Search NASA⌕ Search

SEARCH · Search NASA

Results for “SOLDERING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

Age-aware solder performance models : level 2 milestone completion.

Legislated requirements and industry standards are replacing eutectic lead-tin (Pb-Sn) solders with lead-free (Pb-free) solders in future component designs and in replacements and retrofits. Since Pb-free solders have not yet seen service for long periods, their long-term behavior is poorly characterized. Because understanding the reliability of Pb-free solders is critical to supporting the next generation of circuit board designs, it is imperative that we develop, validate and exercise a solder lifetime model that can capture the thermomechanical response of Pb-free solder joints in stockpile components. To this end, an ASC Level 2 milestone was identified for fiscal year 2010: Milestone 3605: Utilize experimentally validated constitutive model for lead-free solder to simulate aging and reliability of solder joints in stockpile components. This report documents the completion of this milestone, including evidence that the milestone completion criteria were met and a summary of the milestone Program Review.

36 MATERIALS SCIENCE↗

Soldering Tested in Reduced Gravity

Whether used occasionally for contingency repair or routinely in nominal repair operations, soldering will become increasingly important to the success of future long-duration human space missions. As a result, it will be critical to have a thorough understanding of the service characteristics of solder joints produced in reduced-gravity environments. The National Center for Space Exploration Research (via the Research for Design program), the NASA Glenn Research Center, and the NASA Johnson Space Center are conducting an experimental program to explore the influence of reduced gravity environments on the soldering process. Solder joint characteristics that are being considered include solder fillet geometry, porosity, and microstructural features. Both through-hole (see the drawing and image on the preceding figure) and surface-mounted devices are being investigated. This effort (the low-gravity portion being conducted on NASA s KC-135 research aircraft) uses the soldering hardware currently available on the International Space Station. The experiment involves manual soldering by a contingent of test operators, including both highly skilled technicians and less skilled individuals to provide a skill mix that might be encountered in space mission crews. The experiment uses both flux-cored solder and solid-core solder with an externally applied flux. Other experimental parameters include the type of flux, gravitational level (nominally zero,

Struk, Peter M.↗

Study on the Reliability of Carbon Nanotube-Reinforced Sn-58Bi Lead-Free Solder Joints

The wettability, microstructure and mechanical properties of multi-walled carbon nanotube (CNT)-reinforced Sn-58Bi composite solder joints were investigated. The results indicate that the wettability of the Sn-58Bi solder is improved and the growth of interfacial intermetallic (IMC) compounds for solder joints is restrained by CNTs. The thickness of the IMC layers is decreased with increasing CNTs concentration. The microstructure of the Sn-58Bi composite solders is refined, the maximum tensile strength and shear strength are obtained by adding the optimum CNTs content about 0.01 wt.%. However, excessive content of CNTs addition can deteriorate the properties. The creep rupture life of Sn-58Bi solder joint and Sn-58Bi-0.01CNTs solder joint is decreased with increasing load, temperature and current density. The average creep rupture life of Sn-58Bi-0.01CNTs composite solder joint is 60% higher than that of the plain solder joint.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Microstructural development and mechanical properties of a near-eutectic directionally solidified Sn–Bi solder alloy

Sn–Bi solders may be applied for electronic applications where low-temperature soldering is required, i.e., sensitive components, step soldering and soldering LEDs. In spite of their potential to cover such applications, the mechanical response of soldered joints of Sn–Bi alloys in some cases does not meet the strength requirements due to inappropriate resulting microstructures. Hence, careful examination and control of as-soldered microstructures become necessary with a view to pre-programming reliable final properties. The present study aims to investigate the effects of solidification thermal parameters (growth rate — V{sub L} and cooling rate — T-dot{sub L}) on the microstructure of the Sn–52 wt.%Bi solder solidified under unsteady-state conditions. Samples were obtained by upward directional solidification (DS), followed by characterization through metallography and scanning electron microscopy (SEM). The microstructures are shown to be formed by Sn-rich dendrites decorated with Bi precipitates surrounded by a complex regular eutectic mixture, with alternated Bi-rich and Sn-rich phases. Experimental correlations of primary (λ{sub 1}), secondary (λ{sub 2}), tertiary (λ{sub 3}) dendritic and eutectic spacings (λ{sub coarse} and λ{sub fine}) with cooling rate and growth rate are established. Two ranges of lamellar eutectic sizes were determined, described by two experimental equations λ = 1.1 V{sub L}{sup −1/2} and λ = 0.67 V{sub L}{sup −1/2}. The onset of tertiary branches within the dendritic array along the Sn–52 wt.%Bi alloy DS casting is shown to occur for cooling rates lower than 1.5 °C/s. - Highlights: • The Sn–52 wt.%Bi solder was shown to have two eutectic sizes. • The fishbone eutectic is preferably located adjacent to the Bi-rich lamellar phases. • The onset of tertiary dendritic branches in Sn–Bi is associated with T-dot{sub L} < 1.5 °C/s. • Higher eutectic fraction and λ{sub 3} provoked a reverse increase in σ{sub u} and σ{sub y}.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

