Search NASA⌕ Search

SEARCH · Search NASA

Results for “FUEL PELLETS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

Evaluation of ceria as a surrogate material for UO 2 in experiments on fuel cracking driven by resistive heating

A variety of normal operation and accident scenarios can generate thermal stresses large enough to cause cracking in light-water reactor (LWR) fuel pellets. Cracking of fuel pellets can lead to reduced heat removal, larger centerline temperatures, and localized stress in cladding all of which impact fuel performance. Furthermore, pellet cracking also contributes to a temperature reduction in the pellet since the pellet fragments tend to move towards the heat sink (cladding), and the heat flow remains predominantly radial despite the presence of cracks. It is important to understand the temperature profile on the pellet before and after cracking to improve cracking models in fuel performance codes However, in-reactor observation and measurement of cracking is very challenging owing to the harsh environment and design of fuel rods. Recently, an experimental pellet cracking test stand was developed for separate effects testing of normal operations and accident temperature conditions, using thermal imaging to capture the pellet surface temperature for evaluation of thermal stresses and optical imaging to capture the evolution of cracking in real time. Cracking experiments were initially performed using ceria (CeO 2 ) as a surrogate fuel material, which is useful for developing and demonstrating the experimental approaches but is also valuable in its own right for cracking model development and validation. A combination of induction and resistance heating was used for volumetric heat generation in the pellet creating a thermal gradient. The material properties of CeO 2 and UO 2 are reviewed and compared for use in model development. Simulations of the experiment were performed to evaluate the behavior of the surrogate (CeO 2 ) fuel in BISON. The measured temperature profiles from BISON models match reasonably well with the observed experiments for the ceria pellets before cracking. The findings from this work will help improve confidence in fracture models used for fuel pellets under similar in-reactor conditions.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Self-consistent investigation of density fueling needs on ITER and CFETR utilizing the new Pellet Ablation Module

Abstract Self-consistent modeling using the stability, transport, equilibrium, and pedestal (STEP) workflow in the OMFIT integrated modeling framework (predicting pedestal with EPED, core profiles with TGYRO, current profile with ONETWO, and EFIT for equilibrium) suggests ITER and future devices such as China Fusion Engineering Test Reactor (CFETR) Zhuang et al (2019 Nucl. Fusion 59 112010) will benefit from high-density operation (Greenwald limit fraction f g w ≈ 0.7−1.3). Regimes with an operational density near the Greenwald limit will likely need peaked density profiles so that the pedestal density remains below the Greenwald limit. Peaked density profiles can be achieved with the help of pellet injection. A flexible Pellet Ablation Module (PAM), which predicts the density source based on a comprehensive analytical pellet ablation model, has been developed for predicting pellet fueling for transport studies, and has been incorporated into the STEP workflow for predictive modeling. This workflow is applied to DIII-D and finds good agreement with experiments. On ITER the effect of pellet fueling is examined in an advanced inductive scenario, where a fusion gain of up to Q = 9 is predicted with strong central pellet fueling. On CFETR, with a mid-radius density source, an average of 1.5 × 10 22 electrons s −1 are required to achieve the density and temperature profiles necessary for the 1000 MW advanced scenario with a tritium burn-up fraction of ∼ 3 % .

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

High density UO 2 and high thermal conductivity UO 2 composites by spark plasma sintering (SPS)

Embodiments of the invention are directed to a method for production of a nuclear fuel pellet by spark plasma sintering (SPS), wherein a fuel pellet with more than 80% TD or more than 90% TD is formed. The SPS can be performed with the imposition of a controlled uniaxial pressure applied at the maximum temperature of the processing to achieve a very high density, in excess of 95% TD, at temperatures of 850 to 1600° C. The formation of a fuel pellet can be carried out in one hour or less. In an embodiment of the invention, a nuclear fuel pellet comprises UO 2 and a highly thermally conductive material, such as SiC or diamond.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

High density UO2 and high thermal conductivity UO2 composites by spark plasma sintering (SPS)

