At least 55 records · Page 3

Burner rig hot corrosion of silicon carbide and silicon nitride

A number of commercially available SiC and Si3N4 materials were exposed to 1000 C for 40 h in a high-velocity, pressurized burner rig as a simulation of an aircraft turbine environment. Na impurities (2 ppm) added to the burner flame resulted in molten Na2SO4 deposition, attack of the SiC and Si3N4, and formation of substantial Na2O+x(SiO2) corrosion product. Room-temperature strength of the materials decreased as a result of the formation of corrosion pits in SiC and grain-boundary dissolution and pitting in Si3N4.

Fox, Dennis S.↗

Electron spectroscopy analysis

The Surface Science Laboratories at the University of Alabama in Huntsville (UAH) are equipped with x-ray photoelectron spectroscopy (XPS or ESCA) and Auger electron spectroscopy (AES) facilities. These techniques provide information from the uppermost atomic layers of a sample, and are thus truly surface sensitive. XPS provides both elemental and chemical state information without restriction on the type of material that can be analyzed. The sample is placed into an ultra high vacuum (UHV) chamber and irradiated with x-rays which cause the ejection of photoelectrons from the sample surface. Since x-rays do not normally cause charging problems or beam damage, XPS is applicable to a wide range of samples including metals, polymers, catalysts, and fibers. AES uses a beam of high energy electrons as a surface probe. Following electronic rearrangements within excited atoms by this probe, Auger electrons characteristic of each element present are emitted from the sample. The main advantage of electron induced AES is that the electron beam can be focused down to a small diameter and localized analysis can be carried out. On the rastering of this beam synchronously with a video display using established scanning electron microscopy techniques, physical images and chemical distribution maps of the surface can be produced. Thus very small features, such as electronic circuit elements or corrosion pits in metals, can be investigated. Facilities are available on both XPS and AES instruments for depth-profiling of materials, using a beam of argon ions to sputter away consecutive layers of material to reveal sub-surface (and even semi-bulk) analyses.

Gregory, John C.↗

Failure Analysis of a Helicopter External Fuel-Tank Pylon

An eight-inch-long (0.2 m) crack was found in an external fuel-tank pylon of a U.S. Coast Guard HH-60 helicopter. The damaged pylon was removed from service and destructively examined at NASA Langley Research Center (LaRC) to determine the cause of the crack. Results of the analysis revealed that crack initiation occurred at corrosion pits in a fastener hole and crack propagation was a result of cyclic loading.

Newman, John A.↗

Cyclic Oxidation and Hot Corrosion of NiCrY-Coated Disk Superalloys

Powder metallurgy disk superalloys have been designed for higher engine operating temperatures through improvement of their strength and creep resistance. Yet, increasing disk application temperatures to 704 degrees Centigrade and higher could enhance oxidation and activate hot corrosion in harmful environments. Protective coatings could be necessary to mitigate such attack. Cylindrical coated specimens of disk superalloys LSHR and ME3 were subjected to thermal cycling to produce cyclic oxidation in air at a maximum temperature of 760 degrees Centigrade. The effects of substrate roughness and coating thickness on coating integrity after cyclic oxidation were considered. Selected coated samples that had cyclic oxidation were then subjected to accelerated hot corrosion tests. This cyclic oxidation did not impair the coating's resistance to subsequent hot corrosion pitting attack.

protective coating↗

Molten salt corrosion of SiC: Pitting mechanism

Thin films of Na2SO4 and Na2CO3 at 1000 C lead to severe pitting of sintered alpha-SiC. These pits are important as they cause a strength reduction in this material. The growth of product layers is related to pit formation for the Na2CO3 case. The early reaction stages involve repeated oxidation and dissolution to form sodium silicate. This results in severe grain boundary attack. After this a porous silica layer forms between the sodium silicate melt and the SiC. The pores in this layer appear to act as paths for the melt to reach the SiC and create larger pits.

