Search NASASearch

SEARCH · Search NASA

Results for “Lithium”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

Process Systems Engineering-Informed Design and Scale-Up of Multi-stage Diafiltration Cascades for Lithium and Cobalt Recovery from Spent Lithium-Ion Batteries

These slides present work jointly completed by Tasks in PrOMMiS. The first half of the presentation motivates the importance of critical materials for national security and how the recovery of critical minerals via membrane separations can be more cost effective than currently used technology. The second half of the presentation presents cost-optimal results for the custom cost model for diafiltration using the superstructure flowsheet developed by CMU. These results highlight how PSE can inform process targets (i.e., product purity targets) and suitable design strategies for scaled-up membrane cascades.

critical materials

Content of lithium, beryllium, boron, and titanium, and the isotopic composition of lithium, boron, and magnesium in Luna 16 regolith sample

The abundance of the following elements in the L 16-19 No. 118 regolith sample, zone V was determined by isotopic dilution using a mass spectrometer equipped with a scattering ion source: Li -- 9.8, Be -- 1.2, Be -- 2.6, and Ti -- 1.92 percent. For comparison, these same elements were measured in samples of surface material returned by Apollo 11, Apollo 12, and Apollo 14, and in the terrestrial reference standard diabase W-1. The content of Li, Be, and B in the Luna 16 sample is nearly the same as in the Apollo 11 surface material. The surface material returned by Apollo 12 and Apollo 14 contains two to four times more of these elements. However, the abundance ratios of Li, Be, and B are remarkably similar in the surface materials from the four different lunar regions. With respect to basaltic achondrites and especially with respect to chondrites, the lunar basalts are enriched in Li, Be, and B up to 100 times.

Eugster, O.

Lithium in a short-period tidally locked binary of M67: Implications for stellar evolution, Galactic Lithium evolution, and cosmology

In open clusters, late-F stars exhibit a Li maximum (the Li 'peak' region) at lower abundance with age, which could be due either to stellar depletion or Galactic Li enrichment (or some other cause). We have observed a short-period tidally locked binary (SPTLB) on the Li peak region in the old cluster M67 to distinguish between alternatives. SPTLBs which synchronized in the early pre-main sequence would avoid the rotational mixing which, according to Yale models, may be responsible for depleting Li with age in open cluster dwarfs. We find that both components of the M67 SPTLB have a Li abundance lying about a factor of 2 or more above any other M67 single star and about a factor of 3 or more above the mean Li peak region abundance in M67. Our results suggest that the initial Li abundance in M67 is at least as high as approximately 3.0 = 12 + log (N(sub Li)/N(sub H)). Our high M67 SPTLB Li abundance and those in other clusters support the combination of Zahn's tidal circularization and the Yale rotational mixing theories and may indicate that the halo Li plateau (analogous to the cluster Li peak region) abundance has been depleted from a higher primordial value. Implications are discussed.

Deliyannis, Constantine P.

Superionic conducting vacancy-rich β-Li 3 N electrolyte for stable cycling of all-solid-state lithium metal batteries