Embodiments of the invention are directed to a method for production of a nuclear fuel pellet by spark plasma sintering (SPS), wherein a fuel pellet with more than 80% TD or more than 90% TD is formed. The SPS can be performed with the imposition of a controlled uniaxial pressure applied at the maximum temperature of the processing to achieve a very high density, in excess of 95% TD, at temperatures of 850 to 1600° C. The formation of a fuel pellet can be carried out in one hour or less. In an embodiment of the invention, a nuclear fuel pellet comprises UO 2 and a highly thermally conductive material, such as SiC or diamond.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Advanced Fuel Cycle Cost Basis Report: Module D1-2 LWR Pelletized MOX Fuel Fabrication

Nature of this 2021 Module update from previous AFC-CBRs: Use of U,Pu MOX life cycle cost data from late 1970s Non-proliferation Assessment Systems Analysis Program (NASAP). This archived data has been updated in 2018-2019 to reflect today’s regulatory and economic conditions and is presented in 2017. For the lower unit cost MOX fabrication case the PuO 2 from the reprocessed LWR SNF is assumed to be fabricated immediately after aqueous PUREX reprocessing, thus minimizing the time for undesirable actinide radioisotopes, from the standpoint of radiation safety, to build in. Fabricated MOX utilizing separated and multi-year stored Pu from aqueously reprocessed SNF has also been added to this Module as a second LWR MOX fabrication variant, requiring additional and more costly glovebox design and operations to protect personnel. This new NASAP-informed data augments historical data and unit cost projections appearing in the 2009 (Shropshire et al 2009), 2012 (Dixon et al 2012), and 2017 Dixon et al 2017) AFC-CBRs. The “What-it-takes” 2017 unit fabrication cost values based on the updated NASAP studies are escalated to 2020$ for this 2021 Update Report.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Method of manufacturing a reinforced nuclear fuel cladding using an intermediate thermal deposition layer

A method is described that includes the steps of making a thin walled Zr alloy tube, loading nuclear fuel pellets into the tube, compressing the tube onto the fuel pellets to substantially reduce free space around the fuel pellets, positioning end plugs at each of two ends of the tube, filling the tube with a heat transferring gas, and coating the compressed tube with a corrosion resistant material using a thermal deposition process, such as cold spray, before inserting the tube into a pre-formed SiC composite cover having at least one closed end.

Lahoda, Edward J.↗

UO 2 + 5 vol% ZrB 2 nano composite nuclear fuels with full boron retention and enhanced oxidation resistance

The boron isotope ( 10 B) can be used as a neutron absorber in UO 2 to control the reactivity of nuclear fuel pellets, however, the boron source can react with oxygen source in UO 2 to form B 2 O 3 that vaporize readily at temperatures above 1200 °C. Unfortunately, the sintering of UO 2 fuel requires hours holding at high temperature (>1700 °C), resulting in an inevitable B loss during sintering and unpredictable B concentration in final product. It is challenging to incorporate boron through a conventional sintering method. In this work, we demonstrated that spark plasma sintering (SPS), a field assisted sintering technology, can effectively densify UO 2 + 5 vol% ZrB 2 composite fuel pellets by rapid consolidation at 1600 °C for a short duration of 5 min under an applied pressure of 40 MPa. Further, thermogravimetric analysis (TGA) measurements confirm that ZrB 2 is fully retained inside the composite fuel pellets. Inside the composite fuel pellets, nano sized ZrB 2 particles are uniformly distributed along the grain boundaries of the UO 2 matrix. The ZrB 2 particle transforms to a glassy B 2 O 3 phase covering the sample surface and grain boundaries of UO 2 matrix after a simple post-sintering annealing at 1000 °C in flowing Argon gas for 4 h. The formed glassy B 2 O 3 slows down the diffusion of oxygen ions and postpones the onset temperature for oxidation of UO 2 from 400 °C to 550 °C. This study demonstrates the capability of SPS, an advanced fuel manufacturing technique, to achieve a full retention of ZrB 2 in UO 2 oxide fuel and increase oxidation resistance through a simple post-sintering annealing. The reported work holds great engineering potential for development of advanced oxide fuel for nuclear application.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