Jacobson, N. S.↗

Evaluation Of Corrosion-Resistant Alloys for Use in Acidic and Marine Launch Environments at NASA Kennedy Space Center: 20-Year Study

After the completion of an initial three-year study to qualify corrosion-resistant stainless steel tubing for use in NASA Kennedy Space Center’s acidic and marine launch environment, test specimens remained exposed at the KSC Beachside Atmospheric Corrosion Test Site for long-term exposure. NASA KSC’s lifetime requirement for most ground support equipment is twenty years. After twenty-one years of marine exposure, NASA KSC took the unique opportunity to reevaluate the tubing after long-term exposure to better understand the corrosion resistance of these alloys as they reached their expected lifetime requirement. Metallurgical and corrosion analysis was performed on the CRES tubing components and the alloys were rated on performance. A summary of CRES alloy tubing corrosion-related performance after 20 years of exposure in a marine launch environment is presented in this work.

NASA KSC↗

Stress-corrosion behavior of aluminum-lithium alloys in aqueous environments

The stress corrosion susceptibility of two powder metallurgy (P/M) alloys, Al-Li-Cu and Al-Li-Cu-Mg two mechanically attrited (M/A) alloys, Al-Li-Cu and Al-Li-Mg; and two wrought, ingot alloys, X-2020 and AA7475, are compared. Time-dependent fracture in an aqueous sodium chloride environment under alternate immersion condition was found to vary significantly between alloys. The stress corrosion behavior of the two powder metallurgy processed alloys was studied in detail under conditions of crack initiation, static crack growth, and fatigue crack growth. A variety of stress corrosion tests were performed including smooth surface, time-to-failure tests; potentiostatic tests on smooth surfaces exposed to constant applied strain rates; and fracture mechanics-type tests under static and cyclic loads. Both alloys show surface pitting and subsequent intergranular corrosion. Pitting is more severe in the magnesium-bearing alloy and is associated with stringer particles strung along the extrusion direction as a result of P/M processing.

Pizzo, P. P.↗

Stress-corrosion behavior of aluminum-lithium alloys in aqueous salt environments

The stress corrosion susceptibility of two powder metallurgy (P/M) alloys, Al-Li-Cu and Al-Li-Cu-Mg; two mechanically attrited (M/A) alloys, Al-Li-Cu and Al-Li-Mg; and two wrought, ingot alloys, X-2020 and AA7475, are compared. Time-dependent fracture in an aqueous sodium chloride environment under alternate immersion condition was found to vary significantly between alloys. The stress corrosion behavior of the two powder metallurgy processed alloys was studied in detail under conditions of crack initiation, static crack growth, and fatigue crack growth. A variety of stress corrosion tests were performed including smooth surface, time-to-failure tests; potentiostatic tests on smooth surfaces exposed to constant applied strain rates; and fracture mechanics-type tests under static and cyclic loads. Both alloys show surface pitting and subsequent intergranular corrosion. Pitting is more severe in the magnesium-bearing alloy and is associated with stringer particles strung along the extrusion direction as a result of P/M processing.

Pizzo, P. P.↗

An Engineering Look at Space Shuttle and ISS Operations

This slide presentation, in Spanish, is an overview of NASA's Space Shuttle operations and preparations for serving the International Space Station. There is information and or views of the shuttle's design, the propulsion system, the external tanks, the foam insulation, the reusable solid rocket motors, the vehicle assembly building (VAB), the mobile launcher platform being moved from the VAB to the launch pad. There is a presentation of some of the current issues with the space shuttle: cracks in the LH2 flow lines, corrosion and pitting, the thermal protection system, and inspection of the thermal protection system while in orbit. The shuttle system has served for more than 20 years, it is still a challenge to re-certify the vehicles for flight. Materials and material science remain as chief concerns for the shuttle,

