Search NASA⌕ Search

SEARCH · Search NASA

Results for “Polystyrene”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

Microspheres for laser velocimetry in high temperature wind tunnel

The introduction of non-intrusive measurement techniques in wind tunnel experimentation has been a turning point in error free data acquisition. Laser velocimetry has been progressively implemented and utilized in various wind tunnels; e.g. subsonic, transonic, and supersonic. The success of the laser velocimeter technique is based on an accurate measurement of scattered light by seeding particles introduced into the flow stream in the wind tunnel. Therefore, application of appropriate seeding particles will affect, to a large extent the acquired data. The seeding material used depends on the type of experiment being run. Among the seeding material for subsonic tunnel are kerosene, Kaolin, and polystyrene. Polystyrene is known to be the best because of being solid particles, having high index of refraction, capable of being made both spherical and monodisperse. However for high temperature wind tunnel testing seeding material must have an additional characteristic that is high melting point. Typically metal oxide powders such as Al2O3 with melting point 3660 F are used. The metal oxides are, however polydispersed, have a high density, and a tendency to form large agglomerate that does not closely follow the flow velocity. The addition of flame phase silica to metal oxide helps to break up the agglomerates, yet still results in a narrow band of polydispersed seeding. The less desirable utility of metal oxide in high temperature wind tunnels necessitates the search for a better alternative particle seeding which this paper addresses. The Laser Velocimetry (LV) characteristic of polystyrene makes it a prime candidate as a base material in achieving the high temperature particle seeding inexpensively. While polystyrene monodisperse seeding particle reported has been successful in a subsonic wind tunnel, it lacks the high melting point and thus is not practically usable in a high temperature wind tunnel. It is well known that rise in melting point of polystyrene can be achieved by a cross-linking technique. Since polystyrene already possesses all the desired characteristics for LV, to circumvent the low melting point, a cross-linking technique was investigated.

Ghorieshi, Anthony↗

Method of Making Dye-Doped Polystyre Microparticles

Various embodiments provide dye-doped polystyrene microspheres generated using dispersion polymerization. Polystyrene microspheres may be doped with fluorescent dyes, such as xanthene derivatives including kiton red 620 (KR620), using dispersion polymerization. Certain functionalities, such as sodium styrene sulfonate, may be used to shift the equilibrium distribution of dye molecules to favor incorporation of the dye into the particles. Polyelectrolyte materials, such as poly(diallyldimethyl ammonium chloride), PolyDADMAC, may be used to electrostatically trap and bind dye molecules within the particles. A buffer may be used to stabilize the pH change of the solution during dye-doped polystyrene microsphere generation and the buffer may be selected depending on the pKa of the dye being incorporated. The various embodiments may provide dye-doped polystyrene microspheres, such as KR620-doped polystyrene microspheres that are non-toxic and non-carcinogenic. These non-toxic and non-carcinogenic dye-doped polystyrene microspheres may be suitable for use in wind tunnel testing.

Wohl, Jr., Christopher J.↗

Ceramic Spheres From Cation Exchange Beads

Porous ZrO2 and hollow TiO2 spheres were synthesized from a strong acid cation exchange resin. Spherical cation exchange beads, polystyrene based polymer, were used as a morphological-directing template. Aqueous ion exchange reaction was used to chemically bind (ZrO)(2+) ions to the polystyrene structure. The pyrolysis of the polystyrene at 600 C produces porous ZrO2 spheres with a surface area of 24 sq m/g with a mean sphere size of 42 microns. Hollow TiO2 spheres were synthesized by using the beads as a micro-reactor. A direct surface reaction - between titanium isopropoxide and the resin beads forms a hydrous TiO2 shell around the polystyrene core. The pyrolysis of the polystyrene core at 600 C produces hollow anatase spheres with a surface area of 42 sq m/g with a mean sphere size of 38 microns. The formation of ceramic spheres was studied by XRD, SEM and B.E.T. nitrogen adsorption measurements.