The Use of High-Density UN Fuel in Heat-Pipe Microreactors

Heat-pipe microreactors (HPMRs) are very small-scale nuclear reactors that employ heat pipes (HPs) for heat removal. HPMRs can be easily integrated with other forms of renewable energies, can be used for emergency responses to disaster relief zones, can be deployed in remote locations not connected to the grid, and can be removed from sites and replaced by new ones. HPMRs can also be used for space missions as HPs do not rely on gravity for heat transfer. Conventional fuel materials, such as uranium oxide (UO 2 ) and uranium oxycarbide (UCO), are currently considered in most existing HPMR designs, but ceramic uranium nitride (UN) fuel that has high uranium density, high thermal conductivity, and high melting point may become a better fuel candidate. Through neutronics calculations, this paper assesses the impact of using UN fuel in HPMRs with two different neutron spectra (fast and thermal) and two different fuel forms [traditional solid fuel pellets and TRi-structural-ISOtropic (TRISO) fuel compacts]. It was concluded that retrofitting HPMRs with UN fuel has the potential to reduce the initial 235 U enrichment requirement by ~3 wt% (to keep the same cycle length) or increase the cycle length (by keeping the same initial 235 U enrichment), which enables more compact and transportable HPMR core designs. However, using UN fuel decreases the control element worth [by up to 20% for the Special Purpose Reactor (SPR) and 5% for HP-MR] and is up to 80% more costly. Increasing 15 N enrichment can further decrease the initial 235 U enrichment requirement and increase the control element worth but is more costly. In conclusion, compared to fast-spectrum HPMRs fueled with solid pellet fuels, retrofitting UN fuel is more suitable for thermal-spectrum HPMRs fueled with TRISO fuel compacts, where the neutron spectrum hardening caused by using UN is less significant.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

Experimentally validated multiphysics modeling of fracture induced by thermal shocks in sintered UO 2 pellets

Uranium Dioxide (UO 2 ) fuel powers almost all commercial Nuclear Power Plants (NPPs) worldwide, generating carbon-free energy and contributing to the fight against climate change. UO 2 fuel incurs damage and fractures due to large thermal gradients that develop across the fuel pellet during normal and transient operating conditions. A comprehensive understanding of the underlying mechanisms by which these processes take place is still lacking. A combined experimental and computational approach is utilized here to quantify the behavior of UO 2 fuel fracture induced by thermal shock. Here, this work introduces both (1) an experimental study to understand the fuel fracturing behavior of sintered UO 2 pellets when exposed to thermal shock, and (2) a Multiphysics phase-field fracture model capable of simulating this process. Parametric studies were conducted to evaluate the effects of uncertainties in fracture properties on the fracture behavior of UO 2 due to thermal shocking. A set of energy release rate (or equivalently fracture toughness) and contract area (the part of the fuel pellet in direct contact with the cold bath) were able to capture the overall fracture trends of the corresponding experimental data. Our combined approach presents a new method for accounting for the effects of microstructure and sample size on the energy release rate/fracture toughness. The experimental data were collected from multiple experiments that exposed UO 2 pellets to high-temperature conditions (589–676 °C) followed by a quench in sub-zero water. This work demonstrates that joint experimental and computational efforts are able to advance the understanding of thermal fracture in the primary fuel source for existing and future NPPs.

36 MATERIALS SCIENCE↗

BISON validation of FeCrAl cladding mechanical failure during simulated reactivity-initiated accident conditions*

Here, a reactivity-initiated accident (RIA) is a postulated design basis accident in light water reactors (LWRs) in which a rapid reactivity insertion induces a fission rate increase and a fuel pellet temperature rise. During RIA, the fuel pellet thermally expands and may cause pellet-cladding mechanical interaction (PCMI). Separate effects PCMI tests were performed on C26M FeCrAl cladding tube samples, introducing biaxial stress via a well understood modified burst test (MBT) system. A high-speed camera in the MBT system captured the projections, covering a 360° view of the cladding deformation and enabling a digital image correlation (DIC) method to quantify the surface strains with high fidelity. Representative hot zero-power RIA mechanical loading conditions were applied to the sample, and the test duration ranged from 20 to 500 ms at an average temperature of 573 K. BISON finite element–based fuel performance code modeling was performed against the high-fidelity DIC data produced from the MBTs. Validation calculations were conducted with 2D models and systematically compared with test data of the burst time, burst pressure, burst hoop strains, and hoop strain rates. Based on the behaviors from the separate effects test, BISON calculations satisfactorily predicted the cladding deformation behaviors. Sensitivity analysis was conducted to identify highly influential mechanical properties responsible for the cladding failure behavior during the MBT experiments. The results highlight the significance of the cladding's mechanical strength in governing cladding strain, followed by the significance of the mechanical interactions between the pellet and the cladding.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

