Search NASA⌕ Search

SEARCH · Search NASA

Results for “Mg alloys”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

Development of Low Density Titanium Alloys for Structural Applications

In this report the results of a program designed to reduce the density of titanium by adding magnesium are presented. Because these two elements are immiscible under conventional ingot metallurgy techniques, two specialized powder metallurgy methods namely, mechanical alloying (MA) and physical vapor deposition (PVD) were implemented. The mechanical alloying experiments were done both at the University of Idaho and at the Defense Research Agency in UK. Since titanium is reactive with interstitial elements, a secondary goal of this research was to correlate solubility extensions with interstitial contamination content, especially oxygen and nitrogen. MA was carried out in SPEX 8000 shaker mils and different milling containers were utilized to control the level of contamination. Results showed that solubilities of Mg in Ti were obtained up to 28 at.% (16.4 wt. %) Mg in Ti for Ti-39.6 at. % (25 wt. %) Mg alloys, which greatly exceed those obtained under equilibrium conditions. This reflects a density reduction of approximately 26 %. Contamination of oxygen and nitrogen seemed to increase the solubility of magnesium in titanium in some cases; however, we were not able to make a clear correlation between contamination levels with solubilities. Work at the DRA has emphasized optimization of present PVD equipment, specifically composition and temperature control. Preliminary PVD data has shown Ti-Mg deposits have successfully been made up to 2 mm thick and that solubility extensions were achieved. The potential for density reduction of titanium by alloying with magnesium has been demonstrated; however, this work has only scratched the surface of the development of such low density alloys. Much research is needed before such alloys could be implemented into industry. Further funding is required in order to optimize the MA/PVD processes including contamination control, determination of optimal alloy compositions, microstructure development, and mechanical property determination.

Froes, F. H.↗

Investigate the height dependency of the micro-/defect-structure and mechanical properties of additively manufactured AlF357 aluminum alloy

When the laser powder bed fusion (L-PBF) additive manufacturing method is employed to build parts with increased heights, there is a possibility that defects are increased in part. This study investigates the effect of build height on the micro-/defect-structure and, consequently, the mechanical properties of L-PBF AlF357, an Al-Si-Mg alloy family. Tall vertical cylinders of 316 mm with 15 mm diameter were fabricated and cut into specimens at different heights. Although not much difference is observed in the microstructure (grain size and morphology), the defects' size and population slightly vary with height. Nonetheless, the tensile properties of the L-PBF AlF357 are found to be independent of height. This is ascribed to the approximately identical microstructure and marginal difference in the defect's size and distribution along the heights.

Laser powder bed fusion (L-PBF)↗

The effect of water vapor on fatigue crack Growth in 7475-t651 aluminum alloy plate

The effects of water vapor on fatigue crack growth in 7475-T651 aluminum alloy plate at frequencies of 1 Hz and 10 Hz were investigated. Twenty-five mm thick compact specimens were subjected to constant amplitude fatigue testing at a load ratio of 0.2. Fatigue crack growth rates were calculated from effective crack lengths determined using a compliance method. Tests were conducted in hard vacuum and at water vapor partial pressures ranging from 94 Pa to 3.8 kPa. Fatigue crack growth rates were frequency insensitive under all environment conditions tested. For constant stress intensity factor ranges crack growth rate transitions occurred at low and high water vapor pressures. Crack growth rates at intermediate pressures were relatively constant and showed reasonable agreement with published data for two Al-Cu-Mg alloys. The existence of two crack growth rate transitions suggests either a change in rate controlling kinetics or a change in corrosion fatigue mechanism as a function of water vapor pressure. Reduced residual deformation and transverse cracking specimens tested in water vapor versus vacuum may be evidence of embrittlement within the plastic zone due to environmental interaction.

