albedo white and cool roofing membranes are recognized as a fundamental strategy that dense urban areas can deploy on a large scale, at low cost, to mitigate the urban heat island effect. We are monitoring three generic white membranes within New York City that represent a cross-section of the dominant white membrane options for U.S. flat roofs: (1) an ethylene propylene diene monomer (EPDM) rubber membrane; (2) a thermoplastic polyolefin (TPO) membrane and; (3) an asphaltic multi-ply built-up membrane coated with white elastomeric acrylic paint. The paint product is being used by New York City s government for the first major urban albedo enhancement program in its history. We report on the temperature and related albedo performance of these three membranes at three different sites over a multi-year period. The results indicate that the professionally installed white membranes are maintaining their temperature control effectively and are meeting the Energy Star Cool Roofing performance standards requiring a three-year aged albedo above 0.50. The EPDM membrane however shows evidence of low emissivity. The painted asphaltic surface shows high emissivity but lost about half of its initial albedo within two years after installation. Given that the acrylic approach is an important "do-it-yourself," low-cost, retrofit technique, and, as such, offers the most rapid technique for increasing urban albedo, further product performance research is recommended to identify conditions that optimize its long-term albedo control. Even so, its current multi-year performance still represents a significant albedo enhancement for urban heat island mitigation.

Gaffin, S. R.↗