In-Pile Loss of Coolant Accident Testing at TREAT

Several hot-cell based LOCA test apparatuses still exist in various institutions across the world. These facilities typically surround rods with infrared electrical heaters to simulate LOCA conditions on the cladding. Despite its utility for cladding-focused testing, the furnace-based external heating method creates an inverted temperature gradient in fuel pellets compared to a true LOCA where radioisotope decay heat generates internal heat. Capturing the correct temperature gradient is essential in simulating the thermomechanical stress in fuel pellets, and hence a crucial design parameter investigating FFRD during a postulated LOCA. This thermomechanical stress state, for which the evolution of fuel pellet centerline and cladding temperatures is a good figure of merit, was the primary parameter investigated during conception of the LOCA-SERTTA device.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Separate-Effects Tests for Studying Temperature-Gradient-Driven Cracking in UO 2 Pellets

We report a variety of normal operation and accident scenarios can generate thermal stresses large enough to cause cracking in light-water reactor (LWR) fuel pellets. Cracking of fuel pellets can lead to reduced heat removal, higher centerline temperatures, and localized stress in cladding, all of which impact fuel performance. It is important to experimentally characterize the thermal and mechanical behavior in the pellet before and after cracking to improve cracking models in fuel performance codes. However, in-reactor observation and measurement of cracking is very challenging due to the harsh environment and logistics. Recently, an experimental pellet cracking test stand was developed for separate effects testing of normal operations and accident temperature conditions, using thermal imaging to capture the pellet surface temperature for evaluation of thermal stresses and optical imaging to capture the evolution of cracking in real time. Experiments were performed using depleted uranium dioxide (UO 2 ) pellets, which are useful for collecting data valuable for development and validation of cracking models. A combination of induction and resistance heating was used to create an average temperature gradient of 236°C/cm and 193°C/cm before and after cracking respectively. Characterization of the pellets were done before as well as after cracking. The cracking patterns are somewhat different than those expected in a typical reactor because of the differences in thermal conditions and pellet microstructure. However, if the actual conditions of these experiments are reproduced in computational models, these out-of-pile tests on UO 2 pellets provide relevant data for modeling purposes.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Development and demonstration of a methodology to evaluate high burnup fuel susceptibility to pulverization under a loss of coolant transient

For economic reasons, the US nuclear industry is renewing efforts to build a technical basis to extend rod average burnup limits above the current regulatory burnup limit of 62 GWd/MTU. The primary driver is to increase pressurized water reactor cycle lengths to 24 months, reducing the number of fresh fuel assemblies and core design constraints, thereby making core energy utilization more efficient. However, fuel pellet fragmentation and pulverization, termed high burnup fuel fragmentation (HBFF), has been observed in the high burnup (>90 GWd/MTU) Halden loss-of-coolant-accident (LOCA) integral test series. The issue gained attention when fuel fragmentation and pulverization were also observed closer to the current US regulatory limit during the US Nuclear Regulatory Commission (NRC) sponsored out-of-core integral test at Studsvik Nuclear in early 2011. This led to NRC concerns with potential changes to fuel and core designs relative to fuel pellet pulverization. In a letter to the NRC Commissioners, the staff specifically identified a need to “…define the boundary of safe operation for key fuel design and operating parameters,” stating that “the staff is challenged to evaluate the acceptability of future fuel design advancements and fuel utilization changes.” As such, it can be concluded that HBFF and potential dispersal into the reactor coolant system introduces additional complications in light-water reactor (LWR) fuel safety evaluations. However, it is not clear how much fuel will be susceptible to HBFF; nor has there been a methodology developed to evaluate fuel susceptibility to HBFF. To that end, this paper proposes an analysis methodology to assess fuel susceptibility to HBFF during LOCA scenarios. The work presented here uses the BISON fuel performance code to evaluate a representative pressurized water reactor fuel rod exposed to a rod average burnup of 75 GWd/MTU. Sensitivity studies investigated the impact of the peak cladding temperature, transient fission gas released, and pre-transient fission gas release on cladding ballooning and burst timing. Subsequently, a methodology to assess fuel susceptibility to HBFF will be developed based on experimental data published in the open literature. The methodology will then be demonstrated by calculating the mass of fuel susceptibility to HBFF. The BISON results conclude that increasing peak cladding temperature drastically decreased time to failure, and decreased balloon size both of which have been confirmed experimentally. Additionally, the effect of pre-transient and transient fission gas release affected cladding balloon size and burst timing. Finally, fuel susceptibility to HBFF significantly decreased as a function of peak cladding temperature.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Fabrication of UN-Mo CERMET Nuclear Fuel Using Advanced Manufacturing Techniques