Dicus, D. L.↗

Effect of water vapor on fatigue crack growth in 7475-T651 aluminum alloy plate

The effects of water vapor on fatigue crack growth in 7475-T651 aluminum alloy plate at frequencies of 1 Hz and 10 Hz were investigated. Twenty-five mm thick compact specimens were subjected to constant amplitude fatigue testing at a load ratio of 0.2. Fatigue crack growth rates were calculated from effective crack lengths determined using a compliance method. Tests were conducted in hard vacuum and at water vapor partial pressures ranging from 94 Pa to 3.8 kPa. Fatigue crack growth rates were frequency insensitive under all environment conditions tested. For constant stress intensity factor ranges crack growth rate transitions occurred at low and high water vapor pressures. Crack growth rates at intermediate pressures were relatively constant and showed reasonable agreement with published data for two Al-Cu-Mg alloys. The existence of two crack growth rate transitions suggests either a change in rate controlling kinetics or a change in corrosion fatigue mechanism as a function of water vapor pressure. Reduced residual deformation and transverse cracking specimens tested in water vapor versus vacuum may be evidence of embrittlement within the plastic zone due to environmental interaction.

Dicus, D. L.↗

An Electrochemical Framework to Explain Intergranular Stress Corrosion Cracking in an Al-5.4%Cu-0.5%Mg-0.5%Ag Alloy

A modified version of the Cu-depletion electrochemical framework was used to explain the metallurgical factor creating intergranular stress corrosion cracking susceptibility in an aged Al-Cu-Mg-Ag alloy, C416. This framework was also used to explain the increased resistance to intergranular stress corrosion cracking in the overaged temper. Susceptibility in the under aged and T8 condition is consistent with the grain boundary Cu-depletion mechanism. Improvements in resistance of the T8+ thermal exposure of 5000 h at 225 F (T8+) compared to the T8 condition can be explained by depletion of Cu from solid solution.

Little, D. A.↗

Material variability as measured by low temperature electrical resistivity.

Low temperature electrical resistivity was used to determine the material variability (1) between different manufacturers, (2) between different heats from the same manufacturer, and (3) within a given heat for Al 2024, Al-5% Mg alloys, Inconel 718, A286 stainless, and AISI 316. Generally, the coefficient of variation for solution annealed alloys ranged from 1.2 to 14% between manufacturers, 0.8 to 5.1% between heats, and 0.1 to 1.6% within a heat with stainless steels at the low ends and Al 2024 at the high ends. The variability is increased if the material is in a precipitation-hardened condition. A statistical analysis suggests that the variability within a heat is non-normal.

Clark, A. F.↗

Effect of Thermal Exposure on the Tensile Properties of Aluminum Alloys for Elevated Temperature Service

Tensile properties were evaluated for four aluminum alloys that are candidates for airframe applications on high speed transport aircraft. These alloys included the Al-Cu-Mg-Ag alloys C415 and C416 and the Al-Cu-Li-Mg-Ag alloys RX818 and ML377. The Al-Cu-Mg alloys CM001, which was used on the Concorde SST, and 1143, which was modified from the alloy used on the TU144 Russian supersonic aircraft, were tested for comparison. The alloys were subjected to thermal exposure at 200 F, 225 F and 275 F for times up to 30,000 hours. Tensile tests were performed on thermally-exposed and as-received material at -65 F, room temperature, 200 F, 225 F and 275 F. All four candidate alloys showed significant tensile property improvements over CM001 and 1143. Room temperature yield strengths of the candidate alloys were at least 20% greater than for CM001 and 1143, for both the as-received and thermally-exposed conditions. The strength levels of alloy RX818 were the highest of all materials investigated, and were 5-10% higher than for ML377, C415 and C416 for the as-received condition and after 5,000 hours thermal exposure. RX818 was removed from this study after 5,000 hours exposure due to poor fracture toughness performance observed in a parallel study. After 30,000 hours exposure at 200 F and 225 F, the alloys C415, C416 and ML377 showed minor decreases in yield strength, tensile strength and elongation when compared to the as-received properties. Reductions in tensile strength from the as-received values were up to 25% for alloys C415, C416 and ML377 after 15,000 hours exposure at 275 F.

Edahl, Robert A., Jr.↗

Al-Li Alloy 1441 for Fuselage Applications

A cooperative investigation was conducted to evaluate Al-Cu-Mg-Li alloy 1441 for long service life fuselage applications. Alloy 1441 is currently being used for fuselage applications on the Russian Be-103 amphibious aircraft, and is expected to be used for fuselage skin on a new Tupolev business class aircraft. Alloy 1441 is cold-rollable and has several attributes that make it attractive for fuselage skin applications. These attributes include lower density and higher specific modulus with similar strength as compared to conventional Al-Cu-Mg alloys. Cold-rolled 1441 Al-Li sheet specimens were tested at NASA Langley Research Center (LaRC) and at the All-Russia Institute of Aviation Materials (VIAM) in Russia to evaluate tensile properties, fracture toughness, impact resistance, fatigue life and fatigue crack growth rate. In addition, fuselage panels were fabricated by Tupolev Design Bureau (TDB) using 1441 skins and Al-Zn-Mg-Cu alloy stiffeners. The panels were subjected to cyclic pressurization fatigue tests at TDB and at LaRC to simulate fuselage pressurization/depressurization during aircraft service. This paper discusses the results from this investigation.

