Friction stir welding of multi-walled carbon nanotubes reinforced Al matrix composites

Highlights: • Al/MWCNT composites were successfully welded using friction stir welding. • After FSW, the composites possessed an excellent balance of mechanical properties. • High tensile strength and elongation over BM owing to MWCNTs after FSW. • Microstructures were investigated according to MWCNT contents and FSW conditions. - Abstract: In this study, we prepared composites between Al and multi-walled carbon nanotubes (MWCNTs) using the friction stir welding (FSW) method and investigated their microstructural evolution and mechanical properties by controlling the amount of MWCNT (1 and 3 vol%) and the plunging load (400 and 600 kg) used. After the FSW process, MWCNT showed slight coarsening of grain with random shear textures and accumulated dislocations; the differences obtained by varying the plunging load and MWCNT amount were insignificant. The friction-stir welded composite obtained using 3 vol% MWCNT and a plunging load of 600 kg possessed two-times better balance between strength and ductility than the base metal, due to the presence of both MWCNTs and the partially decomposed Al{sub 4}C{sub 3} in the composite.

36 MATERIALS SCIENCE↗

Room temperature corrosion behaviour of plastically deformed AISI 304 stainless steel by friction stir welding in neutral and acidified chloride solutions

Severe plastic deformation of 304L stainless steel plate was carried out by friction stirring under an isothermal tool temperature at 825°C. The friction stirred zone showed extensive grain refinement, high fraction of low angle grain boundaries due to dislocation rearrangement, Σ3 and Σ9 special grain boundaries and discrete Fe–Cr–Mn-rich particles. Electrochemical polarisation measurements were done on the base metal (BM) and friction stir welded (FSW) specimens in the neutral and acidified 3.5% NaCl solutions. The BM showed marginally better pitting resistance in the neutral chloride solution than the FSW because of a larger fraction of special grain boundaries, and larger grain size. Whereas in acidified 3.5% NaCl solution, the FSW showed better corrosion resistance than the BM. Furthermore, the surface film of the FSW had a lower impedance and a lower defect concentration than the BM indicating higher diffusivity of point defects in the FSW.

36 MATERIALS SCIENCE↗

Chloride-Induced Stress Corrosion Cracking of Friction Stir-Welded 304L Stainless Steel: Effect of Microstructure and Temperature

Dry storage canisters of used nuclear fuels are fabricated using SUS 304L stainless steel. Chloride-induced stress corrosion cracking (CISCC) is one of the major failure modes of dry storage canisters. The cracked canisters can be repaired by friction stir welding (FSW), a low-heat input ‘solid-phase’ welding process. It is important to evaluate the ClSCC resistance of the friction stir welded material. Stress corrosion cracking (SCC) studies were carried out on mill-annealed base materials and friction stir welded 304L stainless U-bend specimens in 3.5% NaCl + 5 N H2SO4 solution at room temperature and boiling MgCl2 solution at 155 °C. The engineering stress on the outer fiber of the FSW U-bend specimen was ~60% higher than that of the base metal (BM). In spite of the higher stress level of the FSW, both materials (FSW and BM) showed almost similar SCC failure times in the two different test solutions. The SCC occurred in the thermo-mechanically affected zone (TMAZ) of the FSW specimens in the 3.5% NaCl + 5 N H2SO4 solution at room temperature, while the stirred zone (SZ) was relatively crack-free. The failure occurred at the stirred zone when tested in the boiling MgCl2 solution. Hydrogen reduction was the cathodic reaction in the boiling MgCl2 solution, which promoted hydrogen-assisted cracking of the heavily deformed stirred zone. The emergence of the slip step followed by passive film rupture and dissolution of the slip step could be the SCC events in the 3.5% NaCl + 5 N H2SO4 solution at room temperature. However, the slip step height was not sufficient to cause passivity breakdown in the fine-grained SZ. Therefore, the SCC occurred in the partially recrystallized softer TMAZ. Overall, the friction-stirred 304L showed higher tolerance to ClSCC than the 304L base metal.