A novel interface strengthening layer: Nanoscale AuCu super-structure formed during Au80Sn20/Cu rapid solidification soldering process

Highlights: • The nanoscale AuCu super-structure formed in Au80Sn20/Cu soldering joint. • The phase-transformation diffusion mechanism of Au80Sn20/Cu soldering process was studied. • The orientation relationship of Au80Sn20/Cu intermetallic compounds was investigated. • The interfacial strengthening mechanism of nanoscale AuCu layer was discussed. - Abstract: Phase composition and orientation of intermetallic compounds layers determine the functional and mechanical properties of solder joints. In this paper, interfacial reaction and strengthening mechanism of Au80Sn20/Cu joint by rapid solidification reflow soldering were studied. The Au80Sn20/Cu solder joint by rapid solidification reflow soldering exhibit a superior shear property, and the shear strength reaches up to 90 MPa. It is found that a new nanoscale AuCu super-structure formed in the interfacial intermetallic compounds layer, which is coherent with the [001] Cu substrate. The orientation relationship of Cu matrix/interfacial intermetallic compounds is determined to be [001]{sub Cu}∥[001]{sub AuCu}∥[ 2-bar 4 2-bar 3]{sub (AuCu){sub 5Sn}} and (200){sub Cu}∥(200){sub AuCu}∥(10 1-bar 0){sub (AuCu){sub 5Sn}}. Nanoscale AuCu super-structure influences the interface slip direction and provides interface misfit dislocation, hinder the dislocation movement, lead to the interface strengthening effect. Our finding on nanoscale AuCu super-structure formed during Au80Sn20/Cu soldering process not only sheds light on future research direction but also provides practical guidance to the engineers in solder industry.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Activation Energy for Solder Bond Degradation: Thermal Cycling of Field-aged Modules at Multiple Upper Temperatures

The reliability of solder joints in the solar cell metallization-interconnect system influences the lifetime of photovoltaic modules. Two field-aged modules-one with Sn 62 Pb 36 Ag 2 solder at the solder joints (Solarex MSX 60), and the other with the standard Sn 60 Pb 40 solder (Siemens M55)-were subjected to a modified thermal cycling (TC) test of IEC 61215. Three sections in each module were maintained at 85 degrees C, 95 degrees C, and 105 degrees C during the 15-minute high temperature dwell time. Current equivalent to the module short-circuit current was injected through the module when the chamber temperature was above 25 degrees C to simulate regular field operation. This novel approach aims to induce thermomechanical fatigue (TMF) at the solder joints and intermetallic compound (IMC) formation at the metal/solder interfaces. The activation energy (E a ) for solder bond degradation was calculated based on the series resistance (R s ) increase in TC testing rather than power drop to avoid the effect of confounding variables. Module-level R s increase in MSX 60 module after TC800 cycles and in M55 module after TC400 cycles was 1.22% and 183.7%, respectively. The E a determined for the module with 2wt% Ag is 0.24 eV and for that with the standard solder is 0.27 eV. The solder bond degradation seems to have been driven by TMF rather than IMC formation for both modules.

