Friction and wear of low-melting binary and ternary gallium alloy films in argon and in vacuum
Friction and wear of low melting gallium alloys on stainless steel and nickel in argon and vacuum environment
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Friction and wear of low melting gallium alloys on stainless steel and nickel in argon and vacuum environment
Syntactic foam formulations were prepared from mixtures of Pyrrone prepolymers and hollow carbon microspheres. Very low curing shrinkages were obtained for high volume loadings of microspheres. The resulting syntactic foams were found to be remarkably stable over a wide range in temperature. A technique was developed for the emplacement of these foam formulations in polyimide-fiberglass, titanium alloy and stainless steel honeycomb without sacrificing low curing shrinkage or thermal stability.
Ultrahigh vacuum elevated temperature low cycle fatigue and thermal fatigue tests of 304 stainless steel and A-286 alloy have shown significant effects of frequency and combined temperature-strain cycling on fatigue life. At constant temperature, the cyclic life of both alloys was lower at lower frequencies. Combined temperature-strain cycling reduced fatigue life with respect to isothermal life at the maximum temperature of the thermal cycle. Life reductions with in-phase thermal cycling (tension at high temperature, compression at low temperature) were attributed to grain boundary cavitation caused by unreversed tensile grain boundary sliding. The proposed mechanism for out-of-phase cavity generation involved accumulation of unreversed compressive grain boundary displacements which could not be geometrically accomodated by intragranular deformation in the low-ductility A-286 alloy.
Some alloy systems, such as aluminum-lithium alloys and dual-phase steels, have been found to show a bilinear Manson-Coffin low-cycle-fatigue relationship. This paper shows that such bilinear behavior is related to the cyclic stress-strain curve. A bilinear cyclic stress-strain curve is a likely indication of a bilinear Manson-Coffin relationship. It is shown that materials other than aluminum-lithium alloys and dual-phase steels also may exhibit bilinear Manson-Coffin behavior. Implications for design are discussed.
The low-cycle fatigue resistance of type 347 stainless steel and Hastelloy Alloy X was evaluated in constant-amplitude, strain-controlled fatigue tests conducted under continuous negative strain cycling at a constant strain rate of 0.001 per sec and at total axial strain ranges of 1.5, 3.0, and 5.0 percent in both hydrogen gas and laboratory air environments in the temperature range 538-871 C. Elevated-temperature, compressive-strain hold-time experiments were also conducted. In hydrogen, the cyclic stress-strain behavior of both materials at 538 C was characterized by appreciable cyclic hardening at all strain ranges. At 871 C neither material hardened significantly; in fact, at 5% strain range 347 steel showed continuous cyclic softening until failure. The fatigue resistance of 347 steel was slightly higher than that of Alloy X at all temperatures and strain ranges. Ten-minute compressive hold time experiments at 760 and 871 C resulted in increased fatigue lives for 347 steel and decreased fatigue lives for Alloy X. Both alloys showed slightly lower fatigue resistance in air than in hydrogen. Some fractographic and metallographic results are also given.
A welded tubular structure constructed of low alloy high strength quenched and tempered steel was tested. The consistency of the mechanical strengths and chemical composition and the degree of difficulty of obtaining full strength welds with these steels is characterized. The results of constructing and testing two typical connections which are used in the structure design are reported.
This is a report of exposure of various metal tubing to oceanfront launch environments. The objective is to examine various types of corrosion-resistant tubing for Space Shuttle launch sites. The metals were stainless steels (austenitic, low-carbon, Mo-alloy, superaustenitic, duplex, and superferritic), Ni-Cr-Mo alloy, Ni-Mo-Cr-Fe-W alloy, and austenitic Ni-base superalloy.
Explore the source record for details and available documents.
Low cycle fatigue of notched steel and aluminum alloy specimens by consideration of crack initiation and propagation
An investigation of the plastic fracture process to improve tensile strength in high strength steels is presented. Two generic types of steels are considered: a quenched and tempered grade and a maraging grade, in order to compare two different matrix microstructures. Each type of steel was studied in commercial grade purity and in special melted high purity form, low in residual and impurity elements. The specific alloys dealt with include AISI 4340 and 18 Ni, 200 grade maraging steel, both heat treated to the same yield strength level of approximately 200 ksi.
