Investigating Capacity Fade of a LiCoO2 Cathode using Reconstructed Microstructures.
Abstract not provided.
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Abstract not provided.
The specific thermal capacity and heat dissipation rate for lithium ion cells containing LiNiO2 and mixed oxide (75%LiCoO2+ 25%LiNiO2) as cathode materials are compared. The experimental measurements were made using a radiative calorimeter consisting of a copper chamber maintained at -168 C by circulating liquid nitrogen and enclosed in a vacuum bell jar. The specific thermal capacity was determined based on warm-up and cool-down transients. The heat dissipation rate was calculated from the values measured for heat radiated and stored, and the resulting values were corrected for conductive heat dissipation through the leads. The specific heat was 1.117 J/ C-g for the LiNiO2 cell and 0.946 J/ C-g for the 75%LiCoO2,25%LiNiO2 cell. Endothermic cooling at the beginning of charge was very apparent for the cell containing 75%LiCoO2,25%LiNiO2 as the cathode. Exothermic heating began at a higher state of charge for the cell with the 75%LiCoO2,25%LiNiO2 cathode compared to the LiNiO2 cathode cell. During discharge, the rate of heat dissipation increased with increase in the discharge current for both types of cells. The maximum heat dissipated at C/5 discharge was 0.065 W and 0.04 W for the LiNiO2 and 75%LiCoO2,25%LiNiO2 cells, respectively, The thermoneutral potential showed variability toward the end of discharge. The plateau region of the curves was used to calculate average thermoneutral potentials of 3.698 V and 3.837 V for the LiNiO2 cell and the 75%LiCoO2,25%LiNiO2 cell, respectively.
LiCoO2 and LiNiO2 fibers have been investigated as alternatives to LiCoO2 and LiNiO2 powders used as lithium-intercalation compounds in cathodes of rechargeable lithium-ion electrochemical cells. In making such a cathode, LiCoO2 or LiNiO2 powder is mixed with a binder [e.g., poly(vinylidene fluoride)] and an electrically conductive additive (usually carbon) and the mixture is pressed to form a disk. The binder and conductive additive contribute weight and volume, reducing the specific energy and energy density, respectively. In contrast, LiCoO2 or LiNiO2 fibers can be pressed and sintered to form a cathode, without need for a binder or a conductive additive. The inter-grain contacts of the fibers are stronger and have fewer defects than do those of powder particles. These characteristics translate to increased flexibility and greater resilience on cycling and, consequently, to reduced loss of capacity from cycle to cycle. Moreover, in comparison with a powder-based cathode, a fiber-based cathode is expected to exhibit significantly greater ionic and electronic conduction along the axes of the fibers. Results of preliminary charge/discharge-cycling tests suggest that energy densities of LiCoO2- and LiNiO2-fiber cathodes are approximately double those of the corresponding powder-based cathodes.
MoO3 has shown promise as a cathode material that can extend the upper limit of operating temperature of rechargeable lithium thin-film electrochemical cells. Cells of this type are undergoing development for use as energy sources in cellular telephones, wireless medical sensors, and other, similarly sized portable electronic products. The LiCoO2 and LiMn2O4 cathodes heretofore used in these cells exhibit outstanding cycle lives (of the order of hundreds of thousands of cycles) at room temperature, but operation at higher temperatures reduces their cycle lives substantially: for example, at a temperature of 150 C, cells containing LiCoO2 cathodes lose half their capacities in 100 charge/discharge cycles. The superiority of MoO3 as a cathode material was demonstrated in experiments on lithium thin-film cells fabricated on glass slides. Each cell included a layer of Ti (for adhesion to the glass slide), a patterned layer of Pt that served as a cathode current collector, a cathode layer of MoO3, a solid electrolyte layer of Li3.3 PO3.8 N0.22 ("LiPON"), and an anode layer of Li. All the layers were deposited by magnetron sputtering except for the Li layer, which was deposited by thermal evaporation. These cells, along with similar ones containing LiCoO2 cathodes, were subjected to several tests, including measurements of specific capacity in charge/discharge cycling at a temperature of 150 C. The results of these measurements, plotted in the figure, showed that whereas specific capacity of the cells containing LiCoO2 cathodes faded to about half its initial value after only 100 cycles, the specific capacity of the cells containing the MoO3 cathodes faded only slightly during the first few hundred cycles and thereafter not only recovered to its initial value but continued to increase up to at least 5,500 cycles.