14 SOLAR ENERGY↗

Stability of molybdenum nanoparticles in Sn-3.8Ag-0.7Cu solder during multiple reflow and their influence on interfacial intermetallic compounds

This work investigates the effects of molybdenum nanoparticles on the growth of interfacial intermetallic compound between Sn-3.8Ag-0.7Cu solder and copper substrate during multiple reflow. Molybdenum nanoparticles were mixed with Sn-3.8Ag-0.7Cu solder paste by manual mixing. Solder samples were reflowed on a copper substrate in a 250 Degree-Sign C reflow oven up to six times. The molybdenum content of the bulk solder was determined by inductive coupled plasma-optical emission spectrometry. It is found that upon the addition of molybdenum nanoparticles to Sn-3.8Ag-0.7Cu solder, the interfacial intermetallic compound thickness and scallop diameter decreases under all reflow conditions. Molybdenum nanoparticles do not appear to dissolve or react with the solder. They tend to adsorb preferentially at the interface between solder and the intermetallic compound scallops. It is suggested that molybdenum nanoparticles impart their influence on the interfacial intermetallic compound as discrete particles. The intact, discrete nanoparticles, by absorbing preferentially at the interface, hinder the diffusion flux of the substrate and thereby suppress the intermetallic compound growth. - Highlights: Black-Right-Pointing-Pointer Mo nanoparticles do not dissolve or react with the SAC solder during reflow. Black-Right-Pointing-Pointer Addition of Mo nanoparticles results smaller IMC thickness and scallop diameter. Black-Right-Pointing-Pointer Mo nanoparticles influence the interfacial IMC through discrete particle effect.

36 MATERIALS SCIENCE↗

Microwave Tissue Soldering for Immediate Wound Closure

A novel approach for the immediate sealing of traumatic wounds is under development. A portable microwave generator and handheld antenna are used to seal wounds, binding the edges of the wound together using a biodegradable protein sealant or solder. This method could be used for repairing wounds in emergency settings, by restoring the wound surface to its original strength within minutes. This technique could also be utilized for surgical purposes involving solid visceral organs (i.e., liver, spleen, and kidney) that currently do not respond well to ordinary surgical procedures. A miniaturized microwave generator and a handheld antenna are used to deliver microwave energy to the protein solder, which is applied to the wound. The antenna can be of several alternative designs optimized for placement either in contact with or proximity to the protein solder covering the wound. In either case, optimization of the design includes the matching of impedances to maximize the energy delivered to the protein solder and wound at a chosen frequency. For certain applications, an antenna could be designed that would emit power only when it is in direct contact with the wound. The optimum frequency or frequencies for a specific application would depend on the required depth of penetration of the microwave energy. In fact, a computational simulation for each specific application could be performed, which would then match the characteristics of the antenna with the protein solder and tissue to best effect wound closure. An additional area of interest with potential benefit that remains to be validated is whether microwave energy can effectively kill bacteria in and around the wound. Thus, this may be an efficient method for simultaneously sterilizing and closing wounds. Using microwave energy to seal wounds has a number of advantages over lasers, which are currently in experimental use in some hospitals. Laser tissue welding is unsuitable for emergency use because its large, bulky equipment cannot be easily moved between operating rooms, let alone relocated to field sites where emergencies often occur. In addition, this approach is highly dependent on the uniformity and thickness of the protein solder as well as the surgeon s skills. In contrast, the use of microwave energy is highly tolerant of the thickness of the protein solder, level of fluids in and around the wound, and other parameters that can adversely affect the outcome of laser welding. However, controlling the depth of penetration of the microwave energy into the wound is critical for achieving effective wound sealing without damaging the adjacent tissue. In addition, microspheres that encapsulate metallic cores could also be incorporated into the protein solder to further control the depth of penetration of the microwave energy.

Arndt, G. Dickey↗

Joint Lead-Free Solder Test Program for High Reliability Military and Space Applications