Bird, R. K.↗

The physical metallurgy of mechanically-alloyed, dispersion-strengthened Al-Li-Mg and Al-Li-Cu alloys

Powder processing of Al-Li-Mg and Al-Li-Cu alloys by mechanical alloying (MA) is described, with a discussion of physical and mechanical properties of early experimental alloys of these compositions. The experimental samples were mechanically alloyed in a Szegvari attritor, extruded at 343 and 427 C, and some were solution-treated at 520 and 566 C and naturally, as well as artificially, aged at 170, 190, and 210 C for times of up to 1000 hours. All alloys exhibited maximum hardness after being aged at 170 C; lower hardness corresponds to the solution treatment at 566 C than to that at 520 C. A comparison with ingot metallurgy alloys of the same composition shows the MA material to be stronger and more ductile. It is also noted that properly aged MA alloys can develop a better combination of yield strength and notched toughness at lower alloying levels.

Gilman, P. S.↗

Consolidation processing parameters and alternative processing methods for powder metallurgy Al-Cu-Mg-X-X alloys

The effects of varying the vacuum degassing parameters on the microstructure and properties of Al-4Cu-1Mg-X-X (X-X = 1.5Li-0.2Zr or 1.5Fe-0.75Ce) alloys processed from either prealloyed (PA) or mechanically alloyed (M) powder, and consolidated by either using sealed aluminum containers or containerless vacuum hot pressing were studied. The consolidated billets were hot extruded to evaluate microstructure and properties. The MA Li-containing alloy did not include Zr, and the MA Fe- and Ce-containing alloy was made from both elemental and partially prealloyed powder. The alloys were vacuum degassed both above and below the solution heat treatment temperature. While vacuum degassing lowered the hydrogen content of these alloys, the range over which the vacuum degassing parameters were varied was not large enough to cause significant changes in degassing efficiency, and the observed variations in the mechanical properties of the heat treated alloys were attributed to varying contributions to strengthening by the sub-structure and the dispersoids. Mechanical alloying increased the strength over that of alloys of similar composition made from PA powder. The inferior properties in the transverse orientation, especially in the Li-containing alloys, suggested deficiencies in degassing. Among all of the alloys processed for this study, the Fe- and Ce-containing alloys made from MA powder possessed better combinations of strength and toughness.

Sankaran, K. K.↗

Characterization of the dimensional stability of advanced metallic materials using an optical test bench structure

The dimensional stability of low-density high specific-strength metal-matrix composites (including 30 vol pct SiC(p)/SXA 24-T6 Al, 25 vol pct SiC(p)/6061-T6 Al, 40 vol pct graphite P100 fiber/6061 Al, 50 vol pct graphite P100 fiber/6061 Al, and 40 vol pct P100 graphite fiber/AZ91D Mg composites) and an Al-Li-Mg metal alloy was evaluated using a specially designed five-strut optical test bench structure. The structure had 30 thermocouple locations, one retroreflector, one linear interferometer multilayer insulation, and various strip heaters. It was placed in a 10 exp -7 torr capability vacuum chamber with a laser head positioned at a window port, and a laser interferometer system for collecting dimensional change data. It was found that composite materials have greater 40-C temporal dimensional stability than the AL-Li-Mg alloy. Aluminum-based composites demonstrated better 40-C temporal stability than Mg-based composites.