Hernandez, Jose M.↗

Electrochemical, Polarization, and Crevice Corrosion Testing of Nitinol 60, A Supplement to the ECLSS Sustaining Materials Compatibility Study

In earlier trials, electrochemical test results were presented for six noble metals evaluated in test solutions representative of waste liquids processed in the Environmental Control and Life Support System (ECLSS) aboard the International Space Station (ISS). Subsequently, a seventh metal, Nitinol 60, was added for evaluation and subjected to the same test routines, data analysis, and theoretical methodologies. The previous six test metals included three titanium grades, (commercially pure, 6Al-4V alloy and 6Al-4V low interstitial alloy), two nickel-chromium alloys (Inconel(RegisteredTrademark) 625 and Hastelloy(RegisteredTrademark) C276), and one high-tier stainless steel (Cronidur(RegisteredTrademark) 30). The three titanium alloys gave the best results of all the metals, indicating superior corrosive nobility and galvanic protection properties. For this current effort, the results have clearly shown that Nitinol 60 is almost as noble as titanium, being very corrosion-resistant and galvanically compatible with the other six metals electrochemically and during long-term exposure. is also quite noble as it is very corrosion resistant and galvanically compatible with the other six metals from both an electrochemical perspective and long-term crevice corrosion scenario. This was clearly demonstrated utilizing the same techniques for linear, Tafel and cyclic polarization, and galvanic coupling of the metal candidate as was done for the previous study. The high nobility and low corrosion susceptibility for Nitinol 60 appear to be intermediate to the nickel/chromium alloys and the titanium metals with indications that are more reflective of the titanium metals in terms of general corrosion and pitting behavior.

Lee, R. E.↗

Controlled-Release Microcapsules for Smart Coatings for Corrosion Applications

Corrosion is a serious problem that has enormous costs and serious safety implications. Localized corrosion, such as pitting, is very dangerous and can cause catastrophic failures. The NASA Corrosion Technology Laboratory at Kennedy Space Center is developing a smart coating based on pH-sensitive microcapsules for corrosion applications. These versatile microcapsules are designed to be incorporated into a smart coating and deliver their core content when corrosion starts. Corrosion indication was the first function incorporated into the microcapsules. Current efforts are focused on incorporating the corrosion inhibition function through the encapsulation of corrosion inhibitors into water core and oil core microcapsules. Scanning electron microscopy (SEM) images of encapsulated corrosion inhibitors are shown.

Source record↗

PH and Electrochemical Responsive Materials for Corrosion Smart Coating Applications

Corrosion is a costly issue for military operations and civil industries. While most corrosion initiates from localized corrosion form, such as pitting, failure directly caused by localized corrosion is the most dangerous kind, because it is difficult to anticipate and prevent, occurs very suddenly and can be catastrophic. One way of preventing these failures is with a coating that can detect and heal localized corrosion. pH and other electrochemical changes are often associated with localized corrosion, so it is expected that materials that are pH or otherwise electrochemical responsive can be used to detect and control corrosion. This paper will review various pH and electrochemical responsive materials and their potential applications in corrosion smart coatings. Current research results in this field will also be reported.

Li, Wenyan↗

Corrosion study of bare and coated stainless steel

A program was conducted at Kennedy Space Center from February 1968 to February 1971 to evaluate the performance of austenitic stainless steel alloys used in fluid systems lines. For several years, there had been numerous failures of stainless steel hardware caused by pitting and stress corrosion cracking. Several alloys were evaluated for effectiveness of certain sacrificial-type protective coverings in preventing corrosion failures. Samples were tested in specially designed racks placed 91 meters (100 yards) above high-tide line at Cape Kennedy. It is concluded that: (1) unprotected tubing samples showed evidence of pitting initiation after 2 weeks; (2) although some alloys develop larger pits than others, it is probable that the actual pitting rate is independent of alloy type; (3) the deepest pitting occurred in the sheltered part of the samples; and (4) zinc-rich coatings and an aluminum-filled coating have afforded sacrificial protection against pitting for at least 28 months. It is believed that a much longer effective coating life can be expected.

