Search NASA⌕ Search

SEARCH · Search NASA

Results for “Microstructural Refinement”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

Melt-Pool Dynamics and Microstructure of Mg Alloy WE43 under Laser Powder Bed Fusion Additive Manufacturing Conditions

Magnesium-based alloy WE43 is a state-of-the-art bioresorbable metallic implant material. There is a need for implants with both complex geometries to match the mechanical properties of bone and refined microstructure for controlled resorption. Additive manufacturing (AM) using laser powder bed fusion (LPBF) presents a viable fabrication method for implant applications, as it offers near-net-shape geometrical control, allows for geometry customization based on an individual patient, and fast cooling rates to achieve a refined microstructure. In this study, the laser–alloy interaction is investigated over a range of LPBF-relevant processing conditions to reveal melt-pool dynamics, pore formation, and the microstructure of laser-melted WE43. In situ X-ray imaging reveals distinct laser-induced vapor depression morphology regimes, with minimal pore formation at laser-scan speeds greater than 500 mm/s. Optical and electron microscopy of cross-sectioned laser tracks reveal three distinct microstructural regimes that can be controlled by adjusting laser-scan parameters: columnar, dendritic, and banded microstructures. These regimes are consistent with those predicted by the analytic solidification theory for conduction-mode welding, but not for keyhole-mode tracks. The results provide insight into the fundamental laser–material interactions of the WE43 alloy under AM-processing conditions and are critical for the successful implementation of LPBF-produced WE43 parts in biomedical applications.

36 MATERIALS SCIENCE↗

Impact of Materials Processing on Microstructural Evolution and Hydrogen Isotope Storage Properties of Pd-Rh Alloy Powders.

Cryomilled Pd - 10Rh was investiga ted as potential solid - state storage material of hydrogen. Pd - 10Rh was first atomized, and then subsequently cryomilled. The cryomilled Pd - 10Rh was then examined using microstructural characterization techniques including op tical microscopy, electron microscopy, and X - ray diffraction. Pd - 10Rh particles were significantly flattened, increasing the apparent surface area. Microstructural refinement was observed in the cryomilled Pd - 10Rh, generating grains at the nanom etric scale through dislocation - based activity. Hydrogen sorption properties were also characterized, generating both capacity as well as kinetics measurements. It was found that the microstructural refinement due to cryomilling did not play a significant role on hyd rogen sorption properties until the smallest grain size (on the order of %7E25 nm) was achieved. Additionally, the increased surface area and other changes in particle morphology were associated with cryomilling changed the kinetics of hydrogen absorption.

36 MATERIALS SCIENCE↗

Surface composition, microstructure and corrosion resistance of AZ31 magnesium alloy irradiated by high-intensity pulsed ion beam

High-intensity pulsed ion beam (HIPIB) irradiation of AZ31 magnesium alloy is performed and electrochemical corrosion experiment of irradiated samples is carried out by using potentiodynamic polarization technology in order to explore the effect of HIPIB irradiation on corrosion resistance of magnesium alloy. The surface composition, cross-sectional morphology and microstructure are characterized by using electron probe microanalyzer, optical microscope and transmission electron microscope, respectively. The results indicated that HIPIB irradiation leads to a significant improvement in corrosion resistance of magnesium alloy, in terms of the considerable increase in both corrosion potential and pitting breakdown potential. The microstructural refinement and surface purification induced by HIPIB irradiation are responsible for the improved corrosion resistance. - Research Highlights: {yields} A modified layer about 30 {mu}m thick is obtained by HIPIB irradiation. {yields} Selective ablation of element/impurity phase having lower melting point is observed. {yields} More importantly, microstructural refinement occurred on the irradiated surface. {yields} The modified layer exhibited a significantly improved corrosion resistance. {yields} Improved corrosion resistance is ascribed to the combined effect induced by HIPIB.

