Search NASA⌕ Search

SEARCH · Search NASA

Results for “Ni superalloys”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

Science-Based Acceleration of the Full Value Stream for Metal Additive Manufacturing: Expedited Powder Development and Additive Manufacturing Deployment in the Areas of Ni-Base Superalloy and Custom Alloy Powders for AM (Final Report)

The overall Science-based Acceleration of the Full Value Stream for Metal Additive Manufacturing (AM): Expedited Powder Development and Additive Manufacturing Deployment (“X-P4AM”) project objective is to drastically reduce the time-to-market barriers for new additive alloys of interest in automotive and aerospace applications, through computational alloy design with rapid screening and down- selection via synthesis of candidate alloys with rapid solidification. The project will also refine the technology in high pressure gas atomization to improve the production of commercial quantities of selected powders with high powder yields and enhanced powder quality. Production of modified nickel-based superalloys and a Ni-containing alloy based on a high entropy composition, enhanced powder production methods, and optimized AM build parameterization provided critical steps in widespread adoption of AM technology for aerospace applications, in this case. The individual backgrounds and capabilities of the Parties are ideally suited to the successful execution of this work. The included work enhanced the Contractors’ AM capabilities, a core competency of the Contractors, and develop a close working relationship with the Participant in the area of nickel-based powder superalloys and custom alloys and their end use.

36 MATERIALS SCIENCE↗

Science-Based Acceleration of the Full Value Stream for Metal Additive Manufacturing: Expedited Powder Development and Additive Manufacturing Deployment in the Areas of Ni-Base Superalloy and Custom Alloy Powders for AM

The overall Science-based Acceleration of the Full Value Stream for Metal Additive Manufacturing (AM): Expedited Powder Development and Additive Manufacturing Deployment (“X-P4AM”) project objective is to drastically reduce the time-to-market barriers for new additive alloys of interest in automotive and aerospace applications, through computational alloy design with rapid screening and down- selection via synthesis of candidate alloys with rapid solidification. The project will also refine the technology in high pressure gas atomization to improve the production of commercial quantities of selected powders with high powder yields and enhanced powder quality. Production of modified nickel-based superalloys and a Ni-containing alloy based on a high entropy composition, enhanced powder production methods, and optimized AM build parameterization provided critical steps in widespread adoption of AM technology for aerospace applications, in this case. The individual backgrounds and capabilities of the Parties are ideally suited to the successful execution of this work. The included work enhanced the Contractors’ AM capabilities, a core competency of the Contractors, and develop a close working relationship with the Participant in the areas of nickel-based powder superalloys and custom alloys and their end use.

36 MATERIALS SCIENCE↗

Science-Based Acceleration of the Full Value Stream for Metal Additive Manufacturing: Expedited Powder Development and Additive Manufacturing Deployment in the Areas of Ni-Base Superalloy and Custom Alloy Powders for AM

The overall Science-based Acceleration of the Full Value Stream for Metal Additive Manufacturing (AM): Expedited Powder Development and Additive Manufacturing Deployment (“X-P4AM”) project objective is to drastically reduce the time-to-market barriers for new additive alloys of interest in automotive and aerospace applications, through computational alloy design with rapid screening and down- selection via synthesis of candidate alloys with rapid solidification. The project will also refine the technology in high pressure gas atomization to improve the production of commercial quantities of selected powders with high powder yields and enhanced powder quality. Production of modified nickel-based superalloys and a Ni-containing alloy based on a high entropy composition, enhanced powder production methods, and optimized AM build parameterization provided critical steps in widespread adoption of AM technology for aerospace applications, in this case. The individual backgrounds and capabilities of the Parties are ideally suited to the successful execution of this work. The included work enhanced the Contractors’ AM capabilities, a core competency of the Contractors, and develop a close working relationship with the Participant in the areas of nickel-based powder superalloys and custom alloys and their end use.