Hsieh, Cheng↗

Solution chemistry effects on the stress corrosion cracking behavior of alloy 2090 (Al-Li-Cu) and alloy 2024 (Al-Cu-Mg)

The SCC initiation behavior of alloys 2090 and 2024 is examined in various NaCl-based environments. The pre-exposure and bulk/local solution chemistry effects discovered by Holroyd et al. (1986) are investigated, with emphasis on the effect of bulk solution chemistries and atmospheric CO2 on the occluded cell environment and the role of the occluded environment in the crack initiation and early-stage propagation processes. It was found that constant immersion in NaCl does not promote SCC in alloy 2090 or alloy 2024. Upon removal from NaCl, SCC is quickly facilitated, but only in the presence of atmospheric CO2. The need for CO2 is attributed to an increase in carbonate concentrations, eventually allowing passivation of blunted fissures by precipitation of Li2CO3. It is inferred that any effects due to aging are small in magnitude, relative to the effects of subtle changes in the bulk/local solution chemistries.

Moran, James P.↗

Ignition and combustion of aluminum/magnesium alloy particles in O2 at high pressures

The ignition and combustion of Al, Mg, and Al/Mg alloy particles in 99 percent O2/1 percent N2 mixtures is investigated at high temperatures and pressures for rocket engine applications. The 20-micron particles contain 0, 5, 10, 20, 40, 60, 80, and 100 wt pct Mg alloyed with Al, and are ignited in oxygen using the reflected shock in a single-pulse shock tube near the endwall. Using this technique, the ignition delay and combustion times of the particles are measured at temperatures up to 3250 K as a function of Mg content for oxygen pressures of 8.5, 17, and 34 atm. An ignition model is developed that employs a simple lumped capacitance energy equation and temperature and pressure dependent particle and gas properties. Good agreement is achieved between the measured and predicted trends in the ignition delay times.

Roberts, Ted A.↗

Microstructural and Mechanical Property Characterization of Shear Formed Aerospace Aluminum Alloys

Advanced manufacturing processes such as near-net-shape forming can reduce production costs and increase the reliability of launch vehicle and airframe structural components through the reduction of material scrap and part count and the minimization of joints. The current research is an investigation of the processing-microstructure-property relationships for shear formed cylinders of the Al-Cu-Li-Mg-Ag alloy 2195 for space applications and the Al-Cu-Mg-Ag alloy C415 for airframe applications. Cylinders which had undergone various amounts of shear-forming strain were studied to correlate the grain structure, texture, and mechanical properties developed during and after shear forming.

Troeger, Lillianne P.↗

Microstructural and Mechanical Characterization of Shear Formed Aluminum Alloys for Airframe and Space Applications

Advanced manufacturing processes such as near-net-shape forming can reduce production costs and increase the reliability of launch vehicle and airframe structural components through the reduction of material scrap and part count and the minimization of joints. The current research is an investigation of the processing-microstructure-property relationship for shear formed cylinders of the Al-Cu-Li-Mg-Ag alloy 2195 for space applications and the Al-Cu-Mg-Ag alloy C415 for airframe applications. Cylinders which have undergone various amounts of shear-forming strain have been studied to assess the microstructure and mechanical properties developed during and after shear forming.

Troeger, L. P.↗

Metals Technology for Aerospace Applications in 2020: Development of High Temperature Aluminum Alloys For Aerospace Applications

The role of trace additions on the nucleation and stability of the primary strengthening phase, omega, is of paramount importance for the enhancement of mechanical properties for moderate temperature application of Al-Cu-Mg-(Ag) alloys. In order to better understand the competition for solute, which governs the microstructural evolution of these alloys, a series of Al-Cu-Mg-Si quaternary alloys were prepared to investigate the role of trace Si additions on the nucleation of the omega phase. Si additions were found to quell omega nucleation in conjunction with the enhanced matrix precipitation of competing phases. These initial results indicate that it is necessary to overcome a critical Mg/Si ratio for omega precipitation, rather than a particular Si content.

Dicus, Dennis↗

Intermediate temperature thermomechanical processing of Al 2090 for superplasticity

The Al-Cu-Li phase diagram indicates that during thermomechanical processing of Al 2090 at 300 C both T(1) and T(2) phases will precipitate. Following work on Al-Mg-X alloys, it is possible that TMP at such temperatures might promote intragranular formation of these phases and promote microstructural refinement during recrystallization. Microstructural analyses reveal that the T(2) phase in Al 2090 may play a similar role to the beta-phase in Al-Mg-X alloys during microstructural evolution. Mechanical property data indicate that Al 2090 can be moderately (215-245 percent) superplastic at 370 C following processing at 300 C.

Hales, S. J.↗