The advancement of all-solid-state lithium metal batteries requires breakthroughs in solid-state electrolytes (SSEs) for the suppression of lithium dendrite growth at high current densities and high capacities (>3 mAh cm -2 ) and innovation of SSEs in terms of crystal structure, ionic conductivity and rigidness. Here we report a superionic conducting, highly lithium-compatible and air-stable vacancy-rich β-Li 3 N SSE. This vacancy-rich β-Li 3 N SSE shows a high ionic conductivity of 2.14 × 10 -3 S cm -1 at 25 °C and surpasses almost all the reported nitride-based SSEs. A Li- and N-vacancy-mediated fast lithium-ion migration mechanism is unravelled regarding vacancy-triggered reduced activation energy and increased mobile lithium-ion population. All-solid-state lithium symmetric cells using vacancy-rich β-Li 3 N achieve breakthroughs in high critical current densities up to 45 mA cm -2 and high capacities up to 7.5 mAh cm -2 , and ultra-stable lithium stripping and plating processes over 2,000 cycles. The high lithium compatibility mechanism of vacancy-rich β-Li 3 N is unveiled as intrinsic stability to lithium metal. In addition, β-Li 3 N possesses excellent air stability through the formation of protection surfaces. All-solid-state lithium metal batteries using the vacancy-rich β-Li 3 N as SSE interlayers and lithium cobalt oxide (LCO) and Ni-rich LiNi 0.83 Co 0.11 Mn 0.06 O 2 (NCM83) cathodes exhibit excellent battery performance. Extremely stable cycling performance is demonstrated with high capacity retentions of 82.05% with 95.2 mAh g -1 over 5,000 cycles at 1.0 C for LCO and 92.5% with 153.6 mAh g -1 over 3,500 cycles at 1.0 C for NCM83. Utilizing the vacancy-rich β-Li 3 N SSE and NCM83 cathodes, the all-solid-state lithium metal batteries successfully accomplished mild rapid charge and discharge rates up to 5.0 C, retaining 60.47% of the capacity. Notably, these batteries exhibited a high areal capacity, registering approximately 5.0 mAh cm -2 for the compact pellet-type cells and around 2.2 mAh cm -2 for the all-solid-state lithium metal pouch cells.

25 ENERGY STORAGE

Water acidification aggravates lithium-induced toxicity represented by energy supply, oxidative stress, and cell fate in Daphnia magna neonates

Lithium is extensively utilized in industrial energy production, particularly in lithium-ion batteries, and in pharmaceuticals for the treating clinical mood disorders. Consequently, lithium is frequently detected in various environmental matrices. It has been reported to cause a range of toxic effects on aquatic organisms including oxidative stress, neurological disorders, and reproductive suppression. Water acidification is a global issue with numerous negative impacts on aquatic organisms. It can alter the physio-chemical properties and bioavailability of metal ions. The acidic leaching process during lithium battery treatment and global water acidification both suggest that lithium contamination often occurs in acidic environments. In the present study, Daphnia magna neonates were exposed to four treatments (control, lithium alone, low pH, and combined) to investigate whether an acidic environment exacerbates the toxic effects of lithium on aquatic organisms and to explore potential toxic action mechanisms. The results indicated that low pH posed a significant threat to the growth and reproduction of D. magna. When exposed to both lithium and low pH, there was increased lithium accumulation and an energy trade-off response, leading to increased energy allocation to reproduction and reduced energy for growth. Lithium exposure stimulated D. magna activity, while low pH inhibited it, suggesting that an imbalance in energy consumption and supply. Combined exposure to lithium and low pH resulted in severe oxidative stress due to mitochondrial dysfunction, under-utilization of energy substances, and increased ionic homeostasis disturbances. Consequently, the exposed organism altered apoptosis and autophagy processes to maintain homeostasis. In conclusion, the present study demonstrated that lithium and water acidification posed a population-level threat to D. magna, and their combined exposure significantly largely exacerbated the toxic effects.

63 RADIATION, THERMAL, AND OTHER ENVIRON. POLLUTAN

Final Design for Thermal/Epithermal eXperiments (TEX) with Lithium Absorbers to Provide Validation Benchmarks for Y-12 Electrorefining Facility

