Variability in Chromium Segregation at Lath Boundaries in Proton-Irradiated 9 wt.% Cr Model Steel Determined by Quantitative X-Ray Mapping
No abstract prepared.
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
No abstract prepared.
Highlights: • Fractions of lath martensite and its packets decrease with the increasing of strain. • Length and width of blocks of lath martensite decrease with an increase in strain. • Severe work-hardening and completed DRX hamper transformation of lath martensite. • As for austenite with the state of work-hardening, the lath width changes little. • As for austenite with the state of DRX and subsequent growth, the lath width changes. - Abstract: 300 M steel was isothermally compressed on a Gleeble 1500 simulator at a deformation temperature of 1173 K, a strain rate of 0.1 s{sup −1} and strains ranging from 0.11 to 1.20. The morphologies and structure characteristics of martensite transformed from deformed austenite during water quenching were observed and analysed via scanning electron microscope and transmission electron microscope. Subsequently, effects of prior austenite state on martensitic transformation behavior of 300 M steel were analysed. The experimental results showed that predominant lath martensite and complemental twinned martensite and retained austenite coexisted in deformation-quenched 300 M steel at various strains. The volume fraction of lath martensite and packets of lath martensite decreased with the increasing of strain, and the length and width of the blocks in lath martensite concurrently decreased. Prior austenite with the state of severely work-hardening or just completed dynamic recrystallization would hamper the nucleation and subsequent growth of lath martensite. Additionally, as for austenite with the state of work-hardening, the morphologies and width of laths changed little with the increasing of strain, whereas dislocations in the interior of laths dramatically increased. However, as for austenite with the state of dynamic recrystallization and subsequent growth, the width of laths obviously increased with the increasing of austenite grain size.
Highlights: • Structure and crystallography of M-A constituent in ICCGHAZ of X100 weld joint was studied via multi-scale characterization. • Majority of M-A constituent preferred to form lamellar lath structure, which primarily consisted of lath martensite (87%). • The retained austenite had K-S orientation relationship with its neighboring martensite. • Adjacent martensite laths within M-A had large misorientation but no fixed crystallographic orientation relationship. • Martensite laths within the M-A constituent did not inherit the crystallographic orientation of the parent matrix. - Abstract: The structure and crystallography of martensite-austenite (M-A) constituent in the intercritically reheated coarse-grained heat affected zone (ICCGHAZ) of X100 (690 MPa) pipeline steel weld joint was studied via multi-scale characterization. The results suggested that majority of the necklace-type M-A constituent in the ICCGHAZ preferred to form lamellar lath structure, which primarily consisted of lath martensite (87%). Only small fraction of retained austenite (9%) was found between martensite laths. The retained austenite had K-S orientation relationship with its neighboring martensite: (10-1){sub M} // (11-1){sub γ} and [111]{sub M} // [011]{sub γ}. Adjacent martensite laths within M-A constituent had large misorientation but no fixed crystallographic orientation relationship which implied that martensite laths may nucleate independently and encounter with each other during growth. M-A constituent and matrix microstructure belonged to different prior austenite grains. The martensite laths within the M-A constituent did not inherit the crystallographic orientation of the parent matrix during the intercritical reheating and subsequent cooling process of the second pass welding.
Highlights: • Lath martensite islands and bands were indexed in variations of dual-phase steels. • Detail insight was obtained by combined EBSD, APT, TEM, nano-indentation analysis. • The islands predominantly consist of one main packet with all six variants. • The bands are composed of connected domains, each largely made of one main packet. • Tempering at ~450 °C causes carbon partition to lath boundaries and dislocation cores. - Abstract: Lath martensite is important in industry because it is the key strengthening component in many advanced high strength steels. The study of crystallography and chemistry of lath martensite is extensive in the literature, however, mostly based on fully martensitic steels. In this work, lath martensite in dual phase steels is investigated with a focus on the substructure identification of the martensite islands and microstructural bands using electron backscattered diffraction, and on the influence of the accompanied tempering process during industrial coating process on the distribution of alloying elements using atom probe tomography. Unlike findings for the fully martensitic steels, no martensite islands with all 24 Kurdjumov-Sachs variants have been observed. Almost all martensite islands contain only one main packet with all six variants and minor variants from the remaining three packets of the same prior austenite grain. Similarly, the martensite bands are typically composed of connected domains originating from prior austenite grains, each containing one main packets (mostly with all variants) and few separate variants. The effect of tempering at ~450 °C (due to the industrial zinc coating process) has also been investigated. The results show a strong carbon partitioning to lath boundaries and Cottrell atmospheres at dislocation core regions due to the thermal process of coating. In contrast, auto-tempering contributes to the carbon redistribution only in a limited manner. The substitutional elements are all homogenously distributed. The phase transformation process has two effects on the material: mechanically, the earlier-formed laths are larger and softer and therefore more ductile (as revealed by nanoindentation); chemically, due to the higher dislocation density inside the later-formed laths, which are generally smaller, carbon Cottrell atmospheres are predominantly observed.