36 MATERIALS SCIENCE↗

Mass transport in a highly immiscible alloy on extended shear deformation

Forced mixing to a single phase or supersaturated solid solution (SSS) and its prerequisite microstructure evolution in immiscible systems has been a focus of research for both fundamental science and a variety of applications. Controlling the formation of SSS by shear deformation assisted processing could enable a material design beyond conventional equilibrium microstructure in immiscible systems. Here, a highly immiscible (mixing enthalpy of ~ 20 kJ·mol -1 ) Cu-50 at. % Cr binary alloy was employed to investigate the microstructure evolution and localized tendencies of SSS during severe shear deformation. The present results demonstrate distinctive microstructure refinement process in each phase and how they lead to localized SSS as a function of shear strain. Preferential dynamic recrystallization occurs in the softer Cu phase due to strain localization, leading to substantial grain refinement. The refinement of Cr phase in the top-most layer, however, is enabled by the progressive evolution of grain lamination, splitting, and fragmentation as a function of shear strain. The eventual SSS is found to be strongly dependent on the local environments that affect the dislocation activity, including the level of microstructure refinement, the interfacial orientation relationship, hardness difference, and supposed stability of oxidation. Ab initio simulations comfirm that it is more favorable to oxidize Cr than Cu at incoherent Cu/Cr interfaces which then limits the mass transport on an incoherent boundary. Our results shed light on the underpinning mechanism for non-equilibrium mass transport in immiscible systems upon severe deformation that can be applicable to a variety of processing techniques aimed at producing immiscible alloys with superior mechanical properties.

36 MATERIALS SCIENCE↗

Effect of tool design and pass strategy on defect elimination and uniform, enhanced tensile properties of friction stir processed high-pressure die-cast A380 alloy

This work reports implementation of friction stir processing (FSP) to locally modify microstructure and create a defect-free processing zone with the aid of different tool designs and altering the passing strategy for two different process parameter combinations. Here, FSP is applied on high pressure die-cast (HPDC) A380 alloy, a widely used Al-Si alloy fabricated in the die casting sector for automotive and aerospace applications. However, the presence of gas and shrinkage porosity, brittle needle-shaped Fe-containing ß-FeSiAl 5 intermetallic compounds, Al-dendrites, coarse and acicular silicon particles, and large second-phase particulates have a detrimental influence on the uniformity of tensile properties across the thickness direction of an HPDC plate. FSP is able to eliminate porosity, refine microstructure and improve tensile properties. An FSP tool design and a passing strategy are identified for the best microstructure consolidation and uniform enhanced tensile properties. This study noted the importance of tool features such as scroll design and flats on tool pin and multiple pass orientation strategy to find best combination of defect-free refined microstructure and uniform tensile strength and ductility across the processing zone of HPDC Al alloys.

36 MATERIALS SCIENCE↗

Phase stability in cast and additively manufactured Al-rich Al-Cu-Ce alloys

Additively manufactured (AM) eutectic Al alloy systems have been studied extensively for advantageous thermal stability and mechanical properties due to their refined microstructures. Al-Cu-Ce alloys are one subset of these AM eutectic alloys. Here we studied phase stability in AM Al-Cu-Ce alloys and compared it to that of conventionally cast ones. A new phase, Al 8 Cu 3 Ce, was identified in the microstructures of both AM and cast Al-Cu-Ce alloys. This Al 8 Cu 3 Ce phase was not previously included on experimental or thermodynamically calculated phase diagrams of the Al-Cu-Ce system. Therefore, we performed additional thermodynamic modeling of the system. These models were experimentally validated with cast and subsequently heat-treated Al-Cu-Ce alloys. We found that despite the refined microstructure of the AM alloys, the phases formed were consistent with the cast alloys, suggesting that AM processing did not significantly alter the formation and stability of phases from that in the conventional alloys. In conclusion, this work has resolved inconsistent previous descriptions of the Al-Cu-Ce ternary phase diagram in the Al-rich region and resulted in the addition of the Al 8 Cu 3 Ce as an equilibrium phase above 500 °C.