The fabrication of robust interfaces between transition metal oxides and non-aqueous electrolytes is one of the great challenges of lithium ion batteries. Atomic layer deposition (ALD) of aluminum tungsten fluoride (AlWxFy) improves the electrochemical stability of LiCoO2. AlWxFy thin films were deposited by combining trimethylaluminum and tungsten hexafluoride. in-situ quartz crystal microbalance and transmission electron microscopy studies show that the films grow in a layer-by-layer fashion and are amorphous nature. Ultrathin AlWxFy coatings (<10 Å) on LiCoO2 significantly enhance stability relative to bare LiCoO2 when cycled to 4.4 V. The coated LiCoO2 exhibited superior rate capability (up to 400 mA/g) and discharge capacities at a current of 400 mA/g were 51% and 92% of the first cycle capacities for the bare and AlWxFy coated materials. These results open new possibilities for designing ultrathin and electrochemically robust coatings of metal fluorides via ALD to enhance the stability of Li-ion electrodes.
(LiCoO2)3SbO2 crystallizes in the triclinic P-1 space group. The structure is one-dimensional and consists of one antimony;dihydrate molecule and three LiCoO2 ribbons oriented in the (0, 1, 1) direction. In each LiCoO2 ribbon, Li1+ is bonded in a linear geometry to two equivalent O2- atoms. Both Li–O bond lengths are 1.59 Å. Co+2.67+ is bonded in a linear geometry to two equivalent O2- atoms. Both Co–O bond lengths are 1.46 Å. O2- is bonded in a distorted linear geometry to one Li1+ and one Co+2.67+ atom.
(LiCoO2)2Li3CoO4 crystallizes in the triclinic P-1 space group. The structure is two-dimensional and consists of one Li3CoO4 ribbon oriented in the (-2, 1, 1) direction and one LiCoO2 sheet oriented in the (0, -1, 1) direction. In the Li3CoO4 ribbon, there are two inequivalent Li1+ sites. In the first Li1+ site, Li1+ is bonded in a distorted linear geometry to two O2- atoms. There is one shorter (1.59 Å) and one longer (1.61 Å) Li–O bond length. In the second Li1+ site, Li1+ is bonded in a distorted linear geometry to two equivalent O2- atoms. Both Li–O bond lengths are 1.67 Å. Co+3.67+ is bonded in a distorted linear geometry to two equivalent O2- atoms. Both Co–O bond lengths are 1.58 Å. There are two inequivalent O2- sites. In the first O2- site, O2- is bonded in a 2-coordinate geometry to two Li1+ atoms. In the second O2- site, O2- is bonded in a 2-coordinate geometry to one Li1+ and one Co+3.67+ atom. In the LiCoO2 sheet, there are two inequivalent Li1+ sites. In the first Li1+ site, Li1+ is bonded in a 2-coordinate geometry to four O2- atoms. There is two shorter (1.74 Å) and two longer (2.19 Å) Li–O bond length. In the second Li1+ site, Li1+ is bonded in a 2-coordinate geometry to four O2- atoms. There is two shorter (1.72 Å) and two longer (2.21 Å) Li–O bond length. Co+3.67+ is bonded in a distorted linear geometry to two O2- atoms. Both Co–O bond lengths are 1.49 Å. There are two inequivalent O2- sites. In the first O2- site, O2- is bonded in a 2-coordinate geometry to two Li1+ and one Co+3.67+ atom. In the second O2- site, O2- is bonded in a 2-coordinate geometry to two Li1+ and one Co+3.67+ atom.
