Search NASA⌕ Search

SEARCH · Search NASA

Results for “LOW ALLOY STEELS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

LEC System Development

The Lajet Energy Company (LEC) 460 is described. A parabolic dish which incorporates a microprocessor to automatically point it toward the Sun from sunrise to sunset is used. The dish is composed of a set of mirrors (made of reflective polymeric film) which focus and concentrate the Sun's energy on a receiver, producing intense but controlled amounts of heat. The LEC 460 employs a design concept that permits the use of common and low cost materials. All major structural components are fabricated from low carbon, low alloy steel using methods adaptable to mass production. The mirrors are supported on a steel tubing frame. This frame is attached near its center of gravity to a cantilevered support structure. The mirrors and frame are counterbalanced by the weight of the receiver, thus reducing the energy needed to move the collector (parasitic load) and allowing movement on two axes. Each LEC 460 solar concentrator contains a reflective array consisting of twenty four 60 inch diameter mirrors.

Halbert, D. D.↗

Pitting Propagation Behavior on Low Alloy AISI 4130 (UNS G41300) Steel Exposed to Various Alkali and Alkaline Earth Metal Chlorides

Pit propagation studies were conducted to elucidate whether alkali and alkali earth metal cations such as Na+ and Rb+ present in the form of metal chloride salts such as RbCl affect pitting behavior in distinctly different manner than NaCl. Pit propagation studies were conducted on a low alloy steel using one-dimensional (1-D) pit method over pit depths from 300-1000 µm. LSV and EIS of planar electrodes of 4130 in a range of Cl- solutions were conducted and revealed no detected differences in impedance, open circuit, corrosion potential (Ecorr), passive current density (ipass), and pitting potential (Epit) as a function of salt type. In the case of one-dimensional pits during fast downward scan rates, the saturation potential (Esat) varied as a function of cation identity when pit depths were shallow. Mass transported limited current density also differed with cations in shallow pits when various alkali metal and alkaline metal cations were present. The limiting current density was increased for RbCl relative to NaCl The pit surface potential (Esurf) of activated pit surfaces reached Ecorr prior to establishing a condition where the pit electrolyte surface concentration (Csurf) was less than the critical concentration for active acidified pitting (i.e. Csurf<Ccrit) in this marginally passivating steel. For various Esurf and pit current density (ipit) combinations at constant Csurf where Ccrit< Csurf < Csat, E-log(i) plots were constructed using the method of Tianshu to create IR ohmic voltage corrected Tafel plots for various fixed pit solution concentrations. Under these conditions, the influence of cation identity on charge transfer controlled kinetics indicated slight differences in Tafel behavior where RbCl was slightly more aggressive than NaCl for low alloy steel oxidation. Differences in metal cation identity exert no effect on passive or breakdown on planar electrodes and only effect pit propagation stage in shallow pits.

Demarest, Chalres↗

Tuning austenite stability through prior microstructure control in a low-alloy Q&P steel

Quenching and partitioning (Q&P) processing is a widely accepted heat treatment methodology for creating high strength steels consisting of ferrite, martensite, and austenite, while maintaining relatively low manufacturing costs. Though the research on effects of prior microstructure is limited, an understanding of the heat treatment response of different starting microstructures is critical to processing and creating steels with complex microstructures that contain retained austenite and may afford opportunities to further optimize properties. This study investigates the influence of starting microstructure (ferrite/pearlite versus martensite) and prior levels of cold work (38 verses 58 %) on the microstructural development and mechanical properties of a 0.2 C-2.0 Mn-1.5 Si (wt.%) steel exposed to Q&P processing. Samples with a starting martensitic microstructure resulted in higher retained austenite fractions and a more homogeneous microstructure after Q&P processing compared to a starting microstructure of ferrite-pearlite. Starting martensitic microstructures also displayed higher work hardening rates and higher uniform elongations. Larger cold reductions saw accelerated dissolution kinetics and austenite formation during intercritical annealing, resulting in more similar final microstructures from the ferrite-pearlite and martensitic starting microstructures. Finally, the results presented here indicate that varying prior processing can be a route to manipulate and control austenite stability in a Q&P processed steel.