Ceramic-metallic nuclear fuels are a candidate fuel for nuclear thermal propulsion systems due to their high heat transport properties, which are necessary in very high-temperature environments. The conventional fabrication of uranium nitride–molybdenum fuel has been thoroughly studied in the past, but modern manufacturing techniques have presented a unique opportunity for further development within this field. This work demonstrates the use of advanced manufacturing techniques to produce nuclear fuel pellets composed of uranium nitride microspheres encased in a molybdenum matrix. Binder jetting is used to print molybdenum disks that are filled with uranium nitride microspheres and afterward sintered using spark plasma sintering. Two fuel pellets were fabricated to demonstrate the methodology and to provide a baseline analysis of the effects of temperature and pressure processing conditions. Characterization of the sintered fuel pellets includes detailed microstructural analysis and thermal conductivity measurements.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Manufacturing porous U10Zr fuels with controlled porosities by SPS and thermal properties

To accommodate the swelling of metallic fuels induced by the fission gas release during burnup in sodium fast reactor for a sodium-free fuel option, advanced U-10Zr fuels with controlled porosity were designed and demonstrated by spark plasma sintering. U-10Zr fuel pellets with manufactured porosities varying from 35% up to fully dense fuel pellets have been fabricated by controlling ball milling times of the starting uranium powders, sintering temperature, pressure, and duration, and the correlation among the microstructure control – porosity – sintering conditions has been established. To further mimick the pore structure in irradiated fuels, different pore formers (NaCl and NH4HCO3) have been used to control the pore size and distribution. Microstructure characterization indicates a lamellar reaction zone of U and Zr, differing from the arc-melted U-10Zr as a result of rapid consolidation of SPS at lower temperature and short durations. The thermal conductivity of U10Zr with different porosities are also measured. Here this work demonstrates the success in manufacturing new metallic fuel forms with controlled porosities and pore distribution, which can be used as model systems to investigate the thermal transfer behavior of metallic fuels in the reactor.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Status Report on Characterization of High Burnup Fuel with Advanced Nondestructive Pulsed Neutron PIE

Characterizing irradiated or spent nuclear fuels with pulsed neutron techniques provides microstructural data such as phase fractions as well as crystallographic data, e.g. lattice parameters, from diffraction analysis. Diffraction characterization is complemented by spatially resolved mapping of isotope densities from energy-resolved neutron imaging, in particular neutron absorption resonance imaging, and overall bulk isotope assay with better sensitivity for minority isotopes from neutron absorption resonance spectroscopy without spatial resolution. Furthermore, after characterization at ambient condition, heating of irradiated or spent fuel will allow to characterize differences of e.g. lattice thermal expansion or phase transition temperature and kinetics compared to fresh fuel as well as enable the study of disappearance of irradiation defects. This data enables benchmarking of predictions of properties of irradiated fuels for which otherwise experimental data is sparse. The effort described here strives to characterize a section cut from a high-burnup fuel. Volumes smaller than entire fuel pellets or rodlets as proposed here, e.g. sections cut from a fuel pellet, to pave the way to characterize entire pellets or rodlets in the future.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Fracture behavior of irradiation induced nanocrystalline UO 2 studied by in-situ mechanical testing in transmission electron microscopy