One of the main goals of the Thermal/Epithermal eXperiments (TEX) project is to use existing Nuclear Criticality Safety Program (NCSP) assets to create critical experiment plutonium and uranium test beds for materials important to criticality safety that have insufficient benchmark evaluations. The plutonium test bed experiments were completed in 2018 and are published in the 2020 edition of the International Criticality Safety Benchmark Evaluation Project (ICSBEP) Handbook. The uranium test bed assemblies were completed in 2023 and accepted in the 2024 edition of the ICSBEP Handbook. The Nuclear Criticality Safety (NCS) group at Y-12 National Security Complex has identified programmatic need for validation cases for uranium electrorefining operations at Y-12. The electrorefining operation credits lithium enriched in 6 Li in addition to 35 Cl as absorbers in the design criticality safety evaluation for precluding criticality under upset conditions in the large and geometrically unfavorable electro-refiner. There is, however, inadequate experimental validation for the 6 Li absorbers. As an extension of the TEX uranium test bed, TEX-Cl critical experiments were performed with sodium chloride salt to address the 35 Cl thermal absorption as well as other validation needs at Los Alamos National Laboratory (LANL). These experiments were completed in 2024 and accepted into the 2025 ICSBEP Handbook. To continue the methodology used in TEX-Cl, TEX-Li aims to accomplish the same. The overall design of both experiments was to use commercially available, high purity, salts with polyethylene moderator and HEU plates to configure a critical assembly. Three experiments are planned for TEX-Li using encapsulated lithium carbonate (Li 2 CO 3 ), with natural 6 Li abundance. For all experiments, the highly enriched uranium (HEU) Jemima plates will be used as fissile material. Multiple layers will be stacked together with encapsulated Li 2 CO 3 alternated with polyethylene in standard configurations. Standard stacking was found to be optimal in matching the different sensitivity profiles provided by the Y-12 models. Three configurations are proposed with varying polyethylene moderation and a constant 1/4” absorber thickness. The first uses 11 layers of 5/4” polyethylene, the second uses 9 layers of 3/4” polyethylene, and the third uses 10 layers of 1/2” polyethylene. Calculations showed that some alternative forms of lithium-based materials provided slightly less-optimal sensitivity profiles when compared to lithium carbonate but come with other drawbacks. These alternatives included lithium aluminate (LiAlO 2 ), Aluminum-2050 alloy, Aluminum-8090, Aluminum-2095, lithium hydride (LiH), and lithium fluoride (LiF). Lithium aluminate and aluminum-2050 provided comparable sensitivity profiles when compared to lithium carbonate and can be used instead if lithium carbonate cannot be readily procured. After a broad material study, lithium carbonate outperformed any alternative material with a balance in affordability and workability. The assessment of experimental uncertainties of the non-absorber and absorber components was predicted to be 0.00089 and 0.00093 Δk eff , respectively. The largest uncertainties may be reduced with precision dimensional inspection of the components. Many of the parts and equipment for IER 575 have already been fabricated or procured for previous projects and therefore do not contribute significantly to the overall cost of this experiment. This includes the Jemima plates and Comet critical assembly machine, which are existing NCSP assets, as well as the aluminum platen and polyethylene reflector rings, which were fabricated and authorized for the TEX experiment involving HEU with polyethylene. Lithium carbonate containers will be procured by LANL and will be filled by LLNL. The total material costs for TEX-Li experiments are estimated to be on the order of $\$$47,400. Precision inspection, including dimensional, mass, density, and impurity, is recommended for all components for an estimated cost of $\$$12,000.

35Cl

Investigation of Drift Effects in UEDGE Simulations of NSTX-U Edge Plasma With Lithium Divertors