36 MATERIALS SCIENCE↗

Irradiation-assisted cracking of SA508-304L weldments with 308L groove filler and 309L butter in hot water immersion constant rate extension tests

Low alloy SA508 bainitic steel is often welded to 300 series austenitic stainless steel in nuclear power plants. These dissimilar metal weldments use 309L butter applied to the low alloy steel and 308L groove filler material to join the 309L to austenite. High alloy steels (such as the 308L and 309L material used here) have been identified as having greater susceptibility to irradiation-assisted stress corrosion cracking (IASCC). Evidence is presented here of cracking under tensile loads in 309L weldment butter in LWR hydrothermal conditions that correlates irradiation induced changes at δ ferrite–γ austenite phase boundaries and γ–γ grain boundaries; specifically intergranular Cr 23 C 6 precipitates. Cracking is not observed in irradiated 308L groove filler under the same conditions. Both the 309L butter and 308L filler material have a duplex or mixed δ–γ phase microstructure due to solidification during the welding procedure. We have performed constant extension rate autoclave immersion tests in BWR normal water chemistry hot water (288 °C, 10 MPa, 2000 wt. ppb dissolved oxygen, <100 nS/cm conductivity, neutral pH) of proton irradiated (2 MeV, approximately 3 displacements per atom at a depth of 10 μm) tensile specimens. Proton irradiation to the dpa levels used here induced Cr 23 C 6 carbide precipitation at γ–γ grain boundaries and δ–γ phase boundaries in the 309L butter but not the 308L filler. Cracking was observed in the proton-irradiated volume of 309L at these interfaces in the vicinity of the Cr 23 C 6 precipitates. We hypothesis the SA508 is the source of carbon in the 309L butter. Cr depletion at γ–γ grain boundaries was also observed and may also be a root cause of cracking. Furthermore, the 309L butter is under significant tensile residual stress in the weldment that adds to applied tensile loads and this too may be a contributing factor.

309L weld butter↗

Interpolation and extrapolation of creep rupture data by the minimum commitment method. III - Analysis of multiheats

An outline is presented of approaches for treating multiheats on the basis of the focal point convergence method. The method has been employed in the case of two highly characterized multiheats, including a 304 stainless steel studied in Japan and a low alloy carbon steel studied in England. The method makes use of the same functional form for all materials. Only the constants are varied for each multiheat. Completely computerized procedures are employed for the determination of the constants. Once the basic analysis has been performed, the representation of various members in the same system is achieved by adding linear expressions of log stress, changing only two constants in the equations to represent a selected heat.

Manson, S. S.↗

Ignition of steel alloys by impact of low-velocity iron/inert particles in gaseous oxygen

The ignition of carbon steel and 316 and 304 stainless steels caused by the impact of low-velocity particles (a standard mixture consisting of 2 g of iron and 3 g of inert materials) in gaseous oxygen was investigated using NASA/White Sands Test Facility for the ignition test, and a subsonic particle impact chamber to accelerate the particles that were injected into flowing oxygen upstream of the target specimen. It was found that the oxygen velocities required to ignite the three alloys were the same as that required to ignite the particle mixture. Ignition occurred at oxygen velocities greater than 45 m/sec at 20 to 24 MPa and was found to be independent of pressure between 2 and 30 MPa. Comparison of the present results and the past results from Wegener (1964) with the Compressed Gas Association (CGA) oxygen velocity limits for safe operations indicates that the CGA limits may be excessively conservative at high pressures and too liberal at low pressures.

Benz, Frank J.↗

Oxidation and corrosion behavior of modified-composition, low-chromium 304 stainless steel alloys

The effects of substituting less strategic elements than Cr on the oxidation and corrosion resistance of AISI 304 stainless steel were investigated. Cyclic oxidation resistance was evaluated at 870 C. Corrosion resistance was determined by exposure of specimens to a boiling copper-rich solution of copper sulfate and sulfuric acid. Alloy substitutes for Cr included Al, Mn, Mo, Si, Ti, V, Y, and misch metal. A level of about 12% Cr was the minimum amount of Cr required for adequate oxidation and corrosion resistance in the modified composition 304 stainless steels. This represents a Cr saving of at least 33%. Two alloys containing 12% Cr and 2% Al plus 2% Mo and 12% Cr plus 2.65% Si were identified as most promising for more detailed evaluation.

Stephens, J. R.↗

Interpolation and Extrapolation of Creep Rupture Data by the Minimum Commitment Method. Part 3: Analysis of Multiheats

The Minimum Commitment Method was applied to two sets of data for which multiple heat information was available. For one alloy, a 304 stainless steel studied in Japan, data on nine well characterized heats were used, while for a proprietary low alloy carbon steel studied in the United Kingdom data were available on seven heats - in many cases to very long rupture times. For this preliminary study no instability factors were used. It was discovered that heat-to-heat variations would be accounted for by introducing heat identifiers in the form A + B log sigma where sigma is the stress and the constants A and B depend only on the heat. With these identifiers all the data could be collapsed onto a single master curve, even though there was considerable scatter among heats. Using these identifiers together with the average behavior of all heats made possible the determination of an accurate constitutive equation for each individual heat. Two basic approaches are discussed for applying the results of the analysis.