Dynys, F. W.↗

Migration of lymphocytes on fibronectin-coated surfaces: temporal evolution of migratory parameters

Lymphocytes typically interact with implanted biomaterials through adsorbed exogenous proteins. To provide a more complete characterization of these interactions, analysis of lymphocyte migration on adsorbed extracellular matrix proteins must accompany the commonly performed adhesion studies. We report here a comparison of the migratory and adhesion behavior of Jurkat cells (a T lymphoblastoid cell line) on tissue culture treated and untreated polystyrene surfaces coated with various concentrations of fibronectin. The average speed of cell locomotion showed a biphasic response to substrate adhesiveness for cells migrating on untreated polystyrene and a monotonic decrease for cells migrating on tissue culture-treated polystyrene. A modified approach to the persistent random walk model was implemented to determine the time dependence of cell migration parameters. The random motility coefficient showed significant increases with time when cells migrated on tissue culture-treated polystyrene surfaces, while it remained relatively constant for experiments with untreated polystyrene plates. Finally, a cell migration computer model was developed to verify our modified persistent random walk analysis. Simulation results suggest that our experimental data were consistent with temporally increasing random motility coefficients.

NASA Program Fundamental Space Biology↗

Development and Evaluation of Elastomeric Materials for Geothermal Applications

A material was formulated having about 250-350 psi tensile strength and 30-80 percent elongation at 260 C for at least 24 hours in simulated brine. The relationship between these laboratory test results and sealing performance in actual or simulated test conditions is not entirely clear; however, it is believed that no conventional formation or casing packer design is likely to perform well using these materials. The synthetic effort focused on high temperature block copolymers and development of curable polystyrene. Procedures were worked out for synthesizing these new materials. Initial results with heat-cured unfilled polystyrene 'gum' at 260 C indicate a tensile strength of about 50 psi. Cast films of the first sample of polyphenyl quinoxaline-polystyrene block copolymer, which has 'graft-block' structure consisting of a polystyrene chain with pendant polyphenyl quinoxaline groups, show elastomeric behavior in the required temperature range. Its tensile strength and elongation at 260 C were 220-350 psi and 18-36 percent, respectively. All of these materials also showed satisfactory hydrolytic stability.

Mueller, W. A.↗

Imidazolium-Based Polymeric Materials as Alkaline Anion-Exchange Fuel Cell Membranes

Polymer electrolyte membranes that conduct hydroxide ions have potential use in fuel cells. A variety of polystyrene-based quaternary ammonium hydroxides have been reported as anion exchange fuel cell membranes. However, the hydrolytic stability and conductivity of the commercially available membranes are not adequate to meet the requirements of fuel cell applications. When compared with commercially available membranes, polystyrene-imidazolium alkaline membrane electrolytes are more stable and more highly conducting. At the time of this reporting, this has been the first such usage for imidazolium-based polymeric materials for fuel cells. Imidazolium salts are known to be electrochemically stable over wide potential ranges. By controlling the relative ratio of imidazolium groups in polystyrene-imidazolium salts, their physiochemical properties could be modulated. Alkaline anion exchange membranes based on polystyrene-imidazolium hydroxide materials have been developed. The first step was to synthesize the poly(styrene-co-(1-((4-vinyl)methyl)-3- methylimidazolium) chloride through a free-radical polymerization. Casting of this material followed by in situ treatment of the membranes with sodium hydroxide solutions provided the corresponding hydroxide salts. Various ratios of the monomers 4-chloromoethylvinylbenzine (CMVB) and vinylbenzine (VB) provided various compositions of the polymer. The preferred material, due to the relative ease of casting the film, and its relatively low hygroscopic nature, was a 2:1 ratio of CMVB to VB. Testing confirmed that at room temperature, the new membranes outperformed commercially available membranes by a large margin. With fuel cells now in use at NASA and in transportation, and with defense potential, any improvement to fuel cell efficiency is a significant development.

Narayan, Sri R.↗

Emission spectra and kinetics of copolymer films of styrene and 2,3,4,5,6-pentafluorostyrene

The temperature-dependent steady-state emission spectra and fluorescence kinetics of copolymer films of styrene and 2,3,4,5,6-pentafluorostyrene are reported. The polystyrene excimer emission is efficiently quenched in the presence of relatively small amounts of the pentafluorophenyl quencher in spite of the fact that direct energy transfer from the excimer to the quencher chromophores is not possible. The quenching of the polystyrene excimer emission at room temperature and of the polystyrene monomer emission at 13 K is attributed to the interception of the migrating monomer excitation by the quencher. The data suggest that this quenching mechanism is independent of temperature.