36 MATERIALS SCIENCE↗

Effects of rolling processes on ridging generation of ferritic stainless steel

Highlights: • The effects of microstructural refinement and texture on ridging are analysed. • Optimal reduction during cold rolling benefits the enhancement of ridging resistance. • A Steckel-mill rolling method is proposed to improve ridging resistance of FSS 430. • 30% of ridging height reduction can be achieved with proposed rolling method. - Abstract: In order to reduce the ridging generation of ferritic stainless steel (FSS) during forming process, the crystallographic texture of the FSS was modified by optimisation of both rolling and annealing processes. A systematic study was carried out to improve the ridging resistance of the FSS by investigating the sequential changes in microstructure and texture during different rolling and annealing processes. The results show that the surface roughness of the final sheet strained by 20% along the rolling direction is decreased by 20% to 30% using Steckel-mill rolling compared to traditional tandem rolling. A direct correlation is found between the ridging resistance of the FSS and the rolling routines. It has been observed that an optimal reduction value during cold rolling process is critical to the microstructural refinement and surface quality improvement of the FSS. Reduction of the fraction of {001} <110> component by optimisation of the rolling processes is found to be effective in reducing the ridging height of the FSS during the formation process.

36 MATERIALS SCIENCE↗

Rapid Strengthening Without Loss of Ductility via Electropulsing Treatment in Ti-6Al-4V Alloy

The commercial (hot-rolled and annealed) Ti-6Al-4V alloy subjected to electropulsing was investigated in this study. The results show that the electropulsing-treated sample with optimized parameter exhibits greatly refined microstructure and notable strength improvement without loss of ductility. The main strengthening mechanism is recognized as phase transformation and rapid grain refinement induced by recrystallization under EPT.

36 MATERIALS SCIENCE↗

Fe-24 wt.%Cr-4.1 wt.%C hardfacing alloy: Microstructure and carbide refinement mechanisms with ceria additive

The microstructure and carbide refinement mechanisms of Fe-24 wt.%Cr-4.1 wt.%C hardfacing alloys with 0 wt.%, 0.5 wt.%, 1.0 wt.%, 2 wt.%, and 4 wt.% ceria additives have been systematically investigated in this work. Optical microscopy, field emission scanning electron microscopy with energy dispersive spectrometer, and X-ray diffraction were collectively used to study the microstructure, the phase components, and the chemical formation of inclusion formed in the welding process. Wear-resistance of the alloys was comparatively studied using an abrasive wear testing machine. The structure analysis results show that the Fe-Cr-C hardfacing alloy mainly consists of martensite, retained austenite, MC carbide and M{sub 7}C{sub 3} carbide. With increasing ceria additive contents, the average size of the primary M{sub 7}C{sub 3} carbide decreases and reaches a most refined state in the alloy with 2 wt.% ceria additives. Comparative wear tests data shows that the wear resistance of the hardfacing alloys with ceria additives is better than that without ceria additive. In a good agreement with the carbide refinement results, the wear resistance of the alloy reaches an optimum level in the sample with 2 wt.% ceria additive. The main RE inclusion type identified with in-situ XRD analysis is RE inclusion Ce{sub 2}O{sub 2}S. Thermodynamics calculation confirms that this type of RE inclusion could precipitate prior to M{sub 7}C{sub 3} carbides, and act as a heterogeneous nucleus for M{sub 7}C{sub 3} in the welding process, which effectively provides a mechanism for significant refinement of the M{sub 7}C{sub 3} carbide and improves its wear resistance. - Graphical Abstract: Rare Earth inclusion (Ce{sub 2}O{sub 2}S) distributes in the primary M{sub 7}C{sub 3} carbide. Moreover, Ce{sub 2}O{sub 2}S, which acts as heterogeneous nuclei of the primary M{sub 7}C{sub 3} carbide, is medium effective. Therefore, the primary M{sub 7}C{sub 3} carbide has been refined. Highlights: Black-Right-Pointing-Pointer Micro-hardness of primary M{sub 7}C{sub 3} carbide in Fe-Cr-C hardfacing alloy is 1594 HV. Black-Right-Pointing-Pointer RE inclusion Ce{sub 2}O{sub 2}S can be observed in the primary M{sub 7}C{sub 3} carbide. Black-Right-Pointing-Pointer Ce{sub 2}O{sub 2}S as heterogeneous nuclei of the Cr{sub 7}C{sub 3} is medium effective. Black-Right-Pointing-Pointer Primary carbide is most refined with 2 wt.% ceria additive.