Manson, S. S.↗

Application of hard coatings to substrates at low temperatures

BIRL, the industrial research laboratory of Northwestern University, has conducted unique and innovative research, under sponsorship from the NASA Marshall Space Flight Center (MSFC), in the application of hard, wear resistant coatings to bearing steels using the high-rate reactive sputtering (HRRS) process that was pioneered by Dr. William Sproul, the principal investigator on this program. Prior to this program, Dr. Sproul had demonstrated that it is possible to apply hard coatings such as titanium nitride (TiN) to alloy steels at low temperatures via the HRRS process without changing the metallurgical properties of the steel. The NASA MSFC program at BIRL had the specific objectives to: apply TiN to 440C stainless steel without changing the metallurgical properties of the steel; prepare rolling contact fatigue (RCF) test samples coated with binary hard coatings of TiN, zirconium nitride (ZrN), hafnium nitride (HfN), chromium nitride (CrN), and molybdenum nitride (MoN), and metal coatings of copper (Cu) and gold (Au); and develop new alloyed hard coatings of titanium aluminum nitride (Ti(0.5)Al(0.5)N), titanium zirconium nitride (Ti(0.5)Zr(0.5)N), and titanium aluminum vanadium nitride.

Sproul, William D.↗

Chemical, Structural, and Microstructural Changes in Metallic and Silicon-Based Coating Materials Exposed to Iodine Vapor

The chemical, structural and microstructural behavior of steels (304, 316 and A36), titanium-aluminum alloy (Ti-Al, (6Al-4V)), aluminum-magnesium alloy (Al-Mg, 6061), and coatings (Silcolloy and Dursan (SilcoTek Corporation)) were probed after exposure to iodine laminar flow. Exposures were carried out in a custom-built Iodine Vapor RIG (IVR) at 300 degrees C to an iodine laminar vapor flow of 1 mg min(exp. -1), carried by 145 mL-min(exp. -1) argon gas, for 5, 15 and 30 days. Samples were characterized before and after the experiment by gravimetric analysis, X-ray diffraction (XRD) and cross section electron microscopy analysis coupled with energy dispersive X-ray spectroscopy (EDS). All steels exposed for 30 days formed scales consisting mainly of metal (Cr, Fe, Ni) oxides showing different chemistry, microstructure and crystalline phases. Elemental iodine was only detected by EDS analysis in the scales of stainless steels 304 and 316. After 30 days, the Ti-Al exhibited no detectable scale, suggesting only a very thin film was formed. A scale consisting mainly of aluminum, iodine, and oxygen formed on the Al-Mg sample exposed to 30 days. Some pockets rich in magnesium, iodine and oxygen also formed in this Al-Mg alloy. Stainless steel 316, low carbon steel A36 and Ti-Al alloy coated with Silcolloy and stainless steel 304 coated with Dursan that were exposed for 30 days exhibited no oxidation. Stainless steel 304 coated with Silcolloy exposed for 30 days did not exhibit corrosion although the sample gained weight and the coating exhibited expansion. The weight gain per area performance of the materials exposed in iodine lamina flow containing oxygen at impurity level for 10, 15 and 30 days are reported from the lowest to the highest weight gain per area as follows: Steels: Less than 316 less than 304 less than A36; Ti-Al-Mg based alloys: Al-Mg less than Ti-Al: Considering the experimental uncertainties, no weight change was observed for Stainless steel 316, low carbon steel A36 and Ti-Al alloy coated with Silcolloy and stainless steel 304 coated with Dursan. The corrosion of the alloys is catalyzed by iodine in the presence of oxygen as impurity.

Costa, Gustavo C. C.↗

Tribological and microstructural characteristics of ion-nitrided steels

Three steels AISI 4140, AISI 4340 and AISI 304 stainless steel were ion nitrided in a plasma consisting of a 75:25 mixture of H2:N2, sometimes with a trace of CH4. Their surface topography was characterized by SEM and two distinct compound phases were identified: the gamma and the epsilon. The core-case hardness profiles were also established. The low Cr alloy steels have an extended diffusion zone in contrast to the 304 stainless steels which have a sharp interface. The depth of ion-nitriding is increased as the Cr content is decreased. Friction tests reveal that the gamma surface phase has a lower coefficient of friction than the epsilon phase. The lowest coefficient of friction is achieved when both the rider and the specimen surface are ion nitrided.