Lithium is a low-Z material, and lithium-based plasma-facing components (PFCs) are planned for the National Spherical Torus Experiment Upgrade (NSTX-U) to explore potential benefits for divertor power exhaust and core plasma management. NSTX-U is a medium-sized spherical tokamak with up to 12 MW of auxiliary heating, capable of generating reactor-relevant plasma conditions. This work presents boundary plasma simulations for NSTX-U with lithium PFCs using the UEDGE code, incorporating full magnetic and 𝐄 ×𝐁 drift physics. The simulations show that drifts strongly influence heat and particle transport: they enhance convective transport, broaden the scrape-off layer heat-flux width 𝜆 𝑞 , and reduce the anomalous heat diffusivity 𝜒 required to reproduce predicted SOL heat-flux width. 𝐄 ×𝐁 drifts provide poloidal transport, while ∇𝐵 (which includes both gradB and curvature) drifts provide radial heat and particle transport. Lithium transport is also affected by drifts, with lithium ions migrating from the outer divertor to the inner divertor through the private flux region (PFR) following the 𝐄 ×𝐁 drifts flow, lowering upstream impurity lithium densities. UEDGE is self-consistently coupled with the Wall-Li model to study plasma lithium PFC interactions depending on the local lithium sourcing based on local plasma conditions and lithium surface temperature. In these simulations, lithium evaporation shows a vapor-shielding effect that reduces divertor heat flux and increases radiative losses once surface temperatures exceed 450°C. This research work provides a first step toward self-consistent modeling of lithium PFCs in NSTX-U, demonstrating the impact of drift-driven plasma transport in SOL and divertor regions.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY

Self-consistent modeling of tokamak edge plasma transport with lithium sources

Magnetic confinement fusion devices require effective heat and particle exhaust solutions on the divertor plates to operate sustainably, especially under reactor-relevant conditions. Liquid lithium divertors have been proposed to address two major challenges: control of excessive heat flux to plasma-facing components through vapor shielding and minimization of core plasma contamination from impurities. The National Spherical Torus Experiment-Upgrade (NSTX-U) will explore lithium as a divertor material due to its potential to meet both objectives. We present a self-consistent coupling framework between the plasma boundary transport code UEDGE and the lithium wall transport code Wall–Li to evaluate the feasibility and operational limits of lithium-based divertors. The model aims to optimize lithium sourcing levels to prevent core plasma contamination via fuel dilution while ensuring divertor protection through vapor shielding. This integrated framework, applicable to any tokamak with lithium sources, dynamically adjusts lithium sourcing based on local plasma conditions and surface temperature. The coupled model is tested using NSTX-like geometry and plasma conditions to assess its performance and reliability. Wall–Li calculates lithium fluxes from plasma-facing components, incorporating physical sputtering, thermally enhanced sputtering, and evaporation driven by surface temperature and ion flux. These fluxes are reintroduced into UEDGE as neutral lithium atoms, enabling simulation of their transport and distribution within the plasma. UEDGE computes plasma and neutral transport, surface heat flux, and iteratively feeds this information back to Wall–Li. A small time step is employed to ensure numerical stability and convergence, enabling accurate simulations over typical tokamak discharge durations. This integrated modeling approach provides a robust tool for identifying operational regimes that balance effective lithium sourcing with minimal core plasma contamination, offering critical insights for optimizing lithium-based divertor systems in current and future fusion devices.

Magnetic confinement fusion

Composite Lithium Metal Structure to Mitigate Pulverization and Enable Long‐Life Batteries

In lithium metal batteries, non‐uniform stripping of lithium results in pit formation, which promotes subsequent non‐uniform, dendritic deposition. This viscous cycle leads to pulverization of lithium which promotes cell shorting or capacity degradation, symptoms further exaggerated by high electrode areal loading and lean electrolytes. Here, to address this challenge, a composite lithium metal anode is engineered that contains uniformly distributed, nanometer‐sized carbon particles. This composite lithium is shown to strip more uniformly since the growth of non‐uniform pits is intercepted by the carbon particles. This mechanism is corroborated by a continuum electrochemical model. Subsequent lithium deposition on carbon particles is also found to be more uniform than on the surface with irregular pits. Notably, the pulverization rate of composite lithium is 26 times slower than that of commercial lithium. Moreover, in a Li‐S battery with sulfurized polyacrylonitrile cathode, the use of the composite anode extends the cycle life by three times when the areal capacity is 8 mAh cm −2 . The approach of using an engineered lithium composite structure to address challenges during both stripping and plating can inform future designs of lithium metal anodes for high areal capacity operations.

high areal capacity