36 MATERIALS SCIENCE↗

The Effect Stacking Fault Segregation and Phase Transformations have on Creep Strength in Ni-based Superalloys

In this study, two commercially similar polycrystalline Ni-based disk superalloys (LSHR and ME3) were creep tested at 760C and 552MPa to approximately 0.3% plastic strain. LSHR consistently displayed superior creep properties at this stress/temperature regime even though the microstructural characteristics between the two alloys were comparable. High resolution structural and chemical analysis, however, revealed significant differences between the two alloys among active gamma prime shearing modes involving superlattice intrinsic and extrinsic stacking faults. In ME3, Co and Cr segregation and Ni and Al depletion were observed along the intrinsic faults - revealing a gamma prime -to- gamma phase transformation. Conversely in LSHR, an alloy with a higher W content, Co and W segregation was observed along the intrinsic faults. This observation combined with scanning transmission electron microscopy (STEM) simulations confirm a gamma prime-to-D019 phase transformation along the intrinsic faults in LSHR. Using experimental observations and density functional theory calculations, a novel local phase transformation strengthening mechanism is proposed that could be further utilized to improve the high temperature creep capabilities of Ni-base disk alloys.

Superalloy↗

Creep resistant Ni-based superalloy casting and method of manufacture for advanced high-temperature applications

One or more embodiments relates to a method of casting a creep-resistant Ni-based superalloy and a homogenization heat treatment for the alloy. The method includes forming a feed stock having Nickel (Ni) and at least one of Chromium (Cr), Cobalt (Co), Aluminum (Al), Titanium (Ti), Niobium (Nb), Iron (Fe), Carbon (C), Manganese (Mn), Molybdenum (Mo), Silicon (Si), Copper (Cu), Phosphorus (P), Sulfur (S) and Boron (B). The method further includes fabricating the creep-resistant Ni-based superalloy in a predetermined shape using the feed stock and at least one process such as vacuum induction melting (VIM), electroslag remelting (ESR) and/or vacuum arc remelting (VAR).

Jablonski, Paul D.↗

Effect of Alloying Additions on Twinning in Ni-based Superalloys

Micro-twinning is the dominant creep deformation mechanism in Ni-based superalloys at temperatures above 700 °C. We use atomistic simulations to study two mechanisms of twin nucleation and growth that are characterized by qualitatively different rate limiting processes. In case of the mechanism proposed by Kolbe, the rate limiting process is diffusion-mediated atomic reshuffling. In case of the other mechanism, we proposed recently, the rate limiting process is nucleation of Shockley partial dislocation. We demonstrate the effects of alloying additions on functionality of these mechanisms.

Valery V Borovikov↗

Simulation and analysis of small angle scattering (SAS) patterns of Ni-based superalloy microstructures generated by a phase-field model

This paper investigates the relationship between microstructural features and small-angle scattering (SAS) patterns in Ni-based superalloys using a combined phase-field and SAS simulation approach coupled with microstructure analyses. The simulated SAS patterns accurately capture key experimental observations previously reported in the literature, including the time-dependent transition from circular to square-shaped precipitates and the development of anisotropic SAS patterns. Importantly, our analysis reveals the correlations between characteristic length scales extracted from SAS profiles and microstructural descriptors, such as precipitate size and inter-precipitate distance. These findings provide a comprehensive understanding of the link between SAS profiles and microstructure evolution in Ni-based superalloys, offering valuable insights for materials characterization and design.

Microstructure↗

Ab Initio Simulation of Structure and Properties in Ni-Based Superalloys: Haynes282 and Inconel740

The electronic structure, interatomic bonding, and mechanical properties of two supercell models of Ni-based superalloys are calculated using ab initio density functional theory methods. The alloys, Haynes282 and Inconel740, are face-centered cubic lattices with 864 atoms and eleven elements. These multi-component alloys have very complex electronic structure, bonding and partial-charge distributions depending on the composition and strength of the local bonding environment. We employ the novel concept of total bond order density (TBOD) and its partial components (PBOD) to ascertain the internal cohesion that controls the intricate balance between the propensity of metallic bonding between Ni, Cr and Co, and the strong bonds with C and Al. We find Inconel740 has slightly stronger mechanical properties than Haynes282. Both Inconel740 and Haynes282 show ductile natures based on Poisson’s ratio. Poisson’s ratio shows marginal correlation with the TBOD. Comparison with more conventional high entropy alloys with equal components are discussed.

36 MATERIALS SCIENCE↗

Rapid solidification characteristics in melt spinning a Ni-base superalloy

The solidification kinetics involved in the process of melt spinning a Ni-base superalloy have been characterized. Through a correlation of ribbon thickness to melt puddle residence time, it was found that the solidification front velocity, V, is typically about 100 mm/sec at the ribbon surface not in contact with the spinning wheel. The rate of solidification varies within the ribbon, increasing with decreasing distance, S, from the wheel-contact surface as V = 3.65/s. Ribbon microstructure and texture characteristics are discussed in light of this kinetics result. The thickness-vs-time correlation was further analyzed to yield information about thermal history during ribbon formation. These thermal results are generally consistent with those deduced from dendrite arm spacing measurements.