Current and future space and defense systems face potential risks from the continued use of tin-lead solder, including: compliance with current environmental regulations, concerns about potential environmental legislation banning lead-containing products, reduced mission readiness, and component obsolescence with lead surface finishes. For example, the United States Environmental Protection Agency (USEPA) has lowered the Toxic Chemical Release reporting threshold for lead to 100 pounds. Overseas, the Waste Electrical and Electronic Equipment (WEEE) and the Restriction on Hazardous Substances (RoHS) Dicctives in Europe and similar mandates in Japan have instilled concern that a legislative body will prohibit the use of lead in aerospace/military electronics soldering. Any potential banning of lead compounds could reduce the supplier base and adversely affect the readiness of missions led by the National Aeronautics and Space Administration (NASA) and the U.S. Department of Defense (DoD). Before considering lead-free electronics for system upgrades or future designs, however, it is important for the DoD and NASA to know whether lead-free solders can meet their systems' requirements. No single lead-free solder is likely to qualify for all defense and space applications. Therefore, it is important to validate alternative solders for discrete applications. As a result of the need for comprehensive test data on the reliability of lead-free solders, a partnership was formed between the DoD, NASA, and several original equipment manufactures (OEMs) to conduct solder-joint reliability (laboratory) testing of three lead-free solder alloys on newly manufactured and reworked circuit cards to generate performance data for high-reliability (IPC Class 3) applications.

Brown, Christina↗

ESD Test Apparatus for Soldering Irons

ESDA (Electrostatic Discharge Association) ESD STM 13.1-2000 requires frequent testing of the voltage leakage from the tip of a soldering iron and the resistance from the tip of the soldering iron to the common point ground. Without this test apparatus, the process is time-consuming and requires several wires, alligator clips, or test probes, as well as additional equipment. Soldering iron tips must be tested for electrostatic discharge risks frequently, and this typically takes a lot of time in setup and testing. This device enables the operator to execute the full test in one minute or less. This innovation is a simple apparatus that plugs into a digital multimeter (DMM) and the Common Point Ground (CPG) reference. It enables the user to perform two of the electrostatic discharge tests required in ESD STM 13.1-2000. The device consists of a small black box with two prongs sticking out of one end, two inputs on the opposite end (one of the inputs is used to connect the reference CPG to the DMM), and a metal tab on one side. Inside the box are wires, several washers of various materials, and assembly hardware (nuts and screws/bolts). The device is a passive electronic component that is plugged into a DMM. The operator sets the DMM to read voltage. The operator places the heated tip of the soldering iron onto the metal tab with a small amount of solder to ensure a complete connection. The voltage is read and recorded. The operator switches the DMM to read resistance. The operator places the heated tip of the soldering iron onto the metal tab with a small amount of solder to ensure a complete connection. The resistance is recorded. If the recorded voltage and resistance are below a number stated in ESDA ESD STM 13.1-2000, the test is considered to pass. The device includes all the necessary wiring internal to its body so the operator does not need to do any independent wiring, except for grounding. It uses a stack of high-thermal-resistance washers to minimize the heat transfer from the soldering iron to the wiring used to measure the resistance and voltages. This minimizes thermal error. The device allows very rapid execution of a test that is performed frequently.

Sancho, Jose↗

Understanding the Reliability of Solder Joints Used in Advanced Structural and Electronics Applications: Part 2 - Reliability Performance.

Whether structural or electronic, all solder joints must provide the necessary level of reliability for the application. The Part 1 report examined the effects of filler metal properties and the soldering process on joint reliability. Filler metal solderability and mechanical properties, as well as the extents of base material dissolution and interface reaction that occur during the soldering process, were shown to affect reliability performance. The continuation of this discussion is presented in this Part 2 report, which highlights those factors that directly affect solder joint reliability. There is the growth of an intermetallic compound (IMC) reaction layer at the solder/base material interface by means of solid-state diffusion processes. In terms of mechanical response by the solder joint, fatigue remains as the foremost concern for long-term performance. Thermal mechanical fatigue (TMF), a form of low-cycle fatigue (LCF), occurs when temperature cycling is combined with mismatched values of the coefficient of thermal expansion (CTE) between materials comprising the solder joint “system.” Vibration environments give rise to high-cycle fatigue (HCF) degradation. Although accelerated aging studies provide valuable empirical data, too many variants of filler metals, base materials, joint geometries, and service environments are forcing design engineers to embrace computational modeling to predict the long-term reliability of solder joints.

