Developing the ability to inform and tailor aerosol deposition coatings using laser induced particle impact testing
Explore the source record for details and available documents.
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Explore the source record for details and available documents.
For resilient energy delivery PV modules and systems must withstand extreme weather events such as hailstorms, which are the leading cause of PV insurance claims. Currently, the industry testing is limited to one strike at a time, but in real hailstorms multiple hail strikes can occur within a fraction of a second. In this project we test if multiple simultaneous or near-simultaneous hail strikes cause more damage than with single hail strike testing.
Explore the source record for details and available documents.
Abstract not provided.
Abstract not provided.
Presentation to be presented during the Site-Directed Research and Development (SDRD) program FY 2021 review meeting (Webex), September 22–23, 2021.
Explore the source record for details and available documents.
Three prototypes the ORNL-SFC-W-1 special form capsules (SFCs) of the same design were evaluated to determine if the requirements of Title 49, Code of Federal Regulations (CFR), Part 173.469, Tests for Special Form Class 7 (Radioactive) Materials, were met. The results of the special form tests are documented in this test report. This report describes the special form testing activities performed on the three ORNL-SFC-W-1 capsules. The test units were designated as TU-1, TU-2 and TU-3. TU-1 was subjected to leak testing, impact testing and percussion testing. TU-1 was leak tested using the leak rate test specified in 49 CFR 173.469(a)(4)(i). The impact test was conducted according to the requirements in 49 CFR 173.469 (b)(1). The percussion test that was carried out on TU-1 was conducted in accordance with 49 CFR 173.469 (b)(2). Both TU-2 and TU-3 were subjected to a leak rate test as specified in 173.469(a)(4)(i) and a heat test as specified in 49 CFR 173.469(b)(4). Each test unit was leak tested before and after these respective tests. The leak rate tests performed were helium back-pressure tests and bubble tests as specified in American National Standards Institute (ANSI) N14.5-2014.The measured leak rates were converted to standard condition leak rates as specified in American Society for Testing and Measurement (ASTM) E 493. The determined standardized leak rates obtained from the test and the calculations for all the test units met the requirements for special form certification. The testing was performed under the direction of the Oak Ridge National Laboratory (ORNL) Package Testing Program (PTP).
Poly(lactide) (PLA) and poly(methyl methacrylate) (PMMA) are melt compounded with chopped glass fiber using laboratory scale twin-screw extrusion. Physical properties are examined using differential scanning calorimetry (DSC), dynamic mechanical thermal analysis (DMTA), thermogravimetric analysis (TGA), tensile testing, impact testing, X-ray computed tomography (CT) scanning, and field emission scanning electron microscopy (FE-SEM). Molecular weight is determined using gel permeation chromatography (GPC). Miscibility of the blends is implied by the presence of a single glass transition temperature and homogeneous morphology. PLA/PMMA blends tend to show positive deviations from a simple linear mixing rule in their mechanical properties (e.g., tensile toughness, modulus, and stress at break). The addition of 40 wt % glass fiber to the system dramatically increases physical properties. Across all blend compositions, the tensile modulus increases from roughly 3 GPa to roughly 10 GPa. Estimated heat distortion temperatures (HDTs) are also greatly enhanced; the pure PLA sample HDT increases from 75 degrees C to 135 degrees C. Fiber filled polymer blends represent a sustainable class of earth abundant materials which should prove useful across a range of applications.