304L austenitic stainless steel↗

HEAT INPUT AND POST WELD HEAT TREATMENT EFFECTS ON REDUCED-ACTIVATION FERRITIC/MARTENSITIC STEEL FRICTION STIR WELDS

Reduced-activation ferritic/martensitic (RAFM) steels are an important class of structural materials for fusion reactor internals developed in recent years because of their improved irradiation resistance. However, they can suffer from welding induced property degradations. In this paper, a solid phase joining technology friction stir welding (FSW) was adopted to join a RAFM steel Eurofer 97 and different FSW parameters/heat input were chosen to produce welds. FSW response parameters, joint microstructures and microhardness were investigated to reveal relationships among welding heat input, weld structure characterization and mechanical properties. In general, FSW heat input results in high hardness inside the stir zone mostly due to a martensitic transformation. It is possible to produce friction stir welds similar to but not with exactly the same base metal hardness when using low power input because of other hardening mechanisms. Further, post weld heat treatment (PWHT) is a very effective way to reduce FSW stir zone hardness values.

Tang, Wei↗

Friction Stir Processed Repair Welding of Dry Storage Canisters and Mitigation Strategies: Effect of Engineered Barrier Layer on Environmental Degradation

The proposed project aims to develop a friction sir based repair technique to heal cracks of stainless steel dry storage canisters (DSCs), created by the effect of stress corrosion cracking (SCC). In real service conditions, the welded parts of the canisters become prone to SCC under exposure to aggressive chemical environment. The focus of the project is on developing a mitigation strategy that can be implemented for countering SCC in DSCs following a two-pronged approach: (i) apply friction stir processing (FSP) as a crack repair technique while creating compressive residual stresses at the canister material surface, thus improving resistance against SCC; (ii) add molybdenum and/or nitrogen by friction stir based alloying process to create compositions that improve pitting resistance and thus enhance resistance against SCC. The specific project objectives are listed below: • Investigate FSW of 304L SS a potential repair welding technique of dry storage canisters; • Optimize the FSW parameters to introduce surface compressive stress profiles in the weldments; • Develop a FSP method to surface alloy the 304L with nitrogen and Mo by adding CrN and Mo powders; • Evaluate the surface compressive residual stress profile during FSW and FSP processes; • Evaluate the localized corrosion resistance of the FSW and FSP samples as a function of temperature, chloride concentration, and surface alloy composition; • Evaluate the SCC behavior of the FSW and FSP samples as a function of stress, chloride concentration, and temperature at different surface chemistries and induced residual stress profiles.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Characterization of microstructure and residual stress following the friction stir welding of dissimilar aluminum alloys

Friction-stir-welding (FSW) has gained importance as an effective way to join dissimilar materials due to its solid-state nature. However, FSW produces substantial residual stresses in aluminum welding, often deteriorating the component's structural performance and reliability. In the current study, the d-spacing (inter-atomic distance) of several locations on a battery tray and stress-free reference samples are measured with neutron diffraction to calculate the residual stresses in a lap 6061 to A365 dissimilar friction-stir-weld. Furthermore, the present study connects the measured residual stress to microstructure properties through electron backscatter diffraction (EBSD) and optical microscopy analyses. The EBSD results indicate that the FSW operation affects the grains’ orientation, thereby producing location-specific directionally varying elasticity across the weldment. Further, this varied elasticity creates unique d-spacing profiles even in the stress-free material. Additionally, the resulting stressed and stress-free d-spacing profiles show dependencies on the FSW tool geometry, traverse direction, and rotational direction. Lastly, this study suggests that the final component residual stress can be influenced by the sequence of multi-pass welds contributing to a rise in temperature in the presence of a completed weld relaxing its residual stress.