Huang, S. C.↗

Gaseous Hydrogen Embrittlement of L-PBF Ni-Based Superalloys for Service in Natural Gas Turbines

Efforts to improve efficiency of industrial gas turbine engines have focused on increasing operating temperatures by use of fuel-flexible gas blends. Ni-based superalloys are susceptible to hydrogen embrittlement (HE), leading to potential risk of premature component failure. Certain turbine components exposed to hydrogen-rich environments are manufactured from additive processes like laser powder bed fusion (L-PBF). The HE susceptibility was evaluated for three Ni-based superalloys: solid solution strengthened Alloy 625, γ’/γ’’-precipitation strengthened Alloy 718, and γ’-precipitation strengthened Haynes® 282®. L-PBF samples were pre-charged under medium and high pressure gaseous hydrogen before tensile testing at temperatures up to 260 °C using a fast strain rate. Selected samples were subjected to a service conditioning heat treatment prior to hydrogen charging to evaluate the change in susceptibility after prolonged service. The susceptibility to HE and HE mechanisms of these three alloys is compared.

additive manufacturing↗

Improved Creep and Tensile Properties of a Corrosion Resistant Ni-Based Superalloy Using High Temperature Aging and Nb/Ta Additions

Resistance to creep deformation is essential for cast and wrought Ni-based superalloys in next generation energy systems due to the considerable exposure times required at the operating temperature. Here the amount of precipitate strengthening was increased in variants to Inconel alloy 725 (IN725), a corrosion resistant alloy, to improve its elevated temperature mechanical strength. Additions of Nb or Ta coupled with a high temperature aging (HTA) heat treatment promoted the formation of γ" precipitates and grain boundary phases which led to significant increases in time to failure. The HTA increased the creep life of various alloy formulations as compared to the standard aging heat treatment with a maximum improvement of 371%. The Nb and Ta additions lowered the minimum creep rate (MCR) and had a similar effect on increasing creep life. The positive effect of the additions was more pronounced when coupled with the HTA which employed a higher temperature in the first step of the heat treatment to promote precipitate phase formation. The Ti/Al ratio was used to design alloys with preferential formation of ' or γ" precipitates. Compact morphology precipitates were formed in the alloys with a low Ti/Al ratio. While a low Ti/Al ratio was primarily associated with lower MCRs, the effect on the creep life was less evident than that of the HTA. By using additions of Nb or Ta and a HTA heat treatment, the creep life of IN725 for testing at 973 K (700 °C) and 483 MPa was improved by up to 256%.

36 MATERIALS SCIENCE↗

Characterization of γ′/γ″ compact and sandwich type precipitates during long-term high-temperature exposure in Ni-based superalloys

Here, the formation of γ′/γ″ co-precipitates is investigated in Ni-based superalloys with a varying Ti/Al ratio and Ta content and their stability is studied using long-term high-temperature exposure. Transmission electron microscopy and atom probe tomography analyses demonstrate that both higher Ti/Al ratios and increased Ta promote γ″ phase formation, leading to sandwich and compact structures. The compact co-precipitation significantly reduces γ′ precipitate coarsening during 10,000 h exposure at 700°C by restricting elemental diffusion, particularly of aluminum, from the γ matrix to the γ′ phase. For the alloy without a compact structure, and only γʹ precipitates, at the beginning of the exposure, the coarsening rate over 10,000 h was 3.5 times faster than for the alloy with compact γʹ/γʺ precipitates. Evidence of destabilization of the compact morphology was found to occur between 5,000 and 10,000 h exposure and originated from the extensive formation and growth of δ platelets that extended throughout the grains. Thus, the outer layer of the compact, which consists of γʺ, was subjected to the γ″ to δ phase transformation.

gamma double prime↗

Temperature-Dependence of Corrosion of Ni-Based Superalloys in Hot CO 2 -Rich Gases Containing SO 2 Impurities