Significant advances in energy density, rate capability and safety will be required for the implementation of Li-ion batteries in next generation electric vehicles. We have demonstrated atomic layer deposition (ALD) as a promising method to enable superior cycling performance for a vast variety of battery electrodes. The electrodes range from already demonstrated commercial technologies (cycled under extreme conditions) to new materials that could eventually lead to batteries with higher energy densities. For example, an Al2O3 ALD coating with a thickness of ~ 8 A was able to stabilize the cycling of unexplored MoO3 nanoparticle anodes with a high volume expansion. The ALD coating enabled stable cycling at C/2 with a capacity of ~ 900 mAh/g. Furthermore, rate capability studies showed the ALD-coated electrode maintained a capacity of 600 mAh/g at 5C. For uncoated electrodes it was only possible to observe stable cycling at C/10. Also, we recently reported that a thin ALD Al2O3 coating with a thickness of ~5 A can enable natural graphite (NG) electrodes to exhibit remarkably durable cycling at 50 degrees C. The ALD-coated NG electrodes displayed a 98% capacity retention after 200 charge-discharge cycles. In contrast, bare NG showed a rapid decay. Additionally, Al2O3 ALD films with a thickness of 2 to 4 A have been shown to allow LiCoO2 to exhibit 89% capacity retention after 120 charge-discharge cycles performed up to 4.5 V vs Li/Li+. Bare LiCoO2 rapidly deteriorated in the first few cycles. The capacity fade is likely caused by oxidative decomposition of the electrolyte at higher potentials or perhaps cobalt dissolution. Interestingly, we have recently fabricated full cells of NG and LiCoO2 where we coated both electrodes, one or the other electrode as well as neither electrode. In creating these full cells, we observed some surprising results that lead us to obtain a greater understanding of the ALD coatings. We have also recently coated a binder free LiNi0.04Mn0.04Co02O2 electrode containing 5 wt% single-walled carbon nanotubes as the conductive additive and demonstrated both high rate capability as well as the ability to cycle the cathode to 5 V vrs. Li/Li+. Finally, we coated a Celgard (TM) separator and enabled stable cycling in a high dielectric electrolyte. These results will be presented in detail.
Li dendrites are known to cause deterious, and in many cases catastrophic, effect on the performance of Li rechargeable batteries. However, the mechanistic failure mechanism of cathodes upon in contact with Li metal is far from clear. In this study, using in situ transmission electron microscopy, we directly visualize at an atomic scale the interaction of Li dendrites with well-defined, epitaxial thin films of LiCoO2, the most widely used cathode material. We show that a spontaneous and prompt chemical reaction is trigged once the Li contact is made, leading to expansion and amorphization of the LiCoO2 structure, with Li2O and Co metal being the final reaction products. A topotactic phase transition is identified close to the reaction front, resulting in the formation of CoO as a metastable intermediate. Dynamic structural and chemical imaging in combination with ab inito simulations reveal that a high density of antiphase grain boundaries are formed at the reaction front, which are critical for enabling the short-range topotactic reactions and long-range Li propagation. The fundamental insights are of general importance in mitigating Li dendrites related issues and guiding the design principle for more robust energy materials.
Here, particle/polymer electrospinning was used to prepare fiber mat cathodes containing LiCoO 2 nanoparticles, carbon powder, and poly(vinylidene fluoride) for Li-ion batteries. The fibers had a high LiCoO 2 particle content (70 wt%) which allowed for a high gravimetric capacity of 90 mAh g -1 (corresponding to 128 mAh g$-1\atop{LiCoO2}$) at 0.1C (1C = 274 mAh g$-1\atop{LiCoO2}$). Cathode performance was stable in a half cell with 78% capacity retention over 200 cycles at 0.5C. Unlike previous work on electrospun LiCoO 2 nanofibers prepared using sol-gel chemistry and high temperature processing, the particle/polymer fiber mat cathodes reported here were made thick with a high fiber volume fraction for high areal and volumetric capacities at fast charge/discharge rates (e.g., 0.81 mAh cm -2 and 62 mAh cm -3 at 2C) which were much greater than that of a slurry cast cathode of the same composition (0.004 mAh cm -2 and 0.30 mAh cm -3 at 2C). Full cells containing a LiCoO 2 /C/PVDF fiber mat cathode and C/PVDF fiber mat anode were also prepared and characterized. These electrospun batteries exhibited a high energy density of 144 Wh kg -1 at 0.1C and an areal capacity of 1.03 mAh cm -2 at 1C. The excellent performance of the electrospun particle/polymer cathodes and anodes is attributed to electrolyte penetration throughout the 3D fiber electrode mats, a large electrode/electrolyte interfacial area, and short Li + transport pathways between the electrolyte and active material nanoparticles in the radial fiber direction.