36 MATERIALS SCIENCE↗

Nugget Structure Evolution with Rotation Speed for High-Rotation-Speed Friction-Stir-Welded 6061 Aluminum Alloy

High-rotation-speed friction stir welding (HRS-FSW) is a promising technique to reduce the welding loads during FSW and thus facilitates the application of FSW for in situ fabrication and repair. In this study, 6061 aluminum alloy was friction stir welded at high-rotation speeds ranging from 3000 to 7000 rpm at a fixed welding speed of 50 mm/min, and the effects of rotation speed on the nugget zone macro- and microstructures were investigated in detail in order to illuminate the process features. Temperature measurements during HRS-FSW indicated that the peak temperature did not increase consistently with rotation speed; instead, it dropped remarkably at 5000 rpm because of the lowering of material shear stress. The nugget size first increased with rotation speed until 5000 rpm and then decreased due to the change of the dominant tool/workpiece contact condition from sticking to sliding. At the rotation speed of 5000 rpm, where the weld material experienced weaker thermal effect and higher-strain-rate plastic deformation, the nugget exhibited relatively small grain size, large textural intensity, and high dislocation density. Consequently, the joint showed superior nugget hardness and simultaneously a slightly low tensile ductility.

36 MATERIALS SCIENCE↗

Microstructure Evolution and Mechanical Properties of High-Speed Friction Stir Welded Aluminum Alloy Thin Plate Joints

Sound friction stir welded (FSW) joints of 6061-T6 aluminum alloy sheets with an 0.8 mm thickness were obtained at conventional speed (2000 rpm, 300 mm/min) and high speed (11,000 rpm, 1500 mm/min). The recrystallization mechanism, precipitate evolution, mechanical properties and fracture behavior were investigated in detail. Microstructure analyses revealed that the grain structure evolution in the nugget zone (NZ) was dominated by continuous dynamic recrystallization. In the process of FSW, high speed facilitates the formation of finer equiaxed recrystallized grains, higher density of dislocations and substructures, and a larger number of precipitates in the NZ compared to the conventional speed, which further significantly improves the hardness and tensile strength of the joints. The maximum tensile strength was obtained with 292.6 MPa, 83.2% for the 6061-T6 aluminum alloy and 122.6% for the conventional-speed FSW joints. This work provides an effective method for preparing FSW aluminum alloy thin plate joints with excellent mechanical properties.

36 MATERIALS SCIENCE↗

Optimization of Tensile and Corrosion Properties of Dissimilar Friction Stir Welded AA2024-7075 Joints

In this work, we performed some joining experiments of dissimilar aluminum alloys AA2024-T351 and AA7075-T651 using friction stir welding (FSW) technique with different process parameters (rotational speed, welding speed and plunge depth). Response surface methodology based on a central composite rotatable design was used to establish the mathematical models predicting the tensile properties and corrosion rate of dissimilar FSW joints with some high confidence level. Analysis of variance method was employed to verify the developed models. Besides, the influences of FSW process parameters on tensile and corrosion properties of joints were analyzed. In order to obtain a desirable combination property of the dissimilar FSW joints, the optimum process parameters after experimental verification were proposed as: rotational speed 1495 rev/min, welding speed 187 mm/min and plunge depth 0.03 mm. This verification illustrated that the developed models are appropriate for the modeling and optimization of process.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Behavior of Friction Stir-Welded Sc-Modified Al-Zn-Mg Alloys Made Using Different Base Metal Tempers

The microstructure and property of friction stir weld joints of a Sc-modified Al-Zn-Mg alloy developed using base metal in hot-rolled (HR) and T6 temper were studied and compared in this work. The results showed that the microstructure and property exhibited significant difference between the two friction stir weld joints. The weld efficiency of the FSW joint developed using base metal in HR condition is over 90%, while that of the FSW joint developed using base metal in T6 condition is only 70%. The hardness of the weld nugget of HR joint is obviously higher than that of the weld nugget of T6 joint, due to the different changes in the original precipitates during the friction stir welding process. The strengthening mechanism in different zones of the two FSW joints was discussed to examine the microstructure–properties relationship, and the main difference of the strengthening mechanism between the two FSW joints was revealed.