In this paper, we describe experiments on welded joints of Ti-6Al-4V alloy specimens exhibiting fatigue characteristics in the base metal (BM), hot affected zone (HAZ) and fuse zone (FZ). The effect of micromorphology on crack propagation at the tip of the fatigue crack in joints formed by electron beam welding was investigated using an optical microscope, transmission electron microscope and other methodologies. The results demonstrated that the fatigue crack originated in and propagated along α/β boundaries in the BM. In the HAZ, the fatigue crack occurred at the boundary between martensite laths, and propagated through most irregular-equiaxed α phases and a few martensite laths. In the FZ, the fatigue crack originated at the boundaries between the fine crushing phases among martensite laths, and propagated along a majority of α/β boundaries and several narrow martensite laths. The electron beam welded joint of Ti-6Al-4V alloy showed instances of zigzag fatigue cracks that increased in degree from lowest in the HAZ, moderate in the FZ to greatest in the BM. Conversely, fatigue crack growth rate (FCGR) was greatest in the HAZ, less in the FZ and slowest in the BM. - Highlights: •Ti-6Al-4V welded joint exhibits different fatigue characteristics. •The fatigue crack propagates along α/β boundaries in the BM. •The fatigue crack propagates through α phases and martensite laths in the HAZ. •The fatigue crack propagates along α/β boundaries and martensite laths in the FZ. •Fatigue crack growth rate is fastest in the HAZ, less in the FZ, slowest in the BM.
Highlights: • The fine-scale microstructure of HSLA-100 steel intercritically aged at 677 °C was characterized. • Continuous austenite films evolved into isolated islands; large islands transformed to brittle martensite upon quenching. • Copper precipitates in martensite were coarse, and some sub-grain coarsening occurred within martensite. • Intercritically aged steel possessed an inferior strength-toughness balance as compared with sub-critically aged steel. - Abstract: Fine-scale structural features of an HSLA-100 steel intercritically aged at 950 K (677 °C) for 4.2 ks (70 min.) were investigated via transmission electron microscopy. The microstructure consisted of approximately 90 vol. pct. of low‑carbon lath martensite. Average lath width was about 0.25 μm, unchanged from the as-quenched condition, owing to a high number density of epsilon‑copper precipitates at these boundaries. About 10 vol. pct. of medium‑carbon austenite existed as coarsened, broken-up islands between laths; martensite lath boundary coverage by austenite was notably reduced compared to the as-quenched condition. Greater continuity between adjacent low‑carbon martensite laths was accompanied by coarse copper precipitates within laths and an order of magnitude lower dislocation density than the as-quenched martensite. Collectively, these features produced a sub-grain coarsening effect. Austenite islands larger than about 0.5 μm were unstable with respect to the formation of fresh, medium‑carbon martensite regions. Copper precipitation within austenite islands (owing to carbon and copper enrichment) might also have contributed to austenite transformation upon quenching. Intercritical aging was associated with a strong-and-undesirable deviation from strength-toughness behavior at sub-critical aging temperatures. Two key factors were identified as being responsible for this negative outcome: (i) a sub-grain coarsening effect associated with “delamellarization” of low‑carbon martensite and austenite and (ii) the formation of brittle martensite upon quenching. Quantitative estimates of the changes in strength and impact toughness are provided for microstructural differences between intercritically aged and subcritically aged material.