Ionic liquids based on methylpropylpyrrolidinium (MPPY) and methylpropylpiperidinium (MPPI) cations and bis(trifluoromethanesulfionyl)imide (TFSI) anion have been synthesized and characterized by thermal analysis, cyclic voltammetry, impedance spectroscopy as well as gavanostatic charge/discharge tests. 10 wt% of vinylene carbonate (VC) was added to the electrolytes of 0.5 M LiTFSI/MPPY.TFSI and 0.5 M LiTFSI/MPPI.TFSI, which were evaluated in Li || natural graphite (NG) half cells at 25 oC and 50 oC under different current densities. At 25 oC, due to their intrinsic high viscosities, the charge/discharge capacities under the current density of 80 A cm-2 were much lower than those under the current density of 40 A cm-2. At 50 oC, with reduced viscosities, the charge/discharge capacities under both current densities were almost indistinguishable, which were also close to the typical values obtained using conventional carbonate electrolytes. In addition, the discharge capacities of the half cells were very stable with cycling, due to the effective formation of solid electrolyte interphase (SEI) on the graphite electrode. On the contrary, the charge/discharge capacities of the Li || LiCoO2 cells using both ionic liquid electrolytes under the current density of 40 A cm-2 decreased continually with cycling, which were primarily due to the low oxidative stability of VC on the surface of LiCoO2.
A new strategy for suppressing dendritic lithium growth in rechargeable lithium metal batteries is introduced, in which TiO2 nanotube (NT) array electrodes prepared by anodization are used as a metallic lithium storage medium. During the first charge process, lithium ions are inserted into the crystal structure of the TiO2 NT arrays, and then, lithium metal is deposited on the surfaces of the NT arrays, i.e., in the NT pores and between NT walls. From the second cycle onward, the TiO2 material is used as lithium ion pathways, which results in the effective current distribution for lithium deposition and prevents disintegration of the deposited metallic lithium. Compared to a Li(Cu foil)-LiCoO2 cell, the Li(TiO2 NT)-LiCoO2 cell exhibits enhanced cycling efficiency. This new concept will enable other 3D structured negative active materials to be used as lithium metal storage media for lithium metal batteries.
Li2O2LiCoO2(CoO)2Lix0CoO2 crystallizes in the triclinic P1 space group. The structure is one-dimensional and consists of one cobalt dihydroxide molecule; one CoO ribbon oriented in the (0, 1, 1) direction; one Li2O2 ribbon oriented in the (0, 1, 1) direction; and one LiCoO2 ribbon oriented in the (0, 1, 1) direction. In the CoO ribbon, there are two inequivalent Co+3.25+ sites. In the first Co+3.25+ site, Co+3.25+ is bonded in a distorted linear geometry to two equivalent O2- atoms. Both Co–O bond lengths are 1.63 Å. In the second Co+3.25+ site, Co+3.25+ is bonded in a linear geometry to two equivalent O2- atoms. Both Co–O bond lengths are 1.34 Å. O2- is bonded in a 2-coordinate geometry to two Co+3.25+ atoms. In the Li2O2 ribbon, there are two inequivalent Li1+ sites. In the first Li1+ site, Li1+ is bonded in a distorted linear geometry to two O2- atoms. There is one shorter (1.63 Å) and one longer (1.64 Å) Li–O bond length. In the second Li1+ site, Li1+ is bonded in a linear geometry to two O2- atoms. There is one shorter (1.38 Å) and one longer (1.39 Å) Li–O bond length. There are two inequivalent O2- sites. In the first O2- site, O2- is bonded in a distorted bent 150 degrees geometry to two Li1+ atoms. In the second O2- site, O2- is bonded in a distorted bent 150 degrees geometry to two Li1+ atoms. In the LiCoO2 ribbon, Li1+ is bonded in a distorted linear geometry to two O2- atoms. There is one shorter (1.61 Å) and one longer (1.69 Å) Li–O bond length. Co+3.25+ is bonded in a distorted linear geometry to two O2- atoms. Both Co–O bond lengths are 1.30 Å. There are two inequivalent O2- sites. In the first O2- site, O2- is bonded in a distorted linear geometry to one Li1+ and one Co+3.25+ atom. In the second O2- site, O2- is bonded in a distorted linear geometry to one Li1+ and one Co+3.25+ atom.