36 MATERIALS SCIENCE↗

Interfacial microstructure and properties of copper clad steel produced using friction stir welding versus gas metal arc welding

A preliminary study compares the feasibility and microstructures of pure copper claddings produced on a pressure vessel A516 Gr. 70 steel plate, using friction stir welding versus gas metal arc welding. A combination of optical and scanning electron microscopy is used to characterize the grain structures in both the copper cladding and heat affected zone in the steel near the fusion line. The friction stir welding technique produces copper cladding with a grain size of around 25 μm, and no evidence of liquid copper penetration into the steel. The gas metal arc welding of copper cladding exhibits grain sizes over 1 mm, and with surface microcracks as well as penetration of liquid copper up to 50 μm into the steel substrate. Transmission electron microscopy reveals that metallurgical bonding is produced in both processes. Increased diffusion of Mn and Si into the copper cladding occurs when using gas metal arc welding, although some nano-pores were detected in the FSW joint interface. - Highlights: • Cladding of steel with pure copper is possible using either FSW or GMAW. • The FSW yielded a finer grain structure in the copper, with no evidence of cracking. • The FSW joint contains some evidence of nano-pores at the interface of the steel/copper. • Copper cladding by GMAW contained surface cracks attributed to high thermal stresses. • The steel adjacent to the fusion line maintained a hardness value below 248 HV.

36 MATERIALS SCIENCE↗

The Significance of Environmental Attributes as Indicators of the Life Cycle Environmental Impacts of Packaging and Food Service Ware

The environmental impacts of packaging and food service ware (FSW) are increasingly the subject of government policy, public discourse, and industry commitments. While some consideration is given to reducing the impacts of packaging across its entire life cycle, most of the focus is on packaging waste or feedstock substitution. Efforts typically focus on specific packaging characteristics, or material attributes, commonly perceived to be environmentally preferable. This article summarizes an extensive meta-review of existing published literature that was performed to determine whether the material attributes recyclability, recycled content, compostability, and biobased, commonly considered to be environmentally beneficial, correlate with lower net environmental impacts across the full life cycle of the packaging and FSW. Seventy-one unique life cycle assessment (LCA) studies that quantify the environmental impacts throughout the entire life cycle of packaging and FSW were analyzed. These studies included over 5000 comparisons for 13 impact categories commonly analyzed in LCA studies. The results from the meta-review identified a number of instances where material attributes do not correlate with environmental benefits for packaging and FSW. Rather, other characteristics such as material choice or mass of the packaging/FSW products can have higher influence in determining life cycle impacts.

54 ENVIRONMENTAL SCIENCES↗

Flexible Friction Stir Joining Technology

Reported herein is the final report on a U.S. Department of Energy (DOE) Advanced Manufacturing Office (AMO) project with industry cost-share that was jointly carried out by Oak Ridge National Laboratory (ORNL), ExxonMobil Upstream Research Company (ExxonMobil), and MegaStir Technologies (MegaStir). The project was aimed to advance the state of the art of friction stir welding (FSW) technology, a highly energy-efficient solid-state joining process, for field deployable, on-site fabrications of large, complex and thick-sectioned structures of high-performance and high-temperature materials. The technology innovations developed herein attempted to address two fundamental shortcomings of FSW: 1) the inability for on-site welding and 2) the inability to weld thick section steels, both of which have impeded widespread use of FSW in manufacturing. Through this work, major advance has been made toward transforming FSW technology from a “specialty” process to a mainstream materials joining technology to realize its pervasive energy, environmental, and economic benefits across industry.

