Power factor improvement in hydrothermally synthesized Bi{sub 2-x}Sb{sub x}Te{sub 3} (x=1.5) - carbon sphere composites
We report fabrication of compacted Bi{sub 0.5}Sb{sub 1.5}Te{sub 3} composites by adding 1 wt% of carbon spheres in the hydrothermal synthesis. The processing parameter of sintering temperature is investigated in order to optimize the thermoelectric power factor of pressed Bi{sub 0.5}Sb{sub 1.5}Te{sub 3} composites. As a result, we find that the composite sintered at 360 Degree-Sign C shows the best power factor performance among the composites and has a largest power factor of 15.4 {mu}W/cm K{sup 2} at 205 K and 13.5 {mu}W/cm K{sup 2} at 290 K. When compared with the samples without addition of carbon sphere in the hydrothermal synthesis, the composites sintered at 340 Degree-Sign C and 360 Degree-Sign C both surpass the largest power factor of 12.1 {mu}W/cm K{sup 2} at 280 K and 11.9 {mu}W/cm K{sup 2} at 290 K for the 340 Degree-Sign C-sintered counterpart. - Graphical abstract: Compacted Bi{sub 0.5}Sb{sub 1.5}Te{sub 3-{delta}} composites obtained by adding 1 wt% of carbon spheres in the hydrothermal synthesis. The composites sintered at 340 Degree-Sign C and 360 Degree-Sign C both surpass the largest power factor of 12.1 {mu}W/cm K{sup 2} at 280 K and 11.9 {mu}W/cm K{sup 2} at 290 K for the 340 Degree-Sign C-sintered counterpart. Highlights: Black-Right-Pointing-Pointer Fabrication of Bi{sub 0.5}Sb{sub 1.5}Te{sub 3-{delta}} composites. Black-Right-Pointing-Pointer Addition of 1 wt% carbon spheres in the hydrothermal synthesis. Black-Right-Pointing-Pointer Investigation of sintering temperature using encapsulating-and-sintering techniques. Black-Right-Pointing-Pointer 360 Degree-Sign C-sintered composite showing the largest power factor of 15.4 {mu}W/cm K{sup 2} at 205 K. Black-Right-Pointing-Pointer 10-60% improvement over the counterpart without adding carbon spheres.