Future power plants will require Ni-based superalloys resistant to high-temperature corrosion in CO 2 -rich environments containing impurities. In this work, several commercially available Ni-based alloys (617, 230, 625, 263, 740H) were exposed at 600°C, 650°C, 750°C and 1 atm to 95% CO 2 , 4% H 2 O, 1% O 2 without/with 0.1% SO 2 to simulate compositions expected in a direct-fired supercritical CO 2 power cycle. The results indicate no effect of SO 2 at 750°C, a small negative effect at 650°C, and a large negative effect at 600°C. Alloys exposed at the higher temperatures (650–750°C) formed thin Cr-rich oxide scales, whereas the lowest temperature (600°C) resulted in thicker scales consisting of non-protective oxides and sulfates. Thermodynamic analysis indicates this increased corrosion is associated with a transition in the stable compounds in contact with the gas. Understanding the factors that affect this transition will aid in the selection or design of alloys for future CO 2 -based power systems.

36 MATERIALS SCIENCE↗

The effects of Cr, Co, Al, Mo and Ta on the cyclic oxidation behavior of a prototype cast Ni-base superalloy based on a 2(5) composite statistically designed experiment

A series of cast Ni-base superalloys were systematically varied at selected levels of Co, Cr, Mo, Ta, and Al. The elemental levels varied were Mo, 0 to 4 percent; Cr, 6 to 18 percent; Co, 0 to 20 percent, Ta, 0 to 8 percent; and Al, 3.25 to 6.25 percent. The cyclic oxidation resistance was determined from specific weight change data as a function of time for 1 hr cycles in static air at 1100 C. The significant terms in decreasing order of their importance were Al, Ta, Cr2, Al-Cr, Cr-Co, Co2, Al-Mo, Cr-Mo, Al-Al, and Mo-Ta. The Al term alone accounted for close to 82 percent of the explained variability. The estimating equation showed that the Al level was the most important and should be at its 6.25 wt % maximum value. The Mo and Ta levels should also be at their maximum 4 and 8 wt % respectively. The cobalt composition should be as low as possible, i.e., 0 wt%. The Cr level optimum varies depending on the other 4 levels. The X-ray diffaction results indicate the most protective scales are alumina/aluminate spinel stabilizized with a tri-rutile oxide high in Ta and Mo.

Barrett, C. A.↗

A study of microstructural characteristics and differential thermal analysis of Ni-based superalloys

The objective of this work is to correlate the mechanical properties of the Ni-based superalloy MAR M246(Hf) used in the Space Shuttle Main Engine with its structural characteristics by systematic study of optical photomicrographs and differential thermal analysis. The authors developed a method of predicting the liquidus and solidus temperature of various nickel based superalloys (MAR-M247, Waspaloy, Udimet-41, polycrystalline and single crystals of CMSX-2 and CMSX-3) and comparing the predictions with the experimental differential thermal analysis (DTA) curves using Perkin-Elmer DTA 1700. The method of predicting these temperatures is based on the additive effect of the components dissolved in nickel. The results were compared with the experimental values.

Aggarwal, M. D.↗

Reduction of chromium in Ni-base superalloys through element substitution and rapid solidification processing

The reduction in the use of Cr in Ni base superalloys by the combined approaches of both elemental substitution and rapid solidification processing is studied. The elements Si, Zr, Y and Hf were chosen as potential partial substitutes for Cr in Waspaloy and IN 713LC sine their separate addition to other alloys has previously resulted in enhanced oxidation resistance. The roles of Cr and these replacement elements in determining the microstructure and properties are evaluated. The elements Si, Zr, and Y and Hf are used as partial replacements for Cr in the base superalloys and these resultant alloys are processed using rapid solidification techniques. The mechanical properties and oxidation resistance of the processed materials are evaluated. The microstructure is characterized using state of the art techniques (e.g. analytical transmission electron microscopy), and the mechanism by which these structures are produced is determined.

Fraser, H. D.↗

The detrimental effect of elemental contaminants when using B additions to improve the creep properties of a Ni-based superalloy

The effect of Si contamination when using B to improve the creep properties of a Ni-based superalloy was investigated using advanced characterization techniques and first-principles simulations on alloys with high and low B levels with varying Si contents. The positive effect of B segregation along grain boundaries on the creep properties was mitigated by the presence of Si which showed a similar segregation preference. Density functional theory calculations were used for validation by calculating grain boundary cleavage energies. Silicon was shown to decrease grain boundary cohesion which offsets the positive effect of B.

36 MATERIALS SCIENCE↗