We investigated the microstructural evolution of high strength low alloy steel, Fe–2.0Mn–0.15Si–0.05C (wt.%), by varying the continuous cooling rates from 1 K/s to 50 K/s using three-dimensional electron backscatter diffraction and transmission electron microscopy. Granular bainitic microstructure was prevalent under a slow cooling rate of 1–10 K/s, while lath-type bainite was dominant at a high cooling rate of 50 K/s. The acicular ferrite that was the major microstructure under the intermediate ranges of cooling rates between 10 K/s and 30 K/s was tangled with each other, leading to a three-dimensional interwoven structure with highly misoriented grains. Because of the formation of three-dimensional structures, we propose that the terms “acicular ferrite” and “bainitic ferrite,” which are currently used in steel, be replaced by the terms “interwoven acicular bainite” and “lath bainite,” respectively. Moreover, we also confirmed that the cooling rate is an important factor in determining whether bainitic microstructures occur in the form of granular bainite, interwoven bainite, or lath bainite. - Highlights: • The morphology of bainitic grains was characterized by 3D-EBSD. • The ‘interwoven bainite’ and ‘lath bainite’ were suggested. • Interwoven bainite consisted of lenticular plates that were interlinked in 3D regime. • The packets of lath bainite were aligned in a specific direction.
The post-weld tempered microstructure of hybrid laser-arc welded CA6NM, a cast low carbon martensitic stainless steel, was investigated. The microstructural evolutions from the fusion zone to the base metal were characterized in detail using optical microscopy, scanning electron microscopy (SEM), electron backscatter diffraction (EBSD), X-ray diffraction (XRD) and microhardness techniques. The fusion zone, in its post-weld tempered condition, consisted of tempered lath martensite, residual delta-ferrite with various morphologies, reversed austenite and chromium carbides. The reversed austenite, which can be detected through both EBSD and XRD techniques, was found to be finely dispersed along the martensite lath boundaries, particularly at triple junctions. Based on the EBSD analysis, the orientation relationship between the reversed austenite and the adjacent martensite laths seemed to follow the Kurdjumov-Sachs (K-S) model. The results also revealed the presence of the reversed austenite in the different regions of the heat affected zone after post-weld tempering. The microindentation hardness distribution was measured, and correlated to the evolution of the corresponding microstructure across the welds. - Highlights: •The EBSD analysis was performed on hybrid laser-arc welded CA6NM. •The FZ consisted of tempered lath martensite, reversed austenite, carbides and δ ferrite after tempering. •The reversed γ was formed along the α′ lath boundaries, particularly at triple junctions.
Highlights: • EBSD in situ tensile test on a Ti-6Al-4V alloy and laser weld • Mainly prismatic, basal and pyramidal a slip activity in the base metal • Damage nucleation in the vicinity of the β phase and at α grain boundaries • Alignment of 10-10 crystallographic direction with the tensile axis in the α′ laths of the weld metal • Crack initiation along specific laths interfaces, former β grain boundary or twinned martensite laths in the weld metal The present work addresses the mechanisms of plasticity and damage nucleation in a Ti-6Al-4V alloy and its laser weld. To this end, in situ tensile tests are performed in a Scanning Electron Microscope (SEM) equipped with a Electron BackScatter Diffraction (EBSD) camera. The slip activity is automatically analyzed using a modified Schmid analysis. It is shown that the slip activity of the base metal consists mainly in prismatic, basal and pyramidal a slip. Damage nucleation in the vicinity of the β phase and at α grain boundaries is also evidenced in the base metal. In the α{sup ′} weld metal (a microstructure similar to the one often obtained in additive manufacturing Ti-alloy parts), plastic deformation results in a crystallographic rotation of the laths tending to align the 〈10 1-bar 0〉 direction with the tensile axis. The rare events of crack initiation in the martensite are shown to occur along specific laths interfaces, former β grain boundary or twinned martensite needles.
The structure of a hafnium crystal undergoing β → α (bcc → hcp) polymorphic transformation upon gradual cooling and the structure of Hf{sub 55}Ti{sub 45} and Hf{sub 30}Ti{sub 70} alloys formed under various kinetic conditions of polymorphic transformation are studied. The structure of the α phase in cast hafnium is shown to consist of lath crystals grouped into packets. The misorientations between separate laths in a packet are less than 1°. The Hf–Ti alloys in the cast state exhibit a mixed structure consisting of α-phase crystals of several morphological types. A structure of packet martensite is observed in the Hf–Ti alloys after quenching. Each packet includes laths of several crystallographic orientations. There is no regular alternation of differently orientated laths in the packet. The same set of α-phase orientations within an initial β-phase grain is observed independently of the cooling rate of the Hf–Ti alloys upon β → α polymorphic transformation. The misorientation of substructural elements within an α-phase crystal in the Hf–Ti alloys is ~5° for the cast state and ~2.2° after quenching.