42 ENGINEERING↗

Rapidly solidifying Pb-free Sn-Ag-Cu-Al or Sn-Cu-Al solder

A solder alloy includes Sn, optional Ag, Cu, and Al wherein the solder alloy composition together with the solder alloy superheat temperature and rapid cooling rate from the superheat temperature are controlled to provide a dispersion of fine hard Cu—Al intermetallic particles in an as-solidified solder alloy microstructure wherein the particles are retained even after multiple solder reflow cycles often used in modern electronic assembly procedures to provide a particle strengthening to the solder joint microstructure as well as exert a grain refining effect on the solder joint microstructure, providing a strong, impact- and thermal aging-resistant solder joint that has beneficial microstructural features and is substantially devoid of Ag3Sn blades.

36 MATERIALS SCIENCE↗

Effect of Ag3Sn nanoparticles and temperature on Cu6Sn5 IMC growth in Sn-xAg/Cu solder joints

Highlights: • The number density of Ag{sub 3}Sn grains precipitated upon Cu{sub 6}Sn{sub 5}, increases with Ag content and reflow temperature (T). • Raising of wt. % of Ag in solder and lowering of T can cause an increase in grain diameter of Ag{sub 3}Sn nanoparticles. • The blockading effect of Ag{sub 3}Sn particles on Cu{sub 6}Sn{sub 5} IMC growth is more pronounced in Sn-3Ag and Sn-3.5Ag alloys. • IMC suppressing nanoparticles can be utilized for solder materials design. - Abstract: The growing importance of Pb-free Sn-xAg solders and high cost of Ag has attracted the attention of researchers to perform experiment with solders with varied content of Ag element. In this study, Sn-xAg(0,1,2,3.5) solder balls on Cu substrate have been reflowed at 250/275/300 °C for 60 s and air cooled. Finite element method has been utilized to simulate the concentration and temperature during cooling. The experimental results suggest that the Cu flux through grain boundary diffusion is the dominant mechanism for Cu{sub 6}Sn{sub 5} intermetallic compound growth in Pure Sn and Sn-1Ag solders. When the Ag content is increased, as in case of Sn-3Ag and Sn-3.5Ag alloys; the shielding effect of Ag{sub 3}Sn nanoparticles is the determinant factor for affecting the thickness of Cu{sub 6}Sn{sub 5} IMC. Both Cu influx rate and shielding effect of Ag{sub 3}Sn nanoparticles are enhanced with the raise in pre-cooled isothermal reflow temperature. Sn-1Ag solder is observed to have the thickest Cu{sub 6}Sn{sub 5} IMC.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Comparison of Extensive Thermal Cycling Effects on Microstructure Development in Micro-alloyed Sn-Ag-Cu Solder Joints

Pb-free solder alloys based on the Sn-Ag-Cu (SAC) ternary eutectic have promise for widespread adoption across assembly conditions and operating environments, but enhanced microstructural control is needed. Micro-alloying with elements such as Zn was demonstrated for promoting a preferred solidification path and joint microstructure earlier in simple (Cu/Cu) solder joints studies for different cooling rates. This beneficial behavior now has been verified in reworked ball grid array (BGA) joints, using dissimilar SAC305 (Sn-3.0Ag-0.5Cu, wt.%) solder paste. After industrial assembly, BGA components joined with Sn-3.5Ag-0.74Cu-0.21Zn solder were tested in thermal cycling (-55 C/+125 C) along with baseline SAC305 BGA joints beyond 3000 cycles with continuous failure monitoring. Weibull analysis of the results demonstrated that BGA components joined with SAC + Zn/SAC305 have less joint integrity than SAC305 joints, but their lifetime is sufficient for severe applications in consumer, defense, and avionics electronic product field environments. Failure analysis of the BGA joints revealed that cracking did not deviate from the typical top area (BGA component side) of each joint, in spite of different Ag3Sn blade content. Thus, SAC + Zn solder has not shown any advantage over SAC305 solder in these thermal cycling trials, but other characteristics of SAC + Zn solder may make it more attractive for use across the full range of harsh conditions of avionics or defense applications.