Morrison, J. D.↗

An evaluation of microbial growth and corrosion of 316L SS in glycol/seawater mixtures

Glycol/seawater mixtures containing > 50% glycol inhibit corrosion of 316L stainless steel and do not support bacterial growth. The results indicate bacteria are able to use low concentrations of glycol (10%) as a growth medium, but bacterial growth decreased with increasing glycol concentration. Pitting potential, determined by anodic polarization, was used to evaluate susceptibility of 316L SS to corrosion in seawater-contaminated glycol. Mixture containing a minimum concentration of 50% propylene glycol-based coolant inhibited pitting corrosion. A slightly higher minimum concentration (55%) was needed for corrosion protection in ethylene glycol mixtures.

Biofilms/growth & development↗

Hot corrosion attack and strength degradation of SiC and Si(sub)3N(sub)4

Thin films of Na2SO4 and Na2CO3 molten salt deposits were used to corrode sintered SiC and Si3N4 at 1000 C. The resulting attack produced pitting and grain boundary etching resulting in strength decreases ranging from 15 to 50 percent. Corrosion pits were the predominant sources of fracture. The degree of strength decrease was found to be roughly correlated with the depth of the pit, as predicted from fracture toughness considerations. Gas evolution and bubble formation were key aspects of pit formation. Many of the observations of furnace exposures held true in a more realistic burner rig test.

Smialek, James L.↗

Long term storage test of titanium material with liquid fluorine propellant

The compatibility of 6AL-4V Ti with propellant grade GF2 and LF2 at 77 K for up to 3 years was investigated. Titanium double coupons, annealed or heat treated, with 16 or 64 RMS finishes, were immersed in F2 in individual Pyrex capsules and stored under LN2 for 29 and 39 months. Pre and post immersion tests were performed on the propellant and coupons. Chemical analysis of the propellant did not reveal any significant changes due to titanium corrosion. Gravimetric, visual, microscopic, and metallurgical examination with pitting analysis did not reveal gross corrosion of the titanium although pitting appears to be greater after 39 months exposure. The increase in pit size and number raises the possibility of unpredictable crack propagation instability. Fracture toughness tests are necessary to define this possibility.

Denson, J. R.↗

Hot Corrosion of Single-Crystal NiAl-X Alloys

Several single-crystal NiAl-X alloys (X=Hf, Ti, Cr, Ga) underwent hot corrosion testing in a Mach 0.3 burner rig at 900 deg. C for 300 1-hr cycles. The surface morphology after testing consisted of either mounds or an inward, uniform-type of attack which preserved surface features. It was observed that the surface morphology was affected by the surface preparation treatments. Microstructurally, the hot corrosion attack initiated as pits but evolved to a rampant attack consisting of the rapid inward growth of Al2O3. Electropolishing and chemical milling produced many pits and grooves on the surface. However, the presence of pits and grooves did not appear to strongly influence the hot corrosion response. Attack on many samples was strongly localized which was attributed to compositional inhomogeneity within the samples. It was found that increasing the Ti content from 1% to 5 % degraded the hot corrosion response of these alloys. In contrast, the addition of 1-2% Cr reduced the susceptibility of these alloys to hot corrosion attack and negated the deleterious effect of the 4-5% Ti addition.

Nesbitt, James A.↗

Material Selection Considerations for Solar Ponds

Among the various candidate materials tested, stainless steel shows the best potential for applications as heat exchanger components in solar ponds. Even stainless steel may lead to pitting type of corrosion. Weight loss measurements are probably unsatisfactory for corrosion evaluation in solar pond situations. Also included are the results from the potentiodynamic anodic polarization analysis, corrosion rate calculation via corrosion behavior diagrams, and immersion weight loss measurements.

Sastri, S.↗