Outline - Introduction: The motivations for the project, and some background on inclusions in uranium, and about the samples; Lath Inclusion Morphology: Looking at the morphology of a specific family of carbide inclusions in casting 20; Clustering of Lath Inclusions: Investigating the group behavior of these lath shaped inclusions from the inner to outer edges; Conclusions: Final thoughts on the lath inclusions and future work ideas.
Laser powder bed fusion additive manufacturing (LPBF-AM) of a low-alloy, high-performance AF-9628 steel results in exceptionally high strength and good ductility. The reasons for such mechanical properties are investigated through detailed microscopy performed at several length scales. Thus, the characterization of melt pool, porosity, grain morphology, phases, and dislocations is performed in the as-printed material. The as-printed material consists of only 0.004 vol% of uniformly distributed porosity, single-phase martensitic laths with an average lath size of ≈2.5 μm, the absence of carbides indicating interstitial trapping of C atom, and high dislocation density in the martensitic laths. Experimental data through microscopy are then fed in analytical models for calculating strengthening contributions from various strengthening mechanisms. Calculated yield strength agrees well with experimentally determined value, and therefore, activation of various strengthening mechanisms is established in as-printed AF-9628.
The presence of α/α' on prior β/β grain boundaries directly impacts the final mechanical properties of the titanium alloys. The β/β grain boundary variant selection of titanium alloys has been assumed to be unlikely owing to the high cooling rates in laser powder bed fusion (L-PBF). However, we hypothesize that powder characteristics such as morphology (non-spherical) and particle size (50–120 µm) could affect the initial variant selection in L-PBF processed Ti-6Al-4V alloy by locally altering the cooling rates. Despite the high cooling rate found in L-PBF, the results showed the presence of β/β grain boundary α' lath growth inside two adjacent prior β grains. Electron backscatter diffraction micrographs confirmed the presence of β/β grain boundary variant selection, and synchrotron X-ray high-speed imaging observation revealed the role of the “shadowing effect” on the locally decreased cooling rate because of keyhole depth reduction and the consequent β/β grain boundary α' lath growth. The self-accommodation mechanism was the main variant selection driving force, and the most abundant α/α boundary variant was type 4 (63.26°//[ $\bar{10}$ 5 5 $\bar{3}$ ]). The dominance of Category II α lath clusters associated with the type 4 α/α boundary variant was validated using the phenomenological theory of martensite transformations and analytical calculations, from which the stress needed for the β→α' transformation was calculated.
Here, a reduced activation ferritic/martensitic steel, Eurofer97, was neutron irradiated in the vicinity of 300 °C in the High Flux Isotope Reactor (HFIR) up to 72 dpa. Advanced analytical scanning transmission electron microscopy and conventional transmission electron microscopy were applied to investigate the radiation-induced segregation and phase instability behavior after neutron irradiation. Amorphization was observed in M 23 C 6 carbides. Cr-rich clusters were seen within the matrix, near the lath boundaries and close to the M 23 C 6 carbides. Cr enrichment and Fe depletion were detected at both prior austenite grain boundaries and lath boundaries, despite different segregation magnitude. In addition, the enrichment of Ni, the depletion of V, and tiny cavities (presumably helium bubbles) are also found at lath boundaries. This work interrogates the evolution of microstructures after neutron irradiation, which provides detailed understanding on the microstructural aspects controlling the mechanical integrity of Eurofer97 under high-dose neutron damage.