O'Connor, Donald B.↗

Organometallic Polymeric Conductors

For aerospace applications, the use of polymers can result in tremendous weight savings over metals. Suitable polymeric materials for some applications like EMI shielding, spacecraft grounding, and charge dissipation must combine high electrical conductivity with long-term environmental stability, good processability, and good mechanical properties. Recently, other investigators have reported hybrid films made from an electrically conductive polymer combined with insulating polymers. In all of these instances, the films were prepared by infiltrating an insulating polymer with a precursor for a conductive polymer (either polypyrrole or polythiophene), and oxidatively polymerizing the precursor in situ. The resulting composite films have good electrical conductivity, while overcoming the brittleness inherent in most conductive polymers. The highest conductivities reported (approximately 4/Scm) were achieved with polythiophene in a polystyrene host polymer. The best films using a polyamide as base polymer were four orders of magnitude less conductive than the polystyrene films. The authors suggested that this was because polyimides were unable to swell sufficiently for infiltration of monomer as in the polystyrene. It was not clear, however, if the different conductivities obtained were merely the result of differing oxidation conditions. Oxidation time, temperature and oxidant concentration varied widely among the studies.

Source record↗

Ultrasonic wave velocity measurement in small polymeric and cortical bone specimens

A system was refined for the determination of the bulk ultrasonic wave propagation velocity in small cortical bone specimens. Longitudinal and shear wave propagations were measured using ceramic, piezoelectric 20 and 5 MHz transducers, respectively. Results of the pulse transmission technique were refined via the measurement of the system delay time. The precision and accuracy of the system were quantified using small specimens of polyoxymethylene, polystyrene-butadiene, and high-density polyethylene. These polymeric materials had known acoustic properties, similarity of propagation velocities to cortical bone, and minimal sample inhomogeneity. Dependence of longitudinal and transverse specimen dimensions upon propagation times was quantified. To confirm the consistency of longitudinal wave propagation in small cortical bone specimens (< 1.0 mm), cut-down specimens were prepared from a normal rat femur. Finally, cortical samples were prepared from each of ten normal rat femora, and Young's moduli (Eii), shear moduli (Gij), and Poisson ratios (Vij) were measured. For all specimens (bone, polyoxymethylene, polystyrene-butadiene, and high-density polyethylene), strong linear correlations (R2 > 0.997) were maintained between propagation time and distance throughout the size ranges down to less than 0.4 mm. Results for polyoxymethylene, polystyrene-butadiene, and high-density polyethylene were accurate to within 5 percent of reported literature values. Measurement repeatability (precision) improved with an increase in the wave transmission distance (propagating dimension). No statistically significant effect due to the transverse dimension was detected.

Non-NASA Center↗

Microcraters formed in glass by low density projectiles

Microcraters were produced in soda-lime glass by the impact of low density projectiles of polystyrene (p = 1.06 g/cu cm) with masses between 0.7 and 62 picograms and velocities between 2 and 14 km/s. The morphology of the craters depended on the velocity and the angle of incidence of the projectiles and these are discussed in detail. It was found that the transitions in morphology of the craters formed by polystyrene spheres occurred at higher velocities than they did for more dense projectiles.

Mandeville, J.-C.↗

Microcraters formed in glass by low density projectiles

Microcraters were produced in soda-lime glass by the impact of low density projectiles of polystyrene with masses between 0.7 and 62 picograms and velocities between 2 and 14 kilometers per second. The morphology of the craters depends on the velocity and angle of incidence of the projectiles. The transitions in morphology of the craters formed by polystyrene spheres occur at higher velocities than they do for more dense projectiles. For oblique impact, the craters are elongated and shallow with the spallation threshold occuring at higher velocity. For normal incidence, the total displaced mass of the target material per unit of projectile kinetic energy increases slowly with the energy.

Mandeville, J.-C.↗

Polymer-gas reactions (air pollutants: NO2 and SO2) as function of pressure, UV light, temperature, and morphology: A survey

Reactions of various polymers, such as polystyrene and its stereo-specific isomers, butylrubber, nylon, etc., with nitrogen dioxide and sulfur-dioxide were studied over the past few years. More recently, work has been initiated on the influence of polymer morphology on degradation of polymers in presence of these gases, near UV radiation and oxygen. Unexpected effects have been observed during chain scission near room temperature. Thus, for instance, isotactic polystyrene of various crystallinities, as far as extent and type are concerned, show marked differences in their degradation characteristics. Thus, for instance, crystalline polymers show faster degradation than amorphous ones, which seems to be contrary to expectations. However, this phenomenon can be explained in quite a consistent manner. The importance of all these reactions in connection with air pollution is briefly discussed.