36 MATERIALS SCIENCE↗

Complete Status Report Documenting the Development of Friction Stir Welding for Producing a Butt Joint in Thin Wall Tubing of ODS Alloys

A challenging attempt using friction stir welding to produce a butt joint between two 1.0 mm thick plates of 14YWT was nearly successful. The modified tool pin mostly penetrated the thickness of the adjoined thin plate samples resulting in a small blunt notch on the bottom surface of the butt joint. A bend occurred in the thin plate sample due to formation of stresses from clamping the thin plate sample during FSW. The peak displacement of the bend occurred along the center line of the butt joint. The weld zone showed good microstructure mixing with some flashing mostly on the retreating side that suggested excess heat input by friction between the traveling and spinning tool pin and thin plates of 14YWT. Neutron diffraction experiments were performed on the bent sample of 14YWT to measure the residual stresses in the butt joint on the HB-2B beam line at the Neutron Residual Stress Facility at HFIR. However, the neutron scattering to background noise ratio was very low during data acquisition. Measurements of lattice strains were obtained in the rolling (RD) and normal (ND) directions but not in the extrusion direction (ED) of the thin plate sample. Unfortunately, the quality of the data was not sufficient for determining the residual stresses in the butt joint. From the previous neutron scattering experiments conducted on four hot rolled plates (R1, R2, R3 and R4) of 14YWT, the residual stresses were calculated from lattice strain data and plotted in 2-D color contour maps for ED, RD and ND. The results showed variations in the magnitude and spatial position of residual stresses in the microstructure of the four plates. The magnitude in residual stresses in ED and RD increased gradually with increasing rolling deformation for R1 (50%) to R2 (76%), followed by larger increases in R3 (89%) and R4 (95%). The maximum peaks in residual stresses for R4 was ~710-730 MPa in ED and RD. The residual stresses in ND were below ~300 MPa for each of the 4 rolled plates, with a maximum residual stress in R4 (95%) of ~400 MPa. These results indicated that significant residual stresses representing ~57% of the yield stress of 14YWT (SM13) had accumulated in the 14YWT plate after hot rolling to the 1 mm thickness, which was used in the FSW experiments. The microstructure analysis of the 1.0 mm thick plate of 14YWT containing the butt joint produced by FSW revealed significant changes in the grain structure and texture between the unaffected zone (UZ) of the rolled plate and the butt joint weld. In the UZ, the grains were severely elongated after 95% deformation and mainly possessed the {101} texture component in the ED. Two predominant grain misorientation angles were observed: one consisting of small misorientations of <5º between highly elongated grains and the other consisting of large misorientations of >15º in pockets of small grains that might have formed by dynamic recrystallization processes during rolling of the plate at 1000ºC. The morphology and texture of grains in the heat affected zone (HAZ) were similar to those in UZ, except the grains had coarsened due to excess heat input during FSZ. A population of pores formed and the grains both coarsened and changed to isotropic morphology in the microstructure of the butt joint on both the advancing and retreating sides. The texture of grains in both regions were randomly orientated between the 3 poles {001}, {101} and {111}. The main difference in texture of grains between the advancing side and retreating side was with the misorientation angles of neighboring grains. Most of the grains in the advancing side had misorientation angles of >5º indicating that these grains experienced recrystallization. On the retreating side, areas containing larger grains showed high misorientation angles of >15º compared to areas appearing as bands of grains with misorientation angles of <5º and between 5º-15º. Numerous small pockets of grains with low misorientation angles of <5º were distributed in the microstructure among the grains showing high misorientation angles of >15º. It was determined that the grains associated with low misorientation angles contained sub-grain structures, which was consistent with both recrystallization and recovery mechanisms for grains located on the retreating side of the butt joint. These results demonstrate the complex microstructure that evolves in the microstructure of 14YWT resulting from the input of high temperatures and severe deformations during FSW.