Fatigue testing and determination of low temperature properties of structural metal alloys - aluminum alloy, stainless steel, and nickel alloys
Spectrographic method determines individual stainless steel components in molten bismuth-42 w/o tin eutectic to determine the solubility of Type 304 stainless steels. It utilizes the high sensitivity and precision of the spark-ignited, low-voltage ac-arc excitation of samples rendered homogeneous by dissolution.
Procedures based on modification of the conventional Strainrange Partitioning method are proposed to characterize the time-dependent degradation of engineering alloys in high-temperature, low-cycle fatigue. Creep-fatigue experiments were conducted in air using different waveforms of loading on 316 stainless steel at 816 C (1500 F) to determine the effect of exposure time on cyclic life. Reductions in the partitioned cyclic lives were observed with an increase in the time of exposure (or with the corresponding decrease in the steady-state creep rate) for all the waveforms involving creep strain. Excellent correlations of the experimental data were obtained by modifying the Conventional Strainrange Partitioning life relationships involving creep strain using a power-law term of either: (1) time of exposure, or (2) steady-state creep rate of the creep-fatigue test. Environmental degradation due to oxidation, material degradation due to the precipitation of carbides along the grain boundaries and detrimental deformation modes associated with the prolonged periods of creep were observed to be the main mechanisms responsible for life reductions at long exposure times.
Grain-refining heat treatments increase toughness without substantial strength loss. Five alloys selected for study, all at or near technological limit. Results showed clearly grain sizes of these alloys refined by such heat treatments and grain refinement results in large improvement in toughness without substantial loss in strength. Best improvements seen in HP-9-4-20 Steel, at low-strength end of technological limit, and in Maraging 200, at high-strength end. These alloys, in grain refined condition, considered for model applications in high-Reynolds-number cryogenic wind tunnels.
For a wide range of compositions, Fe-Cr-Ni alloys can solidify by a two-step process: a metastable solid forms first, subsequently transforming into the stable solid phase. This two-step solidification produces a profoundly different microstructure, and therefore different properties, in the final solid. The delay time between the two steps of the solidification process varies from microseconds to seconds. This delay time is a strong function of composition and a weak function of the undercooling of the melt below the metastable liquidus. From the results obtained during the MSL-1 mission and in ground based electrostatic levitation testing at NASA MSFC, we know that convection also has a significant effect on the delay time. By examining the effect of convection on delay time over a wide range of convection, for several different alloys, we can gain a better understanding and better control of the microstructural evolution and final structure of stainless steel alloys. MSFC provides ESL for ground-based testing in a low-convection state, and the numerical modeling that enables estimation of the convection levels under the different process conditions.
The significance of the role that creep can play in governing high-temperature, low-cycle fatigue resistance is investigated by conducting strain cycling tests on two high-temperature stainless steel alloys and making concurrent measurements of stress, temperature, and strain at various frequencies. The results are then analyzed in terms of damage imposed by creep and fatigue components. It is shown that creep can play an important and sometimes dominant role in low cycle fatigue at high temperatures. The results of the study include the findings that: (1) the simple life-fraction theory described is adequate for calculating creep damage when the cyclic creep rupture curve is used as a basis for analysis; (2) a method of universal slopes originally developed for room temperature use is sufficiently accurate at high temperature to be used to calculate pure fatigue damage; and (3) a linear creep-fatigue damage rule can explain the transitions observed from one failure mode to another.
Explore the source record for details and available documents.
The theoretical and experimental strength of aluminum reinforced with stainless steel wire is analyzed. Various methods of producing the composite material and it's static and cyclical strengths are considered. The reinforcement of aluminum with stainless steel wire was accomplished from the perspective of increasing the specific strength of aluminum and it's alloys, increasing the strength of the material with respect to high and low temperatures, as well as increasing the cyclical strength. The production of the composite aluminum-stainless steel wire material with approximated or calculated strengthening is possible by any of the considered methods. The selection of the proper production technology depends on precise details and conditions of application of the material.