Jellinek, H. H. G.↗

Electrophoresis demonstration on Apollo 16

Free fluid electrophoresis, a process used to separate particulate species according to surface charge, size, or shape was suggested as a promising technique to utilize the near zero gravity condition of space. Fluid electrophoresis on earth is disturbed by gravity-induced thermal convection and sedimentation. An apparatus was developed to demonstrate the principle and possible problems of electrophoresis on Apollo 14 and the separation boundary between red and blue dye was photographed in space. The basic operating elements of the Apollo 14 unit were used for a second flight demonstration on Apollo 16. Polystyrene latex particles of two different sizes were used to simulate the electrophoresis of large biological particles. The particle bands in space were extremely stable compared to ground operation because convection in the fluid was negligible. Electrophoresis of the polystyrene latex particle groups according to size was accomplished although electro-osmosis in the flight apparatus prevented the clear separation of two particle bands.

Snyder, R. S.↗

Concentration-response data on toxicity of pyrolysis gases from six synthetic polymers

Concentration-response data are presented on the toxic effects of the pyrolysis gases from six synthetic polymers on Swiss Webster male mice, using a toxicity screening test method. The polymers consisted of one sample each of polycarbonate and polystyrene, and two samples each of polyethylene and acrylonitrile-butadiene-styrene (ABS). All six samples were evaluated using the rising temperature program, and three samples were evaluated using the fixed temperature program. The pyrolysis gases from polycarbonate, polyethylene, and ABS appeared to exhibit the concentration-response relationships commonly encountered in toxicology. The polystyrene sample gave variable results; probably due to poor reproducibility of the essentially anaerobic pyrolysis. Carbon monoxide seemed to be the principal toxicant in the pyrolysis gases from polycarbonate and polyethylene, but did not appear to be the principal toxicant in the pyrolysis gases from ABS.

Hilado, C. J.↗

Toxicity of pyrolysis gases from some cellular polymers

Various samples of cellular polymers were evaluated for toxicity of pyrolysis gases, using the screening test method developed at the University of San Francisco. The cellular polymer samples included polyimide, polymethacrylimide, polybismaleimide, polyurethane, polyisocyanurate, polyethylene, polychloroprene, polyvinyl chloride, polystyrene, polysiloxane, and polyphosphazene. The cellular polymers exhibited varying levels of toxicity under these test conditions. Among the rigid cellular polymers, times to death were shortest with the imide type foams and longest with polyvinyl chloride and polystyrene. Among the flexible cellular polymers, times to death were shortest with polyimide and polyester, and longest with polychloroprene and polysiloxane. Increased char yield was not necessarily associated with reduced toxicity.

Hilado, C. J.↗

Toxicity of pyrolysis gases from some synthetic polymers

Nine samples of synthetic polymers were evaluated for toxicity of pyrolysis gases, using the toxicity screening test method developed at the University of San Francisco. The materials were polyoxymethylene, polyethylene (five samples), polypropylene, polymethyl methacrylate, and polystyrene. Of the five polyethylene samples, three contained known levels of chlorine. These test results were combined with earlier data to provide a comparison of 25 samples of synthetic polymers. Polyoxymethylene appeared to exhibit the greatest toxicity, and polystyrene the least toxicity, under these particular test conditions

Hilado, C. J.↗

Deuteron NMR (Nuclear Magnetic Resonance) in relation to the glass transition in polymers

H-2NMR is introduced as a tool for investigating slow molecular motion in the glass transition region of amorphous polymers. In particular, we compare H-2 spin alignment echo spectra of chain deuterated polystyrene with model calculations for restricted rotational Brownian motion. Molecular motion in the polyztyrene-toluene system has been investigated by analyzing H-2NMR of partially deuterated polystyrene and toluene, respectively. The diluent mobility in the mixed glass has been decomposed into solid and liquid components where the respective average correlation times differ by more than 5 decades.

Roessler, E.↗