36 MATERIALS SCIENCE↗

(Project 18-15531) Repair and Mitigation of Chloride-Induced Pitting and Chloride-Induced Stress Corrosion Cracking in Used Spent Nuclear Fuel Dry Cask Canister Materials (Final Technical Report)

Several experimental techniques were utilized to understand the corrosion and SCC performance of possible techniques for repairing cracks and pits in SS304 utilized for dry cask storage of spent nuclear fuel. The repairs examined included cold spray, FSW, soldering, and VFAW. The corrosion and SCC assessment techniques utilized for comparing repairs against the base material were 4-pt bending SCC testing in boiling MgCl 2 at stress levels between 0 MPa and 350 MPa, immersion testing in 40% RH brine solution meant to mimic a service-like environment, SSRT SCC testing in 40% RH brine solution. For FSW alone, scanning electrochemical cell microscopy and microelectrochemical syringe cell were utilized to understand the corrosion performance across the weld, in the retreating/advancing sides, and base material. Based on the results of this study, the FSW and cold spray repair techniques proved most viable for SCC repair in SS304 dry cask storage applications and continuing research is highly recommended to understand and quantify in further detail their SCC performance compared to unrepaired SS304. Additionally, solder and VFAW (patch or incline) would not be recommended based on the corrosion and SCC findings in this study.

42 ENGINEERING↗

In Situ Study on Fracture Behavior of Thick-Section Friction Stir-Welded AA 5083 Alloy

Friction stir welding (FSW) produces a gradient microstructure with distinct metallurgical zones. Here, the present study focuses on characterizing the fracture behavior during uniaxial loading across thick-section FSW joint in nonheat-treatable 5083 aluminum alloy. The hardness variation is linked to microstructural features across the weld zones through correlative microscopy. Notably, the heat-affected zone (HAZ) exhibits a lower hardness of 75 HV, while the thermomechanically affected zone (TMAZ) and stir zones (SZ) display a hardness of around 79HV. A marginal difference in hardness in HAZ prompts strain localization in HAZ on the advancing side of the weld, resulting in offset in fracture from the SZ, which is captured through in situ monitoring of the tensile test. Further, the postdeformation analysis reveals crack propagation along the maximum shear stress plane due to the coalescence of microvoids resulting from the fracturing and debonding of second-phase particles. Overall, this study provides valuable insight for optimizing the FSW process of AA 5083 alloy for thick-section applications.

36 MATERIALS SCIENCE↗

Towards High-Speed friction stir welding of 25 mm Thick AA2139-T8: tool innovation and process development

Joining thick plates (≥ 12 mm) of aluminum (Al) alloys is challenging due to high tool forces, uneven material flow, and non-uniform heat distribution through the material’s thickness. Recent advancements in tool design and welding parameters for friction stir welding (FSW) in thick plates butt joining have encountered a developmental plateau, highlighting the need for innovative approaches to overcome existing limitations. Here, this study focuses on the systematic development of single-pass and double-pass FSW processes for high-strength aluminum alloy AA2139-T8, to improve joint efficiency and enable high-speed welding capabilities. Experimental evidence is presented for a novel tool design with opposing pin threads, enabling high-speed (178 mm/min) single-pass friction stir butt welding of 25 mm thick AA2139-T8. A series of FSW trials was conducted both in air and with a trailing water spray, using steel backing plates (BPs) to investigate the impact of quenching and cooling rates on process response and joint performance. A joint efficiency of 83% was attained using the novel tool features and effectively controlling process forces and thermal boundary conditions.

AA2139-T8↗

Prediction of hardness minimum locations during natural aging in an aluminum alloy 6061-T6 friction stir weld

This study describes a simple model that can predict the evolution of hardness distribution as a function of natural aging time in a heat-treatable 6061-T6 Al alloy plate subjected to friction stir welding (FSW). First, two dimensional thermal distributions were simulated as a function of time in the FSW plate by finite element modeling. Second, the hardness changes during natural aging were measured as a function of aging time for a number of Al specimens that had been previously isothermally heat-treated to different hold temperatures in order to determine the natural aging kinetics. Finally, the simulated temperature profiles and the natural aging kinetics were correlated to predict the hardness profiles in the FSW plate. The predicted hardness variations are consistent with measured hardness profiles in that the location of minimum hardness moves away from the centerline as the aging time and/or heat input increases. The hardness variation was also related to the location of failure in cross-weld tensile samples.

36 MATERIALS SCIENCE↗