An automatic method to colorize and quantify the classical Pitsch, Kurdjumov–Sachs, Greninger–Troiano and Nishiyama–Wasserman orientation relationships in the electron backscatter diffraction maps of martensitic/bainitic steels is detailed. Automatic analysis of variant grouping is also presented. The method was applied to low and high carbon steels, and to iron–nickel Widmanstätten meteorites. Many results of recent literature are confirmed. In low carbon steels the individual laths exhibit continuous orientation gradients between the classical orientation relationships, and the laths tend to be grouped by close-packed plane (morphological) packets. A crystallographic scenario describing the formation of the packets is proposed on the base of the one-step model. When the carbon content increases, the orientation spreading is reduced; and martensite tends to form plate groups and burst configurations. In iron–nickel meteorites, the centimeter long Widmanstätten laths do not exhibit continuous orientation gradients but are constituted of subgrains with uniform orientation relationship; the kamacite grains in the plessite regions are grouped into Bain zones, probably due to a recrystallization during the slow cooling of the meteorites. - Highlights: • Analysis of different low and high carbon steels and Widmanstätten meteorites • Automatic color mapping of the classical orientation relationships in EBSD maps • Quantification of variant pairing and grouping tendencies • Crystallographic scenario for the formation of morphological packets.
The microstructure and mechanical properties of the Ti–6.5Al–3.5Mo–1.5Zr–0.3Si alloy produced by laser melting deposition have been investigated. The columnar grains of the Ti–6.5Al–3.5Mo–1.5Zr–0.3Si alloy due to the layer-by-layer epitaxial growth from the underlying template grains during laser melting deposition, which is roughly parallel to the deposition direction, had been found by optical microscopy; strong [101{sup ¯}2]{sub α} crystallographic texture has been confirmed by X-ray diffraction and electron backscattered diffraction. Depending on the last heating history, the microstructure of the alloy undergoes a continued change opposite to the deposition direction: martensitic α′ (transformed β); coarsened primary α laths with transformed β; coarsened primary α laths; and the fine basketweave microstructure with a few coarsened α laths or annealed martensitic α′. The average Vickers micro-hardness value of the alloy is 364 HV. The alloy parallel to the deposition direction presents lower tensile strength (925 MPa) and better elongation (18.8%), compared with 1025 MPa and 8.2% of that vertical to the deposition direction, which has been discussed using its microstructure characterization. - Highlights: • The columnar grains and strong [101{sup ¯}2]{sub α} crystallographic texture of the Ti–6.5Al–3.5Mo–1.5Zr–0.3Si alloy due to the epitaxial growth from the underlying template grains • The microstructure evolution of the alloy depends on the last heating history. • The specimen parallel to the deposition direction presents lower ultimate tensile strength and higher elongation than the specimen vertical to the deposition direction.
Coarse austenite to bainite transformation in low carbon steel under simulated welding thermal cycles was morphologically and crystallographically characterized by means of optical microscope, transmission electron microscope and electron backscattered diffraction technology. The results showed that the main microstructure changes from a mixture of lath martensite and bainitic ferrite to granular bainite with the increase in cooling time. The width of bainitic laths also increases gradually with the cooling time. For a welding thermal cycle with relatively short cooling time (e.g. t{sub 8/5} is 30 s), the main mode of variant grouping at the scale of individual prior austenite grains changes from Bain grouping to close-packed plane grouping with the progress of phase transformation, which results in inhomogeneous distribution of high angle boundaries. As the cooling time is increased, the Bain grouping of variants becomes predominant mode, which enlarges the effective grain size of product phase. - Highlights: • Main microstructure changes and the width of lath structure increases with cooling time. • Variant grouping changes from Bain zone to close-packed plane grouping with the transformation. • The change of variant grouping results in uneven distribution of high angle grain boundary. • Bain grouping is main mode for large heat input, which lowers the density of high angle boundary.
Highlights: • Micro galvanic couple forms between steel matrix and secondary phase for LCB steel. • Micro galvanic couple causes non-uniform corrosion on micro area surface of steel. • The ω secondary phase acts as the micro anode in lath bainitic steel. • The M secondary phase acts as the micro cathode in granular bainitic steel. • Galvanic accelerated corrosion is obvious initially and weakened for long term. - Abstract: The corrosion behavior of lath bainitic and granular bainitic steels in 0.01 mol/L NaCl solution was studied by SEM and TEM observation, electrochemical monitoring and weight loss test. The results indicate that the micro galvanic couple forms between the steel matrix and the secondary phase, which causes non-uniform micro corrosion on surfaces of two steels. In lath bainitic steel, the secondary phase ω acts as the micro anode. While in granular bainitic steel, the secondary phase M acts as the micro cathode. Moreover, the corrosion acceleration caused by micro galvanic couple is obvious in the initial immersion stage, and then it becomes weak during the long term corrosion.