Uranium Dioxide (UO 2 ) is widely used as a fuel in current light water reactors (LWRs). Upon accumulation of radiation damage, LWR UO 2 fuel pellets start to develop a different microstructure at the pellet periphery when fuel burnup exceeds 45–50 GWd/tHM. The resulting porous, nanocrystalline microstructure is one of the most prominent microstructural changes occurring in such fuel. Its fracture mechanisms, which causes fuel fine fragmentation, could impact safety limits when the cladding breaches. Direct measurements of these properties are challenging, therefore a surrogate obtained via ion irradiation can be used. In this study, multiple microcantilevers were fabricated by focused ion beam from both fresh UO 2 and UO 2 irradiated with 84 MeV Xe 26+ ions to a peak dose of 1357 displacements per atom (dpa). Further, the irradiation produced a pseudo high burnup structure approximately 2 µm below the surface. In-situ nano-mechanical bending tests were conducted to investigate the fracture behavior and the effect of the surrogate UO 2 high burnup structure on local fracture properties. Fresh UO 2 fuel was observed to fracture in transgranular mode without nucleation or movement of dislocations. However, the Xe-irradiated nanocrystalline microcantilevers fractured along the grain boundaries, with no influence from the pre-existing micro-cracks in the microcantilever. Fracture toughness for this type of surrogate high burnup UO 2 structure is reported for the first time in literature. Both the fracture stress and toughness show degradation for UO 2 as a result of Xe-irradiation.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

FY2022 Progress Report for Advanced Re-fabrication/Re-instrumentation Capability Development

In support of performing follow-on irradiation experiments with previously irradiated materials, the Halden Reactor Project developed unique and state of the art capabilities to refabricate and re-instrument previously irradiated materials. Such materials were used in in-pile tests at the Halden reactor, and out-of-pile tests for example using furnaces as a heat source. The decision to close the Halden Reactor Project results in the loss of this refabrication and re-instrumentation capability. As a result, the United States (U.S.) Department of Energy (DOE) has determined to develop refabrication and re-instrumentation capability at the unique shielded facilities at Idaho National Laboratory (INL). The development of refabrication capability has been completed and demonstrated. This report focuses on the complementary aspects of reinstrumentation and the progress to-date. Halden spent nearly 30 years developing both refabrication and re-instrumentation. Collaboration with Halden is allowing Idaho National Laboratory (INL) to develop this capability much more rapidly. In FY-21 the results include development of the capability to drill annular center holes in ceramic UO2 fuel pellets, development of fuel rod end caps with feedthroughs for centerline instrumentation inside the rodlet, The procurement of both fuel drilling and welding demonstration equipment from Halden, evaluation of surface thermocouple attachments to support better understanding of temperature measurement uncertainties, and finally, the conceptual design of a new shielded enclosure where advanced refabrication and re-instrumentation equipment can be housed. In FY-22, the results include; Completing set up of the drilling and welding modules procured from Halden, and early experimental trials using that equipment.; Completing set up of an out-of-cell circumferential weld system to allow for further weld development to take place and support fabrication of fuel for fresh fuel experiments.; Evaluation of the Hot Fuel Examination Facility (HFEF) infrastructure to support future installation of advanced re-fabrication/re-instrumentation equipment, specifically related to necessary infrastructure for cryo-drilling.; Developments in dry-drilling alternative. Including experimental studies showing cordierite is the most suitable surrogate for UO 2 for performing drilling studies. That drilling performance is enhanced when a fuel-clad bonding condition is simulated.; Conceptual design completed for attaching surface thermocouples to irradiated fuel in support of TWIST capsule experiments. The authors would like to thank the numerous colleagues at INL and Halden who provided support in accomplishing this work. Their support both material and intellectual is invaluable in advancing the state of the art and establishing the capabilities for refabrication and re-instrumentation at INL.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