36 MATERIALS SCIENCE↗

Ultra-Fine Grain Structures Of Model Al-Mg-Si Alloys Produced By Hydrostatic Extrusion

Microstructure and mechanical properties were studied in model Al-Mg-Si alloys (Al-1 % Mg-0.8% Si and Al-0.5% Mg-0.3% Si-wt %) deformed by hydrostatic extrusion (HE) to strains of 1.4 and 3.8. In these alloys the different percentage of two hardening second-phase precipitates (Mg{sub 2}Si and Si) were observed. The microstructure was characterized by transmission electron microscopy and optical microscopy. The microstructure of the alloys in the initial state was built of coarse grains of an average diameter of {approx}30 rim. The refined microstructure was examined qualitatively and quantitatively using the stereological method and a computer image analysis. The deformation-processed structures evolved very rapidly, forming ultrafine grained (UFG) materials with grains of about 0.4 {mu}m. In addition, the grain refinement in the HE-treated materials has a substantial effect on their properties, such as the mechanical strength and micro-hardness which increase significantly. It has been found that, after {epsilon} = 3.8 in the Al-1% Mg-0.8% Si alloy, the micro-hardness increases approximately twofold. The yield stress is more than four times higher in the UFG alloys, in comparison to the initial state. Similar results were identified in the Al-0.5% Mg-0.3% Si. This is due to the very rapid refinement of the microstructure during the deformation and presence of second-phase particles.

36 MATERIALS SCIENCE↗

Effect of rapid solidification on the microstructure and mechanical properties of hot-pressed Al-20Si-5Fe alloys

The aim of this work is to study the effect of cooling rate and subsequent hot consolidation on the microstructural features and mechanical strength of Al-20Si-5Fe-2X (X = Cu, Ni and Cr) alloys. Powder and ribbons were produced by gas atomization and melt spinning processes at two different cooling rates of 1 x 10{sup 5} K/s and 5 x 10{sup 7} K/s. The microstructure of the products was examined using optical microscopy, scanning electron microscopy, transmission electron microscopy, and X-ray diffraction. The particles were consolidated by hot pressing at 400 deg. C/250 MPa/1 h under a high purity argon atmosphere and the microstructure, hardness and compressive strength of the compacts were evaluated. Results showed a profound effect of the cooling rate, consolidation stage, and transition metals on the microstructure and mechanical strength of Al-20Si-5Fe alloys. While microstructural refining was obtained at both cooling rates, the microstructure of the atomized powder exhibited the formation of fine primary silicon ({approx} 1 {mu}m), eutectic Al-Si phase with eutectic spacing of {approx} 300 nm, and {delta}-iron intermetallic. Supersaturated Al matrix containing 5-7 at.% silicon and nanometric Si precipitates (20-40 nm) were determined in the microstructure of the melt-spun ribbons. The hot consolidation resulted in coarsening of Si particles in the atomized particles, and precipitation of Si and Fe-containing intermetallics from the supersaturated Al matrix in the ribbons. The consolidated ribbons exhibited higher mechanical strength compared to the atomized powders, particularly at elevated temperatures. The positive influence of the transition metals on the thermal stability of the Al-20Si-5Fe alloy was noticed, particularly in the Ni-containing alloy.