(LiMnO2)2LiCoO2Lix0CoO2 crystallizes in the triclinic P-1 space group. The structure is one-dimensional and consists of one cobalt dihydroxide molecule; one LiCoO2 ribbon oriented in the (1, 1, 1) direction; and two LiMnO2 ribbons oriented in the (1, 1, 1) direction. In the LiCoO2 ribbon, Li1+ is bonded in a linear geometry to two equivalent O2- atoms. Both Li–O bond lengths are 1.53 Å. Co2+ is bonded in a linear geometry to two equivalent O2- atoms. Both Co–O bond lengths are 1.49 Å. O2- is bonded in a distorted bent 150 degrees geometry to one Li1+ and one Co2+ atom. In each LiMnO2 ribbon, Li1+ is bonded in a linear geometry to two equivalent O2- atoms. Both Li–O bond lengths are 1.44 Å. Mn+4.50+ is bonded in a distorted linear geometry to two equivalent O2- atoms. Both Mn–O bond lengths are 1.54 Å. O2- is bonded in a distorted linear geometry to one Li1+ and one Mn+4.50+ atom.
The current spike obtained during the hard external short test is small (8.2 A) compared to those obtained from a LiCoO2 system (60 to 80 A). The simulated internal short did not result in an explosion or fire as it does with the LiCoO2 systems. The temperatures obtained during the heat-to-vent test are not very high compared to the cobaltate cells. The cells do not retain capacity very well, but the capacity can be recovered with cycling. The spinel cells are much safer under abuse conditions than the lithium-ion cells with other transition metal oxides.
Co-intercalation is an effective approach to tune the diffusion coefficient with which cations insert into the electrodes for energy storage devices. By applying this concept in aqueous Zn batteries, a prospective system for stationary energy storage, we demonstrate the critical role of structural H2O on Zn2+ intercalation into bilayer V2O5·nH2O. The H2O solvation of Zn2+ largely reduces its effective charge and thus electrostatic interaction with the V2O5 framework, evidently promoting the diffusion of solvated Zn2+. Benefited from the ‘lubricating’ effect, the aqueous Zn battery shows a specific energy of ~ 305 Wh kg-1 (based on cathode), comparable to those of LiCoO2//Graphite batteries. Meanwhile, it can maintain an energy density of 199 Wh kg-1 at a high power density of 24 kW kg-1 with a capacity retention of 88% after 900 cycles, making it a promising candidate for high-performance, low-cost, safe and environmentally friendly energy storage device.
Ni-rich layered oxides (LiNi1-xMxO2; M = Co, Mn, ...) are appealing alternatives to conventional LiCoO2 as cathodes in Li-ion batteries for automobile and other large-scale applications due to their high theoretical capacity and low cost. However, preparing stoichiometric LiNi1-xMxO2 with ordered layer structure and high reversible capacity, has proven difficult due to cation mixing in octahedral sites. Herein, in situ studies of synthesis reactions and the associated structural ordering in preparing LiNiO2 and the Co-substituted variant, LiNi0.8Co0.2O2, are made, to gain insights into synthetic control of the structure and electrochemical properties of Ni-rich layered oxides. Results from this study indicate a direct transformation of the intermediate from the rock salt structure into hexagonal phase, and during the process, Co substitution facilities the nucleation of a Co-rich layered phase at low temperatures and subsequent growth and stabilization of solid solution Li(Ni, Co)O-2 upon further heat treatment. Optimal conditions are identified from the in situ studies and utilized to obtain stoichiometric LiNi0.8Co0.2O2 that exhibits high capacity (up to 200 mA h g(-1) ) with excellent retention. The findings shed light on designing high performance Ni-rich layered oxide cathodes through synthetic control of the structural ordering in the materials.