Spalvins, T.↗

Tribological and microstructural characteristics of ion-nitrided steels

Three steels AISI 4140, AISI 4340 and AISI 304 stainless steel were ion nitrided in a plasma consisting of a 75:25 mixture of H2:N2, sometimes with a trace of CH4. Their surface topography was characterized by SEM and two distinct compound phases were identified: the gamma and the epsilon. The core-case hardness profiles were also established. The low Cr alloy steels have an extended diffusion zone in contrast to the 3034 stainless steels which have a sharp interface. The depth of ion-nitriding is increased as the Cr content is decreased. Friction tests reveal that the gamma surface phase has a lower coefficient of friction than the epsilon phase. The lowest coefficient of friction is achieved when both the rider and the specimen surface are ion nitrided. Previously announced in STAR as N83-24635

Spalvins, T.↗

Influence of fabrication on microstructure and heat affected zone width in weldments of nuclear reactor pressure vessel steel

Advanced manufacturing routes such as electron beam welding and powder metallurgy with hot isostatic pressing are increasingly used across energy and aerospace industries, where the reliable prediction of weld behavior and heat affected zone (HAZ) evolution is critical. This study examines how fabrication routes and post-weld heat treatments influence phase distribution, crystallite size, microstrain, and dislocation density in nuclear reactor pressure vessel steels using synchrotron X-ray diffraction (SXRD). Retained austenite occurs only in samples that did not undergo austenitization, whereas an austenitizing heat treatment fully eliminates retained austenite and produces a more uniform microstructure across the weldment in terms of phase fraction, dislocation density, and microstrain. The Rosenthal solution underestimates the HAZ width for powder metallurgy samples. A newly proposed modified Rosenthal solution, reducing density by accounting for porosity, matches the SXRD-measured HAZ width with a 0.65% error. Structure–property correlations reveal that dislocation density correlates strongly with nanohardness in homogenous microstructures, while in heterogenous weldments nanohardness is further influenced by the presence of dissimilar phase boundaries. These findings provide new insight into the thermal and microstructural response of powder metallurgy fabricated steels and offer a framework for optimizing welding procedures and heat treatments in advanced manufacturing applications.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

Effect of post-weld heat treatment on microstructure and mechanical properties of rotary inertia friction welded dissimilar 422-4140 martensitic steel piston joints

The study investigated how post‐weld heat treatment (PWHT) temperature affects the microstructure and localized deformation/fracture during bend testing of rotary inertia friction welds (RIFW) between AISI 422 stainless steel and AISI 4140 steel. RIFW produced a fully martensitic interface with approximately 550 HV hardness in both the thermo-mechanically affected (TMAZ) and heat‐affected zones (HAZ). Due to differences in temper resistance, the 4140 TMAZ/HAZ softened progressively under PWHT temperatures from 525 °C to 700 °C, while the 422 TMAZ unexpectedly maintained about 550 HV up to 600 °C before significantly softening at temperatures ≥625 °C. This asymmetric softening generated steep hardness gradients across the interface at temperatures ≤600 °C. Furthermore, carbon migration across the interface was minimal up to 600 °C, moderate at 625 °C, and by 700 °C produced a carbide‐rich eutectoid layer in the 422 TMAZ alongside a carbon‐depleted soft ferrite layer in the 4140 TMAZ. Strain during bending was PWHT‐dependent, concentrating on the 4140 side; in as-welded joints, the high hardness led to deformation and crack initiation in the base metals, whereas in PWHT samples, cracking initiated in the softened 4140 TMAZ near the interface. The intermediate PWHT temperature of 625 °C offered the best balance of limited carbon diffusion across the interface, relatively low peak weld hardness and minimized hardness gradients across the interface, more homogenous deformation, and good bend test performance.

4140 low-alloy steel↗

Microstructure, Hardness, and Residual Stress of the Dissimilar Metal Weldments of SA508-309L/308L-304L

A dissimilar metal weldment consisting of SA508-309L-308L-304L is widely used in light-water nuclear reactors. These weldments demonstrate dissimilar susceptibility to stress corrosion cracking that are related to the microstructure, properties, and residual stress. In this work, microstructures, hardness, and the residual stress distribution of the dissimilar metal weldments were investigated, with the correlation of increased hardness in the heat-affected zone (HAZ) to the microstructure. 304L HAZ demonstrated similar grain morphology as the base material, and the increase in hardness was primarily attributed to the increased dislocation density. SA508 HAZ demonstrated a change of grain morphology resulting from the different peak temperatures and cooling rates. The increased hardness in the SA508 HAZ was attributed to the refined grain morphology, higher dislocation density, and higher number density of precipitates. A ~ 20–30-μm-wide martensitic zone formed at the fusion boundary of SA508-309L, where Cr-rich carbide precipitates were observed, with the average size and the number density of 44.1 ± 16.9 nm and 1.5 × 10 21 m ₋3 , respectively. In conclusion, residual stress results demonstrated the largest tensile stress at 309L butter, indicating its high cracking susceptibility.

36 MATERIALS SCIENCE↗