36 MATERIALS SCIENCE↗

Effect of Cooling Rate on Nano-Eutectic Formation in Laser Surface Remelted and Rare Earth Modified Hypereutectic Al-20Si Alloys

Laser Surface Remelting (LSR) was applied to arc-melted Al-20Si-0.2Sr, Al-20Si-0.2Ce, and Al-20Si hypereutectic alloys to refine microstructures. Experiments revealed that microstructures in the melt pool varied from fully eutectic to a mixture of Al dendrites and inter-dendritic eutectic. We calculated cooling rates using the Eagar-Tsai model and correlated cooling rates with characteristic microstructures, revealing that a cooling rate on the order of 104 K/s could lead to maximized fully eutectic microstructure morphology. Due to rapid solidification, the Si composition in the LSR eutectic was measured at 18.2 wt.%, higher than the equilibrium eutectic composition of 12.6 wt.%Si. Compared to Al-20Si, Ce addition had no significant effect on the volume fraction of the fully eutectic structure but refined Si fibers to approximately 30 nm in diameter. Sr addition did not further refine the diameter of eutectic Si fibers compared to Al-20Si but increased the volume fraction of the fully eutectic microstructure morphology. The refinement ratio (φ) of the Si fiber diameter from the bottom of the melt pool to the surface for the three alloys was similar, at around 28%. The established correlation between the cooling rate and the size and morphology of the microstructure within the melt pool will enable tailoring of the microstructure in laser-processed as well as deposited alloys for high strength and plasticity.

36 MATERIALS SCIENCE↗

Microstructure of titanium on complex deformation paths: Comparison of ECAP, KOBO and HE techniques

Highlights: • Method for producing CP titanium rods for medical implants is searched. • Three processing methods producing ultra-fine grain titanium are compared. • Microstructure and textures are examined and analysed. • Mechanical characteristics are determined based on microhardness and tensile tests. • Hydrostatic extrusion (HE) leads to the best properties of titanium rods for medical implants. - Abstract: In this work samples of commercial purity grade 2 titanium were severely deformed by three different extrusion techniques: equal-channel angular pressing (ECAP), extrusion through oscillating die (KOBO), and hydrostatic extrusion (HE). Resulting microstructures and mechanical properties of processed titanium samples are studied and compared with regard to potential application as a material for dental implants. The obtained results demonstrate the effect of different strain paths, involved by three applied deformation methods, on microstructure refinement, mechanical properties and textures of the studied material. Heterogeneous microstructures with bimodal grain size distributions are observed for all deformation techniques in the examined material, however differences in their internal structures and grain boundary distributions point to different grain refinement mechanisms. The fraction of ultra-fine grains is the highest in titanium deformed by HE. Also the internal grain fragmentation is the most important after HE deformation. This leads to the best mechanical and microstructural properties obtained in this type of deformation. Consequently, the HE process seems to be very interesting for production of material for medical implants.

36 MATERIALS SCIENCE↗

Lattice misorientation evolution and grain refinement in Al-Si alloys under high-strain shear deformation

The starting microstructure of an alloy can be tailored to achieve varying degrees of microstructural refinement and enhance mechanical properties through severe plastic shear deformation during solid-phase processing. Crystal plasticity-based grain misorientation modeling, coupled with systematic pin-on-disk tribometry-based subsurface shear deformation experiments on as-cast Al-xSi alloys (x = 0, 1, 4 at %), was conducted. The post-deformation microstructural analysis, through a combined computational and experimental approach, conclusively shows that the initial volume fraction of the hard Si phase enhances the evolution of local lattice misorientation, leading to efficient grain refinement during severe plastic shear deformation. The shear–deformation-induced nanostructure resulted in more than double the nanoindentation hardness in the processed alloy.

Gwalani, Bharat↗

Additive friction stir deposition of SS316: Effect of process parameters on microstructure evolution

Solid state nature of additive friction stir deposition (AFSD) additive manufacturing process is very advantageous in terms of defect formation and microstructural refinement in the material. Current study presents the process optimization, microstructural evolution and kinetics of recrystallization for AFSD deposited low stacking fault energy material - SS316. As deposited microstructure shows equiaxed ultra fine grains with an average grain size of ~5.0 ± 0.5 μm. Shear deformation at high temperature during processing leads to the operation of restoration mechanisms. Observation of necklace type microstructure in the as deposited SS316 is attributed to discontinuous dynamic recrystallization during processing. Recrystallization kinetics of the AFSD SS316 is characterized using Johnson-Mehl-Avarami-Kolmogorov (JMAK) model. Deformation – thermal cycling during AFSD process resulted in inconsistent recrystallization kinetics. Variation in strain, strain rate and temperature during processing with processing parameters result in varying microstructure and tool wear. Further, high strength-ductility combination and sustained work hardening in as deposited SS316 appear to arise from transformation and twinning during deformation, leading to the formation of hierarchical twins and martensitic phase after deformation.