36 MATERIALS SCIENCE↗

Development of Sn-Ag-Cu-X Solders for Electronic Assembly by Micro-Alloying with Al

Of Pb-free solder choices, an array of solder alloys based on the Sn-Ag-Cu (SAC) ternary eutectic (T eut = 217°C) composition have emerged with potential for broad use, including ball grid array (BGA) joints that cool slowly. This work investigated minor substitutional additions of Al (<0.25 wt.%) to Sn-3.5Ag-0.95Cu (SAC3595) solders to promote more consistent solder joint microstructures and to avoid deleterious product phases, e.g., Ag3Sn “blades,” for BGA cooling rates, since such Al additions to SAC had already demonstrated excellent thermal aging stability. Consistent with past work, blade formation was suppressed for increased Al content (>0.05Al), but the suppression effect faded for >0.20Al. Undercooling suppression did not correlate specifically with blade suppression since it became significant at 0.10Al and increased continuously with greater Al to 0.25Al. Surprisingly, an intermediate range of Al content (0.10 wt.% to 0.20 wt.% Al) promoted formation of significant populations of 2-μm to 5-μm faceted Cu-Al particles, identified as Cu33Al17, that clustered at the top of the solder joint matrix and exhibited extraordinary hardness. Clustering of Cu33Al17 was attributed to its buoyancy, from a lower density than Sn liquid, and its early position in the nucleation sequence within the solder matrix, permitting unrestricted migration to the top interface. Joint microstructures and implications for the full nucleation sequence for these SAC + Al solder joints are discussed, along with possible benefits from the clustered particles for improved thermal cycling resistance.

36 MATERIALS SCIENCE↗

Imaging and Analysis of Void-defects in Solder Joints Formed in Reduced Gravity using High-Resolution Computed Tomography

As a part of efforts to develop an electronics repair capability for long duration space missions, techniques and materials for soldering components on a circuit board in reduced gravity must be developed. This paper presents results from testing solder joint formation in low gravity on a NASA Reduced Gravity Research Aircraft. The results presented include joints formed using eutectic tin-lead solder and one of the following fluxes: (1) a no-clean flux core, (2) a rosin flux core, and (3) a solid solder wire with external liquid no-clean flux. The solder joints are analyzed with a computed tomography (CT) technique which imaged the interior of the entire solder joint. This replaced an earlier technique that required the solder joint to be destructively ground down revealing a single plane which was subsequently analyzed. The CT analysis technique is described and results presented with implications for future testing as well as implications for the overall electronics repair effort discussed.

Easton, John W.↗

Microstructural Evaluation and Comparison of Solder Samples Processed Aboard the International Space Station

Samples from the In-Space Soldering Investigation (ISSI), conducted aboard the International Space Station (ISS), are being examined for post-solidification microstructural development and porosity distribution. In this preliminary study, the internal structures of two ISSI processed samples are compared. In one case 10cm of rosin-core solder was wrapped around a coupon wire and melted by conduction, whereas, in the other a comparable length of solder was melted directly onto the hot wire; in both cases the molten solder formed ellipsoidal blobs, a shape that was maintained during subsequent solidification. In the former case, there is clear evidence of porosity throughout the sample, and an accumulation of larger pores near the hot end that implies thermocapillary induced migration and eventual coalescence of the flux vapor bubbles. In the second context, when solder was fed onto the wire. a part of the flux constituting the solder core is introduced into and remains within the liquid solder ball, becoming entombed upon solidification. In both cases the consequential porosity, particularly at a solder/contact interface, is very undesirable. In addition to compromising the desired electrical and thermal conductivity, it promotes mechanical failure.

Grugel, R. N.↗

Long-term reliability of hand-soldering M55365 Ta capacitors

This is a continuation of the report “Effects of Hand Soldering MIL-PRF-55365 Tantalum Capacitors,” which discusses the parametric effects of convection reflow soldering, JPL standard hand soldering, and optimized hand soldering on solid tantalum capacitors. The current focus is determining the long-term reliability effects of the various soldering techniques. Unfortunately, the 100-piece sample size chosen for the highly accelerated life tests was too small to reliably determine the effects of the different soldering techniques on the lifespan of the parts. In hindsight, this likely could have been predicted based on the large alphas and small betas of the Weibull failure distributions discovered during the scouting trials. Now that the effects of inadequate sample size are better understood, an opportunity exists to not only discover whether there are real differences in the reliability associated with the various soldering techniques, but also the potential to discover the voltage acceleration model and the temperature acceleration effect for these capacitors. It is recommended that the testing be repeated with a more appropriate sample size to capture this useful information.

Spence, Penelope↗