Two prototypes the welded ISOTEK-SFC-W-3 special form capsules (SFCs) of the same design were evaluated to determine if the requirements of Title 49, Code of Federal Regulations (CFR), Part 173.469, Tests for Special Form Class 7 (Radioactive) Materials, were met. The results of the special form tests are documented in this test report. This report describes the special form testing activities performed on the two welded ISOTEK-SFC-W-3 capsules. The test units were designated as TU-1 and TU-2. TU-1 was subjected to leak testing, percussion testing, and impact testing. TU-1 was leak tested using the leak rate test specified in 49 CFR 173.469(a)(4)(i). The impact test on TU-1 was conducted according to the requirements in 49 CFR 173.469 (b)(1). The percussion test that was carried out on TU-1 was conducted in accordance with 49 CFR 173.469 (b)(2). TU-2 was subjected to a leak rate test as specified in 173.469(a)(4)(i) and a heat test as specified in 49 CFR 173.469(b)(4). Each test unit was leak tested before and after these respective tests. The leak rate tests performed were helium back-pressure tests and bubble tests, as specified in American National Standards Institute (ANSI) N14.5-2014. The measured leak rates were converted to standard condition leak rates as specified in American Society for Testing and Measurement (ASTM) E 493. The determined standardized leak rates obtained from the test and the calculations for all the test units met the requirements for special form certification. The testing was performed under the direction of the Oak Ridge National Laboratory (ORNL) Package Testing Program (PTP).
Mechanical behavior and texture evolution of Mg rare-earth alloy WE43 is investigated for strain-rates 10 -3 /s to upwards of 10 5 /s for the two material conditions - as-cast (AC) and T6 age hardened, rolled plate (RT6). The high strain-rate behavior is tested using both Taylor cylinder impact tests (TC) and split Hopkinson pressure bar tests (SHB) and bulk textures are obtained using neutron diffraction. Unlike the quasi-static strained material, AC and RT6 SHB retained high hardening rates throughout the test, even up to 30% true strain. Moreover, the high strain-rate data revealed that the RT6 material has a much higher strength than the AC material, but similar hardening rates despite significantly different initial texture. The flow stress near yield increased up to I 0% for RT6 and up to 30% for AC as the strain-rate increased six orders of magnitude from quasi-static rates 10 -3 /s to 10 3 /s. Neither material exhibited significant plastic anisotropy over the broad range of strain rates, despite the fact that the RT6 material had a moderately strong initial texture. In the TC tests, the geometric cross-sectional changes and texture along the cylinder from the cylindrical sample foot to head are measured and from the neutron diffraction texture analysis, upper-bound estimates of twin volume fraction are obtained as well as dislocation density from analyzing diffraction peak broadening. Recorded geometrical changes along several loading directions show that the material has deformed remarkably homogeneously under impact. Analysis of deformed textures indicates that {101¯2} extension deformation twinning occurred in the RT6 condition over the range of strain rates, with an upper bound estimate of 40% twin volume fraction for approximately 0.10-0.25 true strain. The peak texture components after the impact have their c-axes closely aligned with the impact direction. As a result, these observations are presented and rationalized in the paper.
Cladding hard-surfacing alloys on tool steel is an effective approach to enhance the surface properties of tool steel. In this study, a Co-based alloy was deposited on tool steel by Directed Energy Deposition (DED) following a three-factor three-level design of experiment matrix with varied laser power, scan speed, and powder flow rate. The microstructure of the deposits was characterized using scanning electron microscopy (SEM). The residual stress on the surface of the samples was measured by the X-ray diffraction (XRD) sin2? technique. The parameters that produced promising deposits were used to fabricate samples for tensile test, four-point bending test, Charpy impact test, and hardness measurement. Our result reveals that the processing parameters have a significant role in the residual stress of the coatings. Residual stress reduces with the increase of laser energy density. Cracks were found at samples with energy density below a threshold. Tensile testing of the coating/substrate combined structure reveals fracture at the coatings with an ultimate tensile strength of 633.9 ± 54.7 MPa. The bi-material interface survived the tensile test, indicating a strong interfacial bond. The four-point bending test of coating/substrate laminates shows an ultimate flexure strength of 860.6 ± 36.9 MPa. Cracks initiated from the coatings ignored the interface and penetrated the substrate, suggesting a solid bi-material bond. Charpy impact test shows the absorbed energy of coating/substrate laminates is more than doubled that of the substrate.