36 MATERIALS SCIENCE↗

Effect of Minor Yttrium on Microstructure and Mechanical Properties of Bioimplant Mg-5Zn Alloy

This paper explores cast Mg-5Zn alloy, containing small amounts of yttrium (Y: 0.1-1.5 wt.%), through microstructure evaluation and tensile and hardness tests. The results reveal that addition of Y to the alloy refines microstructure, especially when secondary phases, Mg{sub 3}Zn{sub 6}Y (I) and Mg{sub 3}Zn{sub 3}Y{sub 2} (W), form. I-phase is detected when 0.3 wt.% Y is added to the alloy, while W-phase is only observed in Mg-5Zn-1.5Y alloy. The results also show that the addition of Y improves yield and tensile strength as well as the hardness value of the Mg-5Zn alloy at the expense of its formability. The three effects of the solid solution of Y in α-Mg, grain refinement, and the formation of I- and W-phases are the reasons for such behavior. The improvement is more pronounced when W-phase appears in the microstructure. In other words, Mg-5Zn-1.5Y alloy behaves stronger and harder than other alloys and may be considered as a potential candidate for bioimplant applications if its degradation behavior meets the requirements.

36 MATERIALS SCIENCE↗

Microstructural Evolution of Al-1Fe (Weight Percent) Alloy During Accumulative Continuous Extrusion Forming

As a new microstructure refining method, accumulative continuous extrusion forming (ACEF) cannot only refine metal matrix but also refine the phases that exist in it. In order to detect the refinements of grain and second phase during the process, Al-1Fe (wt pct) alloy was processed by ACEF, and the microstructural evolution was analyzed by electron backscatter diffraction (EBSD) and transmission electron microscopy (TEM). Results revealed that the average grain size of Al-1Fe (wt pct) alloy decreased from 13 to 1.2 μm, and blocky Al{sub 3}Fe phase with an average length of 300 nm was granulated to Al{sub 3}Fe particle with an average diameter of 200 nm, after one pass of ACEF. Refinement of grain was attributed to continuous dynamic recrystallization (CDRX), and the granulation of Al{sub 3}Fe phase included the spheroidization resulting from deformation heat and the fragmentation caused by the coupling effects of strain and thermal effect. The spheroidization worked in almost the entire deformation process, while the fragmentation required strain accumulation. However, fragmentation contributed more than spheroidization. Al{sub 3}Fe particle stimulated the formation of substructure and retarded the migration of recrystallized grain boundary, but the effect of Al{sub 3}Fe phase on refinement of grain could only be determined by the contrastive investigation of Al-1Fe (wt pct) alloy and pure Al.

36 MATERIALS SCIENCE↗

Microstructure of the spray formed Vanadis 4 steel and its ultrafine structure

The as-sprayed microstructure of the Vanadis 4 steel was studied. It was observed that the as-sprayed microstructure consists of martensite, retained austenite and uniformly distributed spheroidal carbides. The Kurdiumov-Sachs crystallographic relation between martensite and retained austenite is confirmed by transmission electron microscope. No macro segregation or network carbides are found. This can be explained in terms of the rapid solidification of spray forming for microstructure refining. The steel obtained by the new processing has a uniform carbide distribution, and the average carbide size is even smaller than the equivalent in the powder metallurgical Vanadis 4 steel. It was proved that spray forming can be considered as a new and high-efficient way to replace powder metallurgy for the production of Vanadis 4 steel.

36 MATERIALS SCIENCE↗